A common reason die casting release agent trials end in a fail is that a switch back to the old product mid-trial goes unrecorded, and the dilution ratio, spray time and die condition change along with the product, leaving a trial that cannot be judged. A trial that can be judged is one whose baseline, single changed variable, period, pass criteria and reversions are written on one sheet before the start and set together at the die.

Background

It was the third day of a release agent sample trial at an aluminum die casting plant. When I went to the spray unit beside the die, the concentrate hose feeding the dilution tank was plugged back into a drum of the old release agent. On the night shift before, aluminum had soldered to a core pin and the machine had been stopped twice, so the operator had switched back to the familiar product to keep output up. The work log said not a word about it.

Two weeks later the plant's trial report read "soldering up, fail." That report cannot tell you whether the new release agent suits that die or not, because it leaves out up to which shot it was the new product, from which shot the two were mixed, and what else changed in between. In the plants I have visited, more sample trials ended in a fail because they could not be judged, like this one, than because the product really fell short. A common reason sample trials fail is that they were not set up to be judged.

The trial a switched-back release agent erased

Release agent trials run on dies in production. Few plants can free a die just for a trial. So the line still has to meet delivery during the trial, and when trouble comes the operator acts first. One soldering event means stopping the machine and scraping the aluminum off the die face, and production stops meanwhile. For a night shift operator, switching back to the old product is the fastest way back onto a known road. I do not think that call was wrong.

The problem is that the switch back leaves no record. Switch back and then return to the new product, and for a while the dilution tank and lines carry a mix of the two, and films of both products layer on the die face. The report lumps the whole trial period together as the new product's result, and counts the soldering from the mixed period against the new product as well.

Look closer and it is not even clear yet that the night's soldering was the new product's fault. With a core pin, maintenance first checks that the pin cooling water is flowing properly. When a cooling line clogs and the pin runs hot, aluminum sticks to it easily whatever the release agent. The cycle or melt temperature that night may also have been off. Unless you decide in advance how many soldering events count as normal variation, one night of soldering becomes the verdict on the whole trial.

Conditions that change along with the product

Changing release agent looks like changing one product, but in practice several conditions move together. If the new product's TDS recommends a different dilution ratio from the current one, the proportioner setting changes. When samples arrive in small containers, they are sometimes mixed by eye in a separate container instead of going through the line's proportioner. Then the ratio wobbles with who mixes it and on which day. So I record the dilution ratio each shift, not as the set value but as a refractometer reading of fluid caught in front of the nozzle. The factor that converts a refractometer reading to concentration differs by product, so get the new product's factor first.

Spraying both leaves a film on the die face and cools the die, and how much the die cools depends on where and how the spray lands (Sabau & Dinwiddie, 2008). When the dilution ratio changes, the same spray leaves a different share of solids on the face and of water that boils off carrying heat away. So die temperature and film thickness can differ even at the same spray time. I have also seen plants cut spray time at the start of a trial to shorten the cycle while they were at it.

Look at a hot spot right after spraying and there are places where the fluid cannot settle on the face but bounces off in beads and runs down. No white film is left there. When the die face is hot enough, a vapor layer forms under the spray droplets and keeps the liquid off the face. This is the Leidenfrost effect (Bernardin & Mudawar, 1999). Where no film has settled and the die surface passes a critical temperature, the molten aluminum reacts with the iron in the die steel and soldering forms (Han & Viswanathan, 2003). If a change in spray pattern or cycle has made one hot spot hotter, the soldering there may be the work of temperature. Release agents designed to form a film on even hotter dies are being developed (Cuadrado et al., 2025), but even those cannot show a difference if the nozzle is not aimed at that hot spot.

In a trial where the product, dilution ratio, spray time and die temperature all changed together, if soldering drops no one knows why, and if it rises the product takes the blame.

The film on the die face and the state of the die

Even after you empty and rinse the tank and lines so only the new dilution comes out of the nozzle, the previous product's film built up on the die face wears off little by little over many shots. The shots in that first stretch are results of the changeover. The state of the die itself is also a trial condition. Die faces roughened by long use showed a higher Leidenfrost point (Zabala et al., 2018). A film settles on a hotter face there, so even at the same die temperature, how well the film settles depends on surface condition. The same release agent settles differently on a die fresh from polishing and on one with spreading heat checks. If the die is pulled mid-trial for polishing or resurfacing, the die before and after are different dies. So before setting a trial date, I ask how many shots that die has run since its last maintenance.

A baseline measured in another month

The new product's numbers are compared with the numbers from a baseline period. If those come from last winter's records or another shift's log, the two periods differ in much more than the release agent. If the water that cools the die and core pins runs through a cooling tower, it cannot get colder than the outdoor wet-bulb temperature (Buecker, 2017). In summer, when the wet-bulb temperature is high, cooling water is less cold at the same flow, and the pins take the next shot hotter than in winter. Soldering forms where the die face passes a critical temperature (Han & Viswanathan, 2003), so comparing a winter baseline with a summer trial mixes the release agent and the cooling water temperature into one number.

Shifts are the same. Day and night differ in operators and in how many times the machine was stopped and reheated. I have seen a summer trial that used last winter's records as its baseline. A baseline is comparable only if it is measured just before the trial, in the same shift order as the trial, with the current product.

Putting it to work

Before sending samples, I fill in a one-page trial report with the customer first. With this page filled in, the trial gives a verdict, pass or fail.

The top line, baseline conditions, records the die and spray conditions the current product runs under. First the die number and shots since last maintenance, the alloy and the cycle time. Then the spray program number, air blow time, nozzle check date, pin cooling water flow and inlet temperature, and the die temperature controller setting.

Next come measuring methods and samples. For concentration, note the refractometer reading and the dilution water. For hot spot temperature, image the same spot with a thermal camera twice, before and after spraying, at the same moment after each die opening. Note the sample drum's lot number and storage condition too. A water-based release agent can split its emulsion if it freezes and thaws in an outdoor warehouse in winter. Beside that, put the numbers measured with the current product over the same length of time just before the trial: die cleanings for soldering per shift, defects by type, and concentrate use per shot. Without these numbers, the new product gets compared with the operators' impressions.

The line below holds only one changed variable. Usually it is the product with the dilution ratio its TDS recommends. The product is made to be used at that ratio, so a trial at the old ratio does not test the product. Leave the spray program and cycle as they are. If the new product needs a different spray time or nozzle aim, finish the product-only trial first, then schedule a second trial that changes the spray. The period line starts from the shot counter reading after the tank and lines are emptied and cleaned. Write down in advance how many shots of the first changeover stretch to leave out of the verdict. Set the end by shot count rather than date as well, and plan it so no die maintenance falls inside.

Fill the pass criteria line with numbers before the start. Stops for soldering do not rise above the baseline by more than a set count. Cleanings for drag marks and for residue built up on the die face stay within a band set the same way. Surface stain and porosity rejects stay within the baseline range. Nothing goes wrong in later steps such as painting or impregnation. Last, write the name of the person who will sign the verdict.

The last line is reversions. I do not tell people not to switch back. The line must not stop, and the person on the spot should decide whether to switch back. Instead I ask them to write down the time, the shot counter reading and the reason right there, and if they go back to the new product, the period is counted fresh from that shot. A report with this line blank and one with a 0 in it are different. The first means no one was watching. The second means someone was.

Filling in this page together takes someone from the supplier standing at the die before the trial. Whether to empty the tank, whether to leave the spray program alone, which hot spot to watch: none of that is settled by sending a sample drum. When you request samples, decide along with the product name who will fill in this page with you, and the same product gives a trial that can be judged.

Conclusion

When a sample trial ends in a fail, I reread the report before striking the product off the list. In a retrial with the conditions set right, the same product has caused less soldering than the baseline period. As more release agents aim at hotter dies, trials will more often need not just a product swap but a second trial that resets the spray.

If any one line is blank, whether baseline conditions, changed variable, period, pass criteria or reversions, that trial's fail is not yet a result.

Sources

  • Bernardin, J. D., & Mudawar, I. (1999). The Leidenfrost point: Experimental study and assessment of existing models. Journal of Heat Transfer, 121(4), 894–903. https://doi.org/10.1115/1.2826080
  • Buecker, B. (2017, July 12). Cooling tower heat transfer fundamentals. Power Engineering. https://www.power-eng.com/operations-maintenance/cooling-tower-heat-transfer-fundamentals/
  • Cuadrado, N., Vidales, E., da Silva, M., Wajana, W., Muntada, L., Navarro, A., Beltran, L., & Vilaseca, M. (2025). Ester-based lubricant and anti-Leidenfrost additive solutions on aluminum high-pressure die-casting applications. Lubricants, 13(1), 32. https://doi.org/10.3390/lubricants13010032
  • Han, Q., & Viswanathan, S. (2003). Analysis of the mechanism of die soldering in aluminum die casting. Metallurgical and Materials Transactions A, 34(1), 139–146. https://doi.org/10.1007/s11661-003-0215-9
  • Sabau, A. S., & Dinwiddie, R. B. (2008). Characterization of spray lubricants for the high pressure die casting processes. Journal of Materials Processing Technology, 195(1–3), 267–274. https://doi.org/10.1016/j.jmatprotec.2007.05.021
  • Zabala, B., Igartua, A., Scarpis, V., Timelli, G., Girot, F., & Nevshupa, R. (2018). Multiparametric study of Leidenfrost point and wettability of lubricants on high-pressure die-casting dies. International Journal of Thermal Sciences, 125, 66–73. https://doi.org/10.1016/j.ijthermalsci.2017.11.014

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.