KALTEC

Rail

From car body forming to rail friction management

The rail industry manufactures and operates rolling stock and infrastructure for passenger and freight transport.

Rail
  • 44%

    Maintenance share of rolling-stock lifetime cost

  • 4×+

    Life of a lubricated curve rail vs unlubricated

  • £355M

    Cost of low rail adhesion each autumn

What is the rail industry?

The rail industry builds rolling stock such as commuter trains and high-speed trains, and operates and maintains them on track over long periods. Trains must depart on schedule every day, and they carry many points where metal keeps touching metal, such as wheels and rails and current collectors, so wear, noise and friction management decide service quality. Steel sheet is formed into car bodies, running gear is assembled and handed over to operation, so forming and cutting lubrication, surface treatment and anticorrosion painting, axle and gearbox lubrication, and friction management at the wheel-rail interface are split between manufacturing and operation.

In rail, too little friction is a problem and so is too much. Insufficient lubrication wears wheel flanges and rails quickly, and lubricant applied to the gauge face that spreads to the rail head lengthens braking distance. Application amount and position, changes with season and humidity, and behavior within the maintenance interval decide results as much as the product's own performance. Rail is an industry where keeping the timetable comes first, so a new proposal only gets reviewed when it comes with a way to verify it without stopping service.

  1. 01

    Steel plate cutting and press forming

    Steel sheet is cut, pressed and drawn into car body parts. A broken oil film leaves scratches and cracks that show even after painting. Choose forming oil by lubricity, application amount and how well it washes off.

  2. 02

    Machining and welding

    Members are milled and turned, and structures welded. Drifting water-soluble fluid concentration worsens surface roughness first. Choose cutting fluid by machining performance and concentration stability in long use.

  3. 03

    Surface treatment and rust protective coating

    Welds and cut edges receive phosphate pretreatment and conversion coating, followed by anticorrosion paint. Poor pretreatment lets paint peel and wet corrosion appear. Choose pretreatment chemicals and paint by corrosion performance and intercoat adhesion.

  4. 04

    Assembly and inspection

    Parts are assembled and tested for performance and durability. Poorly lubricated fasteners do not turn torque into clamping force. Choose assembly grease and fixing agents by friction and rust protection in testing.

  5. 05

    Axle bearing and gearbox lubrication

    Axle bearings and reduction gearboxes are filled with grease and gear oil, and automatic lubrication systems managed. Heat buildup leads to hot boxes where bearings seize. Choose lubricants by temperature range, load and change intervals.

  6. 06

    Wheel flange and rail gauge face lubrication

    Lubricant is supplied by trackside or onboard systems where wheel flanges and the rail gauge face meet. Too little speeds flange wear on curves, while too much spreads lubricant to the rail head and lengthens braking distance. Choose lubricant by adhesion and carry distance.

  7. 07

    Top-of-rail friction management

    A friction modifier is applied where the rail head meets the wheel tread to hold the friction coefficient within a target range. Over-application loses traction and braking force, while no application lets fatigue cracking and corrugation progress. Choose a friction modifier by friction coefficient range and carry behavior.

  8. 08

    Pantograph and door mechanisms

    Current collector contact surfaces and moving parts of door mechanisms are lubricated. Dried-out lubrication throws off door operation, and poor collector contact causes local heating. Choose grease and contact protectants by lubrication performance and temperature range.

  9. 09

    Scheduled vehicle maintenance

    Lubricants are changed and parts are inspected or replaced at set intervals. If degradation outpaces the change interval, old lubricant stays in place and speeds wear. Choose lubricants by life over the maintenance interval and listing in the regulations.

  10. 10

    Long-term storage and transport protection

    Finished vehicles are protected until shipment, and export units are treated to withstand long periods on board. At sea, salt and temperature swings drive corrosion. Choose rust preventives and packaging by protection period and performance in salt environments.

Regulation and certification

  • ISO 22163

    The quality management standard for the rail sector, adding railway requirements to ISO 9001. Adhesives, paints and lubricants used in building vehicles and parts are often controlled through customer requirements and change management procedures.

  • EN 45545-2

    The European standard setting fire behaviour requirements for materials and components in railway vehicles. Sealants, adhesives and coatings inside vehicles must meet the flame, smoke and toxicity limits for their hazard level.

  • EN 17460

    The European standard for adhesive bonding of railway vehicles and components, succeeding DIN 6701. Companies that bond must be certified, and adhesive selection and process control follow its procedures.

  • Railway Safety Act type approval

    The Korean system requiring type approval from the transport ministry for rolling stock and railway products. Changing materials in an approved design may need change approval, so lubricants and adhesives are chosen within the approved specification.

FAQ

Flange wear is especially fast on curves. Is adding more lubricant enough?

Adding more often does not solve it. Lubricant supplied to the gauge face that spreads to the rail head brings longer braking distances, so it is better to look at application position and carry distance as well as amount.

The range that can be handled also depends on the application method. Trackside systems can supply only where needed, such as curve entries, but bring installation points and maintenance with them; onboard systems cover the whole trainset but carry more lubricant, which can contaminate the rail head. Whether only the high-wear sections can be targeted tends to decide the method.

Axle bearing temperatures are slowly rising. Should we change grease?

It could be the grease or the lubrication system. Degraded grease can fail to hold an oil film, and automatic lubricator output can drift so lubricant does not reach where it is needed.

Looking only at grease for the cause of rising temperature can leave a lubrication system problem in place to recur. A slight drift in automatic lubricator output leaves certain axles under-lubricated, and changing only the grease in that state often brings brief improvement. A hot box takes the trainset out of service once it occurs, so the cost of reversal is high.

Manufacturing line cutting fluid smells each summer. Will more biocide fix it?

It helps temporarily but often comes back. Spoilage is often not just a microbial issue but a condition created together by concentration, oil-water separation and sludge at the bottom of the tank.

Continually increasing biocide brings other burdens. Higher dosing makes handling and waste treatment conditions heavier, and once resistant microbes take hold, the same dose no longer controls them. Missing the tank cleaning interval to get through one summer tends to bring odor back earlier the following year.

Exported vehicles showed corrosion at the destination. Where should we start?

It is good to look at packaging damage and rust preventive choice together. Sea transport keeps salt and temperature swings in play, so a single breach in packaging can let oxidation spread from that point.

Corrosion found at the destination is hard to trace back, so whether records exist is the deciding point. Without photos of rust protection and packaging before shipment, it is hard to tell damage in transit from condition before dispatch, and discussions with the carrier over responsibility can drag on. These records are also the basis for revising packaging specifications for the next shipment.

Could friction modifiers lengthen braking distance? How should we judge?

Top of rail friction modifiers aim to hold friction within a target range rather than remove it, so they differ in nature from gauge face lubricants. Over-application, however, can lower both traction and braking force.

Setting a validation section and recording braking distance and rail surface condition before and after application builds evidence. Values change with season and humidity, so it is best not to conclude from a single point in time.

Can a lubricant listed in maintenance regulations be replaced with another?

Sections tied to running safety often combine parts technical standards with operator vendor registration. For materials listed as designated items in maintenance regulations, there may be no place for a substitute unless the regulations are revised.

For materials named in the regulations, the regulation revision cycle often sets the adoption schedule; for materials specified only by standard or grade, review proceeds within those conditions. Either way, a history built under service conditions is required, so entries led by performance data alone sometimes stall on the track record item.

Grease on door mechanisms gets stiff in winter. Is that normal?

Viscosity rising at low temperature is natural, but if it throws off operation, the operating temperature range may not match site conditions. Doors cycle many times, so even small increases in resistance can accumulate and show in operating time.

Door lubrication is tied to intervals by maintenance level, so it is hard to lubricate more only in winter. That is why lines with large seasonal swings often choose one product with margin on the low-temperature side to cover all four seasons. Adding more grease to cover winter stiffness can pick up more debris in summer and cause the opposite problem.

Gear oil seems to degrade before the maintenance interval. How can we check?

The set interval and the actual degradation rate sometimes diverge. In trainsets with heavy duty or high heat, oil can wear out first at the same interval, so it is better to check condition rather than rely on the interval alone.

Keeping a small sample of used oil at each change and checking viscosity, acid number and wear metals builds evidence. Looking at the trend over several change intervals shows whether to shorten the interval or change the oil type.