Why does automated adhesive dispensing vary in volume?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Adhesives

Resetting pressure or time is the usual response when dispensed volume drifts, but if the condition behind the drift is still there, the new setting soon drifts as well. What actually lies behind it can be viscosity change with temperature, air bubbles in the material, settled filler, adhesive cured in the nozzle or the limits of time-pressure dispensing, and sometimes two or more at once.

Background

An automated dispenser runs the same program over the same spots, yet some beads come out thick and others thin, dots vary in size and now and then one is missing altogether. Where too much comes out, adhesive spills past the part and has to be wiped off; where too little comes out, the bonded area falls short and strength and sealing suffer. A part short of adhesive can easily look fine, so the fault may surface only after it has passed inspection and shipped, as a part that comes loose or leaks.

Dispensers fall into two broad groups: time-pressure dispensing, which pushes adhesive out by feeding compressed air into the syringe for a set time, and positive-displacement dispensing, where a piston or screw mechanically pushes out a set volume (Chen, 2009). The widely used time-pressure method fixes only air pressure and time, so the amount that actually comes out depends on how readily the adhesive flows under that pressure. Its performance therefore depends heavily on how the material flows, and control gets harder when that behaviour changes over time (Chen et al., 2003).

In the end output drifts in one of two ways: the material flows differently under the same force, or the force actually acting on it changes from shot to shot. Temperature, bubbles and filler in the material, the state of the nozzle tip and the dispensing method each lead into one of these, so when the drift began and what shape it takes narrow the cause sharply.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: weigh several shots to put the size and direction of the drift into numbers, note the material temperature, the amount left in the syringe, the supply pressure, the lot number and the time the pack was opened, and compare them with the adhesive's technical data sheet, the TDS, and the equipment settings.

Hypothesis 1: temperature swings

If output moves with the time of day or the season, start with temperature. That applies when adhesive stored refrigerated or frozen is loaded without enough time at room temperature, when an oven, motor or other heat source sits beside the machine, when air from heating or cooling blows straight onto the syringe, and when the plant's temperature swings widely between night and day. Consider a line that starts production on a Monday morning with a syringe loaded straight from the refrigerator. For the first hour the dots come out smaller than the standard, and by afternoon, with the settings untouched, they come out larger and spread to the edge of the part.

Cold material dispenses less because of viscosity. A liquid's viscosity falls as temperature rises, a relation commonly described with the Arrhenius equation (Mezger, 2020). On a dispenser with fixed pressure and time, lower viscosity means more flows out under the same pressure, and higher viscosity means less. In two-part products, mixed from two components to cure, temperature does one more thing. In tests that followed the viscosity of a mixed room-temperature-curing epoxy paste throughout cure, viscosity shot up from a certain point, and that point came much earlier at 64 °C than at 23 °C (Lapique & Redford, 2002). Warming thins the material at first, so more comes out, but it also shortens pot life, the time the mixed material stays usable.

Measuring the material temperature directly is quickest. Take the surface temperature of the syringe or cartridge with a contact thermometer, and log when it left the refrigerator and when it went on the machine. Dispense a set number of dots onto a coupon on a precision balance with the same settings, and repeat in the morning, at midday and in the afternoon; whether the weight tracks the temperature then shows at a glance. If the TDS gives viscosity at several temperatures or a working temperature range, compare against that as well.

Once temperature is shown to be the cause, holding the material temperature steady lasts longer than adjusting the settings again and again. Give refrigerated material the thaw time the TDS specifies, fit a temperature controller to the syringe or nozzle to keep it at a fixed temperature, and move heat sources and draughts away from the machine. When material is warmed, pot life shortens, so also set how long warmed material may stay on the machine. Where temperature is hard to hold, set a rule to weigh shots several times a day and reset pressure or time.

Hypothesis 2: trapped air bubbles

Bubbles show up as a dot that goes missing now and then, or as adhesive that keeps oozing from the needle after the shot ends and spits out as if bursting. Look at this hypothesis when material from a large container was transferred into syringes, when a two-part product was mixed by hand, when air was left between material and piston as the piston went in, and when material is used without degassing. The scene comes just after a fresh syringe goes on mid-shift. The first few dots are normal, then one comes out empty, and on the next the adhesive spits with a small pop and lands around the spot. After that the dots run evenly again.

Air compresses far more readily than adhesive. When pressure comes on, the bubble shrinks first and takes up the force, so less leaves the needle at that moment; when pressure is cut, the compressed bubble expands again and pushes out extra adhesive, which beads at the tip or spits. As a bubble passes through the needle, its volume is simply missing and the dot comes out small or not at all. A study that modelled time-pressure flow showed that, because air is compressible, the time behaviour of the dispensed flow is sensitive to the air volume in the syringe (Chen, 2002). Positive-displacement dispensing, which pushes with a piston, is no exception: analysis showed that when very small amounts are dispensed, the compressibility of the material has a large effect on the volume dispensed (Chen & Kai, 2004). A bubble mixed into the material adds exactly this kind of compressibility.

Begin by noting when the missing and spitting dots occur. If they cluster just after a syringe change or after material was transferred, the evidence leans towards bubbles. Hold a clear or translucent syringe up to the light to look for bubbles in the material and gaps beneath the piston; with opaque material, run a long bead onto a glass plate and look for breaks and voids inside it. Weigh a run of consecutive dots as well, to see whether the scatter is spread evenly or a few dots stand far apart. If only a few dots jump, suspect first a cause that cuts in intermittently, as bubbles do.

With bubbles confirmed, close the routes by which air gets in. Cut down on transferring material, and when it must be transferred, fill the syringe slowly from the bottom up. Switch hand-mixed two-part products to cartridges with a static mixing nozzle, or degas them under vacuum after mixing. Insert the piston at an angle so air can escape, and after loading a fresh syringe purge the needle and fittings by dispensing a few dots to waste. If the material itself arrives full of bubbles, ask the supplier whether it can be supplied degassed.

Hypothesis 3: settled filler

Suspect settling in materials loaded with a heavy powder, the filler: thermally conductive adhesives, silver-filled conductive adhesives and heavily silica-filled epoxies, for example. This is especially so when syringes were stored upright for a long time, when a syringe was left on the machine over a holiday, and when output differs between the start and the end of one syringe. Say work resumes on Monday morning with a syringe of thermally conductive adhesive that was loaded on the machine on Friday afternoon. The first few dozen dots come out small and stiff, and as the syringe empties the dots grow, spreading thin.

Filler is heavier than the resin around it, so over time it sinks. In a study of underfill materials, filler settling depended on the density difference between filler and resin and on the material's viscosity, and it happened mainly during cure rather than during dispensing (Huang et al., 2004). The longer the particles have to move and the thinner the resin, the more they settle, so watch syringes that stood for a long time or were kept warm. Pressure can also pull the material apart. In tests that pushed paste out of a syringe, the extruded paste carried more liquid than the paste loaded, the paste left in the barrel grew steadily drier, and pushing the plunger faster reduced the separation (O'Neill et al., 2016). Those tests used a medical calcium phosphate paste, but the same principle can apply to adhesives heavily loaded with solid particles. Where the filler share varies from place to place, the material also flows differently under the same pressure, so output shifts in one direction with position in the syringe.

Use one syringe from start to finish and weigh dots at regular intervals; that reveals whether the weight moves in one direction with position in the syringe. On a syringe that stood for a long time, look for a clear resin layer at the top, and scoop equal volumes from the top, middle and bottom and compare their weights to see which way the filler has shifted. If a more exact figure is needed, have a laboratory measure filler content from the share of ash left after burning. If settling is the cause, a fresh syringe from the same lot should dispense evenly from the start.

If settling it is, revise storage and sequence. Follow the TDS storage temperature and the orientation for storing syringes, and where the material is meant to be remixed or rolled before use, follow that instruction. Choose a syringe size that matches the production plan so none is left on the machine over a holiday, and keep warming to just before use. If the remaining material is drying out, do not run the dispensing speed too slow, and switch to smaller syringes so each one spends less time on the machine. If the problem persists, discuss with the supplier whether a formulation that settles less is available.

Hypothesis 4: cure in the nozzle

Material cured in the nozzle gives itself away in the first few dots after a break or a shift change: they string out thin or veer sideways, and a hardened lump shows at the needle tip. The products prone to this are instant adhesives, silicones and urethanes that cure with moisture in the air, anaerobic adhesives that cure on contact with metal when air is shut out, and two-part products whose reaction starts the moment they are mixed. During a lunch stop, a thin clear film forms on the tip of an instant-adhesive needle. The first dot of the afternoon veers off and lands on the edge of the part, and the next few draw out thin like thread.

The small drop left at the needle tip stays in contact with air while the machine stands. With a moisture-curing product, that drop cures where it sits and narrows the outlet, so the next shot has to squeeze through a smaller hole and comes out thin or off line. Cyanoacrylate, the main ingredient of instant adhesives, cures through a fast reaction called anionic polymerisation when it meets the thin film of moisture on a surface (Duffy et al., 2018). Anaerobic adhesives work the other way round: without oxygen and in contact with an active metal such as iron or copper, metal ions trigger the initiator and the adhesive cures (Abenojar et al., 2024). That is why material held for a long time inside a metal needle, where little air reaches, can cure first. In two-part products, the mixed material standing in the static mixing nozzle keeps reacting, and its viscosity climbs steeply from a certain point (Lapique & Redford, 2002).

The first clue is whether the bad first dots are tied to how long the machine stood. If they cluster in the first few dots after a break, pull the needle and examine its tip and bore under a magnifier, then see whether a new needle brings the first dot straight back to normal. For moisture-curing sealants there is a standard test method that measures the time for the surface to lose its tack (ASTM International, 2022); dispense a little of the same material into the workshop air and time how long a skin takes to form, and that gives an estimate of how long the machine can safely stand. For two-part products, compare how long the material sat in the mixing nozzle with the pot life in the TDS.

Having traced the cause to material cured in the nozzle, set a stopping procedure. For stops longer than a set time, wipe and cap the needle tip, and on restarting purge the material that has begun to cure by dispensing to waste. Use plastic rather than metal needles and fittings for anaerobic adhesives, and for two-part products set a rule to fit a new mixing nozzle when a stop approaches the pot life. Keep syringes and containers of moisture-curing products tightly closed when not in use to keep out moisture from the air.

Hypothesis 5: time-pressure limits

When dots shrink steadily as the syringe empties, or output wobbles whenever other equipment in the plant runs, look at the dispensing method itself. Give this hypothesis weight when time-pressure dispensing lays very small dots at high speed, when a two-part product whose viscosity rises over time is dispensed by pressure, and when plant compressed air is used through a single regulator. In the morning, with a full fresh syringe, the dots match the standard. By afternoon, with the syringe half empty, dots laid with the same settings are visibly smaller, and the operator keeps nudging the pressure up to keep pace.

In time-pressure dispensing, air fills the empty space above the material and pushes on it. As material leaves, this air space grows, so the way pressure builds in the syringe with each pulse changes too. Doctoral research on time-pressure dispensing showed that the time behaviour of the dispensed flow is sensitive to the air volume in the syringe and that the air volume changing during work makes the dispensed amount inconsistent, and it proposed an off-line control to reduce this (Chen, 2002). A model linking valve flow, delay in the air line, the air in the syringe and the flow of material into one system has also been confirmed by experiment (Zhao et al., 2005). It follows that wobbles in the line and the supply pressure travel along that chain into the output.

Positive-displacement dispensing is often regarded as delivering exactly the set volume. Analysis showed, however, that when microlitre amounts are dispensed, the compressibility and flow behaviour of the material have a large effect on the volume dispensed (Chen & Kai, 2004). In a model of screw-driven dispensing, too, the flow rate is set by the screw's rotation together with how the material flows (Chen, 2007). So changing the method can largely remove the drift that comes from air volume, but the state of the material still has to be held steady.

Weighing dots against the amount left brings this hypothesis to light. Weigh shots at the same settings with the syringe full, half full and nearly empty, and see whether the weight falls in one direction as the level drops. Fit a gauge or recorder after the regulator to check whether supply pressure dips when other equipment runs, and if pulses are very short, check with the equipment supplier's data whether syringe pressure fully builds within that time. For a two-part product, also log whether weight falls with the time since mixing.

If time-pressure dispensing stays, use a function that corrects time or pressure for the amount left, or change syringes at a set remaining level. Feed the dispenser through its own precision regulator and keep it off air lines shared with other equipment. For materials whose viscosity keeps changing, very small amounts, or processes needing high repeatability, review a move to positive-displacement or screw dispensing with the equipment supplier. Even after the change, compressibility remains at small amounts, so keep the purge at start-up and the regular weight checks.

Finding the cause

Five hypotheses do not mean five separate investigations. Rule them out one at a time, starting with what is easy to measure. Material temperature, the amount left in the syringe and supply pressure can be read without stopping the line, and the needle tip only needs to be pulled and looked at. Bubbles and filler require test dispensing or cutting a syringe open, so they come next.

The first clue is the shape of the drift. A slow movement with the time of day or the season points to temperature. A gradual one-way change within one syringe points to the growing air space of time-pressure dispensing or to shifted filler; if it repeats the same way with every fresh syringe, it is the air space, and if it is worst in syringes that stood for a long time, it is the filler. Mostly even output with a few missing or spitting dots points to bubbles, and faults confined to the first few dots after a break point to cure in the nozzle.

If the shape alone does not settle it, run control trials that change one thing at a time. Load a fresh syringe brought to temperature, change only the needle, and compare a fresh syringe from the same lot with one that stood for a long time at the same remaining level. Change only one thing at a time, or there is no telling which one worked. Always compare by the weight and scatter of a set number of dots, measured the same way as before the change.

The final check does not stop at weight. Once the scatter of dot weights is back within the process standard, look at the width and height of beads dispensed onto real parts, and run a bond strength or sealing test once more at the usual interval to confirm that even output shows up in the parts as well. The job is done only when those figures have recovered.

The hypotheses can overlap. Warmed material has lower viscosity, which makes filler settling easier (Huang et al., 2004), and a warmed two-part product thickens that much sooner, which ties into cure in the nozzle (Lapique & Redford, 2002). With time-pressure dispensing, every one of these material changes passes straight into the output. In such cases, hold the material temperature steady first and then look at the rest again, because while temperature is unsettled, the effect of fixing any other cause cannot be compared fairly.

Limits and cautions

Storage temperature, thaw time, pot life, and suitable dispensing pressure and temperature differ by material and machine, so numeric decisions follow the adhesive's TDS and the dispenser supplier's guidance. Filler content analysis and bond strength evaluation are laboratory work, and for parts where safety or sealing is at stake, do not release them simply because output is even again; get the quality engineer to confirm.

Safety matters too. For adhesives and for chemicals used in degassing and cleaning, follow the product's safety data sheet, the SDS, for protective equipment and ventilation. Epoxy resins are listed among the main causes of occupational dermatitis, and once skin has become sensitised, a small amount can trigger a severe reaction (HSE, 2022). Keep instant adhesives away from skin and eyes, and release the air from a pressurised syringe before removing it.

Sources

  1. Abenojar, J., López de Armentia, S., del Real, J. C., & Martínez, M. A. (2024). Kinetic study of anaerobic adhesive curing on copper and iron base substrates. Materials, 17(12), 2886. https://doi.org/10.3390/ma17122886
  2. ASTM International. (2022). ASTM C679-15(2022), Standard test method for tack-free time of elastomeric sealants. https://store.astm.org/c0679-15r22.html
  3. Chen, D. X. (2002). Modeling and off-line control of fluid dispensing for electronics packaging [Doctoral dissertation, University of Saskatchewan]. ProQuest Dissertations & Theses (305456062).
  4. Chen, X. B. (2007). Modeling of rotary screw fluid dispensing processes. Journal of Electronic Packaging, 129(2), 172–178. https://doi.org/10.1115/1.2721090
  5. Chen, X. B. (2009). Modeling and control of fluid dispensing processes: A state-of-the-art review. The International Journal of Advanced Manufacturing Technology, 43(3–4), 276–286. https://doi.org/10.1007/s00170-008-1700-5
  6. Chen, X. B., & Kai, J. (2004). Modeling of positive-displacement fluid dispensing processes. IEEE Transactions on Electronics Packaging Manufacturing, 27(3), 157–163. https://doi.org/10.1109/TEPM.2004.843083
  7. Chen, X. B., Zhang, W. J., Schoenau, G., & Surgenor, B. (2003). Off-line control of time-pressure dispensing processes for electronics packaging. IEEE Transactions on Electronics Packaging Manufacturing, 26(4), 286–293. https://doi.org/10.1109/TEPM.2003.820824
  8. Duffy, C., Zetterlund, P. B., & Aldabbagh, F. (2018). Radical polymerization of alkyl 2-cyanoacrylates. Molecules, 23(2), 465. https://doi.org/10.3390/molecules23020465
  9. Health and Safety Executive [HSE]. (2022). Health surveillance for occupational dermatitis (G403). Retrieved November 2026. https://www.hse.gov.uk/pubns/guidance/g403.pdf
  10. Huang, Y., Bigio, D., & Pecht, M. G. (2004). Fill pattern and particle distribution of underfill material. IEEE Transactions on Components and Packaging Technologies, 27(3), 493–498. https://doi.org/10.1109/TCAPT.2004.831776
  11. Lapique, F., & Redford, K. (2002). Curing effects on viscosity and mechanical properties of a commercial epoxy resin adhesive. International Journal of Adhesion and Adhesives, 22(4), 337–346. https://doi.org/10.1016/S0143-7496(02)00013-1
  12. Mezger, T. G. (2020). The rheology handbook (5th ed.). Vincentz Network. https://doi.org/10.1515/9783748603702
  13. O'Neill, R., McCarthy, H. O., Cunningham, E., Montufar, E., Ginebra, M.-P., Wilson, D. I., Lennon, A., & Dunne, N. (2016). Extent and mechanism of phase separation during the extrusion of calcium phosphate pastes. Journal of Materials Science: Materials in Medicine, 27, 29. https://doi.org/10.1007/s10856-015-5615-z
  14. Zhao, Y.-X., Li, H.-X., Ding, H., & Xiong, Y.-L. (2005). Integrated modelling of a time-pressure fluid dispensing system for electronics manufacturing. The International Journal of Advanced Manufacturing Technology, 26(1–2), 1–9. https://doi.org/10.1007/s00170-003-1978-2

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.