From slurry mixing to rust protection for pack shipment
The battery industry mass-produces cells for electric vehicles, energy storage systems and information devices.

What is the EV and battery industry?
The battery industry makes the cells, modules and packs that go into electric vehicles and energy storage systems. From making electrodes and assembling cells to filling electrolyte and bundling packs, processes must run while keeping the inside, where electrochemical reactions take place, sealed off from the outside environment. Because aluminum foil, copper foil, active materials, separators and casing metals are handled together, rolling and cutting lubrication, cleaning that leaves no residue, insulation and sealing, and rust protection are each required under different conditions at each stage.
The biggest risk in batteries is invisible contamination. Moisture, trace ionic impurities and residue transferred from equipment change cell life and safety. So chemicals that touch the cell must come with evidence on moisture content, ion concentration, material compatibility and residue composition for every delivered lot, alongside performance data. In batteries, chemistry is a material that leaves traces inside the cell, so not only performance but also those traces must be checked together with the cell maker.
- Scrap rate in lithium-ion cell production5-12%
- 01
Slurry mixing
Cathode and anode active materials are mixed with conductive additives, binder and solvent into a uniform slurry. Agglomerated particles or bubbles carry viscosity variation into coating thickness variation. Choose additives by dispersing, defoaming and batch-to-batch repeatability.
- 02
Electrode coating and drying
Slurry is coated onto aluminum foil for cathodes and copper foil for anodes, then solvent is driven off at high temperature. Drying too fast pushes binder to the surface, cracking the electrode or delaminating it from the current collector. Choose primers and cleaners by adhesion, moisture content and residue.
- 03
Calendering
Dried electrodes are pressed by roll press to bring density and thickness to specification. Active material sticking to the roll surface leaves repeated scratch marks on the electrode. Choose rolling oils and cleaners by friction reduction, electrolyte compatibility and residue.
- 04
Slitting and notching
Calendered electrodes are cut to width and tab shapes are cut and formed. Burrs left on cut edges become starting points for internal shorts. Choose cutting fluids by cut edge quality, tool life and antistatic performance.
- 05
Stacking and winding
Cathode, separator and anode are stacked or wound in turn into the electrode assembly. Misalignment beyond the separator margin leads to internal shorts. Choose equipment fluids by lubrication, low residue and static behavior.
- 06
Tab welding and case insertion
Current collector tabs are welded, and the assembly is inserted into a steel or aluminum casing and sealed. Incomplete cleaning and drying after casing forming seals moisture and oil inside. Choose forming and rust preventive oils by formability, rust protection and removal by cleaning.
- 07
Electrolyte filling and sealing
Organic electrolyte is filled into the casing and sealed in a dry room kept at low dew point. Unstable fill volume or incomplete sealing lets moisture in and shortens cell life. Choose cleaners and sealants by residue, sealing reliability and moisture control.
- 08
Formation, aging and degassing
Cells are charged and discharged repeatedly at high temperature and voltage to form the initial film, aged, then degassed. Cells not fully degassed move on holding gas and later show swelling. Choose formation equipment fluids by cooling performance, insulation and thermal stability.
- 09
Module assembly
Dozens of finished cells are connected with busbars and fixed in an insulating case. Crushed or shifted insulating members cause shorts between cells and busbars. Choose adhesives and sealants by bond strength, sealing and insulation.
- 10
Pack assembly and protection
Modules are fixed in the pack casing, controls, wiring and cooling are integrated, and waterproofing and flame protection are applied. Galvanic corrosion appears where aluminum housings meet steel brackets. Choose a sealant by waterproofing, cure conditions and flame standards.
- 11
Final inspection, packing and transport protection
Finished packs are verified for performance and safety, then packed for long transport. Vibration and humidity changes in transit start corrosion at fastening points and exposed metal. Choose rust preventives and packaging by protection period, protection strength and packing method.
Regulation and certification
UN 38.3
The UN test criteria lithium batteries must pass before they can be transported. Adhesives, thermal materials and insulating coatings in cells and packs are fixed as part of a configuration that has passed vibration, shock and thermal tests.
UN ECE R100
The UN vehicle regulation setting safety requirements for electric powertrains and rechargeable energy storage systems. Pack sealants and thermal or insulating materials are validated within a pack design tested for thermal propagation and fire resistance.
UL 94
The UL standard that tests the flammability of plastic materials and assigns ratings such as V-0 and HB. Potting compounds, adhesives and insulating materials in battery packs are checked for the required rating.
IATF 16949
The quality management system standard for the automotive industry. Chemicals used in battery cell and pack processes are also supplied through production part approval (PPAP) and change notification.
FAQ
Will new rolling oil stop recurring electrode scratches after calendering?
It could be the rolling oil, but it is often caused by active material sticking to the roll surface. In that case, marks repeat in the same place even with a different fluid, and if they repeat at regular intervals across the width or disappear only right after the roll is wiped, the roll is the more likely cause.
If roll contamination is the cause, cleaning intervals and release conditions are addressed first, and trying to cover it with more release agent can also increase residue transferred to the electrode. Looking at the friction properties and residue of the rolling oil is not too late after the roll surface condition is sorted out.
We fear equipment fluids may transfer onto electrodes. How far must we check?
Even trace transfer can change cell characteristics, so in calendering and assembly, compatibility data for electrolyte and active materials is often reviewed. Performance data alone usually does not finish the review.
Where there is direct contact, residue composition data is normally needed; where cleaning sits in between, confirming residue after cleaning is the usual scope. Adding another cleaning step, however, brings new moisture and cleaner residue, so choosing a fluid that transfers less often makes management simpler than covering it with cleaning.
How should dry room chemicals be chosen differently from a regular line?
First, whether they bring moisture in themselves. In a space kept at low dew point, hygroscopic ingredients can make the dew point fluctuate from the material side rather than the equipment, and in that case no amount of equipment inspection finds the cause.
Package size and handling after opening also matter. For materials used in small portions, time left open can be the actual moisture entry route, and if the staging area before entry is outside the dry room, materials sometimes come in already holding moisture.
We hear cell maker vendor registration is long. What is the sequence?
Data review usually comes first. Only after ion and moisture certificates and compatibility data for electrolyte and active materials are checked does it move on to trial on the line. Leading with performance data alone sometimes stops at this stage.
Next come small-volume trial application and field test history, then internal approval with those results attached, after which volume increases. The closer a stage is to cell performance, such as electrolyte filling or formation, the longer the validation period in between, so the adoption schedule is often set by the length of the process rather than by product performance.