BlogApplication notes
Why does a centralized lubrication system starve some points?
- Type
- Application notes
- Published
- 23 November 2026
- Prepared by
- Jonghwan Moon
- Product group
- Equipment/Service Lubricants
Raising pump pressure or lengthening the lube cycle is the usual response when a centralized lubrication system starves some points, but with the blockage or sticking left in place, the dry points stay dry and the lines and distributors just carry more strain. What actually lies behind it can be deposits in the lines, a stuck distributor, oil thickened by cold, air trapped in the lines or pressure lost along long lines, and sometimes two or more at once.
Background
At the morning check, one slideway on a machine tool is dry, and a hand run along it feels fine scratches. The other slideways and ball screws on the same machine glisten with oil, and the lube pump's pressure gauge and alarms show nothing unusual. The system is cycling on schedule, yet a few points are not getting oil.
Points that miss oil wear without a sound. Dry slideways and bearings run with more friction and heat, scoring and seizure follow, machining accuracy drops, and in the end the machine stops for parts to be replaced. Depending on the system design, a single blockage at a distributor can cut oil flow to the whole system and leave every bearing without lubrication (Graco, 2024). Because the system is there so that nobody has to oil by hand, a dry point tends to go unnoticed until something fails.
A centralized lubrication system has a pump send oil down a main line to distributors that split it into set amounts for each point. How much a distributor delivers per cycle depends on conditions such as oil viscosity, ambient temperature, distributor inlet pressure, pressure differences between outlets, air in the system and cycle speed (Graco, 2024). Oil flowing slowly through a narrow tube loses more pressure the higher its viscosity, the longer the tube and the smaller its bore (White, 2016). So oil goes first where resistance is low, and points whose resistance has risen, or that lie far away, are the first to run dry.
In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: mark the dry points on the piping diagram to see whether they gather under one distributor, note the pump pressure, oil temperature and the last inspection and maintenance records, and compare them with the oil's technical data sheet, the TDS, and with the conditions in the lube system manual.
Hypothesis 1: deposits in the lines
The older the system, the more builds up inside its lines and distributors. Look at this hypothesis first on machines whose tank has only ever been topped up, never drained, where the tank lid is left open or chips and dust abound, where lines run close to hot parts, and where different oils have been mixed in top-ups. Suppose a tank that has not been emptied for years is opened. A brown sediment lies on the bottom, and a sticky film covers the pump suction strainer and the distributor inlet screens.
Deposits begin as oil oxidises in contact with heat and air. The products of oxidation are dissolved in the oil at first, but beyond the limit of what can dissolve they settle out as a solid film called varnish. Solubility falls as temperature falls, so this film keeps building up in cooler places and can plug strainers, inlets and small orifices (Hong & Jang, 2023). Distributors and metering parts in a centralized lubrication system have small holes and clearances for the oil to pass, so the same amount of deposit cuts flow there before it does in a larger pipe. Solid particles such as dust and steel fines that get into the tank speed up the blockage further.
Blockages can be found by opening the system in the order the oil flows. With the pressure relieved, remove the pump outlet filter, the distributor inlet screens and the metering parts of the dry points in turn, and look for sticky film, sediment or particles. Take a sample of tank oil, look at its colour and sediment, and send it to a laboratory for the solid particle count as a standard contamination code (ISO, 2021). How much varnish-forming material has built up can be gauged with a standard test that filters the oil through a membrane and measures the colour left on it. That test was written for turbine oils, though, so read its values as a trend on the same system (ASTM International, 2021).
With deposits confirmed, clearing only the blocked part means it blocks again soon. Drain the tank and wipe the bottom, flush the lines with clean oil, replace blocked metering parts and filters, and fill with fresh oil that matches the TDS. One manufacturer's instructions call for refilling the system only with oil filtered to a set cleanliness level (Graco, 2024). Keep the tank lid closed, top up with one oil only rather than mixing, and change the tank oil at regular intervals so that oxidation products do not accumulate.
Hypothesis 2: stuck distributor
If dry points gather under one distributor block, look at that block. Suspect it when a machine restarts after a long stand, on systems carrying varnish or particles, where distributors have gone a long time without service, and after a change to a different oil. Take the day a machine restarts after a long holiday. All five points fed by one distributor block are dry, and that block's cycle indicator pin does not move even with the pump running.
A progressive distributor, whose pistons move one after another to divide the oil, is built so that each piston must finish before the next can move. So when one outlet is blocked, that piston cannot complete its cycle, pressure backs up through the distributor and the whole block stops. The manufacturer's instructions state that such a blockage raises pump pressure above normal and that, depending on system design, it can cut off flow altogether (Graco, 2024). Pistons stick when something lodges in the clearance. Varnish is known to make turbine servo valves stick, and distributor pistons with fine clearances can go the same way (Hong & Jang, 2023). In systems with a separate metering part for each point, only the point served by the stuck part goes dry.
If there is a cycle indicator pin or proximity switch, check first whether it moves while the pump runs. Pump pressure running higher than usual, or a high-pressure alarm, leans towards a blockage. Put a hand pump on the block inlet and push oil through to see whether each outlet delivers, then loosen the outlet lines one at a time to tell whether the block itself or a line after it is blocked. The manufacturer advises pressure-testing distributor blocks every year or after a set number of running hours, replacing seals and distributors as needed (Graco, 2024).
If the block has stuck, replacing it is often surer than stripping and cleaning, and either way the source of the varnish or particles that made it stick must be removed too. After replacement, bleed air from block and lines and confirm oil at every outlet before running the machine. For machines that will stand a long time, set a routine of running a few manual lube cycles before restart to confirm the pistons move.
Hypothesis 3: thick oil in the cold
Oil thickens as it cools. This hypothesis fits winter mornings in unheated plants, machines standing outdoors or near doors, the first start after a weekend, and systems filled with an oil of higher viscosity than the manual calls for. Picture the first start on a Monday morning after a frost. A few slideways furthest from the pump are dry, but in the afternoon, once the plant has warmed up, oil appears at the same points again.
Viscosity rises steeply as temperature falls, and for petroleum oils this relation can be calculated from standard equations and charts (ASTM International, 2020). An oil's viscosity grade is set by its viscosity at 40°C, so even within one grade the actual viscosity on a cold morning can be far above the grade number (ISO, 1992). The pressure lost in a narrow tube grows in proportion to viscosity, so with the pump delivering the same pressure, less oil reaches the far points (White, 2016). As noted earlier, what a distributor delivers per cycle also varies with viscosity and ambient temperature, so on a cold morning oil tends to fall short in both the lines and the distributors.
Logging temperature alongside the dry points is the heart of the check. At first start, measure the tank oil temperature and the air temperature around the furthest lines, and compare whether the same points get oil at warmer times of day. Match the grade filled against the grade the manual specifies, and estimate the viscosity at that morning's temperature from the TDS viscosities at 40°C and 100°C using the standard chart. If the TDS pour point, the lowest temperature at which the oil still flows, is close to that morning's temperature, the oil moves only sluggishly in the lines (ASTM International, 2017). If there is a pressure gauge, see whether pressure runs higher than usual on cold mornings.
If cold is the cause, warm the oil or change to one that suits. Choose with the supplier, within what the machine maker allows, a lower viscosity grade or an oil whose viscosity changes less with temperature, and move or lag the tank and lines out of cold draughts. On cold days, set a warm-up routine that runs the machine idle and puts a few lube cycles through before machining. Raise pump pressure only within component ratings, and sort oil and temperature before that.
Hypothesis 4: trapped air
Air gets in easily once the system has been opened. Suspect air first after a filter or distributor has been changed, after lines have been laid or repaired, after the tank has run dry and been refilled, and on systems with a loose joint on the pump suction side. A typical case is the day after a missed low-level alarm let the pump draw on an empty tank for a while. The tank is refilled and the system restarted, yet some points are still dry, and small bubbles file past in a clear section of line.
Air bubbles in oil sharply lower how stiffly the oil resists pressure, its effective bulk modulus, by an amount that depends on the quantity, size and distribution of the bubbles and on how fast the mixture is compressed (Gholizadeh et al., 2014). In a line carrying air, part of each pump stroke goes into compressing air instead of moving oil forward. If pressure rises slowly, or never rises enough to work the distributor, the metering pistons cannot push out their full set amount each stroke. The manufacturer likewise treats distributor output as affected by air in the system and directs manual air purging after maintenance or repair, before the machine runs again (Graco, 2024). Air trapped at high points in the lines does not leave on its own, and how quickly an oil releases air is measured separately with a standard test (ASTM International, 2019).
Air shows itself when bled. Loosen the outlet line at a dry point and push oil through with a hand pump or a manual lube cycle, watching whether frothy oil comes out first and then turns clear. Check the tank level record for any time it fell to the bottom, and look for weeping at the pump suction joints and filter cover. If there is a pressure gauge, compare whether pressure now takes longer to build each cycle than it used to.
With air confirmed, bleed it out step by step from the pump end outwards, from main line to distributors to point lines. Put air bleeding into the maintenance procedure as the final step, and run a system that has been worked on only after clear oil has been seen at every point. Test that the tank low-level alarm actually sounds, and retighten the suction-side joints. If the oil holds froth for a long time, check too whether another oil or water has got mixed in.
Hypothesis 5: long-line pressure loss
If a system that worked well at first starves its end points after a modification, look at the piping. That covers adding a few lube points during a rebuild, rerouting lines so that they grow longer, changing to narrower tube, points sitting far above the pump, and tying points with differing back pressure to one distributor. Think of a rebuild that added a new conveyor, with a long line run from the last outlet of an existing distributor to three new points. The existing points are fine, but the furthest of the new ones is always dry.
The pressure lost by oil flowing slowly through a narrow tube is proportional to tube length, viscosity and flow, and grows with the inverse fourth power of the bore as the bore shrinks (White, 2016). A point placed higher needs extra pressure for that height. So when the pressure reaching the distributor or metering part at an end point falls below what that part needs to work, the point gets no oil even with a normal reading on the pump gauge. Pressure differences between outlets also change distributor output, and the manufacturer lists fitting balancing valves to remove them as one of the corrective actions (Graco, 2024). In systems that divide oil by resistance, the point with the highest resistance gets the least oil.
Check at the far end. Fit a gauge briefly at the inlet of the furthest point's distributor and see how high pressure climbs during one cycle, to confirm whether it reaches the operating pressure that part requires. Compare the present routing, length, tube bore and height differences with the original piping diagram to find what changed in the modification. Connecting a dry point to its distributor with a short temporary line tells whether length or resistance at the point is to blame.
If pressure runs out before the end points, shorten the path the oil must travel. Put another distributor close to the far points so that long point lines become short ones, increase the tube bore, or relay the route more directly. Group points with different back pressure on separate distributors, and fit balancing valves where needed. Before adding points, recalculate pump output, pressure and distributor capacity with the lube system maker, then connect them.
Finding the cause
The first thing to look at is the pattern the dry points make on the piping diagram. If every point under one distributor block is dry, suspect first that the block has stuck or that something ahead of it is blocked. Dry points starting furthest from the pump point to resistance raised by line length or by cold, and dry points clustered where work was done point to air. Scattered points that have grown in number over months lean towards deposits in the lines and metering parts.
Next come timing and pressure. Dry only on cold mornings and recovering by afternoon points to viscosity in the cold; starting right after maintenance points to air; right after a modification, to line length. Pump pressure running above normal signals that oil is blocked somewhere (Graco, 2024), while pressure that builds later or lower than usual points to air. A normal gauge with only the end points dry means pressure must be measured at the end.
If that still does not settle it, run control trials that change one thing at a time. Look at the same point again at a warm time of day, bleed the dry point, swap the suspect metering part with the one from a neighbouring point, or connect the point to its distributor with a short temporary line. Seeing whether oil returns to the point after a single change narrows the cause.
The final check is at the points. After the fix, open the line end at every point or look at the slideways, confirm by eye that oil arrives with each cycle, and put the same check into the routine inspection sheet. It is done only when the surface is still wet the next morning, not merely when oil appears.
The hypotheses overlap easily. A line already narrowed by deposits gains even more resistance on a cold morning, and at the end of a lengthened line the same cold shows up sooner. Opening the system to replace a stuck distributor lets air in. In such cases, remove deposits and stuck parts first, bleed the air next, then measure end-point pressure again at warm and cold times to settle the piping and the oil, because in a system that is not clean, the effect of changing oil or lines cannot be compared fairly.
Limits and cautions
Lube volume, cycle time, pump pressure, distributor operating pressure and oil viscosity grade differ by machine, lube system and point, so numeric decisions follow the machine and lube system makers' manuals and the oil's TDS. Raising pump pressure or changing distributor capacity is decided with the maker, within the pressure ratings of lines and components. Slideways and bearings that ran dry keep the damage already done even once oil returns, so whether they can stay in service is for a maintenance specialist to judge.
Before loosening lines or distributors, stop and lock out the machine and relieve the lube system pressure first. A system still under pressure can spray oil hard enough to inject it through the skin when opened, so follow the maker's pressure relief procedure (Graco, 2024). Wipe up spilt oil at once because it is slippery, and for oils and the solvents used for cleaning, follow the product's safety data sheet, the SDS, for protective equipment and disposal.
Sources
- ASTM International. (2017). ASTM D97-17b, Standard test method for pour point of petroleum products. https://store.astm.org/d0097-17b.html
- ASTM International. (2019). ASTM D3427-19, Standard test method for air release properties of hydrocarbon based oils. https://store.astm.org/d3427-19.html
- ASTM International. (2020). ASTM D341-20e01, Standard practice for viscosity-temperature equations and charts for liquid petroleum or hydrocarbon products. https://store.astm.org/d0341-20e01.html
- ASTM International. (2021). ASTM D7843-21, Standard test method for measurement of lubricant generated insoluble color bodies in in-service turbine oils using membrane patch colorimetry. https://store.astm.org/d7843-21.html
- Gholizadeh, H., Bitner, D., Burton, R., & Schoenau, G. (2014). Modeling and experimental validation of the effective bulk modulus of a mixture of hydraulic oil and air. Journal of Dynamic Systems, Measurement, and Control, 136(5), 051013. https://doi.org/10.1115/1.4027173
- Graco. (2024). Trabon divider valves: Instructions (Manual 312497, Revision ZAF). https://graco.com/content/dam/graco/tech_documents/manuals/312/312497/312497EN.pdf
- Hong, S.-H., & Jang, E. K. (2023). Varnish formation and removal in lubrication systems: A review. Materials, 16(10), 3737. https://doi.org/10.3390/ma16103737
- International Organization for Standardization [ISO]. (1992). ISO 3448:1992, Industrial liquid lubricants — ISO viscosity classification.
- International Organization for Standardization [ISO]. (2021). ISO 4406:2021, Hydraulic fluid power — Fluids — Method for coding the level of contamination by solid particles.
- White, F. M. (2016). Fluid mechanics (8th ed.). McGraw-Hill Education.