BlogApplication notes
Why does coolant form gel and sediment?
- Type
- Application notes
- Published
- 23 November 2026
- Prepared by
- Jonghwan Moon
- Product group
- Heat Transfer & Cooling
Adding more additive or just changing the filter is the usual response to gel and sediment in coolant, yet over-concentration of antifreeze or additive is itself named as a major cause of silicate gel. What actually lies behind it can be mixed coolants, hard top-up water, over-concentration, aged coolant or oil ingress, and sometimes two or more at once.
Background
At a routine check, the cap comes off the expansion tank to show cloudy coolant, with jelly-like translucent lumps stuck to the floor and walls of the tank. Strainers or filters pulled from the cooling circuit hold a mud-like sediment, and from about the same time the equipment runs hotter than usual. The same picture can turn up in engine-driven generators and construction machines and in closed-loop cooling circuits in a plant.
Gel and sediment are more than unsightly. Gel can cut coolant flow and heat transfer and lead to engine overheating (Hercamp & Hudgens, 1985). Mineral deposits on hot metal surfaces block passages and slow the escape of heat, which can run through hot spots, uneven expansion and wear to cracked heads or blocks. The circuit then has to be flushed thoroughly to remove contamination before fresh coolant goes in, and that means downtime (FMC, 2013).
Coolant is glycol and water with a package of corrosion inhibitors dissolved in it. The inhibitors work only while they stay dissolved, and silicate is used up little by little as it lays a protective layer on metal surfaces (Fritz, n.d.). Whether silicate stays dissolved depends heavily on pH. Silica dissolves readily above pH 9, but as pH falls or dissolved salts build up, its particles link into chains and then networks and become a gel (Iler, 1979). Gel and sediment are usually something that should be in solution coming out of it, or something that got in from outside, so the task is to find what upset that balance.
In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: keep a sample of the gel and sediment in a clear bottle, gather the records of which coolant, which water and which additive went in, when and how much, and compare the concentration read on a refractometer and the pH with the ranges in the coolant's technical data sheet, the TDS.
Hypothesis 1: mixed coolants
Coolants fall broadly into conventional types, which use inorganic inhibitors such as silicate and phosphate, and organic acid types, which protect metal with carboxylates, salts of organic acids. The two meet in one circuit at sites that run different coolants on different machines, after an outside service firm tops up with whatever it carries, and when top-up containers are not labelled. Picture a workshop looking after several machines. On the day the top-up container ran dry, it was filled with a different-coloured coolant used on the machine next door, and a few weeks later a translucent film begins to form on the expansion tank wall.
The two families protect metal in different ways, and each inhibitor package is built around its own pH and balance of ingredients. In a mixture, that balance suits neither. A study that added silicate at different levels to several coolant technologies found that even small amounts reduced corrosion protection for aluminium (Fritz et al., 2000). If the mixture ends up at a lower pH than the original, the silicate tips towards gel, as described above. Gel has indeed formed when high-silicate antifreeze met a supplemental coolant additive, and a test method was developed that judges whether a coolant and an additive suit each other by the insoluble matter, silicate gel, formed on brief heating (Hercamp & Hudgens, 1985; Glomski & Hudgens, 1996).
Begin with the records. List the name and family of every product added at past top-ups and services, and do not assume two coolants are the same because they look the same colour. Let a suspect sample stand in a clear bottle for a while to see what settles and what floats, then ask a laboratory to analyse silicon, the main inhibitor components and pH together. If the results match the TDS of no single product, the coolant can be taken as mixed.
Once mixing is clear, draining, flushing and refilling with one family is surer than trying to rebalance with more inhibitor. Gel tends to stay in narrow tubes and strainers, so open the strainers again after flushing. From then on, post the name of each machine's coolant near its expansion tank and keep separate top-up containers per machine. Add a supplemental additive only after the TDS confirms it suits that coolant family.
Hypothesis 2: hard top-up water
This hypothesis comes up when concentrate is diluted with mains water or groundwater on site, when losses in hot weather are made up often with whatever water is nearby, and when water from rinsing with process water stays in the circuit after a coolant change. Suppose a machine whose expansion tank has been topped up with plant mains water all summer. At the autumn service, a hard layer is found in the hottest passages, and the strainer holds sediment with white powder in it.
Hard water carries dissolved calcium and magnesium. These ions meet the coolant's phosphate inhibitor and form calcium or magnesium phosphate, which builds up as scale on hot engine surfaces, where heat transfer drops and corrosion can proceed underneath (Fritz, n.d.). Silicate also becomes less stable as dissolved salts increase (Iler, 1979), so hard water can unsettle both phosphate and silicate. How sensitive a coolant is to hard water varies by product, and a standard test method holds coolant diluted with synthetic hard water at high temperature to judge its stability (ASTM International, 2019).
Measure the hardness of the top-up water first, which test strips or a titration kit can do on the spot. Engine makers' limits for top-up water hardness ranged from 100 ppm to 300 ppm depending on the maker (FMC, 2013). Scrape off sediment and scale and send them to a laboratory to see how much calcium, magnesium, phosphorus and silicon they contain. If these make up most of the deposit and the top-up water is also hard, the evidence leans towards hard water.
With hard water confirmed, change the water first. Use distilled or deionised water for top-up and dilution, and not water from a softener regenerated with salt (FMC, 2013). Keeping a ready-diluted coolant for top-ups is another option. Scale already in place may not come off with a coolant change alone, so clean it out with a cleaner suited to the circuit's materials before refilling.
Hypothesis 3: over-concentration
Here the coolant is too strong. Concentration creeps up when only concentrate is added for fear of freezing, when water lost to evaporation is replaced with concentrate, when a filter-borne additive and a bottled liquid additive are both used, and when doses are poured generously rather than measured. Think of a machine whose fitter, as winter set in, topped up with concentrate every time and added another bottle of additive at every check. When the strainer is opened in spring, it is clogged with jelly-like lumps.
A filter industry service bulletin names two main causes of silicate gel and its dropout, high-silicate antifreeze and over-concentration of antifreeze or additive, and says to hold antifreeze between 40% and 60%, with 50% as ideal, and it stresses that the right amount of additive is critical too (FMC, 2013). Gel has also formed in antifreeze stored undiluted for long periods (Hercamp & Hudgens, 1985). A study of used heavy-duty engine coolant found many variables that upset the additive level (Woyciesjes et al., 1993).
Concentration can be read straight away on a refractometer. Compare the reading with the TDS range, and work out from the top-up records how much concentrate and how much water went in. For the additive, measure marker components such as nitrite or molybdate with the test kit the supplier recommends, and do not use strips that decide additive dosing on pH alone (FMC, 2013).
If concentration is over range, drain some off and refill with distilled or deionised water to bring it back, and stop adding additive until tests show it is within range. If filter-borne and liquid additives were both in use, settle on one. Where gel has already formed enough to catch in strainers, it is safer to flush and refill the circuit even after the concentration is put right.
Hypothesis 4: aged coolant
In circuits that have only been topped up long past their change interval, in equipment that runs hot for long hours, and in circuits that take in air through loose joints or low levels, ask whether the coolant itself has aged. A standby generator that has done nothing but test runs and top-ups for several years is one example. Under the radiator cap, the once-clear colour has turned a murky brown, and rust-coloured mud rises from the bottom.
Over time, ethylene glycol breaks down mainly into glycolic and formic acids, which pull pH down (Fritz, n.d.). A study of degradation in aqueous glycol found acidic breakdown products under every condition tested, the most degradation when metallic copper was present in aerated solution, and degradation that did not show up directly as a fall in pH (Rossiter et al., 1985). As acid builds up, inhibitor is used up neutralising it, and iron, steel and aluminium left unprotected corrode, with the rust able to clog the circuit (FMC, 2013). Silicate also finds it harder to stay dissolved as pH falls, so aged coolant can show rust-coloured mud and gel together.
Colour, smell and pH are not enough. Since the extent of breakdown does not fully show in pH, asking a laboratory to measure organic acids such as glycolic and formic acid by ion chromatography gives a more direct view of how far the coolant has aged (Rossiter et al., 1985). Analyse the sediment for metals such as iron and copper to see which metal has been dissolving. Set the date of the last change and the top-up records since then alongside the results.
Aged coolant is drained, flushed and replaced rather than revived with more additive. A loose or leaking head gasket can let sulphuric acid from burning fuel leak into the cooling system, so where acid has built up quickly, check gaskets and leaks as well (FMC, 2013). Fix loose joints and low levels that let air in, and set the change interval by regular analysis results, not by the calendar alone.
Hypothesis 5: oil ingress
Where oil and coolant meet across a single thin wall, as in engine oil coolers, hydraulic or transmission oil coolers and compressor oil coolers, consider whether oil has crossed over. In an engine, the head gasket is another such boundary. This is the scene where, at a morning check, the expansion tank cap comes off to reveal a brown oily film on the surface and a band of sticky brown residue around the tank wall.
Oil does not dissolve in glycol and water, so it floats on the surface, and where it tangles with rust or sediment in the circuit it shows as sticky residue. A filter industry service bulletin says rust can appear in coolant containing oil even when the inhibitors are at proper levels, advises checking the oil cooler for leaks when rust is seen, and notes that a coolant filter may remove solid contaminants but not oil (FMC, 2013). One service instruction also treats oil in the coolant of an otherwise healthy engine as a sign of a leaking oil cooler (General Motors, 2025).
Look for the oil film by eye first. Coolant left to stand in a clear bottle shows it as a layer on top. Find which cooler it came through by pressure testing the coolers one at a time. Check the oil side as well, whether oil level is falling and whether oil analysis shows coolant components, to narrow down which way the two fluids are passing.
Once the leak is found, repair that cooler or gasket first and flush afterwards. Flushing with the leak still open only lets oil back in. One service instruction says to flush with hot water from several points and in several directions until nearly all the oil is out, not to use over-the-counter detergents not made for cooling systems because they may attack seals, aluminium and gaskets, and to replace parts soaked with oil (General Motors, 2025).
Finding the cause
Five hypotheses do not call for five separate investigations. Refractometer concentration, pH, top-up water hardness and any oil film can be checked on the spot, and the records show which coolants and additives went in. Rule out what these can rule out first, and send what needs chemical analysis to a laboratory after that.
The form of the deposit is the next clue. Translucent, slippery, jelly-like lumps are usually silicate gel, so look at whether another coolant or additive was mixed in and whether the concentration is too high. A hard layer on hot surfaces leans towards calcium and magnesium from hard water; rust-coloured mud and murky brown coolant point to old coolant in which acid has built up; and an oily surface film with sticky brown residue points to oil ingress.
When it started also narrows things down. Right after a top-up with a different product or a dose of additive, look first at mixing and over-concentration; after frequent water top-ups, at hard water; after long service without a change, at aged coolant. If it appeared with an oil film and no link to any service or top-up, the oil coolers and gaskets are the place to look.
If that still does not settle it, run a comparison test. Have a laboratory mix the circuit's current coolant, fresh coolant and the top-up water and additive in different combinations, heat and cool them under the same conditions, and see which combination forms gel or sediment. This follows the same idea as the standardised method that compares compatibility by the insoluble matter formed on brief heating (Glomski & Hudgens, 1996). After flushing and refilling, open the same strainers and expansion tank at set intervals, and the job is done only when gel and sediment stay away.
The hypotheses can overlap. In strong coolant diluted with hard water, extra salts and high concentration unsettle silicate together, and when another family is mixed into old coolant whose pH has dropped, gel and rust come out together. Coolant containing oil can rust even with enough inhibitor, so it may look like aged coolant (FMC, 2013). In such cases, stop outside ingress such as oil first, put water and concentration right, then refill with fresh coolant of one family and start the records afresh, because while ingress continues, the effect of changing coolant cannot be compared fairly.
Limits and cautions
Suitable concentration, pH, additive level and change interval differ by coolant family and equipment, so numeric decisions follow the coolant's TDS and the equipment maker's guidance. For engines under warranty, circuits with many aluminium heat exchangers, and process cooling where a stop puts production or safety at risk, do not change coolant type on floor judgement alone; get the equipment maker and the coolant supplier to confirm. Chemical analysis and compatibility testing are laboratory work.
Safety matters too. Ethylene glycol can do harm when inhaled, swallowed or in contact with skin and eyes (NIOSH, n.d.), so wear gloves and eye protection as the product's safety data sheet, the SDS, requires. Open the cap of a hot, pressurised circuit only once it has cooled well. Collect drained coolant and flush water in lidded containers out of reach of people and animals, and dispose of them under local rules.
Sources
- ASTM International. (2019). ASTM D7437-08(2019), Standard test method for temperature and hard water stability of engine coolants. https://store.astm.org/d7437-08r19.html
- Filter Manufacturers Council [FMC]. (2013). Technical service bulletin 88-1: Cooling system maintenance for heavy duty engines. Auto Care Association, revised May 2013. https://autocare.org/docs/default-source/communities-files/fmc/bulletins/88-1-cooling-system-maintenance-for-heavy-duty-engines
- Fritz, P. (n.d.). Engine coolant basics. Machinery Lubrication. Retrieved November 2026. https://www.machinerylubrication.com/Articles/Print/841
- Fritz, P. O., Bartley, L., Maes, J.-P., & Van de Ven, P. (2000). Extended life carboxylate coolant compatibility with other coolant technologies: Examining the data (SAE Technical Paper 2000-01-1977). SAE International. https://doi.org/10.4271/2000-01-1977
- General Motors. (2025). Information on flushing oil contamination from cooling system (Service Bulletin 25-NA-052). https://static.nhtsa.gov/odi/tsbs/2025/MC-11016942-0001.pdf
- Glomski, C. E., & Hudgens, R. D. (1996). A new test method for compatibility of supplemental coolant additives (SCA) and engine coolant concentrates (SAE Technical Paper 960646). SAE International. https://doi.org/10.4271/960646
- Hercamp, R. D., & Hudgens, R. D. (1985). Silicate gelation in heavy-duty diesel engine cooling systems (SAE Technical Paper 852327). SAE International. https://doi.org/10.4271/852327
- Iler, R. K. (1979). The chemistry of silica: Solubility, polymerization, colloid and surface properties, and biochemistry. Wiley.
- National Institute for Occupational Safety and Health [NIOSH]. (n.d.). Ethylene glycol. NIOSH Pocket Guide to Chemical Hazards. Retrieved November 2026. https://www.cdc.gov/niosh/npg/npgd0272.html
- Rossiter, W. J., Jr., Godette, M., Brown, P. W., & Galuk, K. G. (1985). An investigation of the degradation of aqueous ethylene glycol and propylene glycol solutions using ion chromatography. Solar Energy Materials, 11, 455–467. https://doi.org/10.1016/0165-1633(85)90016-4
- Woyciesjes, P. M., Woodward, S. M., Gershun, A. V., & Frost, R. A. (1993). The characterization of used heavy duty engine coolant (SAE Technical Paper 930476). SAE International. https://doi.org/10.4271/930476