BlogKaltec Voices
Why the order of cleaning and lubrication matters in rail maintenance
- Type
- Kaltec Voices
- Published
- 24 November 2026
- Prepared by
- Jaemin Seo
- Role
- Technical Staff
How long grease lasts on a rail car's couplers and bogies depends on how much of the cleaner used just before it is left behind and how long the part was dried in between, so when the order slips even grease that meets its standard softens early. The softening stops when cleaner and grease are not chosen separately and washing, drying and lubrication are written into the work standard as one sequence at each point along the car.
Background
It was a few years ago, the year I first took charge of a rail depot. In the inspection shed in late spring, an inspector opened the coupler cover at the front of an electric train to show me. The grease on the contact face and lock of the tight-lock coupler had lost its shape and run, forming a thin streak along the lower edge. The buttery texture it had when applied was gone; it was oil mixed with a cloudy wetness. The grease had been on for less than two months.
At the time I suspected the grease first. New grease from the same lot had a penetration inside its specified range, and couplers at another depot using the same grease were fine. The cause lay in the few hours before the grease went on. That depot washed right up to the coupler heads with the alkaline cleaner it used for bogies, then greased while all but skipping rinsing and drying. When cleaner and grease are chosen separately, grease at a point where the order slips does not perform as its certificate says. In rail maintenance, how long grease lasts also depends on how much of the cleaner used just before it is left behind, and how long the part was dried in between.
Grease loses its structure where cleaner is left behind
Under a bogie, brake dust, iron fines worn from wheels and rails, old grease pushed out of joints and ballast dust cake together. So many depots wash bogies with an alkaline water-based cleaner that cuts grime well, applied with hot water at high pressure. Where rinsing falls short, the very property that dissolves the grime acts the same way on the grease applied next.
A researcher at a bearing maker showed this by test. Alkaline cleaner containing sodium hydroxide and acidic cleaner containing phosphoric acid were diluted in water and mixed into several greases, and both cleaners increased wear in every grease. Aluminum complex and silica greases also lost much of their structure. In the same test, plain water did the greases almost no harm. The explanation given is that the cleaner's surfactants break water into very fine droplets and spread it through the base oil, while the alkali reacts with the base oil to form new soap and damages the grease further. Even calcium sulfonate grease, whose structure held best, showed about ten times more metal-to-metal contact signals on a bearing rig run with alkaline cleaner mixed in (Zhou, 2018).
A poorly rinsed surface is worse for grease than a poorly dried one. Where plain water remains, time spent drying takes care of it, but where cleaner remains, the surfactant and alkali stay through drying and meet the grease applied next. Drying drives off only the water, so the leftover cleaner actually grows more concentrated. That is why, once rinsing is done, I hold pH paper wetted with purified water close to the gaps. If the paper turns the alkaline color, rinsing at that point is not finished. I also check whether the rinse conditions in the cleaner's technical data made it into the depot's work standard.
Set the drying time by the deepest gap
Plain water may not break a grease's structure, but it harms bearings and contact faces another way. Water remains after rinsing. The outside of a bogie frame dries in minutes, but water pools and lingers in the grooves of the coupler lock, the recess around the center plate and the channels of the axle box labyrinth seal. Tests showing that even small amounts of water in oil shorten rolling bearing fatigue life have been around for a long time (Cantley, 1977). Water trapped in grease has no way out, so while the car stands in the depot it sets rust on bearing raceways and contact faces.
How you dry is part of the order too. When blowing with compressed air, use dry air that has passed a drain and a filter, and never spin a bearing with air. Plant air taken straight from the end of a line carries condensate and oil. And write the drying time in minutes. A standard that says only "dry thoroughly" lets that line be skipped on a busy day.
In winter, steel that comes in cold off the main line gathers dew again in the warm shed, so drying also includes the wait for the steel to warm up. After that coupler episode, the depot wrote a separate winter drying time, longer than the summer one.
The center plate and the coupler take over a washed surface
The order slips most easily at two points. One is the center pivot, which the shop floor calls the center plate. The center pin of the bolsterless bogies common on today's electric trains sits in a rubber bushing and takes no grease. But the center plates of bolster bogies and freight cars carry the body's weight and slide on curves, so they are greased. In heavy maintenance, where the bogies come out, the grease goes on just before the body is lowered back, and since this is a recess in the middle of the bogie, wash water and cleaner easily run down and pool there. Once the body is seated, nobody sees inside until the next teardown. At one teardown we scooped thinned, broken-down grease out of a center plate that had been greased with cleaner still pooled in it.
The other is the coupler. It hangs not on the bogie but on the underframe at each end of the body, so its sequence runs outside the bogie work. There is guidance that has the contact face and lock of a tight-lock coupler cleared of old grease and freshly greased at each set inspection interval. An exposed coupler with no cover takes cleaner every time it passes through the body washer, so if the schedule sends the same car through the wash line the day after greasing, the new grease is gone within a day.
At both points, grease goes onto a surface just as the crew before washed it and handed it over. At a depot where a contractor or another crew does the washing and in-house inspectors do the greasing and assembly, the rinse check and drying easily end up with no line of their own in either work standard. The person who washed records that it was washed, and the person who greased records that it was greased. The few hours in between are in nobody's record.
Putting it to work
Walk once around a single car, write down at each point what to look for in washing, drying and lubrication, and the empty lines in the work standard show up. I carry the standard, start at the front coupler, pass the front and rear bogies, and finish at the rear coupler. On a lead car the front is a tight-lock coupler; the semi-permanent couplers between middle cars are lubricated differently, so fill their lines by their own guidance.
At the front coupler, write the body wash schedule into the washing line. Check when the next body wash is, and move the line so the grease goes on after that wash and its drying are done. Whether old grease was cleared first, and whether pH paper was held to the lock grooves, also go on that line.
At the two axle boxes of the front bogie, write the covers around the seals into the washing line. Keep the high-pressure nozzle from aiming at the labyrinth gap, and wash with the area around the front cover covered. In the drying line, write how long the labyrinth channels were blown out with dry air. If the bogie has a center plate, its drying time is the longest. Wipe out and blow off the water and cleaner pooled in the recess, and in winter confirm the steel has warmed before greasing. In the lubrication line, write the grease name, the amount and the time of application, so the gap from the end of washing shows on one line. On a motor bogie, write the breather cover into the gearbox washing line. Wash water that gets into the breather goes into the gear oil.
Fill the same lines once more at the rear bogie and rear coupler, and the round is done. On the rinse check and drying lines, the person applying the grease, not the crew that washed, leaves the time and their name. Only when the person taking over checks do those few hours enter the record.
Once these lines are filled, proposals to change the cleaner or the grease read differently. A proposal to change the cleaner should come with results from mixing it with the grease in use, and with the changed rinse and drying times. A proposal to change the grease should come with how that grease holds up on a surface carrying today's cleaner. A proposal that fills only one side leaves an empty line at every point in the standard. Which car comes in when and must leave within how many hours is set by the inspection schedule. Whether a rinse check and drying time fit inside those hours gets counted out on the standard together with whoever runs that schedule.
Conclusion
A grease certificate assumes a clean, dry surface. A surface carrying cleaner, a gap not fully dry, a body washer the car passes the day after greasing: all of these sit outside that assumption. So a proposal to change the cleaner should bring the drying time and the grease lines with it. The supply that can answer it is the one that sees even the few hours between washing and lubrication as one sequence and tests the two products together.
Solvents dry as they evaporate, but water-based cleaners add rinsing and drying, so in the 2030 standards of depots that switch to water-based cleaning, a rinse check and a drying time each get a line between washing and lubrication.
The cleaner the bogie is washed, the more the grease relies on the few hours after the wash.
Sources
- Cantley, R. E. (1977). The effect of water in lubricating oil on bearing fatigue life. ASLE Transactions, 20(3), 244–248. https://doi.org/10.1080/05698197708982838
- Zhou, X. (2018). Effects of detergent (water) contamination on grease performance [Extended abstract]. STLE Tribology Frontiers Conference 2018. https://www.stle.org/TribologyFrontiers/TribologyFrontiers/Program/Extended_Abstracts_Pages/Control_ID_2976210.aspx