Nuclear & Thermal Power
From heavy forgings to water treatment in the loop
Nuclear, thermal and combined-cycle power build power plants and run them for a long time while managing the water and equipment in each loop. The equipment runs at high temperature and pressure, and an unplanned shutdown is costly.

- $4.2B
Yearly direct corrosion cost of US nuclear power
- Up to 54%
US coal-plant forced outages caused by boilers
- 70%
HRSG tube failures influenced by cycle chemistry
What is the nuclear industry?
The nuclear industry makes large components such as reactor vessels and steam generators, builds power plants, and after completion manages system water and equipment through long operation. Safety-related parts must withstand high temperature, pressure and radiation for decades of operation, so material history and defect control follow them from start to finish. The flow runs from large ingot forging, precision machining and stainless cladding to system water quality management, so forging release, cutting lubrication, low-residue cleaning, inspection aids, corrosion inhibition and water treatment span both manufacturing and operation.
The first question in choosing chemicals for nuclear is what remains. Chlorine and sulfur left in the system come back over time as cracking and pitting, and heavy metals become activation products that raise system radiation levels. So along with performance, ingredient limits and residue behavior, waste treatment routes and lot-level history must be documented. Nuclear is an industry that moves by written procedure, so even changing one product requires collaboration that prepares documents and validation together.

- 01
Material forging and primary machining
Large ingots for reactor vessels and steam generators are pressed and forged at high temperature into initial shapes. Release agent left on surfaces leads to defects. Choose products by lubrication and cooling, high-temperature residue and lot history.
- 02
Precision machining
Forged and formed parts are cut, ground and lapped to drawing specifications. Chlorine and sulfur from machining fluids still show in residue tests after cleaning. Choose machining fluids by cutting performance, halogen and sulfur content and batch test certificates.
- 03
Welding and cladding
Piping and vessel joints are welded, stainless overlay is applied and stress relief heat treatment follows. Beads oxidize where back purge gas is interrupted. Choose auxiliary chemicals by spatter and oxidation prevention and welding code compliance.
- 04
Non-destructive testing such as penetrant testing
Defects on welds and key part surfaces are checked by penetrant and ultrasonic testing. Leftover inspection fluid itself becomes a contamination source. Choose inspection chemicals by defect sensitivity, chlorine and sulfur limits and procedure listing.
- 05
Hydrostatic testing
Piping and vessels are filled with water and pressurized to confirm pressure integrity. Chloride ions in test water trapped in pipe crevices or weld roots start pitting and crevice corrosion. Choose chemicals by corrosion inhibition, pH holding and test water quality.
- 06
Final part cleaning and drying
Cutting fluid and metal fines are removed from finished parts, which are dried under humidity control. Parts that oxidize during drying come back at final verification. Choose cleaners and rust preventives by cleaning power, ionic residue and flash rust control.
- 07
Rust protection and packing for long-term storage
Parts are given rust protection and packed to withstand inventory storage until they enter the plant site. Rust that starts where packaging tears returns as claims at delivery. Choose rust preventives by protection period, residue limits and lot traceability.
- 08
Cleaning before delivery to site
Contamination, rust and soil that entered piping in transit are removed just before entry. Leftover foreign matter contaminates the coolant directly. Choose a cleaner by cleaning power, halogen and heavy metal limits and fit with radiation controlled area entry procedures.
- 09
Pre-operational chemical cleaning by system flushing
Weld scale and metal oxides inside installed piping and equipment are removed by system flushing. Poor neutralization corrodes piping. Choose a cleaner by dissolving power, material compatibility and waste treatment route.
- 10
Primary reactor coolant system water chemistry
Boric acid concentration, pH and dissolved hydrogen in reactor coolant are adjusted to manage reactivity and corrosion together. A drifting boron-lithium balance puts system pH out of the target range. Choose chemicals by purity, impurity limits and content that can be activated.
- 11
Secondary steam generator system water chemistry
Corrosion in steam generators and feedwater and condensate piping is suppressed and ions and corrosion products are removed. Oxygen and chlorine from condenser leaks concentrate in tube crevices and start stress corrosion cracking. Choose chemicals by corrosion inhibition, material compatibility and decomposition products.
What is thermal and combined cycle power generation?
Thermal and combined cycle power generation produces electricity by driving turbines with high-temperature, high-pressure steam and combustion gas from burning fuel. Plants must keep planned operating schedules, and unplanned outages are costly, so the condition of water and oil circulating through the systems must be held constantly. Water circulates through boilers, piping, condensers and cooling towers while oil circulates to turbine bearings, so water purification, deaeration, pH adjustment, scale and microbial control and turbine lubrication run along the systems.
The condition of feedwater and cooling water shows only as numbers on instruments, so nothing looks wrong on the outside even while pipe walls thin. Oxygen and trace impurities left in feedwater attack metal, and in cooling systems, scale and biofilm gradually reduce heat exchange performance. Whether a program fits system materials and operating pressure, and whether it can be used within discharge standards, weigh as heavily as the chemical's own performance. In thermal and combined cycle generation, data read from system condition is the basis for any program, so cooperation starts with looking at water and oil quality together.

- 01
Makeup water pretreatment by UF, RO and ion exchange
Industrial water is purified by filtration and reverse osmosis, then brought to ultrapure levels by ion exchange or electrodeionization. High hardness and silica foul RO membranes. Choose pretreatment chemicals by removal performance, raw water quality and membrane compatibility.
- 02
Condensate purity control and recirculation
Condensate from the condenser is monitored for purity and dosed before returning as makeup. Small condenser tube leaks let chlorides and sulfates in. Choose chemicals by corrosion inhibition, monitoring interference and material fit.
- 03
Boiler feedwater deaeration
Dissolved oxygen left in feedwater is removed to prevent oxidation and corrosion in the system. Overdosing scavenger can dissolve the magnetite film. Choose oxygen scavengers by removal speed and whether copper alloys are present.
- 04
Feedwater pH control and flow-accelerated corrosion suppression
Feedwater pH in the economizer and low-pressure evaporator is held within the control range to suppress iron and copper dissolution. Below range, piping thins first at high-velocity bends and ruptures. Choose pH control chemicals by pH holding power and system materials.
- 05
Boiler evaporator water phosphate treatment
Phosphate is added to boiler water in intermediate and high-pressure evaporator circuits to keep alkalinity. Chlorides concentrating under iron oxide start localized corrosion. Choose boiler treatment chemicals by the concentration range set by operating pressure before alkalinity holding power.
- 06
Turbine lubrication in operation
Lubricating oil is circulated to turbine bearings and governor systems. With frequent starts and stops, oxidation products harden into varnish on servo valves. Choose turbine oil by viscosity and oxidation stability.
- 07
Condenser cooling water treatment
Turbine exhaust steam is condensed with seawater or cooling tower water while scale, corrosion and microbial fouling are controlled. Shellfish and algae at tube inlets lower condensing performance. Choose chemicals by scale control and the tube and tubesheet material combination.
- 08
Cooling tower cycles of concentration and blowdown treatment
Cooling tower cycles of concentration are managed and blowdown is discharged or reused. Raising cycles raises silica and calcium, making chemical control harder. Choose chemicals by treatment performance and scale onset.
Regulation and certification
10 CFR 50 Appendix B
The 18 quality assurance criteria the US Nuclear Regulatory Commission requires of nuclear power plants. Lubricants and sealants for safety-related equipment must be bought and traced under these criteria.
KEPIC
The Korea Electric Power Industry Code covering design, manufacture, testing and inspection of power plant equipment. Materials and consumables for nuclear plant equipment must meet both KEPIC and the plant's purchase specification.
ISO 8068
The international specification for lubricating oils for steam and gas turbines. Turbine oils are selected after checking that oxidation stability, rust protection and air release meet the grade in this standard.
Water Environment Conservation Act
The Korean law that controls water pollutants in wastewater discharged to public waters. Chemicals for equipment cleaning and cooling water treatment are chosen with the wastewater treatment load and discharge limits in mind.
FAQ
Can't general industrial cleaners be used on nuclear parts as they are?
They often run into ingredient limits. Materials that touch coolant have upper limits on chlorine, fluorine and sulfur, and general industrial formulations commonly use these for cleaning power or rust protection.
Safety data sheets often state content only as a range, which is not enough to confirm limits. So in nuclear, the usual method is to obtain chlorine, fluorine and sulfur content on batch test certificates and keep them as records, and if values vary by lot even under the same product name, procedure requirements become hard to meet.
Chlorine was detected in a residue test. Will more cleaning solve it?
More cleaning cycles sometimes lower it, but without finding the entry path it tends to repeat. Chlorine can come in from several places: machining fluid, cleaner, rinse water and packaging.
Chlorine often reattaches somewhere rather than being cleaned away, so narrowing the path gets results faster. Rinse water quality, batch content of machining fluid and packaging composition are the three common culprits, and if any one of them varies by lot, test results vary too even with more cleaning.
Pipes rust inside after hydrostatic tests. Should we add inhibitor to test water?
Inhibitor can delay it, but if draining and drying are the cause, it tends to come back. Where water remains at low points or blocked spots, inhibitor concentration drops and rust starts there.
Marking where rust appeared shows where to act. If it gathers at low points and the ends of drain paths, draining and drying procedures are the issue; if it appears evenly, test water quality and residence time are likely. Shortening residence time is sometimes less work than raising inhibitor.
Are chemical management standards different for Q-class and general items?
In practice they are often run differently. Q-class involves suppliers registered in the quality assurance program and procedure records, so the document system sometimes becomes an issue before product performance.
If both classes are handled on the same line, physically separating materials is safer for traceability. With Q-class, any record of operating differently from procedure puts the whole lot in question, so sites that separated storage locations and issue records from the start had less to trace back later.
How are chemicals for radiation controlled areas different from general sites?
A separate procedure registers the list, composition and recovery plan before entry. Chemicals left over after use in the area and even wipes are subject to recovery, so ways to reduce usage are often reviewed first.
Container size and whether the product can be portioned also weigh heavily in the procedure. Products available only in large drums make leftover contents and containers subject to recovery, raising the burden, so with similar performance, products available in small packs are easier. If a product not on the entry list must be brought in urgently, registration starts over.
Parts in long-term storage show pitting. Should we change rust preventives?
Changing products sometimes helps, but if the storage environment is the cause, it tends to repeat. When warehouse humidity rises and falls, condensation forms inside packaging and pitting remains where the water dries.
When changing rust preventives, upper limits on residual ingredients and lot traceability data come into play along with protection period. Nuclear parts often cannot have a separate removal step added after opening, so the choice narrows to residue-free types, and without a system for receiving and keeping lot test certificates, adoption can be delayed even when performance fits.
We changed turbine oil recently, but servo valves keep sticking. Is it the oil?
Varnish is a likely cause. In units that start and stop often, oxidation products can bake into narrow gaps in control systems, and in that case components left in the system often keep acting even when the oil is new.
What makes varnish difficult is that it does not leave with an oil change. Components stuck to system walls and narrow gaps can redissolve into new oil and build up in the same places, so many set the system cleaning method and outage period in advance along with the oil change. Disassembling and cleaning only the servo valves while leaving the system as is tends to just widen the interval before recurrence.
Feedwater iron is creeping up. Where should we look first?
It is best to start by checking for sections where pH has dropped below the control range. Rising iron is often read as a sign that protective oxide on pipe surfaces is dissolving now, and it tends to appear first at high-velocity bends and low-pressure evaporator inlets.
Splitting values by sampling point narrows the range. If values are high only in one section, look at that section's material and velocity; if the whole system has risen, suspect pH control first. Wall thinning cannot be reversed once it occurs, so it is safer to treat the rising trend itself as the signal.
If corrosion persists despite oxygen scavenger, should we raise the dose?
Increasing is not always the answer. Overdosing makes conditions too reducing, which can dissolve the magnetite film and accelerate flow-accelerated corrosion.
The direction depends on whether the system contains copper alloys and whether cation conductivity stays low. If conditions fit, oxygenated treatment, which reduces scavenger and adds a trace of oxygen, can be the better fit, so it is good to sort out system configuration before adjusting dose. In systems where dosing has been raised for a long time, oxide condition has already changed, and some take a stepwise path when reducing.
In seawater cooling, only the tubesheets degrade fast. Can chemicals fix it?
Chemicals alone often cannot fix it all. In combinations with a large potential difference, such as titanium tubes and carbon steel tubesheets, galvanic corrosion is also at work, so changing only the corrosion inhibitor tends to just slow the rate.
On the tubesheet side, conditions from the material combination often come before chemicals. In combinations with a large potential difference, stronger corrosion inhibitors only slow progress, and raising residual chlorine to control microbes can also increase tubesheet corrosion. That is why the usual order is to sort out the tube and tubesheet material combination first and then set the chemical specification.
What is involved in switching our boiler treatment chemical to another product?
In most cases chemicals must pass both the power company's vendor registration and plant-specific specification listing before dosing. Even within one company, system materials and operating pressure differ by unit, so specifications are often not unified.
Even within the same company, each unit has its own specification, so a chemical approved on one unit may have to go through the process again on the unit next door. If the specification names the chemical, the process starts with listing; if it specifies only composition or grade, review tends to proceed within that range. Which unit hosts the trial dosing volume largely decides the schedule.
Water seems to have gotten into the turbine oil. Can we keep using it?
It depends on the degree of emulsification. If water separates and settles at the bottom, it is often handled by draining and filtration, but if emulsification has progressed and the oil stays cloudy, the film breaks down and bearings can be affected.
Where the water came from matters too. Steam ingress and oil cooler leaks differ in amount and rate, so the fix differs: for the former, seals and vent systems; for the latter, cooling water differential pressure. If emulsification repeats, rust and antifoam additives are consumed first even after water is removed, and the same oil may not hold up as before.