Why do copper and brass parts discolour?

Type
Application notes
Published
20 November 2026
Prepared by
Technical team
Product group
Metalworking Fluids (MWF)

Replacing the whole charge is a common response when copper and brass discolour, on the view that the fluid is simply old, but if the cause is an ingredient the fresh fluid carries too, such as active sulfur, the stains come back with a new charge of the same product. What actually discolours the parts can be spent copper inhibitor, active sulfur EP additive, high pH and amine, hydrogen sulfide from bacteria, or residue left on parts, and more than one can be at work.

Brass fittings that leave the automatic lathe a bright gold pick up red spots or brown stains after a few days in the box, and on some days they come off the machine already black. Copper contact parts lose their shine and go dull. Same fluid, same machine, yet the discolouration sometimes shows straight after machining and sometimes only in storage.

Copper and brass parts go into electrical contacts, plumbing fittings, valves and heat exchangers, where the surface decides both performance and appearance. A discoloured surface is easily rejected on appearance, and it can affect contact resistance, solderability and plating adhesion, which leads to recleaning and rework costs. Deeper changes such as dezincification can reduce strength as well.

In air and water, copper first forms a thin reddish-brown film of cuprous oxide, and where sulfur is present it forms brown to black copper sulfide (Graedel et al., 1983; Revie & Uhlig, 2008). Metalworking fluids therefore carry an inhibitor that adsorbs on copper and blocks these reactions, usually a triazole such as benzotriazole or tolyltriazole (Byers, 2017; Finšgar & Milošev, 2010; STLE, 2012). Discolouration means this protection has failed, so it is a part-quality problem and also a signal about the fluid's chemistry and microbial state.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: keep a discoloured part together with a fluid sample from the same time, and record the colour, whether red, brown, black or bluish, whether it appeared during machining or in storage, and the fluid's smell and pH.

Hypothesis 1: spent inhibitor

Consider this hypothesis after the share of copper-alloy work rises, some weeks after a fresh charge, and in systems where fine chips linger in the sump. On an automatic lathe that has cut nothing but brass for weeks during a rush of fitting orders, faces that started bright gold begin to turn an even, dull reddish brown. There is no smell, and pH is where it always is.

Triazole inhibitors bind directly to copper atoms on the surface and form a thin complex film. The film is usually described as a chain-like polymer of monovalent copper and triazole, and it stops copper from oxidising further and dissolving. The exact adsorption mechanism, however, is not yet fully settled (Finšgar & Milošev, 2010).

Building the film uses up inhibitor. A coolant study found that much of the tolyltriazole loss seen in the field had gone into a strongly bound protective layer on copper surfaces (Fritz et al., 2009). In machining, chips and freshly cut faces keep exposing new copper, so the same loss carries on without pause. Work on synthetic metalworking fluids likewise showed selective depletion, with chips adsorbing inhibitor components and pulling them out of the fluid (Eppert et al., 2003). Once the inhibitor falls below a working level, new surfaces meet air and water without a film and oxidise to a reddish brown (Revie & Uhlig, 2008).

Concentration and inhibitor have to be measured separately. Read concentration weekly on a refractometer against the maker's range; if it is right and parts still discolour, the inhibitor alone may have dropped (Eppert et al., 2003). In that case have the supplier or a laboratory measure triazole content in fresh and in-use fluid side by side. A clearly lower value in the in-use fluid supports this hypothesis.

When inhibitor turns out to be short and concentration is low, bring concentration into range first. If concentration is right but inhibitor alone has fallen, agree a copper inhibitor top-up with the supplier, or move to a fluid with more inhibitor to match the share of copper-alloy work. The longer chips sit in the sump, the faster the loss, so improve chip removal and filtration as well (Byers, 2017; Eppert et al., 2003).

Hypothesis 2: active sulfur

This hypothesis comes up right after a change to a neat oil, used undiluted, or to a heavy-duty fluid, when a steel-cutting fluid is used on brass, and where steel and brass take turns on one machine. Some days a machine cuts alloy-steel shafts in the morning and brass nuts in the afternoon. The afternoon job runs on the same heavy-duty fluid chosen for the steel, and nuts fresh off the machine show brown and purplish stains.

Extreme pressure additives, or EP additives, keep tool and workpiece from welding together under high load and heat. A sulfur EP additive reacts with the metal in the hot contact zone to form a thin sulfide film that eases sliding (Byers, 2017; STLE, 2019). The sulfur that reacts readily even at lower temperatures is called active sulfur (STLE, 2019).

The reaction does not stop at steel. Copper reacts readily with sulfur, so active sulfur forms copper sulfide on copper and brass too, leaving brown, purple or black stains (Revie & Uhlig, 2008; STLE, 2019). Sulfur EP additives are therefore known to be corrosive to copper alloys, and a fluid that also machines them needs a copper inhibitor or inactive sulfur (STLE, 2012; STLE, 2019).

When suspicion falls here, open the product documents first. Check the safety data sheet, the SDS, and the technical data for sulfur EP content and any statement on copper-alloy suitability. How much a fluid stains copper is shown by the copper strip corrosion test, ASTM D130, in which a polished copper strip is heated in the sample and compared with standard colours (ASTM International, 2019). The test is written for petroleum products, so for water-mix fluids use it only to compare fresh and in-use fluid under the same conditions. Stains that start right after a fluid change, with a normal smell, add weight to this hypothesis.

If copper alloys are a large share of the work, change the basis on which the fluid is chosen. Pick a fluid with inactive sulfur or sulfur-free EP additives, or one stated as suitable for copper alloys. If steel and brass must share a machine, compare the candidate fluids with the copper strip test before deciding (ASTM International, 2019). Copper sulfide stains already formed will not go away with a fluid change, so set a separate cleaning or rework method for them.

Hypothesis 3: high pH and amine

This tends to show in sumps run richer than recommended, just after a pH booster has been added, in systems where evaporation thickens the fluid, and on lines machining high-zinc brass. From the week after a pH booster goes in, red spots appear one by one on brass parts and a faint blue tint comes off on the filter paper. Rust on steel parts, meanwhile, has eased.

The starting point is the fluid's alkalinity. Water-mix coolant is kept on the alkaline side to stop steel rusting, and amines such as alkanolamines are widely used to hold the pH (Byers, 2017). Copper is fairly stable in clean water. But once dissolved oxygen turns copper into ions, ammonia or amines hold those ions as soluble complexes, clusters of a metal ion with molecules bound to it. No oxide film can then build up, and copper keeps dissolving (Revie & Uhlig, 2008). The surface dulls evenly or stains, and the dissolved copper can tint the fluid blue or green.

Brass, an alloy of copper and zinc, adds one more step. Under corrosive conditions zinc can dissolve first, which is called dezincification, leaving a porous copper layer that shows as red spots or a red film (Canadian Conservation Institute, n.d.; Sarver et al., 2010). The more zinc a brass contains, the more prone it is (Sarver et al., 2010). Ammonia environments have also long been known to cause stress corrosion cracking in brass that carries residual stress (Revie & Uhlig, 2008).

Set the pH meter reading beside the refractometer reading. Measure pH weekly against the maker's range; concentration above the range means more amine as well. For dissolved copper, have a laboratory measure copper in the fluid and follow the trend. A rising level means copper is going into solution. Red spots on brass together with a blue-tinted filter paper put this hypothesis in front.

What needs restoring is concentration and pH. Bring both back into range, and add no pH booster without the supplier's advice. On lines with a high share of copper-alloy work, choose a fluid whose amine package is proven on copper alloys and which carries enough copper inhibitor (Byers, 2017; Finšgar & Milošev, 2010). Parts with deep dezincification may have lost strength, so do not treat them as an appearance issue only.

Hypothesis 4: hydrogen sulfide

Sumps whose circulation stops over weekends or holidays, sumps with a thick bed of chips and sludge, and systems with corners where fluid sits still are where this hypothesis belongs. On the morning after a long holiday, the pump starts and a rotten-egg smell rises from the sump. Brass parts cut that morning come out unusually black, and the copper piping inside the machine has darkened too.

Hydrogen sulfide forms where the oxygen has been used up. Bacteria grow in water-mix coolant; once oxygen-using bacteria have multiplied and consumed the oxygen, sulfate-reducing bacteria grow in the sludge or in a sump that has stood still. They turn sulfate in the fluid into hydrogen sulfide, and the rotten-egg smell on a Monday morning after a weekend is the classic sign (NIOSH, 1998; Passman & Küenzi, 2020).

Hydrogen sulfide reacts with copper to form copper sulfide. In laboratory work, hydrogen sulfide in humid air formed a sulfide film on copper (Graedel et al., 1983), and the same reaction in the fluid turns copper and brass parts brown to black, along with copper parts inside the machine. Organic acids made by bacteria also lower the pH, which weakens the copper inhibitor film and makes staining easier (Passman & Küenzi, 2020).

Smell is only the first clue; the numbers come from microbial testing. A rotten-egg smell at the first start-up after a break, parts from that time especially black, and fluid that has gone grey or black put this hypothesis first. Record bacteria counts weekly with dipslides, test slides dipped in the fluid and incubated, or with laboratory tests. Tests for bacteria that live without oxygen take several days to give a result (Passman & Küenzi, 2020). A steady fall in pH means microbial activity is rising (Passman & Küenzi, 2020).

To cut bacteria, first take away their hiding places. Clear chips and sludge from the sump, and keep the fluid circulating or aerated during idle periods. With high counts, agree a biocide addition with the supplier; with a strong smell and blackened fluid, clean the system and recharge (NIOSH, 1998; Passman & Küenzi, 2020). Once the smell is under control, check the copper inhibitor level again.

Hypothesis 5: residue in storage

Turn to this hypothesis when parts that were clean straight after machining discolour after some days in storage. It shows on parts that wait a long time for the next step, in humid seasons, in stores where condensation forms, and where parts are stacked or handled bare-handed. Brass connectors boxed with fluid still on them and sent to the store turn up at outgoing inspection a few days later stained, first around holes and on faces that touched.

As the moisture dries, components gather on the surface. When fluid left on a part dries, only the water goes, and amines, salts and other components concentrate into a thin layer that holds moisture and sets up local corrosive conditions (Byers, 2017; Revie & Uhlig, 2008). In humid air copper first forms a cuprous oxide film, and sulfidation follows where sulfur compounds are in the air (Graedel et al., 1983; Revie & Uhlig, 2008).

In research on copper sulfidation in humid air, the thin water film on the surface governed the reaction, which slowed as higher temperature reduced the surface water (Graedel et al., 1983). Condensation in storage, packaging that gives off sulfur compounds and bare-hand handling can therefore make stains appear sooner when they come together.

Checking begins with a record of storage conditions. Note temperature, humidity, any condensation and the packaging in use, and see whether stains appear first in holes where fluid pooled, on stacked faces and where hands touched. Splitting one batch into washed and unwashed parts, stored side by side, and comparing when each discolours makes it clear whether residue is the cause.

Where parts wait long for the next step, wash them after machining, dry them quickly, apply a copper-alloy preservative if needed and pack them sealed. Keep storage free of condensation, cut down bare-hand handling, and check the packaging for sulfur compounds (Graedel et al., 1983).

Testing the hypotheses

The first thing to settle is when the discolouration appeared. If parts are already stained leaving the machine, look first at the causes in the fluid, hypotheses 1 to 4; if it appears in storage, start with residue, hypothesis 5. That one question narrows the field a good deal.

Next come smell and colour. A rotten-egg smell after a break puts bacteria and hydrogen sulfide, hypothesis 4, in front (Passman & Küenzi, 2020). Black and purple point to copper sulfide, so hypothesis 2 or 4; red spots on brass point to dezincification, hypothesis 3; and an even reddish brown points to oxidation, hypothesis 1 or 5 (Revie & Uhlig, 2008; Sarver et al., 2010).

Then measure concentration and pH. Both high points to hypothesis 3, a falling pH to hypothesis 4, and normal values narrow it to hypothesis 1 or 2. Look at recent changes at the same time: a fluid change, a heavy-duty fluid, an additive or a new work material. Straight after a move to a fluid with EP additives, suspect hypothesis 2.

If that still does not settle it, run a control test. Put fresh and in-use fluid through the same copper strip test: if fresh fluid stains copper too, the formulation is at fault, pointing to hypothesis 2; if only the in-use fluid does, spent inhibitor or bacteria are more likely, hypothesis 1 or 4 (ASTM International, 2019). If the cause is still open, have inhibitor content, dissolved copper and bacteria counts analysed as the final check.

The hypotheses often overlap. When bacteria grow, the pH falls, the inhibitor film weakens and hydrogen sulfide forms, so hypotheses 1 and 4 appear together (Passman & Küenzi, 2020); a rich-running fluid that also carries sulfur EP additives combines hypotheses 2 and 3. In such cases correct the fluid's condition, meaning bacteria, pH and concentration, first, and treat any staining that remains as a question of formulation. The job is done only when freshly cut parts stay bright over several batches after the fix and pH and concentration stay in range.

Limits and cautions

Concentration and pH ranges differ by product, so follow the maker's range. ASTM D130 is a method for petroleum products, so results for water-mix fluids are not read against its ratings directly but used only for comparison under the same conditions (ASTM International, 2019). Discolouration that affects part function, cracking and deep dezincification should not be judged on the floor; pass them to a materials analysis specialist.

Hydrogen sulfide is toxic, and at high levels or with constant exposure people stop smelling it. Do not rely on smell; check with a gas detector before working in an enclosed sump or tank (OSHA, n.d.). Mist and skin contact from contaminated metalworking fluid can cause respiratory and skin disease, so wear gloves and eye protection as the SDS directs when handling the fluid, and follow the SDS when handling biocides (NIOSH, 1998).

Sources

  1. ASTM International. (2019). ASTM D130-19, Standard test method for corrosiveness to copper from petroleum products by copper strip test. https://doi.org/10.1520/D0130-19
  2. Byers, J. P. (Ed.). (2017). Metalworking fluids (3rd ed.). CRC Press.
  3. Canadian Conservation Institute. (n.d.). Preventing and treating the dezincification of brass (CCI Notes 9/13). Government of Canada. https://www.canada.ca/en/conservation-institute/services/conservation-preservation-publications/canadian-conservation-institute-notes/dezincification-brass.html
  4. Eppert, DeVor, Kapoor, & Rajagopalan. (2003). The effect of chip adsorption on selective depletion from a multicomponent synthetic metalworking fluid. University of Illinois at Urbana-Champaign, IDEALS. https://www.ideals.illinois.edu/items/110202
  5. Finšgar, M., & Milošev, I. (2010). Inhibition of copper corrosion by 1,2,3-benzotriazole: A review. Corrosion Science, 52(9), 2737–2749. https://doi.org/10.1016/j.corsci.2010.05.002
  6. Fritz, P. O., Van de Ven, P., Pellet, R. J., Bartley, L. S., & Taylor, S. A. (2009). Copper-triazole interaction and coolant inhibitor depletion. ASTM International. https://doi.org/10.1520/STP38240S
  7. Graedel, T. E., Franey, J. P., & Kammlott, G. W. (1983). The corrosion of copper by atmospheric sulphurous gases. Corrosion Science, 23(11), 1141–1152. https://doi.org/10.1016/0010-938X(83)90043-4
  8. National Institute for Occupational Safety and Health [NIOSH]. (1998). Criteria for a recommended standard: Occupational exposure to metalworking fluids (DHHS [NIOSH] Publication No. 98-102). https://www.cdc.gov/niosh/docs/98-102/
  9. Occupational Safety and Health Administration [OSHA]. (n.d.). Hydrogen sulfide: Hazards. U.S. Department of Labor. https://www.osha.gov/hydrogen-sulfide/hazards
  10. Passman, F. J., & Küenzi, P. (2020). Microbiology in water-miscible metalworking fluids. Tribology Transactions, 63(6), 1147–1171. https://doi.org/10.1080/10402004.2020.1764684
  11. Revie, R. W., & Uhlig, H. H. (2008). Corrosion and corrosion control: An introduction to corrosion science and engineering (4th ed.). Wiley. https://doi.org/10.1002/9780470277270
  12. Sarver, E., Zhang, Y., & Edwards, M. (2010). Review of brass dezincification corrosion in potable water systems. Corrosion Reviews, 28(3–4), 155–196. https://doi.org/10.1515/CORRREV.2010.28.3-4.155
  13. Society of Tribologists and Lubrication Engineers [STLE]. (2012, September). Special additive report: Metal deactivators: Inhibitors of metal interactions with lubricants. Tribology & Lubrication Technology. https://www.stle.org/files/TLTArchives/2012/09_September/Tech_Beat.aspx
  14. Society of Tribologists and Lubrication Engineers [STLE]. (2019, April). Sulfurized additives: Types available, key applications and beneficial properties. Tribology & Lubrication Technology. https://www.stle.org/files/TLTArchives/2019/04_April/Forum.aspx

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.