Adding more chemical to bring the number back is the usual response to falling inhibitor, but topping up without knowing what removes it tends to bring the same drop back, with ever more chemical used. What actually lies behind it can be bacteria feeding on nitrite, leaks and make-up water, air getting in, error in the measurement method or mixing with other products, and sometimes two or more at once.

Background

At the monthly coolant check, the nitrite test kit shows a paler colour than last month. The person in charge adds another drum of chemical to bring the value back within range, but a few weeks later the reading has dropped again. Year by year the chemical orders come more often, and no one can explain why the level falls.

While the inhibitor sits below its range, the metals in the loop are less protected. In the closed cooling loop of one industrial plant, iron and suspended solids in the water rose after periods of low nitrite residual, and one unexplained nitrite loss was traced to a leaking air cooler (Santuraki & Al-Sayed, 2014). Tests have also shown that where chloride is high, too little nitrite leaves the risk of pitting high (Valcarce & Vázquez, 2009). The loss is the corrosion that builds up during each dip, on top of the chemical bill.

The most effective inhibitors for closed loops are nitrite and molybdate, used alone or together (NIH, 2025). Nitrite is an anodic inhibitor that oxidises ferrous iron released at the steel surface to ferric iron, filling defects in the protective film, and in tests higher concentrations made pits appear later and in smaller numbers (Zhu et al., 2020). Being that reactive, nitrite is used up as it works and can also be turned into something else by bacteria or oxidants. A falling level means something is using it, converting it or carrying it out of the loop.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: gather the make-up water meter readings and the chemical dosing records over the same period, then take loop water and make-up water samples on the same day and measure nitrite, nitrate, pH and electrical conductivity together.

Hypothesis 1: bacteria consuming it

Bacteria come to mind first in loops that run lukewarm, loops with low-flow or stagnant branches, and loops often topped up with untreated water. Take a cooling loop run at a higher supply temperature through the summer. Every time nitrite is topped up, the next reading falls faster than the last, and opening the filter leaves slippery slime on the hands.

Turning nitrite into nitrate is the second step of nitrification. Nitrite-oxidising bacteria, most often Nitrobacter, gain energy by oxidising nitrite to nitrate, using up dissolved oxygen as they do. Nitrifiers grow slowly and cause trouble where water stays a long time and flow is low, and most strains grow best between 25 and 30°C (EPA, 2002). Denitrifying bacteria, which thrive readily in closed loops, also use nitrite as a nutrient (NIH, 2023). The chemical added to protect the loop ends up as food for bacteria.

The bacterial trail shows up in numbers. Nitrate rising as nitrite falls is good reason to suspect nitrification. Count bacteria in samples taken in sterile containers where water stands. In the industrial plant mentioned above, only coliform tests had been run, and biocide dosing was stopped because they came back negative; when total bacteria were counted, slime-forming bacteria were high (Santuraki & Al-Sayed, 2014). Choose tests for total bacteria and nitrifiers, not coliforms.

If bacteria are the cause, cut them back before adding more nitrite. Remove the biofilm by cleaning and flushing, choose with the supplier a non-oxidising biocide compatible with nitrite, and alternating two biocides is also recommended (Santuraki & Al-Sayed, 2014). Take out unused branches, and count bacteria regularly to confirm the biocide is working. Once counts are down, bring nitrite back into the TDS range.

Hypothesis 2: leaks and make-up

Mechanical pump seals, an overflowing expansion tank, a heat exchanger leaking to the process side and an automatic make-up valve stuck open all send loop water out and bring new water in. On a loop with an automatic make-up valve, no one has added water, yet the make-up meter reads a little higher every week, and the tray under the pump never dries out.

Even a closed loop commonly loses water. Make-up is normally under 5% of loop volume a year, but losing 25% a month through small seal leaks or expansion tank overflow is not uncommon (NIH, 2023). The water that leaves takes inhibitor with it, and the make-up that comes in carries no inhibitor and brings minerals, air, microbes and organic matter. A leak therefore does more than dilute nitrite; it opens the door to bacteria and air as well. On a loop with an automatic make-up valve, the level holds even as water is lost, so leaks are easy to miss.

Estimate by calculation how much water has been replaced. If make-up between two checks, divided by loop volume, roughly matches the fractional drop in nitrite, dilution explains it. If there is no make-up meter, fit one first. Comparing loop water parameters such as hardness or conductivity with mains water reveals intrusion of make-up, under-treatment or inhibitor depletion (NIH, 2025). If a co-dosed component such as molybdate has fallen in the same proportion as nitrite, water loss is the likely cause.

Where a leak shows up, fixing it comes before chemicals. Check pump seals and expansion tank pressure, and leak-test any heat exchanger on the process side. Set daily or weekly alarm limits on the make-up meter, and where make-up cannot be avoided, consider pre-dosing inhibitor into the make-up water.

Hypothesis 3: air getting in

Expansion tanks open to the atmosphere, high pipe runs where pressure falls close to atmospheric, repeated draining and refilling at every service, and heat exchangers leaking in from the process side all add oxygen to the loop. Think of a plant that drains and refills part of the loop at every service. For several days after restart the air vents at the top of the pipework hiss, and the nitrite reading drops noticeably more that week than in others.

Oxygen cuts nitrite in two ways. Air ingress can oxidise nitrite to nitrate (NIH, 2025). Nitrifiers use oxygen to oxidise nitrite, so an oxygen-rich loop also suits them (EPA, 2002). The other way is corrosion. When oxygen drives up corrosion of the steel, more nitrite can be spent oxidising the released iron ions to repair the film (Zhu et al., 2020).

Fit a pressure gauge at the highest point of the loop and check that pressure in service stays well above atmospheric. Measure dissolved oxygen with a meter, reading directly in flowing water so the sample does not touch air. Log the days of draining, refilling and venting, and see whether they line up with the weeks of sharp nitrite loss. If iron in the loop water rises at the same time, read it as a sign that oxygen is driving corrosion. Be sure to check process-side heat exchangers for leaks too; in the industrial plant mentioned earlier, two leaking heat exchangers were pushing a significant amount of oxygen into the loop (Santuraki & Al-Sayed, 2014).

Closing off oxygen's routes centres on pressurisation and fewer drain-downs. Consider replacing an open expansion tank with a sealed one, and set the fill pressure so that even the high points stay under positive pressure. Isolate only the section being serviced so the whole loop need not be drained, and pre-mix inhibitor into any fresh fill water. If a process-side heat exchanger is found leaking, repair it first.

Hypothesis 4: measurement error

After a change of test kit or tester, when the supplier's report and the on-site kit use different units, or when a sample stands for more than a day before testing, the level may not have dropped at all; the way of measuring changed. Sometimes the supplier's laboratory report says the level is in range, while the on-site kit, the same week, reads well below it. No one is sure which to believe.

The usual colour method relies on nitrite reacting with reagents under acid conditions to form a reddish-purple colour, and it is set up for 0.01 to 1.0 mg per litre as nitrogen. Samples should be analysed as soon as possible and may be held 24 to 48 hours at 4°C; strong oxidants or reductants readily change the result, and alkalinity above 600 mg per litre gives low readings (EPA, 1971). Nitrite in a closed loop is far stronger than this range and needs heavy dilution, so a small dilution error is multiplied straight into the result. The international standard specifies a method on the same spectrometric principle (ISO, 1984). On top of that, the same water gives very different figures depending on whether results are reported as nitrogen, as nitrite ion or as sodium nitrite.

Split one sample and test it with the on-site kit and in the laboratory on the same day; that shows at once whether measurement is the problem. Check on each report whether units are given as nitrogen or as ion or salt, and write down the dilution factor and the glassware used. Find in the records the gap between sampling and testing, and whether the sampling point is on well-circulated pipe.

If the measurement has wandered, tie method and units to one standard. Agree on one unit between site and supplier, dilute with graduated pipettes and volumetric flasks, and take samples at a fixed point on circulating pipe and test them at once. Every few months, compare laboratory and site values side by side to confirm the kit reads true.

Hypothesis 5: mixed products

Consider this hypothesis when a new product was poured straight into a loop still holding the old one after a change of supplier, when a chlorine-based biocide was added after slime appeared, or when water from another loop leaked in through a valve. Say slime showed in the filter and some leftover chlorine-based biocide went in once. The next day, nitrite reads far lower than the day before.

Chlorine is nitrite's natural enemy. Hypochlorous acid and chloramine oxidise nitrite to nitrate, and the pathways and rates of these reactions have been studied in detail in water chlorination chemistry (Margerum et al., 1994). Add an oxidising biocide and nitrite disappears through a reaction between chemicals, not through bacteria. Mixing inhibitors can weaken protection even when the nitrite reading holds. In carbon steel tests, combining nitrite with phosphate actually lowered resistance to pitting, and it was lowest when the two were at equal concentrations (Zhu et al., 2020). Triazoles used in chilled water loops turning up in a heating hot water loop are read as a sign that the two loops have mixed (NIH, 2025).

Lay out the dosing records by date and find what went in just before each sharp nitrite drop. If nitrate rose at the same time, nitrite was oxidised; if a marker component of another product shows up in the loop, products have mixed. If another loop is connected, test each loop for the other's marker. Before adding a new product or biocide, get the supplier's written confirmation that it can be used with the chemistry already in the loop.

The basic safeguard against mixing is a rule of one chemistry family per loop. When changing supplier, drain and rinse the loop before filling with the new product, and where a biocide is needed use a non-oxidising one compatible with nitrite. Confirm that valves to other loops are shut, and fit double isolation if needed.

Finding the cause

The first job is to line up the records. Put make-up volumes, chemical doses, drain-downs and refills, biocide additions and the dates when the test kit or tester changed onto one timeline and overlay the nitrite readings. If the drops cluster right after a particular task, that task is the first suspect, and this step needs no sample at all.

Next, see what moved together. If a component dosed along with nitrite fell in the same proportion, look at water loss, meaning leaks and make-up. If only nitrite fell while nitrate rose, it is being converted inside the loop, which points to bacteria, air or an oxidising chemical. A slide over weeks with slime in the filter weighs towards bacteria, while a drop overnight points first to a chemical such as a biocide. If values swing with the tester or the kit, fix the measurement first.

A simple control test can confirm bacteria. Split the same loop water into two bottles, pass one through a bacteria-retaining filter and leave the other as it is, keep both near loop temperature for a few days and then measure nitrite. If it fell only in the unfiltered bottle, bacteria are at work. Whether corrosion has actually increased can be checked by hanging metal coupons in the loop and assessing weight loss and pitting (ASTM International, 2023). Choose coupons of the loop's main metal, and hang them for equal periods before and after a change so the results compare.

Take one action at a time, and judge success by whether nitrite holds flat between doses. Over the same period, check that iron and suspended solids in the loop water do not rise. The revised monitoring set at the industrial plant described earlier was likewise nitrite, conductivity, pH, suspended solids, iron and total bacteria (Santuraki & Al-Sayed, 2014).

The hypotheses feed one another. Leaks bring air and bacteria in with the make-up, and air helps nitrifiers. So the usual order is to stop the leaks and cut back the bacteria before restoring nitrite. Done the other way round, the fresh chemical tends to vanish by the same routes.

Limits and cautions

Suitable nitrite levels, units and pH range depend on the product, the loop's metals and temperature, so numeric decisions follow the chemical supplier's TDS. The plant case and test results cited above came from their own conditions and do not transfer directly to another loop. Bacterial testing and marker analysis are most accurate in a laboratory, and where the loop bears on the safety or quality of production, get the supplier and the quality engineer to confirm before acting. If iron and suspended solids keep rising after the drop has stopped, corrosion may already be under way, so schedule thickness checks on heat exchangers and pipework.

Handle nitrite products, biocides and cleaners with the protective equipment given in each product's safety data sheet, the SDS, and never mix different chemicals in one container or line. Water drained from the loop carries chemicals, so dispose of it under local discharge rules. Drain, refill and inspect heat exchangers only after the pumps are stopped and locked out and the pressure is released.

Sources

  1. ASTM International. (2023). ASTM D2688-23, Standard test method for determination of corrosion rate in a water system. https://store.astm.org/d2688-23.html
  2. International Organization for Standardization [ISO]. (1984). ISO 6777:1984, Water quality – Determination of nitrite – Molecular absorption spectrometric method. https://www.iso.org/standard/13273.html
  3. Margerum, D. W., Schurter, L. M., Hobson, J., & Moore, E. E. (1994). Water chlorination chemistry: Nonmetal redox kinetics of chloramine and nitrite ion. Environmental Science & Technology, 28(2), 331–337. https://doi.org/10.1021/es00051a021
  4. National Institutes of Health [NIH]. (2023). Closed-loop systems water treatment (Technical Bulletin No. 135). Office of Research Facilities. https://orf.od.nih.gov/TechnicalResources/Documents/Technical%20Bulletins/23TB/Closed%20Loop%20Water%20Treatment%20-%20August%202023%20Technical%20Bulletin_508.pdf
  5. National Institutes of Health [NIH]. (2025). Corrosion in closed loop water systems part 2: Evaluation and prevention (Technical Bulletin No. 152). Office of Research Facilities. https://orf.od.nih.gov/TechnicalResources/Documents/Technical%20Bulletins/25TB/Corrosion%20in%20Closed%20Loop%20Water%20Systems%20Part%202%20-%20Evaluation%20and%20Prevention%20-%20June%202025%20TB_508.pdf
  6. Santuraki, M., & Al-Sayed, A. A. (2014). Improving reliability of closed loop cooling water systems: A lessons learnt approach (Paper No. 4291). CORROSION 2014, NACE International.
  7. U.S. Environmental Protection Agency [EPA]. (1971). Method 354.1: Nitrogen, nitrite, spectrophotometric. https://www.nemi.gov/methods/method_summary/5777/
  8. U.S. Environmental Protection Agency [EPA]. (2002). Nitrification (Distribution System Issue Paper). Office of Ground Water and Drinking Water. https://www.epa.gov/sites/production/files/2015-09/documents/nitrification_1.pdf
  9. Valcarce, M. B., & Vázquez, M. (2009). Carbon steel passivity examined in solutions with a low degree of carbonation: The effect of chloride and nitrite ions. Materials Chemistry and Physics, 115, 313–321. https://doi.org/10.1016/j.matchemphys.2008.12.007
  10. Zhu, Y., Ding, J., Zhang, J., & Li, L. (2020). Effects of sodium phosphate and sodium nitrite on the pitting corrosion process of X70 carbon steel in sodium chloride solution. Materials, 13(23), 5392. https://doi.org/10.3390/ma13235392

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.