Draining the milky oil and filling fresh is the usual response when screw compressor oil turns white, but unless the way the water gets in is found and closed, the new oil tends to go the same colour. What actually lies behind it can be cool running, humid intake air, a leaking oil cooler, undrained condensate or poor water separation, and sometimes two or more at once.

Background

At the morning check, the oil in the sight glass, which should be a clear brown, looks like coffee with milk stirred in. Crack the sample valve and oil laced with white froth runs out. A fresh fill looks fine for a few days and then clouds again, and each time the machine has to stop while oil and filters are thrown away.

Milky oil is not just a cosmetic problem. Water is a poor lubricant: it lets metal touch metal, rusts iron parts and breaks additives down into acids (Holdmeyer, 2022). The emulsion formed when oil and water are churned together badly reduces the oil's effectiveness, and condensate can cause serious corrosion inside the compressor (Hart, 1984). In tapered roller bearing life tests, fatigue life fell as the water in the oil rose (Cantley, 1977). Screw compressor rotors also often run on rolling bearings, so the longer the machine runs on wet oil, the more bearing life it can lose.

The water comes from the air. Air at a given temperature can hold only so much water vapour, and when saturated air is cooled, water condenses at a temperature called the dew point. Compressing air crowds the same vapour into a smaller volume, so the dew point under pressure is higher than at atmospheric pressure (DOE, 2016). An oil-injected screw compressor sprays oil into the compression chamber, compresses it with the air and separates it out again in the sump, so if any part of that circuit falls below the dew point, water condensed from the air mixes into the oil (Hart, 1984). Water in oil exists dissolved and invisible, emulsified as fine droplets, or as free water that settles out, and oil looks cloudy because of the emulsified water. The amount of water oil can hold dissolved rises with temperature (Al Sheikh Omar et al., 2024).

So water gets into the oil by one of two routes: vapour in the air condenses inside the circuit, or liquid water gets in somewhere such as the cooler. Whether that water settles and drains, or stays as white emulsion, depends on draining practice and on the oil's water separation. In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: catch an oil sample in a clear bottle and watch whether it separates into layers, while logging discharge temperature, loaded and unloaded hours, and the day's temperature and humidity, then compare them with the equipment manual and the oil's technical data sheet, the TDS.

Hypothesis 1: cool running

Look at this hypothesis when the machine keeps running in a way that never lets the oil warm up properly: a compressor far larger than the demand idling unloaded most of the time, short runs followed by long stops, a cold room in winter, or a failed thermostatic valve that sends all the oil through the cooler. Picture a plant where air demand drops at night. The compressor cycles between loaded and unloaded in short bursts, and the discharge temperature gauge sits well below where it reads on the day shift. By Monday morning, after weekend running, the sight glass has gone cloudy.

An oil-injected compressor holds the oil entering the compression chamber above a minimum temperature, usually by way of the discharge temperature. A thermostatic bypass valve sends some or all of the oil around the cooler so the set temperature holds over a wide range of room temperatures, and holding a suitable temperature is what keeps lubrication and sealing right and avoids condensation in the sump (DOE, 2016). Design practice likewise adjusts oil injection quantity and oil temperature to keep the discharge temperature above the dew point of the water in the gas (Pillis, 1999). Light load means less heat of compression, and if the valve cannot close off the cooler, even that little heat is lost. Once the circuit falls below the saturation temperature of the air, water condensed from it mixes with the oil and is churned into emulsion (Hart, 1984). Water that has mixed in is not all driven off by short spells of heavy load, so it accumulates.

Start with the running records. Compare total running hours with loaded hours on the controller to see how much of the time the machine idles unloaded, and log discharge temperature by time of day against the normal range in the manual. The thermostatic valve's behaviour shows when the temperatures of the pipes into and out of the cooler are taken with a contact thermometer as the machine warms up. If the cooler side gets hot from a cold start, or the discharge temperature never reaches its set value once warmed, the valve is not closing off the cooler. Check too whether the oil clouds at times of light load or cold, such as nights, weekends and winter.

Once the cause narrows to temperature, check the thermostatic valve's sensing element first and replace it if needed. If an oversized machine idles unloaded for long periods, hand the night load to a smaller machine or change the sequence of several machines so that whichever is running carries enough load to warm up. Agree with the manufacturer whether the minimum discharge temperature should be raised. Oil degrades faster the hotter it runs, so running the machine hot regardless is no answer either (Hart, 1984). After the temperature is put right, change the oil that has already turned milky and watch whether the new fill stays clear.

Hypothesis 2: humid intake air

If the oil turns milky only in the rainy season or high summer, look at the intake air. It applies especially when the intake sits near a cooling tower, a washing area or a steam vent, or when equipment using water or steam shares a poorly ventilated room. In a week of steady rain, the compressor room is close and muggy with the doors shut, and droplets form and run down the outside of cold pipes. Oil that stayed clear for months in the dry season starts clouding in the sight glass this week.

Relative humidity is the water the air holds as a share of the most it could hold at that temperature. At the same temperature, humid air brings more water in. Compressed air has a higher dew point than air at atmospheric pressure, so the more water it carries, the higher the pressure dew point climbs, and saturated compressed air gives up water with only a small drop in temperature (DOE, 2016). While a compressor runs, ambient temperature and relative humidity keep changing, and both shift the saturation temperature (Hart, 1984). Put another way, an oil temperature that sat above the dew point in the dry season can sit below it in the humid season. More water then condenses in the sump and circuit, and water beyond what the oil can hold dissolved stays as emulsion (Al Sheikh Omar et al., 2024).

What to check is the state of the air at the intake. Measure temperature and relative humidity with a hygrometer right in front of the intake filter several times a day, and log them beside the discharge temperature at the same times. Look at the temperature difference between the compressor room and outside, and at whether exhaust or steam from other equipment drifts towards the intake. If there is an oil analysis history, see whether the water figure rises and falls with the seasons. If the oil clouds only on humid days and the temperature records show nothing wrong, the intake air has raised the dew point.

If humid air is the cause, draw the intake from somewhere drier. Keep the intake away from places that use steam or water, and if it draws room air, increase ventilation in the compressor room so vapour from other equipment does not build up. Discuss with the manufacturer whether the discharge temperature setting needs adjusting for the humid season, and take oil samples for water more often during that period. Drain water from the bottom of the sump more often in that season too.

Hypothesis 3: leaking oil cooler

Most installations cool the oil with an air-cooled radiator, but water-cooled heat exchangers are also available on most screw packages (DOE, 2016). This hypothesis applies to those water-cooled machines. Suspect it especially when the cooler is old and its tubes have corroded, right after the cooler has been cleaned and reassembled, and after cooling water has frozen and thawed in a machine left standing in winter. Say a compressor is cooled with cooling tower water. The oil was changed, yet it turns milky again within days whatever the season, and the sump level has risen a little overnight while the machine stood idle.

Unlike condensation, a cooler leak lets water in as liquid from the start. Cooler and heat exchanger leaks are named as a way water gets into oil both in industrial lubrication systems and in engine oil (Al Sheikh Omar et al., 2024; Holdmeyer, 2022). This water comes in regardless of air temperature, humidity or running temperature, so it does not follow the seasons, and the amount can exceed what condensation brings. Which way the leak runs depends on the pressure on each side. Many packages use air pressure in the sump to drive oil through the cooler and filter (DOE, 2016), so while running the oil side is usually at higher pressure and oil tends to leak into the water; once the machine stops and the sump pressure falls, the cooling water can be at higher pressure and push water into the oil. If the cooling water contains glycol antifreeze, glycol in the oil can be detected by a standard test, one procedure of which picks up ethylene glycol down to about 100 mg/kg (ASTM International, 2024).

Look at the water side first. See whether an oil sheen appears on the water leaving the cooler or on the cooling tower basin, and whether the oil level rises while the machine stands. If suspicion grows, isolate the cooler from both the oil and the water circuits, pressurise each side in turn, and check whether pressure drops or water or oil appears on the other side. Have oil samples tested for water and, where the system uses antifreeze, for glycol as well. If fresh oil turns milky again at the same rate regardless of season or load, this hypothesis moves to the front.

If a leak is confirmed, repair or replace the cooler and prove it tight with a pressure test before restarting. Oil that has taken in a lot of water leaves water behind in the sump, piping and cooler, so drain it, flush the circuit, then refill with fresh oil, and check the condition of the filter and the oil separator element as well. Drain the water side of machines that stand idle in winter so it cannot freeze, and review the cooling water treatment records to cut down whatever is corroding the tubes.

Hypothesis 4: undrained condensate

The basic maintenance list for oil-injected rotary compressors includes draining water periodically or daily from the reservoir that holds the air and oil together (DOE, 2016). When this is skipped, condensed water builds up in the sump. It happens when a change of staff drops the item from the daily checklist, when an automatic drain at the bottom of the sump has clogged, and when the machine restarts after a long stop over a holiday. In a plant where one person's daily check has been split across several shifts, each shift assumes another has opened the bottom drain valve. Weeks later someone opens it: clear water runs for a while, and then milky oil follows.

Most industrial oils are made to part readily from water, so that once water settles to the bottom as free water it can be drained off (Holdmeyer, 2022). Water that is not drained does not just stay at the bottom. Oil and compressed air keep circulating and churning in the sump, and when water is churned with oil it forms an emulsion that cuts the oil's effectiveness (Hart, 1984). Water that lingers also changes the oil itself. In engine oil experiments, when water above saturation separated out as free water, additives clung to it and left with it, and even after the free water was removed, the dissolved water that remained affected wear (Al Sheikh Omar et al., 2024). The more undrained water builds up, the more there is to be churned back in, and the oil circulates holding more and more of it.

Stop the machine and release the pressure as the manual specifies, allow time for water to settle, then open the drain valve at the bottom of the sump slowly. Catch what comes out in a clear container, see how much clear water runs before oil appears, and record the amount. If there is an automatic drain, check that it actually opens and closes and that its outlet is not blocked. Matching the checklist against the actual drain records shows which days the water was drained and which it was not. If the oil clouded after a long run of days without draining, this hypothesis is likely.

If draining had lapsed, put the drain item back on the daily checklist with a space for the amount of water drained, and settle who does it on each shift. Clean the automatic drain at set intervals and confirm it works. After a long stop, drain the water before starting. If the daily amount drained stays large, draining alone will not fix it; go back to running temperature, intake air and the cooler to find out why so much water forms.

Hypothesis 5: poor water separation

When the amount of water coming in is unchanged but it no longer settles as it used to and simply stays white, the oil itself may have changed. This applies to oil run well past its change interval, oil that has taken in and lost water many times, oil topped up in a hurry with a different product, and oil contaminated with something like a cleaning agent. Take a machine whose oil, already past its change date, was topped up with a drum of another brand from the store. From then on, opening the drain valve yields almost no clear water, and a sample left in a bottle for a day stays evenly cloudy from top to bottom.

How readily an oil parts from water is measured by a standard test. Equal amounts of oil and water are stirred together in a heated cylinder, the volumes of oil, water and emulsion are recorded every five minutes, and the time for the emulsion layer to fall to 3 mL or less is noted. The method was developed for steam turbine oils but is used for other oils and synthetic fluids, with more viscous oils tested at a higher temperature (ASTM International, 2021). The age of the oil, repeated or prolonged water contamination, polar contaminants and the addition of an incompatible lubricant are listed as factors that impair this property (Malcolm, 2015). When water separation fails, water that gets in cannot settle and drain, and it stays in the oil as fine droplets that travel with it to the bearings. The more water the oil carries, the shorter bearing fatigue life becomes (Cantley, 1977).

A bottle test gives the first clue. Leave a sample somewhere warm for about a day and see whether water settles clear at the bottom or the whole sample stays evenly cloudy. Setting it beside fresh oil of the same product with a little water mixed in makes the comparison easy. Then have a laboratory run the water separability test and compare the result with the new-oil value, and measure the amount of water by Karl Fischer titration, a quantitative method for water. It can measure water in oil from mg/kg levels up to per cent levels (ASTM International, 2025). Go through the top-up records as well, to see whether another product ever went in and how far past its change interval the oil has run.

If the oil can no longer let go of water, it is better replaced than nursed along. Drain it, flush the circuit, refill with a single product, and top up only with that product from then on. If another product ever has to be mixed in, check compatibility with the supplier first. Repeated water contamination will wear down the separability of the new oil as well, so close the route the water came in by before changing the oil, and the new fill will last (Malcolm, 2015). After the change, measure water separability and water content at set intervals and watch the trend.

Finding the cause

Five hypotheses do not take long when taken in order. A bottle test and draining the bottom of the sump can be done the same day, and discharge temperature, loaded hours and temperature and humidity at the intake only need the records gathered. A pressure test on the cooler needs the machine stopped, so it comes next, and anything that needs a laboratory, such as water separability and glycol, can be sent off and run in parallel with the other checks.

When the symptom appears is the first fork. Clouding at times of light load or cold, such as nights, weekends and winter, points to cool running; clouding in humid spells such as the rainy season and high summer points to the intake air. If even fresh oil turns milky at the same rate regardless of season or load, and the level rises while the machine stands, a cooler leak is the likely suspect. If a run of skipped drain days came before the clouding, suspect undrained condensate first.

The look of the sample in the bottle also splits the paths. If water parts out clear and settles after a day, the oil is still doing its job, so concentrate on where the water comes from and how much. If it stays evenly cloudy even when kept warm, the oil cannot let go of the water, so look at poor water separation as well. The crackle test, a few drops of oil on a hot plate listened to for crackling, is used on site to pick out gross water above about 500 ppm, while the exact amount is measured by Karl Fischer titration (Holdmeyer, 2022).

If that still does not settle it, change one thing at a time. Raise the discharge temperature by servicing the thermostatic valve or changing the running sequence, draw the intake air from somewhere else, or take the cooler out of the circuit for a pressure test. After each change, renew the oil and measure water at the same interval to compare with before. The job is done only when water in the new oil stops rising, bottle samples stay clear and the amount drained from the bottom falls.

The hypotheses can overlap. In a humid season under light load, cool running and humid air together push the circuit past the dew point, and if the water formed is not drained, it builds up. Repeated water contamination also impairs the oil's water separation (Malcolm, 2015), so what began as water getting in ends with the oil needing replacement too. In such cases, close the routes the water comes in by first, then put draining on a firm footing, and only then fill with fresh oil. Do it the other way round and the new oil is spoiled by the same water.

Limits and cautions

Suitable discharge temperature, thermostatic valve setting, oil change interval and the limit for water in the oil differ by machine and oil, so numeric decisions follow the equipment manual and the oil's TDS. The sump of an oil-injected compressor is a pressure vessel: open drains, take samples or remove the cooler only after the machine is stopped, fully depressurised and locked out. Leave cooler repair, pressure testing and changes to control settings to the manufacturer or qualified service staff.

Oil and piping in a machine just stopped are hot enough to burn, so wear gloves and eye protection. In tests that heat oil, such as the crackle test, watch out for spattering oil. Handle oils, antifreeze and cleaning agents according to the product's safety data sheet, the SDS, and do not pour water drained from the sump or emulsified oil down the drain: it is oily waste, to be disposed of under local regulations.

Sources

  1. Al Sheikh Omar, A., Motamen Salehi, F., Farooq, U., & Morina, A. (2024). Additives depletion by water contamination and its influences on engine oil performance. Tribology Letters, 72, 74. https://doi.org/10.1007/s11249-024-01876-y
  2. ASTM International. (2021). ASTM D1401-21, Standard test method for water separability of petroleum oils and synthetic fluids. https://store.astm.org/d1401-21.html
  3. ASTM International. (2024). ASTM D2982-24, Standard test methods for detecting glycol-base antifreeze in used lubricating oils. https://store.astm.org/d2982-24.html
  4. ASTM International. (2025). ASTM D6304-25, Standard test method for determination of water in petroleum products, lubricating oils, and additives by coulometric Karl Fischer titration. https://store.astm.org/d6304-25.html
  5. Cantley, R. E. (1977). The effect of water in lubricating oil on bearing fatigue life. ASLE Transactions, 20(3), 244–248. https://doi.org/10.1080/05698197708982838
  6. Hart, J. E. (1984). Condensation control apparatus for oil-flooded compressors (U.S. Patent No. 4,431,390). U.S. Patent and Trademark Office. https://patents.google.com/patent/US4431390
  7. Holdmeyer, D. (2022, January). The basics of lubricant water contamination. Tribology & Lubrication Technology. Society of Tribologists and Lubrication Engineers. https://www.stle.org/files/TLTArchives/2022/01_January/Lubrication_Fundamentals.aspx
  8. Malcolm, M. (2015, June). Turbine oil analysis report interpretation. Tribology & Lubrication Technology. Society of Tribologists and Lubrication Engineers. https://www.stle.org/files/TLTArchives/2015/06_June/Webinars.aspx
  9. Pillis, J. W. (1999). Basics of operation and application of oil flooded rotary screw compressors. In Proceedings of the 28th Turbomachinery Symposium. Texas A&M University. https://oaktrust.library.tamu.edu/handle/1969.1/163383
  10. U.S. Department of Energy [DOE]. (2016). Improving compressed air system performance: A sourcebook for industry (3rd ed.). Advanced Manufacturing Office and Compressed Air Challenge. https://www.energy.gov/sites/prod/files/2016/03/f30/Improving%20Compressed%20Air%20Sourcebook%20version%203.pdf

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.