BlogApplication notes
Why does acid number rise and filters plug after switching to biodegradable hydraulic oil?
- Type
- Application notes
- Published
- 23 November 2026
- Prepared by
- Jonghwan Moon
- Product group
- Equipment/Service Lubricants
Changing filters more often is the usual response when they plug after a switch to biodegradable hydraulic oil, but if whatever is making the acid and deposits is still there, the plugging comes back. What actually lies behind it can be ester broken down by water, leftover mineral oil and its deposits, vegetable oil thickened by oxidation, additives that reacted with water, or microbes that have grown, and these can interlock and appear together.
Background
Machines working near water, or on sites with strict environmental requirements, have been switched to biodegradable hydraulic oil. For the first few weeks nothing happens, then the filter differential pressure alarm starts going off often and the acid number on the oil analysis report starts to climb above the new-oil value. Changing the filter quietens things for a while, but the change interval keeps getting shorter.
Plugged filters cost more than the elements and the downtime. As differential pressure keeps rising, a filter with a bypass valve opens it and unfiltered oil circulates, and acid in the oil corrodes metal. A hydraulic fluid that is not stable in water can form acidic and insoluble contaminants that lead to corrosion, valve sticking and viscosity change (ASTM International, 2021). Biodegradable lubricants cost more than comparable mineral oil products (EPA, 2011), so changing the charge again and again without knowing the cause adds to the bill as well.
Biodegradable hydraulic oils fall into four categories by base oil: triglycerides, which are the vegetable oil type, synthetic esters, polyalkylene glycols, and polyalphaolefins with related hydrocarbons (ISO, 2023). The first two are ester structures, an acid joined to an alcohol, so in contact with water that bond can come apart again, and vegetable oils carry many double bonds that react readily with oxygen. Biodegradable also means that microbes can break the oil down completely into water, carbon dioxide and mineral salts, and a lubricant in frequent contact with water is more likely to undergo some biodegradation (EPA, 2011). A property designed to make the oil break down easily can, inside a machine, become a weakness.
In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: confirm which of the four categories the current oil belongs to and check the flushing records from the changeover, then log the acid number and water trends and the appearance of what the plugged filter caught, and compare them with the oil's technical data sheet, the TDS, and the supplier's changeover guidance.
Hypothesis 1: ester hydrolysis
On machines where water gets into oil based on vegetable oil or synthetic ester, look first at hydrolysis, the reaction in which water cuts the ester bond. Think of gates and dam equipment, port and ship deck machinery, construction machinery that is washed often, and machines whose outdoor tanks collect dew as temperatures swing between day and night. Take the hydraulic tank of a riverside gate operator. Water droplets cling to the underside of the tank cap, yet the oil looks clear, and every report shows water content and acid number rising side by side.
An ester bond is formed when an acid and an alcohol join and give off water, so with enough water and heat it turns back into acid and alcohol. At room temperature vegetable oil can dissolve about 1,200 ppm of water, against about 60 ppm for mineral oil, so it holds far more water while still looking clear; with water present, triglycerides hydrolyse to free fatty acids, and the reaction runs faster at higher temperatures (Murru et al., 2021). The same paper explains that the free fatty acids formed can act to promote oxidation. This is why holding back hydrolysis is listed among the jobs of additives in oils based on vegetable oil and synthetic ester (EPA, 2011). A hydraulic fluid that is not stable in water forms acidic and insoluble contaminants together, so the acid raises the acid number and the insoluble matter builds up on the filter (ASTM International, 2021).
Clear to the eye does not mean free of water, so always look at water as a number. The coulometric Karl Fischer test can measure water in oil from the mg/kg level upwards (ASTM International, 2025), and acid number is measured by potentiometric titration (ASTM International, 2024). Measure both on the same sample, overlay the trends, and see whether acid number follows rises in water. If the TDS reports a hydrolytic stability test, which heats the fluid with water and tracks acid change, compare against that value too. On site, look for the ways water gets in as well: the tank breather, cap gaskets and the route taken when washing.
Once hydrolysis is the likely cause, closing off the water comes first. Fit a desiccant breather that traps moisture, replace cap and inspection-port gaskets, and keep wash water away from the tank. Reduce water already in the oil with a method that also removes dissolved water, such as a vacuum dehydrator. If acid number has passed the supplier's change limit, removing water will not remove the acid, so change the oil, and on machines where water cannot be avoided, choose a formulation more resistant to hydrolysis with the supplier.
Hypothesis 2: mineral oil left behind
If filter plugging bunched in the first weeks after the changeover, suspect what the old oil left behind. This happens when only the tank was emptied and the mineral oil left in cylinders, hoses and accumulators stayed as it was, when only one flush was done, or when mineral oil was topped up by mistake during maintenance. One example is the first month after a machine that had long run on mineral oil was converted over a weekend. Filter differential pressure climbs much faster than usual, and black, sticky deposits sit between the pleats of the removed element, closer in colour to the sludge on the old tank floor than to the new oil.
Vegetable oils and synthetic esters mix well with mineral oil, but they loosen and dissolve the deposits mineral oil left behind, so filters can clog in the period just after changeover, and more frequent filter changes are advised during that time (EPA, 2011). The same source states that polyalkylene glycols do not mix with mineral oil, so with that type, leftover mineral oil can itself become a separate layer or sludge. Changeover guidance recommends repeated flushing to bring residual mineral oil down to a low share, keeping mineral oil in the biodegradable fluid below 2% (ISO, 2016). With much mineral oil left, the biodegradability and performance of the mixture also drift from what the TDS promises.
Start by lining up the dates. In the filter change records, see whether the shortening of the interval coincides with the changeover date and whether intervals lengthen again afterwards. Look at the colour, smell and feel of the deposits on the removed filter, and if needed send them to a laboratory to tell oxidation products of the mineral oil from breakdown products of the new oil. Have the laboratory measure residual mineral oil in the used oil, and check the number of flushes and the result of each in the changeover records. If the oil is a polyalkylene glycol type, also check the tank bottom for a separated layer.
Leftover mineral oil and old deposits go only once the changeover is finished. If residual mineral oil exceeds the guidance share, flush once more following the supplier's guidance, and for a few months after the changeover set a shorter filter change interval, returning to the normal one as the differential pressure record allows. Plugging in this period should fade with time, so if it carries on without easing, move on to the other hypotheses. In the workshop, separate top-up containers for mineral oil and biodegradable hydraulic oil by colour and label.
Hypothesis 3: oxidised plant oil
Oxidation becomes the issue on machines whose base oil is a vegetable oil type and whose oil runs hot for long periods. Think of farm and forestry machines running non-stop in high summer, mobile machines with small coolers, machines still on the change intervals used for mineral oil, and circuits carrying a lot of air. Picture opening the hydraulic tank of a farm machine that has harvested all summer. The oil has turned a deeper brown than new and feels sticky on a finger, and the tank walls and filter surface are coated with a thin, varnish-like film.
In the fatty acid chains of vegetable oil, the hydrogen on a carbon lying between two double bonds comes away most easily, and the radical left behind meets oxygen to form peroxides, carrying a chain reaction forward. As oxidation goes on, carboxylic acids build up and raise the acid number, these acids link aldehydes and ketones into larger molecules that raise viscosity, and in the end insoluble oligomers, sludge and varnish-like deposits form. The more double bonds, the lower the temperature at which oxidation starts: for methyl esters, 177°C for oleate, 139°C for linoleate and 117°C for linolenate (Murru et al., 2021). Oxidation has been treated as the key weakness of vegetable oil lubricants (Fox & Stachowiak, 2007), and vegetable oils oxidise more at high temperature and need more frequent oil changes, whereas high-oleic varieties are less susceptible (EPA, 2011).
Hydrolysis and oxidation both raise acid number, but oxidation pulls viscosity up as well. Follow viscosity at 40°C, colour and smell alongside acid number, and check whether viscosity has risen clearly above the new-oil value. In the oil temperature record, see whether hot-running periods coincide with jumps in acid number. A sticky, dark film on the filter surface and tank walls may be oxidation deposits, and a laboratory can confirm whether it consists of oxidation products of the oil. Commissioning a test of how much antioxidant remains at the same time helps judge the oil's remaining life.
If oxidation is confirmed, reset heat and change intervals first. Clean or enlarge the cooler to bring oil temperature down, fix the suction side where air is drawn in, and set the change interval by this oil's acid number and viscosity trends rather than by the mineral oil schedule. Remove deposits on tank walls and pipework before filling with new oil. For machines where running temperature cannot easily be lowered, review with the supplier a high-oleic vegetable oil or an oil based on an oxidation-resistant synthetic ester; research has also continued into raising the oxidation stability and low-temperature behaviour of vegetable oils with additives (Erhan et al., 2006).
Hypothesis 4: additives and water
When a gel-like film forms on the filter after water got in, the additives may be where it started. Think of formulations containing metal-bearing anti-wear or rust inhibitors, oil in which additives from different products have mixed through top-ups, and drums of oil stored long in the cold. Consider the day a machine that stood outdoors through the rainy season is started again. Within hours the filter differential pressure alarm sounds, and the outer surface of the removed element carries a thin, slippery, gel-like layer, while the oil itself has hardly changed in colour or smell.
Some hydraulic oil additives react with water. Zinc dialkyldithiophosphate, long used as an anti-wear additive, hydrolysed at the interface with water into acidic products such as thiophosphoric acid, phosphoric acid and alkyl phosphates (Burn et al., 1995). The acids formed add to the acid number, and the insoluble reaction products can build up on fine filters. Hydraulic systems use fine filters, so passing through them in the presence of water is an important requirement for hydraulic oil, and a standard test measures it. That standard, however, covers mineral-based oils and states that it may not suit oils relying on insoluble or partly soluble additives (ISO, 2025). When using the test on a biodegradable hydraulic oil, agree the conditions with the laboratory and the supplier first.
What the filter caught is the key. Send the element to a laboratory for elemental analysis of the deposit, to see whether elements from additives, such as zinc, phosphorus and calcium, are concentrated there. Comparing additive elements in the used oil with the new oil at the same time confirms whether the picture of additives leaving the oil and building up on the filter holds. Check whether the water trend and the timing of plugging coincide, and whether the TDS reports a filterability test with water present. If in doubt, commission a test comparing filterability of the new oil with water deliberately added.
Additive precipitation needs both water removal and a tidy-up of the oil. Close the water route and dehydrate, and if top-ups have mixed in another product, bring the charge back to one product. Oil that has lost much of its additive does not recover its performance once dry, so agree with the supplier whether to change it. For machines where water cannot be avoided, choose with the supplier a formulation with good filterability data in the presence of water, and lay outdoor drums on their side or cover them so rainwater does not seep in past the bungs.
Hypothesis 5: microbial growth
Microbes grow on machines where water lies on the tank floor and the oil stays warm but not hot for long periods. Think of gates, snow-clearing equipment and farm machines that stand for months each season, plant with large tanks and slow circulation, and pipe ends where oil hardly flows. Suppose a snow-clearing machine laid up from spring through summer is started for the first time in autumn. Opening the tank drain lets out water along with brown or black slimy lumps, there is a sour or rotten smell, and the filter is coated with slick slime.
Bacteria and fungi need water, food, oxygen, a suitable temperature and dark, slow-flowing places to grow; the oil supplies the food, the hydraulic tank provides such a place, and the key among them is water (Motes, 2024). The same report notes that 500 ppm of water emulsified in the oil is enough and that the favoured temperature range is 24 to 49°C, and explains that microbes form a biofilm, a mat of cells and their secretions, in the thin water layer on the tank floor, with by-products that foul filters in fuel systems. The same report, however, finds microbial contamination of hydraulic systems rarer than of fuel systems, and considers that long running at 50 to 65°C can damp or prevent large-scale growth. If the oil is a vegetable oil type, triglycerides split into free fatty acids when water and fat-splitting enzymes are present (Murru et al., 2021), so microbes also open a route to a higher acid number.
Where the sample is drawn is half the check. Oil drawn from the running circuit alone can easily miss the problem, so with the machine stopped, take the water layer and the oil just above it separately from the tank drain. Look for slime, lumps and smell, and ask a laboratory to culture for bacteria and fungi. Examining the deposit from a plugged filter under a microscope shows whether fungal threads or bacterial clumps are present. Also check the oil temperature record for long spells in the warm range and whether the machine stood idle for long.
Once microbes are confirmed, removing water underpins every remedy. Drain water from the tank floor regularly, and drain, clean and refill tanks and pipework that carry a biofilm. Use only a biocide the supplier has confirmed meets biodegradability and environmental criteria and does not harm oil performance. Before laying a machine up for long, drain the water and fit a desiccant breather, and before restarting, check a bottom sample first.
Finding the cause
Three of the five hypotheses start with water, so measuring water and acid number first is a quick route. Measure water, acid number and viscosity at 40°C on the same sample, and put the changeover date and filter change records in one table. Keep plugged filters in a bag rather than throwing them away, and take a tank bottom sample when the machine can be stopped. Elemental analysis of deposits and culture tests come after that.
The combination of numbers points the way. Plugging that bunched just after the changeover and is now easing points to leftover mineral oil and old deposits, and acid number following water upwards while viscosity holds steady points to ester hydrolysis. Acid number and viscosity rising together as the oil darkens, in step with hot-running periods, suggest vegetable oil oxidation. A gel-like film on the filter just after water got in, with additive elements down in the used oil, points to additives reacting with water, and slime and smell in the bottom water layer after a long lay-up point to microbes.
What the filter caught is direct evidence for telling the hypotheses apart. Black, sticky matter rich in mineral oil oxidation products indicates old deposits; a dark, varnish-like film indicates oxidation; a gel concentrated in additive elements indicates additive precipitation; and visible fungal threads or bacterial clumps indicate microbes. If one element shows several of these, weigh their shares from the laboratory results.
If that still does not settle it, run comparison tests. Commission a hydrolytic stability test, which heats a new-oil sample with water and tracks acid change, and a filterability test with water added; on site, compare acid number and filter change intervals over the same period between machines where the water route has been closed and machines where it has not. Change only one thing at a time, and compare afterwards using values measured by the same laboratory and method.
These hypotheses drive one another. Water hydrolyses the ester, makes additives react and feeds microbes, and the free fatty acids from hydrolysis can help oxidation along (Murru et al., 2021). So when several hypotheses seem to overlap, deal with water first, clear out the changeover deposits next, and then look again at whatever acid rise and plugging remain, because while water is present the effect of any other remedy cannot be separated out.
Limits and cautions
Change limits for acid number and water, the allowable share of residual mineral oil, flushing procedures and filter ratings differ by oil category, product and machine, so numeric decisions follow the oil TDS, the supplier's changeover guidance and the machine maker's standards. Where biodegradability and environmental certification must be maintained, check with the supplier and against the certification criteria that mixed oil, biocides or top-up oil do not break those conditions. Deposit analysis and microbial culture are laboratory work.
Handle oils, additives and biocides with the protective equipment in each product's safety data sheet, the SDS, and when handling water and deposits from a tank with microbial growth, wear gloves and eye protection and keep them off the skin. Handle tank bottom samples and filters only with the machine stopped and pressure released. Even for biodegradable hydraulic oil, do not dispose of spilt oil, waste oil or plugged filters as general waste; follow local rules.
Sources
- ASTM International. (2021). ASTM D2619-21, Standard test method for hydrolytic stability of hydraulic fluids, beverage bottle method. https://store.astm.org/d2619-21.html
- ASTM International. (2024). ASTM D664-24, Standard test method for acid number of petroleum products by potentiometric titration. https://store.astm.org/d0664-24.html
- ASTM International. (2025). ASTM D6304-25, Standard test method for determination of water in petroleum products, lubricating oils, and additives by coulometric Karl Fischer titration. https://store.astm.org/d6304-25.html
- Burn, A. J., Gosney, I., Warrens, C. P., & Wastle, J. P. (1995). Phosphorus-31 NMR investigation of the heterogeneous hydrolytic decomposition of zinc(II) bis(O,O-dialkyl dithiophosphate) lubricant additives. Journal of the Chemical Society, Perkin Transactions 2(2), 265. https://doi.org/10.1039/P29950000265
- Erhan, S. Z., Sharma, B. K., & Perez, J. M. (2006). Oxidation and low temperature stability of vegetable oil-based lubricants. Industrial Crops and Products, 24(3), 292–299. https://doi.org/10.1016/j.indcrop.2006.06.008
- Fox, N. J., & Stachowiak, G. W. (2007). Vegetable oil-based lubricants: A review of oxidation. Tribology International, 40(7), 1035–1046. https://doi.org/10.1016/j.triboint.2006.10.001
- International Organization for Standardization [ISO]. (2016). ISO 15380:2016, Lubricants, industrial oils and related products, class L, family H, hydraulic systems: Specifications for hydraulic fluids in categories HETG, HEPG, HEES and HEPR. Replaced by ISO 15380:2023. https://www.iso.org/standard/66277.html
- International Organization for Standardization [ISO]. (2023). ISO 15380:2023, Lubricants, industrial oils and related products, class L, family H, hydraulic systems: Specifications for hydraulic fluids in categories HETG, HEPG, HEES and HEPR. https://www.iso.org/standard/82967.html
- International Organization for Standardization [ISO]. (2025). ISO 13357-1:2025, Petroleum products: Determination of the filterability of lubricating oils, Part 1: Procedure for oils in the presence of water. https://www.iso.org/standard/86969.html
- Motes, D. T., III. (2024). Bacteria and fungi contamination in fuel and hydraulic oil (Report No. HDIAC-BCO-2023-444). Homeland Defense & Security Information Analysis Center, U.S. Department of Defense. https://hdiac.dtic.mil/wp-content/uploads/2023/07/AD1227134_Bacteria-and-Fungi-Contamination-in-Fuel-and-Hydraulic-Oil.pdf
- Murru, C., Badía-Laíño, R., & Díaz-García, M. E. (2021). Oxidative stability of vegetal oil-based lubricants. ACS Sustainable Chemistry & Engineering, 9(4), 1459–1476. https://doi.org/10.1021/acssuschemeng.0c06988
- U.S. Environmental Protection Agency [EPA]. (2011). Environmentally acceptable lubricants (EPA 800-R-11-002). Office of Wastewater Management. https://19january2021snapshot.epa.gov/sites/static/files/2020-02/documents/vgp_environmentally_acceptable_lubricants1.pdf