BlogKaltec Voices
Why packaging and transport decide contamination in chemicals bound for the cleanroom
- Type
- Kaltec Voices
- Published
- 24 November 2026
- Prepared by
- Subum Jang
- Role
- Logistics Staff
The certificate for a high-purity chemical measures the liquid in the container on the day it was filled, and nothing records the particles that settle on the container and its bags afterwards or form in the liquid on the road. From shipment to point of use, where and in what order the bags come off, the shaking and temperature in transit, and the pallet material are the share of cleanliness that logistics has to keep outside the certificate.
Background
It was the day we unloaded a pallet of four lined drums of equipment cleaning chemical at the material entry of a customer's fab. Before entry, the contamination control engineer and I counted particles on the bag surfaces. We wiped the same area with a clean wiper on the top of the outer bag, the bottom of the outer bag and the bottom of the inner bag once the outer one was off, rinsed each wiper in ultrapure water and ran the water through a liquid particle counter. The outer bag bottom, which had sat on the wooden pallet, gave the highest count, and the inner bag bottom was far lower. But on one drum whose outer bag corner a forklift tine had torn during unloading, the inner bag bottom read close to the outer bag bottom.
All four certificates were within grade. Semiconductor IPA is bought to a grade in a standard such as SEMI C41 (SEMI, 2018), and equipment cleaning chemicals to a grade the maker sets. Either way, the certificate measures the liquid of the filled lot. Contamination gets in afterwards by two routes. One is particles that ride on the container and bag surfaces through the door. The other is particles that shaking on the road creates in the liquid inside the liner. So the question I hold onto in logistics is how many layers, in what condition, the packaging that left the filling plant keeps all the way to the point of use.
Packaging where each layer has its own door
High-purity IPA and equipment cleaning chemicals usually come in lined drums or bottles. Two heat-sealed clean bags wrap the container, and the pallet and stretch wrap go on the outside. The two bags look like the same plastic but do different jobs. The outer bag catches dust on the road and, when it comes off outside the cleanroom, takes that dust with it. The inner bag guards the surface up to the last door. That day's drums were going onto a cabinet in the chemical supply room to feed the piping, and the inner bags came off in the airlock in front of it. Containers carried to the point of use, like 4 L bottles, lose their inner bag inside the pass box. For bottles that arrive in divided cardboard boxes, the box is the outer layer, so each bottle must still be in its own bag for a layer to remain once the box is off.
ISO 14644-5, revised in 2025, treats moving materials and portable equipment into and out of the cleanroom as an operational requirement (ISO, 2025). A commentary on it says protective packaging for transport and storage should be removed outside the cleanroom and airlock (Sandle, 2025). If one layer comes off at each door, the number of bags has to match the number of doors on the customer's route. With three doors and two bags, nothing is left to remove at the last door, so the container has to be wiped, and the result of wiping depends on whose hands do it.
Labels follow the layers too. If lot and expiry are only on the outer bag, nobody can tell what the drum is once that bag is off, and someone ends up opening the inner bag in the entry anteroom to check. The lot label belongs on the container and must be readable through the inner bag. A distribution warehouse opening the inner bag for incoming inspection has the same result. When our warehouse receives items bound for a cleanroom, we check only the label and the seal line through the outer bag.
Particles made by shaking and temperature
The liquid inside the bags shakes the whole way too. In a liner with headspace left after filling, the liquid sloshes and particles form where air meets liquid. A patent on a liner design that removes the headspace and leaves room for the liquid to expand with temperature reports that particle generation was held very low compared with shaken samples that kept headspace (Wertenberger, 2005). The particle count on the certificate was taken at the filling plant, so it holds nothing about how many hours the drum shook on what road surface before reaching the plant. Between outer and inner bag, the two bags can rub and shed dust while they shake, and removing the outer bag outside the cleanroom leaves that dust outside as well.
Temperature makes different problems in summer and winter. In a truck bed at summer midday, the liquid expands and pulls the liner tight, and the air in the heat-sealed bag expands and pulls the bag tight. A tight bag bursts easily even from a brush against a pallet corner or a tine tip. A drum unloaded from a truck bed on a winter dawn is colder than the dew point of the dock air, so water condenses on the outer bag. Those droplets catch floating dust and leave stains where they dry. So in winter we leave the drum outside the entry anteroom with the outer bag on until it nears room temperature. If water condenses, it condenses on a bag that will be thrown away.
I also look at how many times transport breaks at a warehouse. On the way from an overseas filling plant through a bonded warehouse and a distribution warehouse to the customer, each extra warehouse stop adds two forklift handlings and one more stacking of the pallet. If other freight goes on top of the pallet at a transit warehouse, the bags below shake while pressed. So items bound for a cleanroom go straight from the distribution warehouse to the customer, and we set a separate loading order so nothing else is stacked on them. That cuts both the hours of shaking and the number of stackings.
The door wood and paper cannot pass
Imported chemicals often arrive on wooden pallets. The HT mark on such a pallet means the wood was heat treated to 56 degrees Celsius through its full cross-section for at least 30 minutes under an international standard meant to stop pests from traveling (IPPC, 2018). It has nothing to do with cleanliness. Heat-treated wood still sheds dust and splinters at the corners and holds moisture. The fabs I supply do not let wooden pallets or cardboard past the dock.
So the load has to move to another pallet somewhere, and that place becomes a new hand-off. Restacking at the customer's dock exposes the bags to truck exhaust and outside air, and cutting the wrap with a knife can easily slash the outer bag. We move items bound for a cleanroom onto plastic pallets in the warehouse before shipment and cut the wrap starting from the side away from the bags. Even a plastic pallet brings dirt and oil on its base if it carried other freight, so pallets for the cleanroom route are kept apart and washed before use.
Putting it to work
On a route that ships from the distribution warehouse and arrives with no transit stop, the packaging passes six places: shipment, transport, unloading, removal of the outer packing, the pass box or airlock, and the point of use. Imports add a bonded warehouse and customs clearance before that, and if customs orders an inspection, the outer packing may be opened on the spot. At each place, the side handing over and the side receiving check the number of bags and the state of their surfaces together.
When the distribution warehouse hands over to the carrier, it records how many bags there are, whether the lot label reads through the inner bag and what the pallet is, and attaches a temperature logger and a shock indicator label. The driver takes the pallet whole without looking at the bags, so the condition of not sharing a truck bed with dusty freight and the number of stops are fixed at dispatch.
When the customer's dock receives, it copies the logger's maximum and minimum temperature and the shock indicator's color onto the receipt, and in winter starts counting the time to reach room temperature from the moment of unloading. If a bag arrives with a burst seal, whether to return the drum or just replace the outer bag is not decided that day but handled by criteria agreed with the customer in advance. If it is a return, the next question on the spot is when the drum to replace it will arrive.
Where outer packing comes off, decide who removes the wrap and outer bag outside the entry anteroom and in what order, and move the unwrapped drum straight onto a clean cart without setting it on the floor. Where the inner bag comes off in the pass box or airlock and what it is wiped with are for the customer's contamination control engineer to decide, and logistics matches how many bags, in what state, reach that point to those criteria. The allowed count of particles on bag surfaces varies by fab, starting with the method of counting, so my measurements could only be used to compare places on the same day.
Conclusion
The stretch a certificate does not speak for runs from the filling plant door to the last door. Cleanliness in that stretch depends on whether the order of removing layers matches the doors and whether the bags stay intact on the road. A drum with a torn bag may be turned back at the dock under the agreed criteria, so keeping things clean leads to whether there is a drum to replace it. With supply that keeps the number of bags and the pallet to the same specification for each item and gives notice before changing them, the criteria for sending a drum back stay steady. If drums packed to the same specification are held in reserve, the next one follows right behind even when one goes back.
Each time entry conditions changed at the fabs I supply, the first things revised were the number of bags, the pallet material and transport temperature records, and purity grades came after. A grade table waits for a revision of the standard, but a packaging specification can be revised by the fab and the supplier that same week, so on lines moving to the next process generation, too, the packaging specification will keep being revised before the purity grade table.
The certificate's grade follows to the point of use only as far as the layers that left the filling plant door stay intact to the last door.
Sources
- International Organization for Standardization [ISO]. (2025). ISO 14644-5:2025 Cleanrooms and associated controlled environments — Part 5: Operations. ISO.
- International Plant Protection Convention [IPPC]. (2018). ISPM 15: Regulation of wood packaging material in international trade. FAO.
- Sandle, T. (2025, August 14). Effective cleanroom operation: the revised operational standard. RSSL Insights.
- SEMI. (2018). SEMI C41-0618 Specification and guide for 2-propanol. SEMI.
- Wertenberger, R. (2005). Returnable and reusable, bag-in-drum fluid storage and dispensing container system (U.S. Patent No. 6,942,123). U.S. Patent and Trademark Office.