Why do anti-seize bolts end up loose or overtightened?
- Type
- Application notes
- Published
- 23 November 2026
- Prepared by
- Jonghwan Moon
- Product group
- Corrosion Special Purpose
Anti-seize coated bolts are often tightened to the same torque as dry ones, but the compound changes friction in the threads and under the head, so the same torque can produce a very different clamp force. What actually lies behind it can be torque that ignores the changed nut factor, overtightening to yield, whether the compound went on the threads or the bearing face, reused bolts, or vibration, and sometimes two or more at once.
Background
At a routine inspection the torque wrench goes on, and some nuts turn before the wrench reaches its setting. On the same machine, other bolts kept turning at assembly without the wrench ever seeming to bite, and when they come out later the threads have stretched. Loose bolts lead to flange leaks, vibration and parts working free; overtightened bolts stretch or break and damage gaskets and threads as well. Either way the equipment has to stop for retightening, and on a joint under pressure it becomes a safety matter.
What tightening by torque is really after is the force that clamps the joint, the clamp force. Torque and clamp force are usually linked by T = KFd, where T is torque, F is clamp force, d is bolt diameter, and K, the nut factor, is set by friction between the threads and friction at the bearing face where the bolt head or nut sits. The friction coefficient can range from 0.04 to 1.10 depending on materials and lubricant, so torque table values must be adjusted for any difference between the friction used to calculate the table and the friction actually present (Barrett, 1990).
Anti-seize changes exactly this friction. In tests on a lubricated high-strength bolt, clamp forces came out nearly 70% higher than the commonly used formula predicted (Seegmiller, 1978). So the same torque gives very different clamp forces depending on what was applied, where, and how many times the bolt has been tightened, and loose bolts and overtightened bolts can come from the same cause.
In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: confirm whether the torque values in the bolting standard assume dry, oiled or anti-seize coated bolts, then set the compound actually used, where it went, whether the bolts were new and the wrench calibration records alongside that assumption.
Hypothesis 1: changed nut factor
This hypothesis comes first when a torque table built for dry bolts is used unchanged on anti-seize coated bolts. It is the same, in reverse, when a torque lowered for another lubrication condition is used with a higher-friction compound, or when the compound changes and the torque value does not. The torque table in the maintenance manual was drawn up years ago for dry bolts, and from this shutdown on, the hot flanges are to get anti-seize. The fitter sets the wrench to the value in the table, and the wrench clicks as it always does.
Where the torque goes explains why. Only part of the torque from the wrench stretches the bolt; the rest is spent overcoming friction in the threads and at the bearing face. When the compound lowers friction, less is lost to it, and the same torque gives more clamp force. Fastener design guidance says torque table values must be adjusted to the actual friction, and for a lubricated condition such as silver-plated nuts coated with wax it cuts the dry torque values in half (Barrett, 1990). Tests have also found that the actual nut factor can differ greatly from textbook values (Taylor & Morrison, 2006), so a factor taken from a table does not guarantee the clamp force. Conversely, if the actual friction is higher than was assumed when the torque was lowered, clamp force falls short and the bolt loosens easily.
The nut factor has to be measured to be known. The standard torque/clamp force test records tightening torque, clamp force and thread torque together, and derives the nut factor and the thread and bearing friction separately (ISO, 2005). On site, build a test joint from the same bolt, nut and washer with the actual compound, measure clamp force with a load-indicating washer or an ultrasonic elongation gauge, and compare it with the clamp force the bolting standard aims for. If the standard does not state a lubrication condition, that is the first thing to correct.
Once the factor is shown to differ, recalculate the torque table. Set a nut factor for each compound from tests or supplier data, work the torque back from the target clamp force, and record the lubrication condition and product name in the table. Put a rule in the bolting standard that a change of compound means recalculating the table, and make sure tables for dry bolts and for anti-seize are not used side by side on the same site.
Hypothesis 2: tightened past yield
Overtightening happens when anti-seize bolts are tightened to dry-bolt torque, when there is a habit of going a little past the setting to be sure, when an impact wrench with coarse torque control is used, and when a small bolt is tightened with a large wrench. A fitter slips an extension bar over the wrench to make sure one last time and leans on it. The wrench swings further than usual, and at some point the resistance in the hand stops building as it did. At the next inspection those bolts are loose.
Within its elastic range a bolt clamps the joint like a stretched spring, in proportion to how far it has stretched. Past the yield point, though, it stretches permanently and loses clamp force as service loads or temperature changes come and go. Bolts are sometimes tightened close to yield for vibration resistance, but past yield the bolt stretches and unloads, and since the exact yield torque cannot be known without instrumentation, tightening close to yield is not advised. The same document explains that the proof load listed in the literature is usually 75% of theoretical yield, set so that torque measurement errors do not yield the bolt (Barrett, 1990). The actual proof load is a test load the bolt must carry without permanent set, which the standard sets separately for each property class, so take the figure from the table for that class (ISO, 2013). A test report prompted by overtightened bolts on an International Space Station joint likewise noted that too high a preload could overload the bolts together with service loads, while too low a preload could let the joint gap and leak (Taylor & Morrison, 2006).
Yield leaves marks on the bolt. Compare the length of a removed bolt with a new one, and check with a thread gauge whether the threads have stretched and whether the bolt has necked in the stretch of thread that was engaged. A nut that will not run down by hand but sticks partway points to stretched threads. Tightening a test joint with the same bolt and compound while recording torque and clamp force together also shows at what torque yield begins (ISO, 2005).
Replace yielded bolts with new ones rather than reuse them. Work the target torque back from the property class and the clamp force the joint needs, and, as design guidance does, allow in advance for the scatter in clamp force that comes with the tightening method, so the bolt stays clear of yield (VDI, 2015). Calibrate wrenches at fixed intervals, and set rules banning extension bars and final tightening with impact wrenches. Measuring bolt elongation instead of torque is more accurate on joints where clamp force matters, but it costs more, so choose according to how critical the joint is.
Hypothesis 3: thread or bearing face
If clamp force varies from bolt to bolt at the same torque, look at whether where the compound goes differs from person to person. Typical cases are compound on the threads only with the bearing face under the nut or bolt head left dry, compound only on the bearing face, and turning the bolt head one day and the nut the next. Some days two fitters split a large flange between them. One brushes compound carefully over the threads and under the nut; the other dabs a little on the thread end and turns from the bolt head. Both wrenches have the same setting.
The friction the torque must overcome lies in two places, the threads and the bearing face, so the clamp force from a given torque depends on which of them is lubricated. A study that applied oils, greases and solid-film lubricants separately to the threads, the nut, under the bolt head and to the joint surface under the head reported that lubrication has a significant effect on friction and on the torque-tension relationship (Zou et al., 2007). In tests on International Space Station bolts, nut-tightened bolts gave similar nut factors whether or not the nut bearing face was lubricated separately, which the report explains by lubricant on the threads readily migrating to that face. Bolts turned at the head with a dry bearing face under the head scattered widely, with nut factors from 0.18 to 0.56, against 0.10 to 0.21 when the face under the head was lubricated too (Taylor & Morrison, 2006). A bolt whose turned-side bearing face is dry tends to fall short of clamp force at the same torque.
Ask the fitters directly where the compound actually went, and when a bolt comes out, see whether there is compound on the threads and on the bearing face. Which side was turned is often missing from work records, so start recording it from the next job. In the laboratory, the test that measures thread and bearing friction separately shows how far the nut factor moves with each application point (ISO, 2005).
If the application point made the difference, specify in the work instruction where the compound goes. Have it applied thin and even to the threads and to the bearing face on the turned side, under the nut if the nut is turned and under the head if the head is turned, and fix which side is turned for each joint. The test report also recommends joint-specific testing for critical joints where the bearing face cannot be lubricated (Taylor & Morrison, 2006). A one-page work standard with photographs kept by the toolbox cuts down on each person applying it differently.
Hypothesis 4: reused bolts
This hypothesis gathers joints where the same bolts are taken out and refitted at every maintenance, habits of applying fresh compound over old without cleaning or not reapplying at all, and zinc-plated bolts used many times. An inspection cover opened every quarter is a good example. The same bolts come out and go back in, and the threads carry last time's compound, mixed with dust and set grey, but they are tightened to the same torque as before. The first few times there was no trouble.
Repeated tightening and loosening changes friction. In tests that tightened a lubricated high-strength bolt to the same torque again and again, relubricating the head area before each application kept clamp force within 3%. With lubricant applied only at the start, 50 applications brought clamp force down to 39% of the first value, with a rapid fall over the first 20 (Seegmiller, 1978). The test was set up to see lubricant being squeezed out with each tightening, and relubricating the bolt brought most of the clamp force back. A study that tightened zinc-plated bolts, nuts and washers repeatedly found significant wear on the threads and the nut bearing face and a marked change in friction coefficient, which affects clamp force and the integrity of the joint (Eccles et al., 2010).
How many times the bolt has been tightened is the first thing to establish. Find in the maintenance records when the bolts on that joint were last replaced, and look on threads and bearing face for scoring, worn marks, stripped plating and old compound left hard. Tightening new and reused bolts on a test joint with the same compound and the same torque and comparing clamp force puts a number on what reuse costs.
If reuse is the cause, make it a rule to clean off old compound and apply fresh every time a bolt is refitted. Fastener design guidance notes of one metal-loaded compound that a new application is needed each time the fastener is installed (Barrett, 1990). Set a limit on how many times each bolt may be reused, and replace bolts with damaged threads or stripped plating, and bolts on joints where clamp force matters, with new ones.
Hypothesis 5: vibration loosening
Look at vibration when bolts keep loosening on equipment that shakes continuously, such as pump and compressor bases, fans, vibrating screens and vehicles, or where joint faces creep a little with each heating and cooling cycle. The less clamp force a bolt has, the stronger the effect. Say a line was drawn across nut and bolt on the side plates of a vibrating screen after assembly. A few weeks later the lines on some nuts are out of step, and the joint face around those bolts shows marks of fine metal dust.
Vibration undoes a bolt through sideways slip at the joint face. A classic study of loosening under vibration set out a theory of how bolts loosen by themselves when the joint shakes and slips sideways, together with a transverse vibration tester to measure it (Junker, 1969). Later experiments described loosening in two stages. First, cyclic plastic deformation of the material lets clamp force drop without the nut turning; then the nut actually backs off. In the same study, below a certain amplitude of sideways displacement at the joint, loosening did not continue, and the larger the clamp force, the higher that limit, though a large clamp force also raised the chance of the bolt failing in fatigue (Jiang et al., 2004). In finite element analysis, localised slip over part of the contact let loosening occur even at relatively low shear loads (Pai & Hess, 2002).
Anti-seize is tied in here in two ways. One is that a shortfall in clamp force left by the earlier hypotheses shows itself under vibration; the other is friction itself. A study that varied thread and bearing friction coefficients by changing coating and lubrication, with phosphate and oil and with a molybdenum disulphide solid film, compared loosening rates under transverse load using a model fed with those friction coefficients and with tests (Housari & Nassar, 2007). Friction, then, is one of the variables that set the loosening rate, so when anti-seize coated bolts go on vibrating parts, measures against loosening need looking at separately from clamp force.
Whether the line has shifted is the easiest clue. If the line is intact but the torque wrench shows the bolt has gone slack, think of the first stage, where clamp force dropped without the nut turning; if the line has moved, the nut has turned. Metal dust and wear marks on the joint face are traces of sideways slip, so measure the equipment's vibration and compare it with other joints. On vibrating joints, reaching the target clamp force comes first, and design guidance also notes that a higher preload raises resistance to vibration (Barrett, 1990). On top of that, consider locking parts or another fastening method, choosing ones whose effect has been shown by a method such as the transverse vibration test.
Finding the cause
There is no need to dig through all five hypotheses at once. Clear first what records and people can answer straight away. Which lubrication condition the torque table assumes, what was applied where, and whether the bolts were new can all be learnt from the records and a talk with the fitters. Measuring bolt length and threads goes along with removing the bolts, and clamp force tests and vibration measurements come after that.
The direction of the symptom is the first fork. If bolts stretch and break or nuts will not turn by hand, look first at a nut factor problem, where torque was not lowered to match the lower friction, and at overtightening and yield. If clamp force varies from bolt to bolt right from assembly, look at differences in application point and turned side; if all was well at assembly but joints weaken with each maintenance, suspect reuse. If it happens only on vibrating equipment, with marking lines shifting over time, it is vibration loosening.
If that still does not settle it, compare on a test joint. Build joints from the same bolt, nut and washer, tighten them to the same torque with no compound, with compound on the threads only, and on threads and bearing face, and measure clamp force; compare new and reused bolts the same way. Change only one thing at a time, or there is no telling what moved the clamp force.
The final check is made on the real equipment. Confirm clamp force at a few joints tightened to the revised torque table and work standard, with load-indicating washers or elongation measurement, and draw marking lines to see that nothing loosens before the next inspection. The job is done only when the figures sit within the target clamp force range and the lines are unchanged at the next inspection.
The hypotheses are bound up with one another. Torque that ignores the nut factor leads to overtightening and yield, and a yielded bolt loses clamp force and loosens under vibration. A reused bolt that was not relubricated loses clamp force at the same torque (Seegmiller, 1978), and it too becomes vulnerable to vibration. In such cases, put the torque table and application rules right first and replace yielded bolts, then treat only the joints that still loosen with vibration measures, because while clamp force is unsettled the effect of locking parts cannot be compared fairly.
Limits and cautions
Nut factor, target clamp force, torque values and reuse limits differ with bolt material and property class, diameter, surface finish, compound and joint design, so numbers follow the bolt and compound suppliers' data and the plant's bolting standard, and on joints covered by rules, such as pressure vessels, piping flanges and rotating machinery, those rules come first. Recalculating a torque table or changing the tightening method should be confirmed by the design engineer.
Safety matters too. Handle anti-seize with gloves and eye protection as the SDS directs. Do not loosen or retighten bolts on a joint that still holds pressure or heat; stop the equipment, release the pressure and lock it out first. A yielded or damaged bolt can snap suddenly during tightening, so do not use extension bars, and stand so that your weight is not thrown in the direction the wrench turns.
Sources
- Barrett, R. T. (1990). Fastener design manual (NASA Reference Publication 1228). NASA Lewis Research Center. https://ntrs.nasa.gov/citations/19900009424
- Eccles, W., Sherrington, I., & Arnell, R. D. (2010). Frictional changes during repeated tightening of zinc plated threaded fasteners. Tribology International, 43(4), 700–707. https://doi.org/10.1016/j.triboint.2009.10.010
- Housari, B. A., & Nassar, S. A. (2007). Effect of thread and bearing friction coefficients on the vibration-induced loosening of threaded fasteners. Journal of Vibration and Acoustics, 129(4), 484–494. https://doi.org/10.1115/1.2748473
- International Organization for Standardization [ISO]. (2005). ISO 16047:2005, Fasteners — Torque/clamp force testing. https://www.iso.org/standard/27788.html
- International Organization for Standardization [ISO]. (2013). ISO 898-1:2013, Mechanical properties of fasteners made of carbon steel and alloy steel — Part 1: Bolts, screws and studs with specified property classes. https://www.iso.org/standard/60610.html
- Jiang, Y., Zhang, M., Park, T.-W., & Lee, C.-H. (2004). An experimental study of self-loosening of bolted joints. Journal of Mechanical Design, 126(5), 925–931. https://doi.org/10.1115/1.1767814
- Junker, G. H. (1969). New criteria for self-loosening of fasteners under vibration (SAE Technical Paper 690055). SAE International. https://doi.org/10.4271/690055
- Pai, N. G., & Hess, D. P. (2002). Three-dimensional finite element analysis of threaded fastener loosening due to dynamic shear load. Engineering Failure Analysis, 9(4), 383–402. https://doi.org/10.1016/S1350-6307(01)00024-3
- Seegmiller, H. L. (1978). Torquing preload in a lubricated bolt (NASA Technical Memorandum 78501). NASA Ames Research Center. https://ntrs.nasa.gov/citations/19780021508
- Taylor, D. M., & Morrison, R. F. (2006). Faying surface lubrication effects on nut factors. In Proceedings of the 38th Aerospace Mechanisms Symposium. NASA. https://ntrs.nasa.gov/citations/20060028253
- Verein Deutscher Ingenieure [VDI]. (2015). VDI 2230 Blatt 1, Systematic calculation of highly stressed bolted joints — Joints with one cylindrical bolt. Beuth.
- Zou, Q., Sun, T. S., Nassar, S. A., Barber, G. C., & Gumul, A. K. (2007). Effect of lubrication on friction and torque-tension relationship in threaded fasteners. Tribology Transactions, 50(1), 127–136. https://doi.org/10.1080/10402000601105490