KALTECKOREA

BlogKaltec Voices

Why changing one metalworking fluid changes five places downstream

Type
Kaltec Voices
Published
24 November 2026
Prepared by
Jonghwan Moon
Role
Technical Staff

A press forming oil stays on the part after forming and travels with it into welding, dimensional inspection, storage between processes, the shop air and the waste oil tank. Whether it can be changed is judged on parts that have passed every downstream process, after coupons and one line.

Background

The photo the welding lead sent showed spatter piled around the weld beads on a bracket, and where the bead had been ground away, a row of pinholes ran through the section. Neither the welding wire nor the shielding gas flow had changed. So I left the welder, went one process back to the press and leafed through the work log. Two weeks earlier, the press crew had switched the drawing oil from a chlorinated product to a chlorine-free one.

A drawing oil, that is, a press forming oil, is chosen in front of the die. The crew checks that parts form without splits or scoring, that nothing galls onto the die, and that the oiler spreads it evenly. By the press crew's standard, that is the right call. Switches from chlorinated to chlorine-free products will become more common. Among the chlorinated paraffins long used as extreme pressure additives, the short-chain ones were listed for elimination under the Stockholm Convention in 2017 and the medium-chain ones in 2025 (SSC, n.d.). The medium-chain listing carries time-limited exemptions for uses such as metalworking fluids, but the direction is set. Yet this oil stays on the part after forming and follows it to the weld, the measuring room, the waiting rack, the shop air and the waste oil tank. Changing a forming oil changes the conditions in all five places the oil reaches. Whether the change is acceptable has to be judged on parts that have passed the last process.

The weld, where the oil's amount and character show first

In arc welding, oil left in the joint breaks down in the arc heat and gives off gas. When that gas is trapped in the solidifying weld metal it becomes porosity, and when the arc wavers, spatter increases. The same amount of oil gives different results depending on where it pools. In a lap joint, where two sheets overlap, oil caught between them has nowhere to escape, and oil also collects in bends and inside flanges. Many products that aim for the same formability without chlorine raise the viscosity or add more of another extreme pressure additive. So both the amount and the character of the oil left on the part change. On galvanized steel, zinc vapor already causes porosity and spatter, so to isolate the oil's share you have to compare before and after on the same coil. On the bracket line from the opening, I started with the oiler settings and the oil pooled in the laps, and found the more viscous new oil going on thicker at the same roller setting. Once the rollers were reset for the new oil, spatter and porosity came back to their level before the change.

Spot welding is a little different. Contact resistance between electrode and sheet, and between sheet and sheet, sets the heat, so the oil film there becomes part of the welding conditions. Oil is not always bad. In spot welding of aluminum sheet, one metalworking lubricant nearly doubled electrode life, and the researchers traced this to a thinner surface oxide layer (Rashid et al., 2007). On the other hand, residue that turns sticky as it dries fouls the electrode tips, forces more frequent dressing and increases spatter. The type and amount of oil, and its state once dry, change the result together.

Brazed parts are more sensitive still. Oil that does not fully evaporate in the furnace stays as carbon residue and keeps the filler metal from spreading. That is why aluminum heat exchanger lines use evaporative forming oils that are gone before brazing temperature, and send parts into the furnace unwashed. Switching such a line to a less volatile oil breaks that premise.

Friction differences that surface in the measuring room

A drawing oil sets the friction between die and sheet, and between blank holder and sheet. When friction changes, so does how far the sheet is drawn into the die and how much it stretches. Flange length, wall thickness and the springback angle after forming then move together. The more springback a material has, as with high-strength steel, the larger the difference. So after a forming oil change, defects sometimes appear first on the measuring room's checking fixtures or CMM results. A flange angle opens slightly, or a hole position drifts off datum after trimming.

Harder still is when the difference is masked. When the press crew sees wrinkles or splits, they adjust die cushion or blank holder pressure. If that adjustment brings the dimensions back, the measuring room's records show only the pressure change, not the oil change. Friction differences between the first hits of the morning and a die heated by continuous running mix in as well. When I look at measurement records from before and after a change, I set the same day's press condition records beside them.

Changes that spread to storage, shop air and waste oil

Between the press and welding, parts wait on racks for days, sometimes weeks. What keeps rust off during that time is usually not a separately applied rust preventive but the drawing oil left on the surface. An evaporative forming oil leaves almost no film, a water-mixed drawing compound leaves moisture, and how much rust inhibitor a chlorine-free product contains varies by product. Rust shows first on the waiting racks in the rainy season, and in winter, when parts moved from a cold warehouse into a warm plant gather dew.

The shop air changes too. Low-viscosity or highly volatile oils spread as mist and vapor from high-speed presses and spray oilers, and oil left on parts burns in the weld booth and adds to the fumes. I compare oil mist values from workplace exposure monitoring before and after a change. The exposure limit the U.S. National Institute for Occupational Safety and Health recommends for mineral oil mist is 5 mg/m³ averaged over a workday of up to ten hours (NIOSH, n.d.). Vapor from evaporative forming oils is poorly captured by filter-based mist sampling, though, so it needs its own check.

The waste oil tank is where change shows last. Oil dripping from the die collects in the press pit and leaves as waste oil, and for months after a change, old and new oil mix in the pit. If a water-soluble compound comes in, oil and water form an emulsion that will not separate, and if chlorine gets in, it becomes a problem for recycling. U.S. federal rules treat used oil with more than 1,000 ppm total halogens as mixed with hazardous waste unless it can be shown that no halogenated hazardous waste was mixed in (EPA, n.d.). Metalworking oils containing chlorinated paraffins are exempt from that rule only when reclaimed under a tolling arrangement. Outside the U.S., ask your recycler what they test at pickup before the change. Also decide in advance whether to empty the pit and start fresh on day one, or run mixed for a few months.

Putting it to work

When someone proposes changing a forming oil, I split the decision into coupons, one line, and parts that have gone all the way through. A stage must pass before the next begins. At an automotive supplier, before the coupons, check whether the customer's 4M change rules cover consumables such as forming oil; if they do, first schedule the change notification and the approval sample submission.

At the coupon stage, put the actual coating weight of oil on the actual material and plating. Match it by weighing the sheet before and after wiping, to get grams per square meter. Check too that the new oil does not turn sticky over the mill rust preventive that comes on the coil. Run the same forming test with the current oil and the new one, and weld the same coupons. For spot welding, compare the usable welding current range and electrode life by the method an international standard sets (ISO, 2016). For arc welding, lay beads on the same coupons and compare spatter and porosity in the section. Stack oiled coupons in a humidity cabinet, and leave some at room temperature to see how much oil evaporates over the waiting time. If the current range narrows or porosity rises here, the oil does not go to the line.

At the one-line stage, start with one press and one die, and change no other condition in the same period. Oiler rollers or spray nozzles must be reset for the new oil's viscosity, so first measure oil weight at several points on the front, back and edges of the blank to confirm it goes on evenly. Record how much oil each shift uses as well. If the same forming takes more oil, that much more rides on to the next process. Record dimensions at the first hit and after the die warms up, die cushion pressure adjustments, and the mist around the press.

The last stage follows parts stamped on that one line through welding, brazing, measurement and the longest wait, all the way to the customer's assembly. Parts that go through washing and paint pretreatment must pass those two gates as well. I judge only after seeing the electrode dressing interval and a waste oil sample from the pit a few weeks later. These values are written by different people on different forms at each process, so I link them by part number and change date into one record. An AI that reads field data and product data together also needs that linked record to point to which process to check first at the next change.

Plan the test of parts that go all the way through together with whoever proposes the oil. Data sheets and forming test results alone do not show what will change downstream. If the proposer has records from following the same change on other lines, you start out knowing which process tends to fail first, so the coupon and one-line stages have fewer places to watch and the trial runs shorter.

Conclusion

Change one drawing oil, and the weld porosity, the flange angle in the measuring room, the rust on the waiting rack, the mist in the shop and the waste oil in the pit all change with it. Over the few years in which chlorinated paraffins are phased out, many press shops will go through this change. Those that judge it only by tests in front of the die pay for it later, downstream. Plants whose supply puts the processes before and after the press into one test plan will get through those years with less upheaval.

Choose a forming oil at the press, and judge it at the last process.

Sources

  • U.S. Environmental Protection Agency [EPA]. (n.d.). 40 CFR 279.10, Applicability. Standards for the management of used oil, Electronic Code of Federal Regulations. Accessed November 2026. https://www.ecfr.gov/current/title-40/chapter-I/subchapter-I/part-279/subpart-B/section-279.10
  • International Organization for Standardization [ISO]. (2016). ISO 18278-2:2016 Resistance welding, Weldability, Part 2: Evaluation procedures for weldability in spot welding. https://www.iso.org/standard/52317.html
  • National Institute for Occupational Safety and Health [NIOSH]. (n.d.). NIOSH pocket guide to chemical hazards: Oil mist (mineral). Accessed November 2026. https://www.cdc.gov/niosh/npg/npgd0472.html
  • Rashid, M., Fukumoto, S., Medley, J. B., Villafuerte, J., & Zhou, Y. (2007). Influence of lubricants on electrode life in resistance spot welding of aluminum alloys. Welding Journal, 86(3), 62s–70s.
  • Secretariat of the Stockholm Convention [SSC]. (n.d.). The new POPs under the Stockholm Convention. Decisions SC-8/11, SC-12/10. Accessed November 2026. https://chm.pops.int/TheConvention/ThePOPs/TheNewPOPs

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.