Precision Machining
From casting and forging to export rust prevention
Precision machining casts or forges metal into shape, then cuts and grinds it into machines and parts. These machines and parts become other industries' production equipment and must withstand heavy loads and repeated stress.

- 7-17%
Cutting fluid share of manufacturing cost
- €850M
Yearly cost of fixing gear distortion in Germany
- 70%
Hot-forging dies withdrawn for wear or plastic deformation
What is the general machinery and precision machining industry?
General machinery and precision machining makes machines and parts that become production equipment for other industries, such as machine tools, molds and hydraulic components. The precision of the molds and parts made here sets the upper limit of quality for the next industry, so fine dimensional errors and surface condition must be held continuously. Aluminum, stainless steel, tool steel and general steel are machined, heat treated and ground, so lubrication and cleaning suited to cutting, EDM, tapping and grinding, and rust protection after machining, each apply separately by process.
What makes this industry demanding is that materials, shapes and machines differ from site to site. The same cutting fluid gives different results when machine and material change, and finished parts face rust risk again while waiting for the next process. So beyond machining performance, the equipment and material the product will meet and the wait until the next process must be considered together. Here, how a product behaves on that site's machines decides adoption more than the specifications in a catalog.

- 01
Mold design and machining
Molds are milled and finished by EDM based on product design. When fine chips and sludge build up in cutting fluid and dielectric, they are drawn back onto the machined surface as defects. Choose machining fluids by cutting performance, EDM stability and sludge settling.
- 02
Rough turning, milling, drilling and boring
Aluminum, stainless steel and steel are turned, milled and drilled to remove large amounts of material close to the target shape. With stainless steel, cutting heat concentrates at the edge, and with aluminum, built-up edge sticks. Choose a cutting fluid by cooling-lubrication balance and chip evacuation.
- 03
Quenching heat treatment
Parts are heated and quenched to reach the required hardness. A vapor blanket breaking unevenly leaves hardness variation and distortion. Choose quench oil by cooling capacity, part shape and agitation.
- 04
Finish turning, milling and reaming
Turning, milling and reaming bring parts to target dimensions and surface finish while correcting distortion from heat treatment. Distortion beyond the finishing allowance cannot be cut into tolerance. Choose a cutting fluid by lubricity, surface finish stability and fluid life.
- 05
Threading and tapping
Threads are made at fastening points with taps and cutting tools. A broken oil film in narrow holes snaps taps or tears threads. Choose tapping oil by extreme-pressure performance, material fit and chip clearing.
- 06
Grinding
Grinding wheels finish parts to ultra-precise size and finish. Heat at the grinding point leaves thermal damage, and clogged grains cause burning. Choose grinding fluid by cooling, cleaning and wheel-material match.
- 07
In-process ultrasonic cleaning
Chips and lubricant particles left from cutting are removed by ultrasonic cleaning. When the cleaning solution is saturated with oil, fine chips settle back onto the surface. Choose a cleaner by cleaning power and flash rust in the drying stage.
- 08
Post-machining corrosion protection
Machined surfaces are rust-protected for storage. Humidity swings cause condensation, and even pinpoint rust means rework. Choose rust preventives by duration and alloy reactivity.
- 09
Final assembly and shipping
Parts are assembled, packed and shipped by sea, land and air. Repeated condensation in containers can leave rust found on arrival. Choose packaging by rust protection and protection period.
What is the casting and forging industry?
Casting and forging makes the parts that form the backbone of machines and equipment, either by melting metal into shape or by pressing heated stock into form. These parts go where they bear heavy loads and repeated stress, so internal structure and surface defects must both be controlled. Cast iron, cast steel and aluminum alloys are handled at high temperatures, so die release, high-temperature lubrication, anti-seize, shakeout and cleaning, quenching and rust protection are needed again at every point where temperature rises and falls.
The difficulty in casting and forging is that heating and cooling sections follow each other directly. Uneven lubrication on die surfaces leaves shapes unfilled or causes soldering, and unstable quenching conditions split hardness and residual stress even within the same part. So beyond chemical performance, fit with die specifications, behavior at high temperature, treatment routes for used oil and wastewater, and records of usage must all be handled. In casting and forging, the same chemistry gives different results depending on die and furnace conditions, so data sheets alone cannot settle a decision unless conditions are set together from the first application.

- 01
Melting for casting
Metal scrap and raw materials are melted in furnaces into liquid metal. Dissolved hydrogen freezes as porosity during solidification. Choose ladle coatings and process chemicals by heat resistance and degassing effect.
- 02
Die preparation and release agent application for casting
Release agent is sprayed on mold and die casting die surfaces to ensure release and set die temperature. Mismatched die temperature and application amount cause gas defects. Choose release agent by release, dilution ratio and die temperature range.
- 03
Pouring and injection for casting and die casting
Molten metal is pushed into molds or die casting dies to fill the shape. Where the sleeve film breaks, plunger tips wear and fill defects increase. Choose plunger lubricant by film life at high temperature and residue buildup.
- 04
Ejection and anti-soldering for casting and die casting
Solidified parts are pushed out of the die and metal is kept from soldering onto the die. When ejector pin lubrication breaks, wear and seizure progress quickly. Choose anti-solder agents by heat resistance, ease of application and residue.
- 05
Sand removal and surface cleaning of castings
Mold sand is shaken off after solidification, and oxide scale and sand residue on the surface removed. Leftover residue causes trouble again in heat treatment and machining. Choose cleaners and pickling chemicals by removal power and material reactivity.
- 06
Billet heating and scale control for forging
Ingots are heated in high-temperature furnaces to a forgeable state. The longer they stay, the thicker the oxide layer and the more tool wear. Choose anti-scale coatings by oxidation suppression and ease of stripping.
- 07
Forging and forming
Heated stock is pressed by presses, hammers and ring rolling into the target shape. Where the film breaks, stock sticks to the die and hot wear starts. Choose forging lubricant by release and residue.
- 08
Cooling and solidification
Forged parts are cooled in air or under controlled cooling to stabilize structure. Uneven cooling rates by area leave hardness variation and warping. Choose cooling fluids by cooling rate curves and oxidation stability.
- 09
Machining, finishing and trimming
Surface scale is removed from forged and cast parts, dimensions brought in and burrs and gates cut off. Unstable fluid management lets chips linger and roughens surfaces. Choose cutting fluid by lubrication and cooling balance and fluid life.
- 10
Hardening and quenching heat treatment
Parts are reheated, quenched and tempered to final strength and hardness. If quench oil cannot follow thickness differences, hardness splits by area. Choose quench oil by cooling performance and thermal stability.
- 11
Final inspection, rust protection and packing
Inspected parts are rust-protected and packed for transport and storage. On long routes, condensation brings up white rust and pitting. Choose rust preventive oil and VCI materials by protection period and application method.
Regulation and certification
IATF 16949
The quality management standard for the automotive supply chain. Plants casting and forging automotive parts need customer approval and change control even when switching release agents, quenchants or rust preventives.
ISO 9950
The test method for measuring the cooling characteristics of industrial quenching oils with a nickel-alloy probe. Quenching oils for heat-treating forgings are checked by their cooling curve and tracked for change in service.
Occupational Safety and Health Act
The Korean law governing chemical handling and exposure at work, including the preparation and supply of safety data sheets. Cutting fluids and cleaners need proper safety data sheets and should be chosen to reduce mist and skin exposure.
K-REACH
The Korean act placing registration and notification duties on those who manufacture or import chemicals. Substances in imported lubricants and processing oils must be confirmed as registered so supply is not interrupted.
FAQ
Can one cutting fluid serve aluminum and stainless alternated on one machine?
Many sites use one, but it is best to decide first which material's conditions to favor. Stainless often needs heat removal most, and aluminum needs lubrication that suppresses built-up edge, so one fluid covering both can fall short on one side.
Alternating materials on one machine also adds to fluid management. Fine chips from aluminum machining float rather than settle and wear out the fluid faster, and setting concentration for stainless can discolor aluminum surfaces. So unless volume leans heavily to one side, addressing filtration and concentration control first is often more practical than splitting fluid types.
Once cutting fluid starts to smell, must it be replaced?
Sometimes it must, but often management brings it back. Odor is usually a sign of microbial growth, commonly against a background of diluted concentration, circulation stopped over the weekend, or tramp oil mixed in.
Measuring concentration and pH first speeds the decision. If they have fallen below the control range, topping up can restore the fluid; if it has already turned brown and the odor returns even after filtering, a full change and tank cleaning is the better route. Biocides used without addressing the cause tend to have a short effect.
Ground areas show what look like burn marks. What causes them?
Often heat could not escape at the grinding point. When chips clog the spaces between grains, the wheel rubs instead of cutting, and the resulting heat remains as discoloration or burn marks on the surface.
Burn marks sometimes do not end there. A surface that grinding heat has passed through changes in structure and residual stress, so plating or paint can adhere poorly in that area, or it can become a crack initiation point in service. Simply removing visible discoloration can let the problem reappear in later processes, so it is safer to adjust dressing intervals and grinding fluid supply conditions together.
Machined parts get pinpoint rust in days. Will a thicker coat of rust preventive do?
A thicker coat can delay it, but if the cause remains on the surface, it tends to return. Where cutting fluid was not fully washed off or bare-hand marks remain, corrosion can progress underneath even with a protective film on top.
A thicker film can also shift the burden to the next process. More must be removed before assembly or painting, lengthening degreasing, and narrow holes and thread interiors may be left less clean. For parts held only a few days, a thin film combined with packaging conditions is usually easier to manage.
How do we check whether our cleaner falls under VOC regulations?
It depends on both the ingredients and the site's emission conditions, so the product name alone is not enough. The usual order is to check ingredients, flash point and vapor pressure in the safety data sheet first, then determine whether the site counts as an emission facility under the Clean Air Conservation Act.
Whether switching to a low-volatility product or installing emission reduction equipment is more practical depends on cleaning volume and equipment setup. Low-volatility products tend to dry more slowly, though, so on lines that pass parts straight to the next process after cleaning, the drying stage or flash rust protection may need adjusting as well.
We want to try a different cutting fluid. What can we measure on site to decide?
There are fewer items to measure on site than one might expect. Comparing three things, tool life, surface finish and fluid life, on the same workpiece under the same conditions settles most decisions.
Recording baseline values for about two weeks before switching makes comparison easier. Also checking compatibility data for existing piping and seal materials and for later processes such as rust protection and painting reduces the chance of reverting after adoption.
We keep getting soldering in die casting. Will a different release agent fix it?
Release agent sometimes helps, but die temperature is often involved. If the die is too hot, release agent evaporates before forming a film, so soldering can repeat in the same place even with more applied.
Changing release agents also means resetting dilution ratio, spray time and blow-off conditions. On the other hand, applying strong cooling to lower die temperature can increase misruns, so moving both conditions at once leaves no record of what worked. Recording where soldering concentrates and the die temperature at the time, by part number, gives values for the next adjustment.
More release agent aids release but adds porosity. Which should we prioritize?
As application increases, moisture and decomposition gas left on the die also increase, so there is a range where porosity and release move in opposite directions. Meeting both with application amount alone is often difficult.
Reducing application to control porosity often brings soldering back, and going back and forth between the two defects with one variable is the trap in this section. In some cases porosity dropped at the same application amount when drying time after spraying was extended slightly, and then adjusting spray equipment and blow-off conditions before the release agent gives better returns.
Forging die life is shorter than expected. Is it the lubricant?
Lubrication can be the cause, but die preheat and cooling conditions are often intertwined. When hot stock touches an under-preheated die, heat checking forms on the surface first, and wear can speed up along those marks.
Looking closely at marks on the die surface tells them apart. Web-like cracking first points to preheat and cooling conditions; scoring in one direction with stuck metal points to a broken lubricant film. Dies where both have progressed rarely recover life with a lubricant change alone.
Parts warp after quenching. Will changing quench oil help?
Some distortion comes from mismatched cooling characteristics, but loading method and flow conditions are often the source. When parts overlap or flow concentrates on one side, cooling rates can split even within the same part.
Slowing cooling to reduce distortion can drop hardness below standard, so matching both with one cooling rate is hard. Adjusting the loading fixture sometimes costs less than changing oil type, and if the warping direction changes from lot to lot, oil temperature, agitation and oil degradation are likely drifting first.
For parts going to defense or nuclear, do we need records even for lubricants?
For volume that requires material traceability, the chemicals used are sometimes included in traceability. For nuclear safety-class parts, materials are designated in quality assurance procedures, so changing a product often means revising the procedure.
In that case, the time needed to revise the procedure decides the adoption point more than product performance. If revision is tied to the regular audit cycle, the change may have to wait a year, so some sites start substitute reviews from the procedural schedule rather than a performance comparison. Collecting lot certificates and composition change history in advance saves time at the revision stage.
Exports show white rust on opening. Will a thicker coat of rust preventive oil do?
A thicker coat can delay it, but if condensation inside the container is the cause, the effect usually does not last. On routes with large day-night temperature swings, water can form and dry inside packaging repeatedly.
A thicker coat increases cleaning burden before assembly, and uneven thickness can trap moisture. When combining with VCI materials, check that the two products do not interfere with each other, and water marks left inside packaging are a signal pointing to sealing and drying before packing rather than coating thickness.