KALTECKOREA

BlogKaltec Voices

Why the first problem, not the first delivery, decides a relationship

Type
Kaltec Voices
Published
24 November 2026
Prepared by
Jonghwan Moon
Role
Technical Staff

The first delivery happens under the best-kept conditions, so it shows little difference between suppliers; the difference shows in the first problem, after conditions drift. What the customer watches that day is the evidence used to narrow the cause and whose format the record is closed in.

Background

Of two plants that started buying a non-water-miscible grinding oil, the kind called neat oil, from us around the same time, the one that now also takes our honing oil and rust preventive is the gear plant, the one whose first problem was bigger. The gear plant ground the tooth flanks of vehicle transmission gears, and the other plant ground shafts for hydraulic parts. Both had their first problem within six months. The relationship with the shaft plant ended at the next year's renewal.

What separated the two was how that problem was handled. A relationship is decided at the first problem, not the first delivery, and what the customer watches that day is the evidence used to narrow the cause and whose format the record is closed in.

The first delivery is the day conditions are best kept

The day of the first delivery is the day both sides are most careful. Oil that passed the sample trial goes in under the trial conditions, and the supplier's engineer stands by the tank to look at the first parts together. A sample trial is usually a few weeks on one or two machines, and those weeks often include no summer and no change of grinding wheel lot. Grinding oil problems come after those conditions move one by one. In a central tank with no chiller or a tight one, tank temperature rises in summer and the oil leaving the nozzles thins out with it. A new wheel lot or a longer dressing interval changes the heat at the grinding point. When the filter starts letting more fine swarf through, the wheel loads up, and the nozzle angle shifts a little at every maintenance. After a few months, whichever supplier's oil you use, the conditions at the grinding point are not the same as on the first delivery day.

So first delivery quality is the threshold for a relationship, not the place where it is decided. Incoming inspection and sample trials guard that threshold. What the customer does not yet know is what this supplier does first when conditions move and a problem appears. You cannot see that directly until your own plant has its first problem, and can only gauge it in advance from past problems the supplier has closed at other plants.

The cause of the burn sat between the oil and the machine

The gear plant's first problem came about two months after the grinding oil change. In the nital etch inspection before shipment, dark bands appeared on the tooth flanks of some gears. That was grinding burn. It is where heat at the grinding point has re-tempered the flank and lowered its hardness, and light temper burn cannot be seen by eye before the etchant goes on. Local overheating on ground steel parts such as gears and shafts is found and graded by this chemical etch (ISO, 2017). Temper burn lowers flank hardness and cuts fatigue life, so every gear ground in that period had to be checked again.

That day the customer's quality team wrote the oil change in the cause field, because the timing overlapped. The first thing we did was sort the burned gears by grinding machine and put them in a table. Four grinders shared the oil from one central tank, but the burn appeared only on gears from one of them. If the oil were the whole cause, it should appear evenly across all four. So we compared that one machine's nozzle flow and spray angle, the number of parts ground after dressing and the wheel lot against the other three. We also checked whether the grinding allowance on the heat treatment lots fed to that machine had grown from heat treatment distortion. With samples drawn from the tank, we measured the oil's viscosity again, not at the lab reference temperature but at the tank's operating temperature.

There was a reason we looked at the nozzles first among those items. Neat grinding oil cannot carry heat away the way water does, but it cuts friction between the wheel and the flank so less heat is made. To do that, the oil has to actually reach the grinding point. A fast-spinning wheel drags a layer of air around it. If the oil from the nozzle is much slower than the wheel's surface speed, much of it is pushed aside by that air layer and scatters before the grinding point. When viscosity changes, the flow and the shape of the jet from the same nozzle change too. So nozzle settings are values to reset whenever the oil changes, and if any machine has a nozzle adjusted on its own, that machine is the one to look at first.

The cause was not on one side. It narrowed to the change in viscosity with the new grinding oil overlapping with nozzle settings left on that one machine to suit the old oil. That nozzles must be reset when the oil changes is something the side supplying the oil should raise first, and bringing the evidence until the cause is clear is also our job.

The record goes in the customer's format

The gear plant supplied gears to a vehicle maker, and the customer's quality team had to close this case with an 8D report. 8D is a problem-solving method that records eight disciplines in one report: forming the team, describing the problem, containment, root cause analysis, planning corrective actions, implementing them, preventing recurrence and recognizing the team (VDA, 2018). We set aside our own claim report form, took the fields of the customer's 8D format as they were and filled in our share. In the containment field we wrote the scope of full inspection on gears ground after the change. In the root cause field we put the burn table by machine, viscosity measured at operating temperature and nozzle flow, all with dates. In the implementation field we attached inspection results over several weeks after the nozzle was fixed to show the effect.

The root cause field of an 8D often asks two questions. Why did the problem happen, and why was it not caught earlier? The first was answered by the oil and the nozzle. The second belongs to the customer's inspection plan, but if the supplier fills in only the first and steps back, the customer's quality staff must explain the second alone. A grinding oil change is usually handled as a 4M change. We proposed, with this case's burn table attached as the basis, that for a few weeks after a change an etch inspection be done at every dressing on top of first-article inspection.

A report the supplier writes in its own format has to be copied over by the customer's quality staff, and in the copying, evidence such as where samples were drawn, the measurement dates and the temperature at which viscosity was measured drops out. A record entered straight into the customer's fields goes up to the vehicle maker as it is, and becomes the record the customer pulls out the next time oil changes on another line. The recurrence prevention field of that 8D set out a changeover procedure that measures nozzle flow and viscosity at operating temperature first whenever the oil changes. The gear plant gave us its honing oil after deciding to use that procedure on other lines too.

Putting it to work

When you propose judging suppliers by how they handle the first problem, three objections come up in the purchasing meeting.

"A supplier with no problems is better." No problems often means the relationship was short or problems went unrecorded. Conditions move within a few months, and moved conditions sooner or later cause a problem. Ask for one past problem record with the customer's name removed, and check whether the root cause field has evidence such as a table by machine or sample values, and whether the recurrence prevention field led to a real procedure.

"First delivery quality comes first." That is right, and that is why incoming inspection and sample trials exist. But first delivery quality is measured under the best-kept conditions. If two suppliers both meet the specification, the first delivery cannot tell them apart, and they separate only after tank temperature, wheels and nozzles have moved.

"Fast response is enough." The shaft plant's first problem was a call saying the paper filter had to be changed more often. That day we reviewed the lot results and sent a one-page reply the next day saying they were within specification. It was fast, but the filter kept clogging early and the cause was never narrowed. The customer's maintenance team could not find which field of their own records to put that reply in. Looking back, we should first have sorted whether what the filter caught was metal fines and wheel grit, a sticky deposit from mixing with the old oil, or water ingress. A fast first contact is essential on a site where the line has stopped. But a reply that is only fast is followed by the same problem coming back. What to look for in a first reply is whether confirmed facts, what is still unknown and what will be measured next are kept apart.

Conclusion

The first delivery shows the product, and the first problem shows how the supplier narrows a cause. That shows in whether they break it down machine by machine, whether they look at conditions on the customer's side too, and whether they close the record in the customer's fields. If your plant handles an oil change as a 4M change, settle with a new supplier which items you will measure together in the week of the change.

A supplier that filled in the first problem's root cause with evidence is one that will bring evidence first to the second problem too.

Sources

  • International Organization for Standardization [ISO]. (2017). ISO 14104:2017 Gears: Surface temper etch inspection after grinding, chemical method. https://www.iso.org/standard/70396.html
  • Verband der Automobilindustrie [VDA]. (2018). 8D: Problem solving in 8 disciplines. Method, process, report (1st ed.). VDA QMC. https://webshop.vda.de/QMC/en/8d-problem-solving-in-8-disciplines

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.