BlogKaltec Voices
Why immersion cooling fluid is a system, not a part
- Type
- Kaltec Voices
- Published
- 24 November 2026
- Prepared by
- Jonghwan Moon
- Role
- Technical Staff
An immersion tank's fluid is shared by the cables, labels and thermal pads of many servers, so what leaches out of one part changes the fluid for the whole tank. Choosing the fluid therefore means putting the materials in the tank, the pumps and filters sized to its viscosity, and years of acid number and water checks on one map together.
Background
On maintenance day, as the fluid ran off a server board lifted out of the tank, one power cable was swollen just behind its connector. The board had spent several months in a single-phase immersion tank filled with synthetic hydrocarbon fluid. A swollen jacket means the jacket has taken up fluid, and while it does, components inside the jacket also move out into the fluid.
Inquiries from sites weighing immersion cooling usually start from the fluid's property sheet. Candidates are compared on a table of specific heat, thermal conductivity, flash point and viscosity. Yet one tank holds many servers in the same fluid, and that fluid runs through the pumps and filters and back over every server. The fluid in an immersion tank is not a part you swap out. It is a system, decided as one bundle with the materials in the tank, the pumps and filters, and years of care.
Every material in the tank trades with the fluid
Public immersion requirements advise single-phase users to avoid mineral oil in favor of synthetics or esters, and cap the sulfur content of new fluid below 10 ppm (Open Compute Project, 2022). Sulfur corrodes copper, and synthetic hydrocarbons start out with almost none. The trouble is what goes into them. Server materials are chosen for air cooling, so cable jackets, labels and adhesives, thermal pads, connector housings and the rubber seals of capacitors were all made with no thought of spending years submerged in oil.
Each material trades in its own direction. A flexible PVC jacket gives up to the fluid the plasticizer added to keep it soft, hardens by that much, and cracks first where it bends. EPDM rubber, used to seal capacitors, does the opposite: it takes up hydrocarbon and swells. Label adhesive dissolves, the label falls off, and a loose label can block a flow path. Thermal pads soften or crumble, and as their ingredients wash out they pass heat less well (Kinkade et al., 2026). A swollen jacket and a hardened one look opposite, but both are traces of a material and a fluid exchanging components.
Harder still is the case where the part is fine but the fluid changes. The component test guideline notes that a server part can contaminate the fluid with no harm to its own performance, and that the contamination can damage other parts through secondary reactions such as corrosion (Kinkade et al., 2026). Plasticizer from one server's cable does not stay with that server; it mixes into the fluid of the whole tank. Dissolved polar substances shift the fluid's dielectric dissipation factor, and the immersion requirements also say to watch this value when materials are incompatible (Open Compute Project, 2022).
Before someone who has kept fish for years puts a new ornament in the aquarium, they soak it for a few days in a separate tub. Whatever comes out of it would otherwise mix into the water all the fish share. In an immersion tank the servers are the fish and the fluid is the water, so one server's materials change the water for the whole tank. That is why, before a new server model goes into a tank, I first soak pieces of its cables, labels and pads in the fluid.
Viscosity sets the pumps and filters
Once the fluid is chosen, the rest of the equipment follows its viscosity. Pump flow is set by the tank's heat load and the allowed temperature rise, and head by the resistance of the piping, filters and heat exchanger at that viscosity. In a plate heat exchanger, fluid-side heat transfer also leans heavily on viscosity, so the number of plates needed for the same heat load changes. Pressure loss through a filter is close to proportional to viscosity, so at the same flow, when the fluid cools and its viscosity doubles, filter differential pressure nearly doubles too.
Hydrocarbon viscosity climbs fast as temperature drops. A running tank is warm from the servers' heat, but the fluid is cold on the day of a first fill from drums brought in from an outdoor store in winter, or when a tank restarts after a long maintenance stop. On a cold start like this, filter differential pressure easily crosses the alarm line. Size the pump at operating-temperature viscosity, check separately that the motor does not overload at the viscosity of the coldest day, and start at low flow. Give the filter a differential-pressure bypass. Lower viscosity eases the pump, but within the same synthetic hydrocarbon family it means more light components and a lower flash point. The immersion requirements call for a flash point of at least 150°C and note that hydrocarbons with a 40°C kinematic viscosity of 20.5 mm²/s or less are classed as aspiration hazard category 1 (Open Compute Project, 2022). Pick one viscosity number, and the pump size, the flash point and the hazard labeling are set together.
The filter is also the first place to report a material problem. Tanks with mechanical circulation filter continuously, and as particles and fibers build up, dielectric strength falls (Open Compute Project, 2022). Scraps of fallen labels and crumbs of broken-down pads show in filter differential pressure before they show in fluid analysis. An element whose differential pressure climbs fast at an unchanged operating temperature usually has label scraps or pad crumbs caught in it.
Read the fluid's life from its trend
The 2022 immersion requirements call for a new-fluid acid number of 0.01 mg KOH/g or less for hydrocarbons, but set no separate acid number limit in service. In service they set minimums such as dielectric strength of 6 kV or more, resistivity of 0.20 GΩm or more and flash point of 150°C or more, and leave it to the supplier to propose which tests to run and how often (Open Compute Project, 2022). Years of care, in other words, have to be planned by someone who knows that tank, not by a table in the requirements.
Synthetic hydrocarbons dissolve very little water, so even a small excess stays as undissolved droplets and breakdown voltage falls. Esters dissolve far more water, so insulation wavers less, but that water hydrolyzes them and the acid number rises by itself. The same acid number trend reads differently by fluid family. A tank whose lid is opened takes in moisture from the air at every maintenance, which is why the immersion requirements ask for lids on open tanks to cut air exchange above the fluid surface (Open Compute Project, 2022).
Water, acid number and breakdown voltage say more as a trend than as a single reading. The trend can be read only if samples come from the same point at the same operating temperature every time. If the acid number is still low but rises with every reading, that slope is the starting point for telling whether the fluid itself is oxidizing or an acidic substance is coming from some part. Some tanks are topped up often to replace fluid carried out on servers each time they are pulled. Such tanks need the date and amount of every top-up in the same table, so a value diluted by new fluid is not misread as an improvement. Without the values from the day of filling, that trend cannot be drawn at all.
Putting it to work
At the meeting before an immersion rollout, put a cross-section of the tank on the table next to the fluid property sheet. On it, mark every material the fluid touches, place by place, and attach the test to confirm at each place.
On the server side, list cable jackets, labels and adhesives, thermal pads, connector housings and capacitor seals. For jackets and seals, record changes in weight, volume and hardness; for pads, thermal performance after soaking; for labels, whether they came off and whether the fluid changed color. For single-phase fluids, the component test guideline recommends 14 days of soaking at 80°C, comparing side by side a part left as is, a part only heated and a part soaked. The fluid is compared three ways too: as received, heated without parts, and after parts soaked in it. To look for plasticizer in the soaked fluid, liquid chromatography fits better than gas chromatography, because plasticizers boil at very high temperatures (Kinkade et al., 2026). The same guideline says it sets no qualification criteria for parts and is not a test of how many years a server will last. On the fluid side, the only question is whether it still meets the minimums of the immersion requirements after soaking. The part-to-fluid ratio in the test differs from the real tank, so next to each result the map notes how much of that part the whole tank holds, to see how large the same change becomes in the tank. The electrical performance of a part is for the server and component makers to judge, not me.
On the circulation side, list pumps and shaft seals, hoses and gaskets, filter housings and heat exchangers. For rubber on this side, first check that it is specified as NBR or FKM, suited to hydrocarbons, then attach the motor margin and filter differential pressure checked at the coldest day's viscosity, and the differential pressure at which the bypass opens. The cooling water beyond the heat exchanger stays at the edge of this map.
At the fluid's place, attach the acid number, water, breakdown voltage and color on the day of filling, with the sampling point, the check interval and the top-up record.
The map earns its keep when the server generation changes. When the parts list for a new server arrives, pick out only the places on the map that changed and soak those again; for unchanged places, reuse the earlier results. The answers for each place are scattered. The server maker knows the jacket materials, the tank vendor knows the pumps and piping, and the data center operations team knows the maintenance cycle. Gathering those answers onto one map built around the fluid, and revising it together with every generation, has to come in with the fluid. With that map, on the day someone proposes changing the fluid, you can point straight to the places to check again.
Conclusion
Choosing the fluid for an immersion tank means choosing the server materials, the pumps and years of checks along with it. As server generations turn over faster and tanks arrive a hall at a time, one fill of fluid takes in several generations of servers in turn. Each generation adds places to soak again, and in a tank where those places go unrevised, the acid number trend grows steeper.
On the day a new server comes into the tank, the fluid sits its test again, against that server's materials.
Sources
- Kinkade, B., Van Vaerenbergh, B., & Yates, S. (2026). Server component immersion material compatibility testing (Version 1.5). Open Compute Project. https://www.opencompute.org/documents/ocp-component-compatibility-testing-guidelines-v1-5-final-june-5-2026-pdf
- Open Compute Project. (2022). Immersion requirements (Revision 2.0). https://opencompute.org/documents/ocp-acs-immersion-requirements-rev-2-v1-00-pdf