From press lines to export packaging for sea freight
Korea's automotive parts industry is a vertically integrated supply chain of Tier-1 and Tier-2 suppliers built around the OEMs.

What is the auto parts industry?
Auto parts manufacturing mass-produces the components that make up a finished vehicle, such as body panels, suspension parts, drive shafts and brake and steering parts. The same parts are made over and over under the same conditions while dimensions, surfaces and corrosion resistance must stay the same every time, so reproducing process conditions without drift is essential. Steel and aluminum sheet is formed, gears and shafts are machined and then heat treated, so chemistry runs across the whole line, from forming and cutting lubrication to cleaning, pretreatment and painting, joining and sealing.
On a high-volume line, a small drift in one process sends defects to the next process in batches. Rust or stains that form while machined parts wait for the next step lead to poor paint adhesion, and export volume faces corrosion risk again at sea. So beyond the performance of individual products, wait times between processes, storage conditions and formulation change history must be managed together. Auto parts manufacturing does not stop at supplying chemicals that meet specification; it comes with technical support that resets formulations whenever line conditions change.
- Global automotive warranty costs in a year$58B
- 01
Sheet metal forming by press, drawing and stamping
Steel and aluminum sheet is drawn and stamped in presses into panel and bracket shapes. Too little lubrication causes galling and die wear, and excess oil adds cleaning burden. Choose forming oil by lubricity, application amount and ease of removal.
- 02
Cutting and turning
CNC machines cut parts such as chassis components, drive shafts and valve bodies to shape. Concentration drift unsettles surface roughness and tool life, and defects pass to the next process in batches. Choose a cutting fluid by machining performance, concentration control and spoilage resistance.
- 03
Quenching and tempering heat treatment
Gears, shafts and bearings are heated, quenched and tempered to give hardness and toughness. Aged or contaminated quench oil cools unevenly and causes hardness variation and distortion defects. Choose a quench oil by cooling characteristics, flash point and degradation checks.
- 04
In-process part storage
Machined parts sit for days to weeks before cleaning and painting. Fine corrosion formed meanwhile later shows as poor paint adhesion. Choose in-process rust preventive by protection period and actual wait time.
- 05
Cleaning
Residue of cutting fluid, forming oil and rust preventive oil is removed with alkaline or solvent cleaners to set conditions for pretreatment. Oil building up in the tank lowers cleaning power. Choose cleaner by cleaning power, takt time and flash rust after rinsing.
- 06
Phosphate and chromate-free conversion coating
Zinc phosphate or chromate-free conversion coating is applied to cleaned surfaces to form the base for paint adhesion and corrosion resistance. Film thickness variation is where paint defects and corrosion start. Choose pretreatment by film properties and treatment conditions.
- 07
Painting
Primer, base and clear coats are layered by spraying, dipping and electrodeposition. Booth temperature and humidity out of range cause bubbles and drying defects. Choose paint by film performance, color and drying conditions.
- 08
Sealing and structural bonding of fasteners and joints
Adhesives, sealants and threadlockers are applied to panel seams, battery pack housings and fasteners to reinforce stiffness and airtightness. Moving on before cure is complete causes bonds to delaminate or leaks. Choose products by bond strength, cure time and substrate combinations.
- 09
Transport and storage
Machined and painted parts are sent to distribution centers or overseas customers. At sea, salt and temperature changes create condensation inside packaging. Choose rust-protective packaging by protection period, package type and destination country regulations.
Regulation and certification
IATF 16949
The quality management standard for automotive parts suppliers. Changing the cutting fluids, cleaners or rust preventives used in production normally goes through customer approval and change control.
IMDS
The International Material Data System, through which carmakers collect the material make-up of parts. Coatings, adhesives and sealants that stay on a part are reported in it, so supplier composition data is needed.
ELV Directive
The EU directive on end-of-life vehicles, which restricts lead, mercury, cadmium and hexavalent chromium. Rust-preventive coatings and surface treatments for parts are chosen free of restricted substances such as hexavalent chromium.
REACH
The EU regulation on the registration, evaluation, authorisation and restriction of chemicals. Chemical products used on parts exported to Europe are checked for substances of very high concern and registration status.
FAQ
We want to change cleaners. Do we need to recheck paint adhesion too?
It is better to recheck. A different cleaner changes the nature of residue and surface wettability, so even when cleaning itself is fine, the following pretreatment film can form differently. In automaker specifications, cleaning, pretreatment and painting are approved as one package, so changing the front affects the back.
This is also why deciding on wastewater conditions alone is hard. Before changing, run an adhesion test on parts from the same line, and confirm that free alkalinity and temperature of the pretreatment bath are in the same range as before; this makes it easier to separate causes.
Stains appear when machined parts sit for a few days. Is it the rust preventive oil?
It may not be the rust preventive oil alone. Covering leftover cutting fluid from the previous process with a protective film can let discoloration continue underneath, and humidity at the storage spot and floor condensation also play a part.
Applying a thicker film does not tend to last. Leftover cutting fluid trapped underneath only delays the problem, and the amount to remove in cleaning before painting increases, adding load to the pretreatment bath. In-process rust protection causes fewer problems when matched to conditions for removal in the next process rather than to protection strength, and the right choice also depends on whether the wait is days or weeks.
The cutting fluid tank smells. Should we treat it as time to replace?
It is better to separate the causes before replacing. Odor is often a sign of microbial growth, and if it gets worse after circulation stops, such as over the weekend, sediment and tramp oil at the bottom of the tank are the likely cause.
Some sites keep repeating fluid changes. If the cause remains in the tank, new fluid spoils at the same rate, adding only replacement cost and waste treatment burden. If concentration has dropped below the control range, topping up can restore it; if odor returns on the same cycle, it is better to address tank cleaning and tramp oil removal first.
How far does corrosion resistance go after switching to chromate-free plating?
Results vary with formulation and process conditions. Chromate-free systems meet required corrosion resistance in some cases when material and treatment conditions fit, but changing only the chemical under the old conditions often forms a thin film that appears to perform worse.
Switching is not just changing chemicals; it means scheduling the work to prove performance equivalence again. Long-term tests such as salt spray are tied to new vehicle development schedules, so if test volume and line downtime do not align, the switch may not happen that year. It is safer to set bath temperature, treatment time and rinse water quality to the new chemical's recommended range before starting tests.
Only export shipments show rust on opening. How should we set up packaging?
Temperature changes during the voyage may have created condensation inside the packaging. Rust preventive oil alone rarely covers these conditions, so the usual setup layers VCI packaging and adds paper or emitters depending on part shape.
Going only toward heavier packaging, however, creates other problems at the destination. Packaging fumigation, quarantine and substance content declarations apply by export country, so more materials also mean more customs documents. Setting the packaging specification with rust protection and destination regulations side by side means less backtracking later.
Why does validating a new cutting fluid take so long?
It is often less about doubting performance and more about seeing what shifts after the change. Cutting fluid carries over not only to tool life and surface roughness but also to cleaning, rust protection and paint adhesion, and short tests cannot confirm spoilage behavior after seasons change or concentration control in summer.
So narrowing the test scope is the faster way to shorten the period. Rather than changing the whole line at once, matching comparison conditions on one machine with the same material and the same tools reduces disputes over whether a difference came from the fluid or another variable.
Hardness is uneven after heat treatment. Should we suspect the quench oil?
Aging or contamination of quench oil is sometimes the cause. When cooling performance drops, the difference in cooling rate between the inside and outside of the load grows, and hardness varies even within the same batch.
Deciding to change the fluid on hardness tests alone is difficult, though. In automaker specifications, heat-treated parts are subject to both hardness and metallurgical structure tests, so changing quench oil often means resubmitting micrographs as well. Even when reviewing a change, sorting out loading method and agitation conditions first reduces the chance of testing twice.
Bubbles form in the same spot in painting. Do we need to change the paint?
Residue from earlier processes is the more likely cause than the paint. Components left from pretreatment or cleaning can escape during drying and create defects repeatedly in the same area. Changing paint triggers approval testing again, so when the defect location is fixed, the usual order is to look at earlier processes first.
Checking whether defects gather on certain shapes narrows it down. If they repeat only in recesses or near welds, look first at rinsing and drying; if they appear evenly across the booth, look first at humidity and temperature control.