Cleaning the lens or window and reassembling is the usual response when it fogs, but if the haze is vapour from the adhesive that has condensed there, it comes back in the same place after cleaning. What actually gives off that vapour can be uncured monomer, low-molecular siloxanes from silicone, plasticisers and additives, or breakdown during a heating step, while a sealed space and a cold optical surface gather it in one place, and sometimes two or more of these act at once.

Background

A few days after a lens holder and a sensor window were bonded and fitted into their housing, inspection finds a thin, mist-like film on the inner face of the lens. Sometimes a white powdery ring also shows round the bond. Opening the housing and wiping the face clears it, but some time after closing it up again, the same place clouds over once more.

A hazy film scatters light and lowers image contrast, so a camera gives a blurred image and a sensor a wrong reading. Caught at inspection, it means rework to open the housing, clean it and seal it again; appearing after shipment, it comes back as returns and complaints from the field. Haze that returns after cleaning means its source is still inside the housing, so cleaning alone does not end it.

Even after cure, an adhesive holds small amounts of small molecules not tied into the polymer network, and their escape as vapour is called outgassing. The standard screening test heats a sample in vacuum and measures the total mass lost and the share of it, the collected volatile condensable material, that condenses on a cooler collector plate (ASTM International, 2021). For vehicle interior materials the same effect is called fogging: volatile components evaporated from the materials condense on the glass, especially the windscreen, and the effect is measured by the reflectance of a glass plate and by the mass condensed on it (DIN, 2011). Lens haze follows the same path: vapour is given off, it cannot escape, and it condenses on a surface colder than its surroundings.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: before wiping the hazy face, photograph it and collect the film on a clean cloth or sample plate, then set the cure conditions in the adhesive's technical data sheet, the TDS, beside the actual process conditions, meaning UV intensity and time, oven temperature and the time from application to closing the housing.

Hypothesis 1: uncured monomer

In a process using instant adhesives or UV-curing adhesives, suspect uncured monomer first. Typical cases are instant adhesive applied generously so that it spills round the joint, dry seasons, covers closed or parts packed straight after bonding, UV adhesive sitting in the shadow of an opaque part and getting less light, and an ageing lamp whose output has dropped. Take the day after lenses were fixed into holders with instant adhesive, the covers closed straight away and the parts stacked on trays. A white powdery ring has formed round each lens, and the whole inner face of the lens is faintly hazy.

The cyanoacrylate monomer behind instant adhesives has a high vapour pressure, so part of it evaporates before it cures. One manufacturer explains that this vapour reacts with moisture in the air, cures and settles round the bond as a white powder, advises using the minimum amount and ventilating the work area, and warns that parts packed straight after bonding trap the vapour before it can cure (Permabond, 2009). The vapour cures wherever it lands. A study of cyanoacrylate fuming as used in fingerprint work reports that moisture already in the print mattered more than humidity in the air for the polymer to form, and that a usable print developed within two minutes (Lewis et al., 2001). Acrylic resins cured by UV light or heat also keep unbound monomer to the degree they are under-cured. A review of dental resin composites finds that a significant amount of monomer and short chains remains unbound in the set material, and that the amount released tracks the degree of cure (Ferracane, 1994).

The shape of the film is the first clue. If there is a white powdery ring round the bond and the haze fades with distance from it, look at instant adhesive vapour. Find in the records how much was applied and how far it spilled, how long passed before the cover was closed, and the humidity that day. For UV adhesives, measure the actual UV intensity with a radiometer and compare it with the dose in the TDS, and check whether bonds lying in a part's shadow are tacky or dent under a fingernail. For two-part products, check the mix ratio and how well they were mixed.

When the cause narrows to uncured monomer, adjust the amount and the timing. Apply only as much instant adhesive as needed, review an accelerator or a low-bloom grade with lower vapour pressure with the supplier, and close covers only after a full cure in a ventilated place. For UV adhesives, change the exposure direction so no shadow is left or add a secondary heat cure where the TDS allows it, and measure and log lamp output at regular intervals.

Hypothesis 2: cyclic siloxanes

If there is even one silicone material inside the housing, this hypothesis cannot be ruled out. Besides silicone adhesives and sealants, thermal pads, thermal grease, potting compounds and silicone rubber gaskets share the same space. Watch especially near newly changed silicone parts, freshly cured silicone and silicone that warms up in service. This happened after a housing whose sensor window was sealed round with silicone sealant went through a heat treatment. An oily film has spread over the inner face of the window, and wiping it leaves iridescent smears.

When silicone polymers are made, small ring-shaped siloxane molecules form alongside them, and some remain in the product without being tied into the network. In a study of parts from mobile devices, the cyclic siloxanes in adhesives were mostly D4, D5 and D6, rings of four to six units, while silicone rubber held more of the larger D7 to D9 (Xing et al., 2024). These molecules come out into the air when heated. In a baking study with silicone moulds, indoor air concentrations were highest just after baking, moulds holding more cyclic siloxanes gave higher air concentrations, and using the same mould several times cut the concentrations substantially (Fromme et al., 2019). Siloxane that escapes settles on nearby surfaces. A study testing miniature relays in air carrying silicone vapour showed that contact reliability changed with the silicone vapour concentration and the humidity (Tamai, 1996).

The first check is to list every silicone material in the housing, confirming the material of not only the adhesive but also pads, grease, gaskets and cable sheaths. A film that spreads like oil and resists wetting by water leans towards siloxane. For certainty, send the collected film to a laboratory to identify its components by infrared spectroscopy or by gas chromatography with mass spectrometry. Heating a housing without the suspect silicone part and one with it under the same conditions and comparing the haze shows which part is responsible.

If siloxane is the cause, choose a low-volatile grade with the supplier and put parts through a pre-heating treatment to drive off volatiles under the conditions the supplier recommends. After curing silicone, let it vent fully in a ventilated place before closing the housing, and where the design can change, move silicone materials away from the optical faces or switch to another material.

Hypothesis 3: volatile additives

If haze appears not right after assembly but after weeks or months of use, look at plasticisers and additives. Typical places are wherever there are sealants, hot melts, polyurethane adhesives, adhesive tapes or soft plastic parts made flexible with plasticiser, and places that stay warm for long periods, such as a car interior in summer or near a window in sunlight. One display module from a car interior came back after its first summer. A thin oily film covers the inside of the cover glass evenly, and water will not remove it.

A plasticiser is a small molecule that slips between polymer chains to make a material softer, and because it is not chemically bound to the chains, it can move to the surface over time and evaporate. The plasticiser handbook treats volatility and migration in their own right, lists fogging among plasticiser quality tests, and names adhesives and sealants among plasticiser applications (Wypych, 2017). The fogging test standard for vehicle interior materials measures, by reflectance and mass, the volatile components that evaporate from the sample and condense on a glass plate, and its previous edition used DOP, a phthalate plasticiser, as the reference compound (DIN, 2011). Vapour pressure rises with temperature, so in places heated for long periods, such as a car interior in summer, more evaporates, and the vapour collects on any glass face even slightly cooler.

Look in the TDS and SDS of the adhesives, sealants and tapes used for plasticiser and additive content, and ask suppliers whether fogging test values exist. If the film is an even oily layer that water will not remove and it has thickened with time and temperature in service, this hypothesis is strong. Putting a suspect material in a small container, warming it and covering it with a cold glass plate imitates the fogging test and compares which material makes a film, one material at a time. Confirm the components by analysing the collected film.

Once the film is traced to plasticiser, review a switch to a low-fogging grade or a plasticiser-free material with the supplier, and add a fogging test limit to the purchase specification for materials used near optical parts. See also whether moving the material away from heat sources can lower its service temperature.

Hypothesis 4: breakdown in heating

Look at this hypothesis if there is a high-temperature step after bonding. Typical cases are a bonded board sent through solder reflow, an oven temperature raised to cure another part, laser welding or heat forming close to the bond, and a bond that runs hot in service beside an LED or a power device. Assume a board carrying a bonded lens module goes through reflow once more afterwards. A yellowish film has formed inside the lens, and the edge of the bond has darkened.

A cured adhesive also has a temperature limit, above which chains break and new small molecules form. A study of the thermal degradation of polyethyl cyanoacrylate, the polymer an instant adhesive becomes, reports that it breaks down by unzipping from the chain ends (Han et al., 2008). Unzipping from the ends releases small molecules close to the monomer, which means an instant adhesive already cured can give off vapour again when heated. Epoxies too decompose at high enough temperatures into a range of small molecules, by routes that depend on the hardener and resin structure (Levchik & Weil, 2004). The outgassing test standard measures volatiles with the sample heated to 125 degrees Celsius, so its values say nothing about what a hotter step gives off (ASTM International, 2021).

Set the temperature history of the post-bonding steps against the maximum service temperature in the adhesive's TDS. Measure how hot the bond actually got with a thermocouple fixed right beside it, not from the oven or reflow set point. Splitting products into those that went through the heating step and samples taken out before it, and checking whether haze appears only in the former, makes this hypothesis easy to separate. At what temperature the adhesive starts to lose mass can be confirmed by thermogravimetric analysis in a laboratory.

When haze follows only the heated products, start with the process order. Where possible, finish the hot steps first and bond the optical parts afterwards; where not, choose a higher temperature grade with the supplier or bring the heating conditions within the adhesive's allowed range. Where the bond runs hot in service, redesign the distance and heat path between the bond and the heat source.

Hypothesis 5: sealed, cold optics

Where the first four hypotheses ask where the vapour comes from, this one asks why it gathers on the lens. Typical cases are camera housings sealed tight against water, sensor windows and lamps through which no air passes, processes that seal the unit straight after bonding, and designs in which the outer window runs cold while the inner board runs warm. Think of a vehicle's exterior camera just after it switches on, on a winter morning. The window facing the cold outside air is cold, the bond on the board warms as power comes on, and the haze starts from the middle of the window.

Vapour condenses on the colder surface. The outgassing test standard defines condensables as what condenses on a collector held at 25 degrees Celsius while the sample is heated to 125 degrees, and states that materials condensing only below 25 degrees are not detected by the test (ASTM International, 2021). The colder a surface, the wider the range of components that condense on it. A closed space blocks the vapour's way out. One manufacturer warns that in parts packed straight after bonding, volatiles are trapped before they can cure and cause blooming (Permabond, 2009). Fields sensitive to optical contamination, such as spacecraft, select materials from outgassing data compilations that shortlist materials with a total mass loss of 1.0% or less and collected volatile condensable material of 0.10% or less (Campbell & Scialdone, 1993).

Start by measuring the temperature distribution in service. Fix thermocouples to the window and the bond, see which is colder and by how much under real operating conditions, and check whether the haze starts at the coldest spot. Run a housing closed straight after bonding and one left open after the same bonding to cure and vent fully before closing, under the same conditions, and compare the haze. If only the one left open to vent stays clear with the same adhesive, the problem is sealing and timing.

If sealing and a cold surface are gathering the vapour, allow time to vent before closing. After bonding and curing, leave parts in a ventilated place or warm them at a temperature the TDS allows to drive off volatiles, then seal, and place bonds away from optical faces and, where possible, where they will not run colder than the window. Select materials used near optics by their outgassing values from a recognised test method and write those values into the purchase specification.

Finding the cause

The first job is to establish when the haze appears. Whether it is already there at inspection right after bonding, appears after a heating step, or develops weeks or months after shipment sorts out which side to suspect. This can be done from process and return records alone, at almost no cost.

Next come the look and position of the film. A white powdery ring round the bond points to instant adhesive vapour; a film that spreads like oil and resists wetting by water points to low-molecular siloxanes from silicone; an even oily film after long service points to plasticisers and additives; and a yellowish film after a heating step points to thermal breakdown. Haze that starts at the coldest spot rather than near the bond means the sealed space and cold optical face are gathering the vapour.

If the look alone does not decide it, run a control trial. Take housings with one suspect material removed or changed at a time, housings vented before closing and housings that skipped the heating step, put them through repeated heating and cooling under the same conditions and compare the haze. Change only one thing at a time, or there is no telling what removed the haze.

The final check is component analysis. Analyse the collected film in a laboratory to establish whether it is siloxane, plasticiser or polymer formed from acrylic monomer, and the cause is confirmed only when that component is matched to a material in the housing. The job is done only when products made with the changed process and materials stay clear through the same heating and cooling test.

The hypotheses can overlap. When a housing giving off both uncured monomer and siloxane from silicone is heated again by reflow, sealed straight after bonding and then faces a cold window in winter, four of the five hypotheses act in one product. In such cases, along with cutting the vapour sources one by one, correct the order of venting before sealing first, because while vapour stays trapped, the effect of changing a material is hard to compare fairly.

Limits and cautions

Cure conditions, maximum service temperature, pre-heating conditions and allowable outgassing and fogging values differ by product and use, so numeric decisions follow the product's TDS and the customer specification. Component analysis of the film and thermogravimetric analysis are laboratory work, and for safety-related optical parts such as vehicle cameras, do not release on floor judgement alone; get the quality engineer and the customer to confirm. Condensed water droplets may have a cause other than the adhesive, so judge only after the film's components are confirmed.

Safety matters too. Instant adhesive vapour can irritate the eyes and airways, so follow the product's safety data sheet, the SDS, for ventilation and protective equipment. When using UV curing equipment, shield eyes and skin from the UV light, and cure silicone or heat parts to drive off volatiles only under extraction. Follow the SDS for lens cleaning solvents as well, and clean coated optical faces only with the solvents and methods the part maker allows.

Sources

  1. ASTM International. (2021). ASTM E595-15(2021), Standard test method for total mass loss and collected volatile condensable materials from outgassing in a vacuum environment. https://store.astm.org/e0595-15r21.html
  2. Campbell, W. A., Jr., & Scialdone, J. J. (1993). Outgassing data for selecting spacecraft materials (NASA Reference Publication 1124, Revision 3). NASA Goddard Space Flight Center. https://ntrs.nasa.gov/citations/19940017416
  3. Deutsches Institut für Normung [DIN]. (2011). DIN 75201:2011-11, Determination of the fogging characteristics of trim materials in the interior of automobiles (superseded by the 2024 edition). https://doi.org/10.31030/1813243
  4. Ferracane, J. L. (1994). Elution of leachable components from composites. Journal of Oral Rehabilitation, 21(4), 441–452. https://doi.org/10.1111/j.1365-2842.1994.tb01158.x
  5. Fromme, H., Witte, M., Fembacher, L., Gruber, L., Hagl, T., Smolic, S., Fiedler, D., Sysoltseva, M., & Schober, W. (2019). Siloxane in baking moulds, emission to indoor air and migration to food during baking with an electric oven. Environment International, 126, 145–152. https://doi.org/10.1016/j.envint.2019.01.081
  6. Han, M. G., Kim, S., & Liu, S. X. (2008). Synthesis and degradation behavior of poly(ethyl cyanoacrylate). Polymer Degradation and Stability, 93(7), 1243–1251. https://doi.org/10.1016/j.polymdegradstab.2008.04.012
  7. Levchik, S. V., & Weil, E. D. (2004). Thermal decomposition, combustion and flame-retardancy of epoxy resins: A review of the recent literature. Polymer International, 53(12), 1901–1929. https://doi.org/10.1002/pi.1473
  8. Lewis, L. A., Smithwick, R. W., III, Devault, G. L., Bolinger, B., & Lewis, S. A., Sr. (2001). Processes involved in the development of latent fingerprints using the cyanoacrylate fuming method. Journal of Forensic Sciences, 46(2), 241–246. https://doi.org/10.1520/JFS14956J
  9. Permabond. (2009). How do I prevent white powdery residue when using instant adhesives? Retrieved November 2026. https://permabond.com/how-do-i-prevent-white-powdery-residue-when-using-instant-adhesives/
  10. Tamai, T. (1996). Effect of silicone vapor and humidity on contact reliability of micro relay contacts. IEEE Transactions on Components, Packaging, and Manufacturing Technology, Part A, 19(3), 329–338. https://doi.org/10.1109/95.536834
  11. Wypych, G. (2017). Handbook of plasticizers (3rd ed.). ChemTec Publishing. ISBN 9781895198973
  12. Xing, Y., Ge, Y., Lu, S., Yang, T., & Peng, X. (2024). Dimethylcyclosiloxanes in mobile smart terminal devices: Concentrations, distributions, profiles, and environmental emissions. Toxics, 12(4), 287. https://doi.org/10.3390/toxics12040287

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.