BlogKaltec Voices
The EV-era lubricant market: why the share of fluids that prove their conditions grows
- Type
- Kaltec Voices
- Published
- 24 November 2026
- Prepared by
- Minkyung Choi
- Role
- Research Analyst
An electric car uses half or less of the fluid a combustion car does, so road-transport lubricant liters and margins shrink, yet every reducer oil and cooling fluid that remains picks up insulation, copper corrosion and conductivity conditions and tests that run for hundreds of hours. What grows meanwhile is the share held by fluids that have proven those conditions, and even if the shift is slow and hybrids last, those tests belong on today's schedule.
Background
In the Ministry of Land, Infrastructure and Transport's registration figures for the end of June 2026, electric cars are 4.1% of registered vehicles (Newsis, 2026a). Seen from those buying engine oil, the shift has barely begun. Beside this number I write down how many conditions customer test requests attach to one fluid. A passenger car engine oil request ends at a viscosity grade and a few approvals, but one reducer oil request from an electric drive parts plant carries several times as many. A change of just over 4% in registrations is already several times larger in how fluids are chosen.
The passenger car engine oil liters our customers order are also coming down only a little at a time. By liters alone, this is a slowly shrinking market. The fluid one car uses over its life clearly falls, and the margin EV fluids leave does not make up for the whole decline in road-transport lubricants (Herrmann et al., 2021). Yet every liter that remains has more conditions and tests to pass, and the fluid that proves them first takes the place left. So even while road-transport liters and margins shrink, I think the share held by fluids that have proven their conditions grows.
Liters fall slowly, with the registered fleet
By McKinsey's analysis, a combustion car uses 50 to 90 liters of engine oil over its life and a battery electric car not a drop. Coolant falls from 20 to 80 liters to 10 to 20, and driveline fluids stay similar at 4 to 12 liters. Altogether an electric car uses one half to one third of the fluid a combustion car does (Herrmann et al., 2021).
This decline follows the share of cars on the road, not the share of sales. Engine oil sells at oil changes, and what comes in for a change is not new cars but every registered car. In the first half of 2026, 198,509 electric cars were newly registered in Korea, up 113.6% on a year earlier and 23.3% of new cars (Newsis, 2026b). Yet of 26,676,000 cars registered at the end of June, 1,095,000 are electric (Newsis, 2026a). Doubling the 850,000 first-half registrations to a full year gives 1.7 million, just over 6% of the fleet, so even if every new car were electric, the registered share would rise only just over 6 points a year.
So I split the force pressing on engine oil liters in two. One is the cumulative EV share of registered vehicles, and the new registration share is its leading signal. The other is drain intervals lengthened by synthetic oils. Read the two together and the shift looks faster than it is.
Hybrids slow the first force further. In the same half, 289,814 hybrids were newly registered, more than electric cars (Newsis, 2026b), and 2.81 million hybrids are registered (Newsis, 2026a). A hybrid keeps using engine oil while putting an electric motor inside the transmission. So liters drain more slowly still, but electrical conditions already attach to hybrids too.
Some numbers show liters and value moving apart. In Kline's 2025 outlook, US commercial lubricant volume across trucks and construction, agricultural and mining equipment stays almost flat at just over 1.8 billion liters from 2024 to 2040, while value rises 45%. What lifts value is the move to lower viscosities and premium products (Kline, 2025). 45% over 16 years is just over 2.3% a year, and the outlook leaves out passenger cars, so I take from it only that value need not fall when liters hold flat. In passenger EVs, what fills that place is the electrical conditions on driveline and cooling fluids.
A driveline where gears and motor share one oil
In a drive unit that combines motor and reducer in one block, the same oil wets the gears and touches the motor windings, sensors and copper wiring. SAE J3200, issued in October 2022, covers fluids for gear units where the electric motor is immersed in or in contact with the oil (SAE International, 2022). Two conditions engine oil never had arise here: insulation, which keeps current from leaking between windings, and copper corrosion performance, which means not corroding copper or leaving conductive residue. A reducer oil inquiry from one drive parts plant listed, beside the viscosity grade, operating temperature, motor voltage, volume resistivity after ageing at that temperature, copper corrosion under voltage and gear protection.
How copper corrosion testing has changed shows the size of the shift. The copper strip test, ASTM D130, was created in 1922 to find corrosive sulfur in gasoline and is still the basic test. But it does not see what corrosion products cause, and an analysis found it falls short for screening the new failure modes of electric drive units (Hunt et al., 2024). ASTM D8544, the 2024 edition, measures conductive deposits building up on the liquid and vapor sides under applied voltage, with a typical condition of up to 500 hours at 150°C (ASTM International, 2024a). A test that can run close to three weeks attaches to every product and every formulation change.
Gear protection and copper protection pull against each other. The sulfur in the extreme-pressure additives that guard gears is aggressive toward copper. Raise gear protection and the copper margin shrinks; protect copper and the gear side must be tested again. So one reducer oil takes more test combinations than an engine oil, and once a formulation is set, even changing one additive sends it back to testing. Hybrid transmissions where the motor is immersed in or touches transmission oil have the same structure J3200 covers.
One insulation condition, over four times the cooling margin
In thermal management fluids, the margin on a liter of cooling splits by condition. Coolant for batteries and power electronics stays glycol-based, but its electrical conductivity must be kept low so that it conducts less even if it leaks. ASTM D8566, the specification for this coolant issued in May 2024, covers everything from battery electric cars to hybrids, but says not to use it for immersion cooling in direct contact with electrical parts (ASTM International, 2024b). The test method for its conductivity, D8634, came out in October 2025 (ASTM International, 2025).
Cooling in direct contact with electrical parts belongs to water-free dielectric coolants. In 2021 McKinsey put the gross margin of water-glycol coolant below 0.5 euros per liter and dielectric coolant at 2 to 3 euros per liter. One condition, insulation, earns a liter of cooling over four times the margin. The same analysis said that in the most aggressive of three scenarios over half of mass-market vehicles could use dielectric coolant, but judged the first two, limited to sports and luxury cars, more plausible (Herrmann et al., 2021). I read the mass-market scenario as the upper bound. Total liters fall, but within them the share of liters proven on insulation and conductivity grows.
Putting it to work
The pace of the shift is still open. The International Energy Agency expects electric cars to be 29% of new cars worldwide in 2026, while noting both the first-quarter sales drop and the second-quarter rebound (IEA, 2026b). The oil EVs displace in 2035 also ranges from about 9 million barrels a day in the Current Policies Scenario to about 10 million in the Stated Policies Scenario: the same direction at different speeds (IEA, 2026a). Given that range, I set up a fast case and a slow case from Korean numbers, and split the plans of engine oil buyers from those of drive unit and parts makers.
The fast case has the EV share of Korean new registrations keep rising from the first half's 23%. Distributors and service chains buying engine oil lower volume floors in long-term contracts and shorten terms. Drive unit and parts makers count reducer oil and cooling fluid test schedules back from part approval dates. The copper corrosion test under voltage alone can take up to three weeks. So they put volume resistivity after ageing and conductivity into the first test plan together.
The slow case has hybrids last a long time. Engine oil buyers keep their liters longer, so they have little reason to rush volume contracts down. Parts makers' test plans are almost the same as in the fast case, because hybrid transmissions with motors immersed in oil carry the same insulation and copper conditions. People often assume a slower shift lets preparation wait too, but between the two scenarios only the timing of liters draining differs; the time to start testing is the same.
The signal that separates fast from slow is the monthly EV and hybrid share of new registrations, and beside it I set the kinds of test requests coming in from customers. Looking at orders and test requests from many industries in one place, requests from parts plants asking about volume resistivity and copper corrosion test conditions rose first, before engine oil orders fell noticeably.
In both cases the yardstick is the value after ageing at operating temperature and voltage. A supplier that has seen test requests rise ahead of orders keeps test data ready for those conditions. One certificate saying a fluid passed a spec number cannot tell you its after-ageing values under your parts' conditions, and when the formulation changes, that test has to run again.
Conclusion
Road-transport lubricant liters and margins are shrinking, only as fast as the registered fleet turns over. What grows within them is the share of fluids that have proven insulation, copper corrosion and conductivity conditions. Even if the shift is slow and hybrids last, the test plan is the same.
Where 50 to 90 liters of engine oil drop out, tests of up to 500 hours come in.
Sources
- ASTM International. (2024a). ASTM D8544-24 Standard Test Method for Determining Conductive Deposits from Fluids in Liquid and Vapor States within an Electrically Charged System. https://store.astm.org/d8544-24.html
- ASTM International. (2024b). ASTM D8566-24 Standard Specification for Glycol-Based Electric Vehicle Coolant with Low Electrical Conductivity, May 15, 2024. https://store.astm.org/d8566-24.html
- ASTM International. (2025). ASTM D8634-25 Standard Test Method for Measurement of Conductivity in Electric Vehicle (EV) Coolants, October 1, 2025. https://store.astm.org/d8634-25.html
- Herrmann, H., Kiewell, D., Klingl, M., & Ramanathan, S. (2021). EV fluids: Say goodbye to the oil change. McKinsey & Company, August 17, 2021. https://www.mckinsey.com/industries/automotive-and-assembly/our-insights/ev-fluids-say-goodbye-to-the-oil-change
- Hunt, G. J., Choo, L., & Newcomb, T. (2024). 100 Years of Corrosion Testing: Is It Time to Move beyond the ASTM D130? The Wire Corrosion and Conductive Deposit Tests. SAE International Journal of Fuels and Lubricants, 17(1), 17-35. https://doi.org/10.4271/04-17-01-0002
- International Energy Agency [IEA]. (2026a). Global EV Outlook 2026, May 2026, oil displacement by scenario in the outlook chapter. https://www.iea.org/reports/global-ev-outlook-2026
- International Energy Agency [IEA]. (2026b). Electric Car Markets in a Time of Uncertainty, first-half 2026 sales and the 2026 outlook. https://www.iea.org/reports/electric-car-markets-in-a-time-of-uncertainty
- Kline & Company. (2025). The Road Ahead: Commercial Vehicle Electrification Through 2040, USA & Canada, presented at ILMA LubeTrends Live, October 7, 2025. https://ilma.org/wp-content/uploads/2025/10/ILMA-AM2025_LubeTrends-Live_Kline.pdf
- Newsis. (2026a). 상반기 신규 등록 4대 중 1대 전기차…누적 110만대 육박, July 30, 2026, citing Ministry of Land, Infrastructure and Transport vehicle registrations as of the end of June 2026. https://mobile.newsis.com/view/NISX20260729_0003728744
- Newsis. (2026b). 상반기 친환경차 점유율 58% 육박…中, 자동차 수입국 1위 등극, August 4, 2026, citing Korea Automobile & Mobility Association analysis of first-half new registrations. https://mobile.newsis.com/view/NISX20260804_0003735247
- SAE International. (2022). J3200_202210 Fluid for Automotive Electrified Drivetrains, October 13, 2022. https://saemobilus.sae.org/standards/j3200_202210-fluid-automotive-electrified-drivetrains