Most of what a brightener trial on a plating line costs arises after the free sample arrives: the line stopped for carbon treatment, replating rejects, corrosion testing and the rollback if it fails. A trial that puts in writing who shares the cost of a failed day checks longer at the cheap Hull cell stage before going into the main tank, so the line pays less to test the same brightener.
Background
After a trial to change the brightener in the bright nickel tank at a decorative chrome plating plant was over, I added up what that one trial had cost, line by line, for the first time. The first line was the few drums of brightener and additive we had sent as a free sample. Below it came the time for Hull cell panels and analysis, the shifts the line stood for carbon treatment, and the cost of stripping and replating rejects. There was also the outside lab's corrosion testing fee, contract disposal of the old solution drained off, and the work on the approval documents the customer resubmitted. Once it was all added up, the sample was the smallest line in the total, and the only line with an owner written in the proposal.
A trial proposal usually carries one line: "samples provided free of charge." That line states only the supplier's share. The lines left out fall on the line hosting the trial. If the trial succeeds, that cost gets buried in a few months of chemical savings and fewer rejects from the new brightener, but if it fails, it stays as pure loss. Yet the order of the trial is usually laid out by the supplier's technical team. Only a supplier who shares the cost of a failed day lays out the trial in an order that keeps that cost down. The order of a trial follows whoever bears its cost.
The lines that grow after the sample arrives
A brightener trial usually starts in a Hull cell. It plates a single tilted cathode panel across a range from high to low current density in one run (Hull, 1939), so a few panels show how far the bright range reaches when the new brightener is mixed into the existing solution. This stage costs little. But a panel cannot capture the line's agitation, temperature distribution or part shapes. Long-standing plating shop guidance also warns that the Hull cell must be used with other analysis and can mislead on its own (Pullizzi, 1988). In the end, the verdict comes from the main tank.
From the day the trial moves to the main tank, the lines grow. A brightener breaks down little by little as it works at the cathode surface, and the breakdown products build up in the solution until they are dragged out on parts or adsorbed onto activated carbon (Pullizzi, 1988). Whether the new system suits the existing solution is checked first in the Hull cell, and if it does not, the solution gets carbon treatment, or part of it is drained and replaced. Carbon treatment means moving the solution to a treatment tank, heating and filtering it, then filling back, so without a spare tank the line stands meanwhile. The output of the shifts lost in that time often becomes a bigger line than the chemicals. The drained solution goes to a contract disposal company as nickel-bearing waste, and the nickel salts and chemicals for refilling are charged separately.
Defects during a trial often show only after the chrome is on. Haze in low current density areas, pits or poor adhesion mean stripping the chrome and nickel and replating. That takes stripper and rectifier time and pushes delivery back. Inspection grows too. During a trial, many plants check low current density areas under magnification, measure thickness more often than usual and plate a Hull cell panel every day. For automotive parts, a brightener change can also shift the potential difference between semi-bright and bright nickel, so thickness and potential are measured again layer by layer. Corrosion resistance is often checked with the copper-accelerated acetic acid salt spray test (ISO, 2022). Each run takes a day or two, so an outside lab charges by test hours and specimen count.
A failure adds one more line. Going back to the original brightener means removing the new brightener and its breakdown products again, so there is one more carbon treatment and one more line stop. The leftover new brightener is scrapped. For automotive parts, a process change brings customer notification and resubmission of the part approval documents (AIAG, 2006), and if the customer requires it, the same documents go back and forth once more for the rollback.
The cost of a failed day and the order of a trial
Lay the lines out by stage and the shape of the cost shows. The Hull cell and lab stages are cheap, it gets expensive from the day it goes into the main tank, and most expensive on the day it fails. For a supplier who bears only the sample, the trial's cost ends at the first line, so the sooner it goes into the main tank, the sooner the sale. A customer who bears every line of a failed day either drops the trial or, pushed by the supplier's schedule and its own delivery dates, opens the main tank with only a short stop rule. A trial opened that way usually stops at the first defect, and whether that defect came from the brightener or from solution control is never settled.
Put in writing that the supplier bears part of the rework or rollback, and both tallies face the same way. The supplier spends more money and time at the cheap stages. It follows the advice to check on Hull cell panels how much a carbon treatment will change the solution before treating the whole tank (Pullizzi, 1988), plates more panels mixed with existing solution, and runs a few racks or a small auxiliary tank before the whole main tank. In one trial where we put in writing that we would bear part of the rework, our technical team reran Hull cell panels mixed with existing solution several times before going into the main tank.
A supplier bearing trial costs means putting part of the failure on its own books. So it can make that promise only as far as it knows the product's chemistry and that line's conditions. When a supplier that does not know makes a big promise, the cost comes back in the prices of other items.
Putting it to work
It is not always right for the supplier to bear trial costs. When a trial proposal arrives, the first thing to sort out is which kind of trial it is.
Some trials are better not borne by the supplier. A trial opened with no plan to switch, only to use in price talks with the current supplier, is one. A trial with no intent to reach a conclusion has no failure to share, and if the supplier bears its cost, that cost rides on the supplier's next quote and comes back to every buyer. The same goes when the customer also changes the pretreatment degreaser, rectifiers or part specs during the trial. If changes were made on the customer's side too, the share of failure stays on the customer's side as well. A free switch, where the supplier offers to bear the whole switching cost, also needs a careful look. I have seen that cost come back later as a higher brightener price or a long exclusive supply term.
Some trials are better shared by the supplier. If the supplier proposed the switch first, part of the failure is the price of that proposal. Whether it put forward a new brightener system as a cost-cutting plan or needs a retest because a formula or raw material changed, the reason the trial was opened lies with the supplier. The same holds when the cause of failure lies in the product's chemistry. Whether the new system clashes with brightener left in the existing solution, or its breakdown products build up fast, is best known by whoever made the product. In such trials, decide before the trial who bears each line. Hull cell work and solution analysis are things a plating chemicals supplier handles anyway, so they are not up for sharing. What gets shared is carbon treatment, line stops, rework and rollback, borne together up to a cap. The cap is set against the size of a year's business on that line if the trial succeeds. A cap larger than a year's business is a promise the supplier cannot keep, and a cap that stops at the sample's value is a promise that shares nothing.
Once the two kinds are sorted, proposals read differently. A proposal that lists only sample quantities and delivery, and one that brings up the lines of a failed day first and offers to share them, become different trials even for the same brightener. The numbers in the second kind come only after looking first at that line's solution, parts and shift schedule.
Conclusion
Most of a trial's cost arises on the line after the sample arrives. A supplier who shares the lines of a failed day sets the trial's order so those lines never appear. So in processes like plating, where a whole line hangs on one solution, wording that shares the lines of a failed day is likely to settle in as a clause of trial proposals.
When a trial proposal arrives, add up the cost of the day that trial fails with the supplier's contact before the sample comes.
Sources
- Automotive Industry Action Group [AIAG]. (2006). Production part approval process (PPAP) (4th ed.). AIAG.
- Hull, R. O. (1939). Current density range characteristics: Their determination and application. Proceedings of the American Electroplaters' Society, 27, 52–60.
- International Organization for Standardization [ISO]. (2022). ISO 9227:2022 Corrosion tests in artificial atmospheres — Salt spray tests. ISO.
- Pullizzi, T. J. (1988). Troubleshooting modern bright nickel plating solutions. Reprinted in the finishing.com library. https://www.finishing.com/library/pullizzi/brightnickel.html