Adding antifoam to knock the foam down is the usual response to a foaming cooling tower, but antifoam only breaks the foam you can see and says nothing about why the water now holds something that stabilises it. What actually lies behind it can be surface-active material leaking in from the process, a quaternary ammonium biocide that foams readily, cycles of concentration run too high, a rise in organic matter and microbes, or more suspended solids, and sometimes two or more at once.

Background

On the morning round, a thick layer of white foam covers the water in the cooling tower basin. When the wind picks up, clumps of foam blow out of the tower and leave marks on the ground and on parked cars, and foam spilling over the basin edge runs towards the drain. It was not there yesterday, so the first thing anyone reaches for is antifoam.

Foam is more than an eyesore. Overflowing foam throws away treated water and chemicals with it, and wind-blown foam scatters whatever it holds around the site. The droplets that leave a tower also carry the same impurities as the circulating water (EPA, 1995). Above all, foam is a sign that something new is in the water, and if that something is a process leak, there is a problem at a heat exchanger and in the product as well.

Clean water stops foaming almost as soon as it stops being shaken. For foam to last, a surface-active substance must collect at the boundary between water and air; it lowers surface tension and slows the thinning and bursting of the foam films. When one spot in a film thins, material at the surface is drawn towards it and restores the film, an elasticity that keeps foam from collapsing easily (Pugh, 1996). A cooling tower drops water over its fill, blows air through it and pounds water into the basin without pause, so bubbles are never in short supply; all foam needs is something to hold them.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: pin down the day the foam first appeared, gather chemical dosing, process changes and make-up and blowdown records from that time onto one timeline, then put tower water and make-up water into clear bottles and shake them the same way.

Hypothesis 1: process fluid leak

Where cooling water meets a process fluid across a single heat exchanger wall, a leak deserves suspicion first. Cleaning solutions, emulsions, cutting fluids, protein-rich food process water and chemical processes that use surfactants are such fluids. A day or two after restarting the process following a scheduled shutdown, foam in the basin suddenly grows and smells of the process side. Among the heat exchangers served by the tower, one shows a cooling water outlet temperature that moves differently from the rest.

When a tube or plate in a heat exchanger develops a hole, fluid passes from the high-pressure side to the low-pressure side. With the process side at higher pressure, process fluid enters the cooling water, and in one industrial plant hydrocarbons that came over from leaking heat exchangers were detected in the cooling water (Santuraki & Al-Sayed, 2014). If the fluid carries surface-active material, its molecules gather at bubble surfaces in the tower and hold the films up (Pugh, 1996), so even a small leak can spread foam through the whole tower.

The clues pointing to the process are smell, colour, an oil sheen and differences between heat exchangers. Take samples at the cooling water inlet and outlet of each exchanger, put equal volumes into identical bottles and shake them the same way, looking for the exchanger whose outlet sample alone holds foam. The foaming of surface-active material can be compared with a standard test that drops a solution from a set height and measures the foam height (ASTM International, 2023). Compare process-side and cooling-side pressures, and isolate the suspect exchanger for a leak test.

Once the leaking exchanger is found, repairing it comes before any antifoam. Until it is repaired, isolate it or lower the process-side pressure, and raise blowdown to flush out what has already got in. Use antifoam only to stop overflow in the meantime, and if a lot of oil or surfactant has entered, replace the circulating water and clean the basin. Where the process side always runs at higher pressure, add oil or organic matter in the cooling water to the routine checks. After the repair, confirm with the same bottle test that foam from that exchanger's outlet has gone.

Hypothesis 2: foaming quat biocide

Look at the biocide in towers that use a quaternary ammonium compound as the non-oxidising biocide, especially those that slug-dose a large amount at once. The same goes for the period right after a change of biocide supplier or product. Take a tower where biocide is poured into the basin all at once on the same morning each week: foam swells that morning, settles over the following days, and the pattern repeats on the next dosing day.

A quaternary ammonium compound is a cationic surface-active substance with a positively charged nitrogen head and a long hydrocarbon tail. Its power to kill bacteria comes from that very structure, since it is a membrane-active agent that acts on bacterial cell membranes and the lipids of viruses (Gerba, 2015). For the same reason, its molecules also gather at the boundary between water and air and hold foam up. High foaming of standard quaternary ammonium biocides in cooling water has long been known, and one study developed a low-foaming quaternary ammonium compound and compared it in the laboratory and in the field (Sweeny & Himpler, 1994).

Laying foam and dosing days side by side by date usually gives the answer. Foam that grows right after dosing and fades with time points strongly to the biocide. Shake tower water taken just before and just after dosing in the same way, compare foam height and collapse time, and recheck that the dose was calculated from the TDS recommendation and the tower's real water volume. Get the volume wrong and the whole dose is off. Some biocide formulations also contain an added surfactant, so read the composition sections of the SDS and TDS too.

If the biocide looks responsible, change the way it goes in first. Splitting the dose, or feeding it slowly where circulation is fast, lowers the peak concentration. If foam persists, review with the supplier a switch to a low-foaming formulation or a biocide from another family, and after the switch count bacteria to confirm the kill is maintained.

Hypothesis 3: high cycles

Consider this hypothesis after cycles of concentration have been raised to save water, after a blowdown valve or conductivity controller has failed, or in midsummer when evaporation has risen sharply and blowdown has not kept up. Suppose that at one plant the actuator on the blowdown valve stopped and nobody noticed. Over a few weeks foam crept up little by little, and white deposits on the basin wall sit higher than usual.

As water evaporates in a cooling tower, the dissolved material stays behind, so dissolved solids in the circulating water rise. Cycles of concentration follow the ratio of make-up to blowdown, and less blowdown means stronger water (DOE, n.d.). It is not only salts that concentrate. Traces of organic matter and chemical residues in the make-up concentrate by the same factor, so an amount that normally could not make foam can cross the threshold. Salts themselves can play a part too: at high enough concentration, some electrolytes stop bubbles from merging, so small bubbles stay as they are (Craig et al., 1993).

Measure the conductivity of tower water and make-up and check that their ratio matches the target cycles, then compare it with the ratio of make-up to blowdown flow. Where the two ratios disagree, check for leaks or unrecorded draw-off (DOE, n.d.). Confirm that the blowdown valve really opens, and compare hand-held readings with the conductivity sensor to see whether fouling is making it read low. If tower water diluted with make-up back to the target cycles stops foaming when shaken, concentration is what fed the foam.

When concentration is confirmed, the first fix is to restore blowdown and bring conductivity back into the target range. Repair the valve and controller, and clean the sensor regularly and check it against hand readings. If cycles were raised to save water, review with the chemical supplier whether make-up quality and treatment can bear that level, since achievable cycles depend on make-up water quality and the treatment regime (DOE, n.d.). Logging make-up volume, blowdown volume and conductivity daily lets the same fault show within days rather than weeks.

Hypothesis 4: organics and microbes

This hypothesis comes up in towers whose basins catch sunlight, towers where biocide control has been slack for a while, towers topped up with organic-rich reclaimed or surface water, and towers near food or biological processes. It is late spring. A slippery brown film has grown under the fill and on the basin walls, and the foam on the basin is tan rather than white and holds firm when pressed with a finger.

Microbes and what they secrete can help hold foam up. A study of activated sludge foam found that stable foam needed three things together: air bubbles, surface-active material and bacterial cells with water-repelling surfaces; with cells that did not repel water the foam was unstable, and without surface-active material the cells formed only a greasy scum (Petrovski et al., 2011). In the same study, adding surface-active material turned a scum-forming population into one that made stable foam. In a cooling tower, too, a rise in microbes and organic matter makes it easy for all three to come together.

The colour and stickiness of the foam, and slime in the basin and fill, are the first clues. Measure bacteria in the tower water with dip slides or ATP tests, and compare organic matter with the make-up as total organic carbon or chemical oxygen demand. Skimming the foam for microscopy or laboratory analysis shows whether it is made of microbial clumps. Check the biocide records for missed days or reduced doses as well.

If microbes are the cause, rebuild the biocide plan. Clean slime out of the basin and fill, choose a biocide family that foams less, and agree with the supplier on the mix and timing of oxidising and non-oxidising biocides. Fit covers to shade the basin from sunlight, and if the make-up is rich in organic matter, review its treatment too. After cleaning and disinfection, count bacteria again to confirm the plan is working.

Hypothesis 5: suspended solids

Solids build up in towers near construction sites, unpaved roads or raw material unloading areas, in seasons heavy with pollen and dust, and in towers whose side-stream filter has stopped or whose basin cleaning has slipped. Earthworks on a neighbouring plot have run for several weeks. The circulating water has turned visibly turbid, and the foam on the basin is greyish, leaving a fine film of silt where it collapses.

A cooling tower is also an air scrubber. A study measuring two power plant cooling towers found that they removed nearly all particles between 2.5 and 10 micrometres from the air entering them (Wexler et al., 2023). The dust caught this way becomes suspended solids in the circulating water. Particles whose surfaces are moderately water-repelling attach to bubble surfaces and resist film thinning and merging, and together with surface-active material they can make foam last longer (Hunter et al., 2008).

Compare turbidity or suspended solids in the tower water with the make-up, and check sludge depth in the basin and the pressure drop and run records of the side-stream filter. Split a tower water sample, filter one half and shake both together; if the filtered half loses its foam much faster, solids are holding the foam. If foam is about the same either way, go back to dissolved substances.

Where solids are holding the foam, start by cleaning the basin and getting the side-stream filter working again. In dusty periods, raise blowdown and shorten the filter backwash interval, and if earthworks or unloading are nearby, ask for dust control on the side facing the air inlets. For a tower with no filter, consider installing side-stream filtration.

Finding the cause

When the foam started is the biggest clue. If it appeared overnight, look first at something that arrived all at once, such as a leak or a chemical dose; if it grew over weeks, look first at what accumulates: concentration, microbes and solids. If it returns on every dosing day, the biocide is the closest suspect. Putting the records on a timeline needs no sample, so it always comes first. Process changes, raw material switches and trial doses of new chemicals all go on the same timeline.

The look of the foam points a direction too. Foam with a process smell or an oil sheen points to a process leak; foam that swells on dosing days, to the biocide. Tan, sticky foam with slime nearby suggests microbes and organic matter, and grey foam that leaves silt behind suggests suspended solids. If conductivity reads above target, keep in mind that concentration may be feeding the foam whatever else is going on.

A control test needs only a few bottles. Put equal volumes of tower water, make-up, filtered tower water and tower water diluted with make-up to the target cycles into identical bottles, shake them the same way, and note foam height and collapse time. Add samples from heat exchanger outlets and from before and after biocide dosing, and several hypotheses can be compared at once. For a finer comparison, have a laboratory run the standard foam test (ASTM International, 2023).

Use antifoam only to stop overflow while the cause is being found. Oil-based antifoams work by forming oil bridges between the two faces of a foam film and tearing it (Denkov, 2004), so as long as whatever holds the foam keeps coming in, the dose has to be repeated. After the cause is fixed, judge the job finished when foam no longer forms without antifoam and the same bottle test gives normal results again.

The hypotheses often overlap. Organic matter leaking from the process feeds microbes, high cycles concentrate surface-active material and solids together, and solids and microbes make foam last longer when surface-active material is present. In such cases the usual order is to stop what is coming in first, meaning fix the leak and correct the dosing, and then clear out what has built up through blowdown and cleaning.

Limits and cautions

Suitable cycles of concentration, biocide type and dose, and antifoam type and dose vary with make-up water quality, tower design and treatment chemicals, so numeric decisions follow the chemical supplier's TDS and the water treatment plan. Antifoam may not suit the treatment chemicals or filters, so check with the supplier before adding it. If a process leak is suspected, do not treat it as a cooling water issue alone; tell the process and product quality owners at once. Foam disappearing does not mean the cause has gone, so keep up the bottle test for a few weeks after antifoam is stopped.

Droplets and foam leaving a tower can carry the chemicals and microbes in the circulating water, so when skimming foam or sampling, wear the protective and respiratory equipment given in the relevant safety data sheet, the SDS, and keep the wind at your back. Clean the basin or work on the fill only after the fans are stopped and locked out. If overflowing foam or blowdown contains biocide or process material, dispose of it under local discharge rules.

Sources

  1. ASTM International. (2023). ASTM D1173-23, Standard test method for foaming properties of surface-active agents. https://store.astm.org/d1173-23.html
  2. Craig, V. S. J., Ninham, B. W., & Pashley, R. M. (1993). Effect of electrolytes on bubble coalescence. Nature, 364, 317–319. https://doi.org/10.1038/364317a0
  3. Denkov, N. D. (2004). Mechanisms of foam destruction by oil-based antifoams. Langmuir, 20(22), 9463–9505. https://doi.org/10.1021/la049676o
  4. Gerba, C. P. (2015). Quaternary ammonium biocides: Efficacy in application. Applied and Environmental Microbiology, 81(2), 464–469. https://doi.org/10.1128/AEM.02633-14
  5. Hunter, T. N., Pugh, R. J., Franks, G. V., & Jameson, G. J. (2008). The role of particles in stabilising foams and emulsions. Advances in Colloid and Interface Science, 137(2), 57–81. https://doi.org/10.1016/j.cis.2007.07.007
  6. Petrovski, S., Dyson, Z. A., Quill, E. S., McIlroy, S. J., Tillett, D., & Seviour, R. J. (2011). An examination of the mechanisms for stable foam formation in activated sludge systems. Water Research, 45(5), 2146–2154. https://doi.org/10.1016/j.watres.2010.12.026
  7. Pugh, R. J. (1996). Foaming, foam films, antifoaming and defoaming. Advances in Colloid and Interface Science, 64, 67–142. https://doi.org/10.1016/0001-8686(95)00280-4
  8. Santuraki, M., & Al-Sayed, A. A. (2014). Improving reliability of closed loop cooling water systems: A lessons learnt approach (Paper No. 4291). CORROSION 2014, NACE International.
  9. Sweeny, P. G., & Himpler, F. J. (1994). A novel nonoxidizing biocide for cooling water systems (CONF-940222). NACE International. https://www.osti.gov/biblio/82975
  10. U.S. Department of Energy [DOE]. (n.d.). Best management practice #10: Cooling tower management. Federal Energy Management Program. Retrieved November 2026. https://www.energy.gov/cmei/femp/best-management-practice-10-cooling-tower-management
  11. U.S. Environmental Protection Agency [EPA]. (1995). AP-42, Compilation of air pollutant emission factors, Section 13.4: Wet cooling towers. https://www.epa.gov/sites/default/files/2020-10/documents/13.4_wet_cooling_towers.pdf
  12. Wexler, A. S., Wallis, C. D., Chuang, P., & Leandro, M. (2023). Assessing particulate emissions from power plant cooling towers (CEC-500-2023-048). California Energy Commission. https://www.energy.ca.gov/sites/default/files/2023-07/CEC-500-2023-048.pdf

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.