KALTECKOREA

BlogKaltec Voices

Why water treatment chemical savings come back as discharge and fuel bills

Type
Kaltec Voices
Published
24 November 2026
Prepared by
Unjung Kim
Role
Operations Staff

Lower a cooling tower's cycles of concentration from 5 to 3 and the same heat load takes 20% more make-up water and twice the blowdown, so what a cheaper treatment chemical saved comes back as water and discharge charges, and on the boiler side as fuel. When comparing chemicals, check whether the supply scope runs from make-up treatment through boiler and cooling tower to discharge, and whether monthly water analysis and cycle-setting checks transfer when the chemical changes.

Background

Last autumn an environmental officer at a customer asked why the discharge charges had gone up, and sent me the cooling tower's make-up and blowdown meter readings. The site ran the auxiliary boilers and cooling towers on a power station's grounds; the high-pressure main boilers that drive the turbines were managed separately, as their water quality standards differ from the start. The cooling load was almost the same as the year before, but blowdown readings had risen noticeably since spring, and make-up had risen with them. That spring was when the boiler treatment and the cooling water treatment were switched to lower-priced products.

Water treatment chemicals do not make anything. They keep boiler tubes and cooling circuits moving heat properly and wasting less water, so their effect shows not on the chemical invoice but in the figures for fuel, water and discharge. If blowdown rose in the year the chemical changed, what the unit price saved comes back as make-up water and discharge charges, and on the boiler side as fuel. The value of a water treatment chemical is set across the whole system the same water runs through, from make-up treatment through boiler and cooling tower to discharge.

Water and chemical that rise as cycles fall

A cooling tower rejects heat by evaporating water. Evaporating water leaves what was dissolved in it behind, so the circulating water grows steadily more concentrated. Drawing off part of it before scale forms is blowdown, and how many times more concentrated the circulating water is than the make-up is the cycles of concentration (DOE, n.d.; EPA, 2012). Many systems run between 2 and 4, and 6 or more is possible depending on water quality and treatment (DOE, n.d.). With the same make-up water, how high cycles can go depends largely on how well the cooling water treatment holds scale in check and prevents corrosion, and microbial control sets that limit too (EPA, 2012). Where the make-up is so high in hardness or silica that cycles cannot be raised in the first place, changing the chemical will not move this limit much.

Switch to a chemical with weaker inhibition, or cut the dose, and operators lower the cycles to avoid scale. At that customer too, the cooling tower's cycles setting had come down after the switch. Leaving out drift and taking evaporation as 100, at 5 cycles the tower takes in 125 of make-up and discards 25 as blowdown. At 3 cycles it takes in 150 and discards 50. Rejecting the same heat takes 20% more water in and twice as much water out.

As more water goes out, chemical goes with it. To hold the inhibitor concentration in the circulating water, whatever leaves with the blowdown has to be added back, so the dose follows the blowdown volume. That customer's monthly dose had risen after the switch as well. With the move to the cheaper chemical, the monthly water analysis and cycles check the previous supplier had done also dropped out. That is why the environmental officer, looking at discharge charges, noticed the drop in cycles before the water treatment staff did.

Scale hidden in the fuel intensity

A boiler boils water and sends out only steam, so most of the calcium, magnesium and silica dissolved in the feedwater stays behind and the boiler water concentrates (DOE, 2012b). If the boiler treatment cannot hold these in the water, they harden on the heating surfaces as scale. Scale covers the wall the flame's heat must cross to reach the water, so the same steam burns more fuel. The U.S. Department of Energy's material on firetube boilers puts the loss from normal scale about 0.8 mm thick at about 2% of fuel, and notes that with silica and iron mixed in, the loss is greater at the same thickness (DOE, 2012a).

That 2% is not written on the chemical invoice. The sign of scale is flue gas temperature creeping up at the same firing rate and oxygen level (DOE, 2012a), and that figure sits in the boiler room log. The fuel bill arrives with load, weather and scale mixed into one number. So the figure to read is not fuel cost but the fuel used to make one tonne of steam, the fuel intensity. As more scale builds up, the tube metal can overheat, lose strength, bulge and rupture, and such failures have been reported in power plant boilers too (DOE, 2012a; Kim et al., 2019). That cost goes beyond fuel into equipment repair.

The same water from make-up treatment to discharge

Follow the water and these costs line up on one path. Water first passes through make-up treatment. Where boiler make-up is produced by softeners, ion exchange or reverse osmosis, every tonne discarded as blowdown also carries the cost of making that water (DOE, 2012a). Ion exchange units discharge wastewater mixed with acid, alkali and salt at every regeneration, and that wastewater leaves by the same drain.

The same happens at the boiler. If the boiler treatment disperses poorly, operators run the boiler water less concentrated to avoid deposits and raise blowdown to match. Boiler blowdown is usually 4 to 8% of feedwater and can reach 10% when the make-up is high in solids (DOE, 2012b). This water has been heated to saturation temperature, so it throws away that much fuel with it, and the same amount of make-up has to be treated again to replace it.

Discharge is where cooling tower and boiler blowdown meet. Sent to the public sewer, it carries the sewer charges set by local ordinance (MOLEG, n.d.-b). Sent to an industrial complex's public wastewater treatment facility, it carries that facility's charge, set on criteria such as the size of the business and the level of pollutants discharged (MOLEG, n.d.-a). So the discharge figure mixes both blowdowns with the regeneration wastewater from make-up treatment. Whichever budget these four costs land in, the water flows along one path, so what is cut at one point shows up again at the next.

Putting it to work

Most of the figures to set beside the chemical invoice at month end are already on site. Cycles of concentration is the conductivity of the cooling tower's circulating water divided by that of the make-up, so it is in the water treatment staff's analysis sheet (EPA, 2012). Make-up meter readings divided by blowdown readings should come out close to it. If that ratio is more than 10% above the conductivity figure, suspect leaks, overflow or drift (EPA, 2012). If cycles fell from the month the chemical changed, make-up and discharge charges follow from the next bill.

Fuel intensity is the boiler room's fuel use divided by steam produced. Without a steam flow meter, use feedwater readings minus blowdown as the steam figure. Keep tube photos and scale thickness from the scheduled inspection when the boiler is opened, and you can match them against that year's intensity trend. Blowdown and make-up are the meter readings at the cooling tower and boiler. The Federal Energy Management Program also advises recording these with conductivity and cycles and watching the trend (DOE, n.d.). If a line has no meter of its own, fitting one comes before changing the chemical.

When comparing chemicals, purchasing can ask, alongside the price per kg, for the chemical cost per tonne of make-up and the cycles that chemical can hold. When looking at suppliers, check where the supply scope stops among make-up treatment, boiler, cooling tower and discharge. Where the scope breaks, no one is left to set make-up quality and cycles together. Also check in the quote scope whether monthly water analysis and cycles checks transfer when the chemical changes. Those two were exactly what that customer lost. My water treatment quotes list monthly water analysis and cycles checks in the same scope, beside the chemical price. Since the discharge figure also carries regeneration wastewater, only a supplier whose scope runs to discharge reads that line correctly.

Conclusion

The higher discharge charges the environmental officer asked about were what lower cooling tower cycles left at the end of the drain. The same water left its cost at the boiler as fuel intensity, and at make-up treatment as water to be made again. With a supply that takes the system from make-up treatment through boiler and cooling tower to discharge as one scope, the decision to change a chemical is made with that system's figures, and the chemical's value is read as the cost of the whole system. The higher fuel and water prices go, the more money rides on a single step of cycles. Recent quote requests, too, more often ask for the cost per tonne of make-up or the cycles that can be held instead of the price per kg. Water treatment quotes will widen the unit they compare, from one drum of chemical to one system.

At that site, the environmental officer's meter readings now go to the month-end meeting with the chemical invoice.

Sources

  • Kim, Y. S., Kim, W. C., & Kim, J. G. (2019). Bulging rupture and caustic corrosion of a boiler tube in a thermal power plant. Engineering Failure Analysis, 104, 560–567. https://doi.org/10.1016/j.engfailanal.2019.06.022
  • Ministry of Government Legislation [MOLEG]. (n.d.-a). Water Environment Conservation Act, Article 48-3, Imposition and collection of charges for public wastewater treatment facilities. Korean Law Information Center. Accessed November 2026.
  • Ministry of Government Legislation [MOLEG]. (n.d.-b). Sewerage Act, Article 65, Charges. Korean Law Information Center. Accessed November 2026.
  • U.S. Department of Energy [DOE]. (2012a). Clean firetube boiler waterside heat transfer surfaces (Energy Tips: Steam, Steam Tip Sheet #7, DOE/GO-102012-3597). Advanced Manufacturing Office. https://www.energy.gov/sites/prod/files/2014/05/f16/steam7_surfaces.pdf
  • U.S. Department of Energy [DOE]. (2012b). Minimize boiler blowdown (Energy Tips: Steam, Steam Tip Sheet #9, DOE/GO-102012-3406). Advanced Manufacturing Office. https://www1.eere.energy.gov/manufacturing/tech_assistance/pdfs/steam9_blowdown.pdf
  • U.S. Department of Energy [DOE], Federal Energy Management Program. (n.d.). Best management practice #10: Cooling tower management. https://www.energy.gov/node/849241
  • U.S. Environmental Protection Agency [EPA]. (2012). WaterSense at work, section 6.3: Cooling towers. https://www.epa.gov/system/files/documents/2023-05/ws-commercial-watersense-at-work_Section_6.3_Cooling_Towers.pdf

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.