KALTECKOREA

BlogApplication notes

Why does EDM slow down and leave a rougher finish?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Metalworking Fluids (MWF)

Making a new electrode or retuning the discharge settings is the usual response when EDM slows down and the finish gets rougher, but where and how evenly sparks fire depends heavily on the state of the oil in the gap, so unless the oil and flushing are checked, the symptom tends to return. What actually lies behind it can be carbon and metal fines in the oil, poor filtration, wrong flushing pressure or direction, an unsuitable viscosity, or insulation lost to water, and sometimes two or more at once.

Background

With the same electrode design and the same discharge settings, sinking one form now takes longer than it used to. The machine display keeps showing short circuits and arcs, the electrode keeps backing off and plunging again, and the finished surface carries uneven rough marks. The extra machining time pushes back the next job, and the rougher surface brings hand polishing and rework. If electrode wear rises too, more electrodes may be needed to hold size.

EDM fills the narrow gap between electrode and workpiece with a dielectric fluid and fires short sparks across it again and again, melting and vaporising metal and carrying it away. The dielectric insulates the gap until a discharge occurs, then cools it and flushes away the debris (Ho & Newman, 2003). The dielectric strength of the gap falls as the gap narrows and as more debris is suspended in it, and conductive debris raises the electric field locally, so discharges tend to occur where debris has gathered (Takeuchi & Kunieda, 2007).

So where sparks fire, and how evenly, depends not only on the discharge settings but on the state of the oil filling the gap. Debris in the oil, the filter that removes it, the flow that pushes debris out of the gap, and the oil's own viscosity and insulating strength all set that state. Retuning the settings may help for a while, but if the gap conditions stay the same, the symptom is likely to come back.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: record the oil colour and tank floor, filter differential pressure and change date, flushing pressure and nozzle direction, and the short-circuit and arc log on the machine display, and compare them with the oil's technical data sheet, the TDS, and the machine manual.

Hypothesis 1: debris build-up

After long roughing with graphite electrodes, when sinking forms such as deep ribs or narrow slots where debris has a long way out, or after weeks of heavy stock removal, start by checking whether fines have built up in the gap and the oil. Graphite electrodes shed carbon dust, and the workpiece sheds metal fines that melted and resolidified. Watch a graphite electrode sinking a deep rib: the feed is smooth for the first few millimetres, but as it goes deeper the electrode hesitates and backs off more often, and arc indications on the display grow more frequent with depth.

Debris is not always harmful. As debris in the gap increases, the wait before a discharge fires gets shorter, but it has been argued that excess debris lines up along the electric field into bridges that short-circuit the gap (Schumacher, 1990). Discharges tend to occur where debris has gathered, so they keep concentrating wherever debris cannot get out (Takeuchi & Kunieda, 2007). As shorts and arcs become frequent, the machine has to pull the electrode back to reopen the gap, which leaves less time actually removing metal, and discharges concentrated in one place can leave uneven marks on the surface.

Check on the machine's discharge monitor or log how the share of shorts and arcs changes with depth and machining time. Leave a sample of tank oil in a clear bottle overnight and compare the black sediment at the bottom with that of new oil. Log depth machined per hour at each depth of the form to see whether speed falls as it goes deeper.

Once fines are shown to be the cause, deal with both getting debris out of the gap and filtering it out of the oil. Increase the height and frequency of the electrode's periodic lift that exchanges oil in the gap, and open new flushing paths for deep forms. Scoop out sediment from the tank floor and change the filter, and if the oil has gone dark and murky, agree on when to replace it with the supplier.

Hypothesis 2: poor filtration

The weight falls here when filter changes have been put off, when a clogged filter is running with its bypass valve open, when several machines share one filtration unit and their workload has grown, or when filters were swapped for a cheaper grade. On a Monday, a machine whose filter gauge needle has been past the change mark for weeks has murkier oil than usual, and changing the electrode does not bring the speed back. Opening the filter housing reveals a filter thickly coated with black sludge.

The gap stays free of debris only if the oil entering it is clean, so the filter is the last device outside the gap that keeps the oil in condition. Guidance for maintaining insulating oils likewise treats a high particle content as lowering the electric strength the oil can withstand, and manages particles separately (IEC, 2013). When a clogged filter opens its bypass, unfiltered oil goes straight back to the tank, and debris builds up through the whole oil volume as machining goes on. The amount of particles in oil can be expressed as a code from particle counts by size, which allows comparison on one scale across times and machines (ISO, 2021).

First check the filter differential pressure, the last change date and whether the bypass valve is closed. Take oil before and after the filter into identical bottles to compare colour and haze, and if needed send samples for particle counting so that the codes for new oil, oil after the filter and tank oil can be set side by side. Check that the filter grade matches the one recommended in the machine manual and, for a shared unit, whether the workload of the connected machines has grown.

For a filter problem, fit a new filter, fix the bypass so it stays shut, and base the change rule on differential pressure rather than dates. Return to the filter grade recommended in the machine manual, and if a shared unit is short of capacity, review with the equipment supplier whether to enlarge it or separate the heaviest-loaded machines. After the change, measure particle counts or haze again in the same way and record them.

Hypothesis 3: wrong flushing

Look at this hypothesis when a deep blind cavity without flushing holes is flushed by a single side nozzle, when the form has changed but the nozzle still points where it used to, or when the pressure is set too low or, the other way, pushed too high. One example is a job where a single nozzle blows oil into a cavity from one side only. The wall facing the nozzle is cut fairly evenly, but rough bands and arc marks gather in the deep corner on the far side.

Flushing puts fresh oil into the gap and pushes debris out. A die-sinking study that varied electrode material, flushing, electrode size and depth of cut reports that injection flushing and the geometry of the cut strongly affect removal rate, electrode wear and surface quality (Lonardo & Bruzzone, 1999). Another study that examined machined surfaces at different flushing rates found an optimum rate at which cracks and average recast layer thickness were smallest, so more is not always better (Wong et al., 1995).

With too little pressure, debris stays in the gap. A study measuring emissions from die-sinking EDM, citing earlier reports that lower flushing pressure can make machining unstable and cause arcing around areas of high debris concentration, reports that in its own measurements higher flushing pressure also reduced aerosol at the operator (Jose et al., 2010). Direction and electrode lift matter too. In a flow analysis of deep-hole EDM, the height to which the electrode jumped changed how debris moved in the side gap, and that changed how far the hole wall became concave (Cetin et al., 2004).

Compare the flushing pressure gauge reading with the value in the program and job sheet, and photograph which part of the present form the nozzle is aimed at. Mark on the machined surface where rough marks and arc marks fall, to see whether they gather opposite the flushing flow or in deep corners. Note the height and frequency of electrode lift as well.

When correcting flushing, the first aim is flow that reaches the deepest part of the form. Where possible, drill holes in the electrode or workpiece to inject or draw oil from inside the gap, and re-aim side nozzles for each form. Change the pressure one step at a time and compare machining time and finish on the same form, adjusting the height and frequency of electrode lift along with it.

Hypothesis 4: unsuitable viscosity

Look at viscosity when speed and finish changed together right after a change of oil product or viscosity grade, when oil from another machine was transferred in, or when the oil temperature is far from usual, as on a winter morning. Discharge setting charts are usually tuned to the oil first used, so when the oil changes, the same chart behaves differently. In the week after a change to another grade, sinking the same part with the same electrode and chart gives machining time and roughness that no longer match the earlier records.

Viscosity changes both how much each discharge removes and how discharges spread. A study comparing three oils that differed only in viscosity in wire EDM found that removal rate and surface roughness both rose with viscosity, with the most viscous oil removing material 6.4% faster than the least viscous (Liu et al., 2024). The authors explain that in the thicker oil each crater removed more volume, which raised the speed, while debris cleared less well and discharges concentrated in one place more often, which roughened the surface, and they cite reports that crater volume also grows with viscosity in die-sinking EDM. Because viscosity can pull speed and finish in opposite directions, when both have worsened, look not only at viscosity itself but at how the change left the setting chart and flushing out of step.

Match the product name and viscosity grade of the oil in use against the TDS, and line up the date of the change with the point at which the machining records shifted. Have a laboratory measure the viscosity of tank oil against new oil, and record oil temperature during machining as well. If another oil may have been mixed in, check the top-up records.

If the viscosity is off, the simplest step is to return to the grade the machine manual and setting chart assume. If the new grade is to stay, retune the setting chart on a few representative forms and revisit the flushing pressure for the new oil. In a shop where oil temperature swings widely, bring the oil into a set temperature range before machining.

Hypothesis 5: water in the oil

Water gets in during humid summers, when the tank lid is left open for long periods, when a chiller or line leaks, or when workpieces or fixtures washed in water-based cleaner go in before they are dry. Think of mould parts taken straight from the washer and put into the tank still wet. A few days later the oil is cloudy instead of clear, and small droplets sit in the corners of the tank floor. From about then, machining has been slower and arc indications on the display more frequent.

The dielectric's job is to insulate the gap until a discharge fires. Guidance for maintaining insulating oils treats water and particles as factors that lower an oil's breakdown voltage and manages the two separately, noting also that the amount of water oil can hold dissolved varies strongly with temperature (IEC, 2013). In an EDM gap, discharges fire first where dielectric strength is lowest, so in oil whose insulation has been lowered unevenly by water, discharges can fire early or in the wrong place and machining can become unstable (Takeuchi & Kunieda, 2007). When the oil cools and dissolved water comes out as fine droplets, these differences can grow.

Look for cloudiness in the tank oil and for droplets or a water layer on the bottom. Water in a sample is measured by Karl Fischer titration, the standard method for insulating liquids (IEC, 1997), and there is a standard test that measures breakdown voltage by raising a power-frequency voltage, so compare the sample with new oil on both (IEC, 2018). Check also for leaks from the chiller and lines, the drying step after washing, and how the tank lid is opened and closed.

If water turns up, close off its way in first. Put workpieces and fixtures in only when fully dry, fix leaks in the chiller and lines, and keep the tank covered when idle. Drain water from the tank floor, and if water has spread through the oil, decide with the supplier between drying treatment and an oil change. Afterwards, measure water content and breakdown voltage again by the same methods and record them.

Finding the cause

The five hypotheses need not be investigated all at once. Rule them out starting with what is easiest to check. Filter pressure and bypass, flushing pressure and nozzle direction, oil colour and water on the tank floor can be checked without a long stop. Viscosity, water content, particle count and breakdown voltage need a laboratory, so they come next; taking one sample and sending it for several tests together saves time.

The pattern of the symptom is the next clue. If machining slows as it goes deeper and rough marks gather deep down or opposite the flow, look at flushing and fines in the gap. A gradual worsening on every form with murkier oil points to filtration and fines contamination; a change that dates from the day the oil was changed points to viscosity; and cloudy oil with symptoms that swing with the weather or the washing process points to water.

If that still does not settle it, run control trials that change one thing at a time, using the same electrode on the same form: fit only a new filter, change only the flushing direction, or run the same job on another machine filled with new oil. Change only one thing at a time, or there is no telling which one worked. Match electrodes for material and machining history so that differences between electrodes do not creep in.

The final check is in numbers. Pick one representative form and measure machining time, surface roughness and electrode wear in the same way as the records from before the problem, and see whether the short and arc rates have returned to their old level. The job is done only when those figures have recovered; keep the particle count or water content of oil samples from before and after treatment as well, and use them as the basis for future control.

The hypotheses can overlap. When a clogged filter lets fines build up through the oil, the oil entering the gap is dirty however good the flushing, and in oil of a different viscosity the same flushing pressure produces a different flow. In such cases, put the state of the oil itself right first, meaning fines, water and filtration, and then match the flushing and setting chart to it, because while the oil is unsettled, the effect of changing flushing or settings cannot be compared fairly.

Limits and cautions

Suitable filter grade, flushing pressure, viscosity grade and oil change timing differ by machine, electrode and workpiece materials, and form, so numeric decisions follow the machine manual and the oil's TDS. The test values above were obtained under those test conditions and should not be carried over to other machines and forms as they are. Recast layers and microcracks cannot be judged by eye, so for fatigue-sensitive parts or critical mould surfaces, confirm them by cross-section inspection with the quality engineer or a laboratory.

Safety matters too. Many EDM oils are hydrocarbons and can catch fire, so even when changing flushing or taking samples, hold the oil level set in the machine manual and never disable level monitoring or the temperature cut-out. Filters and sediment are rich in metal fines, so follow the product's safety data sheet, the SDS, for gloves and eye protection, and dispose of spent filters and oil as controlled waste. Work on nozzles and filters only with the machine stopped and its power locked out.

Sources

  1. Cetin, S., Okada, A., & Uno, Y. (2004). Effect of debris distribution on wall concavity in deep-hole EDM. JSME International Journal Series C, 47(2), 553–559. https://doi.org/10.1299/jsmec.47.553
  2. Ho, K. H., & Newman, S. T. (2003). State of the art electrical discharge machining (EDM). International Journal of Machine Tools and Manufacture, 43(13), 1287–1300. https://doi.org/10.1016/S0890-6955(03)00162-7
  3. International Electrotechnical Commission [IEC]. (1997). IEC 60814:1997, Insulating liquids. Oil-impregnated paper and pressboard. Determination of water by automatic coulometric Karl Fischer titration. https://webstore.iec.ch/publication/3572
  4. International Electrotechnical Commission [IEC]. (2013). IEC 60422:2013, Mineral insulating oils in electrical equipment. Supervision and maintenance guidance.
  5. International Electrotechnical Commission [IEC]. (2018). IEC 60156:2018, Insulating liquids. Determination of the breakdown voltage at power frequency. Test method. https://webstore.iec.ch/publication/28297
  6. International Organization for Standardization [ISO]. (2021). ISO 4406:2021, Hydraulic fluid power. Fluids. Method for coding the level of contamination by solid particles. https://www.iso.org/standard/79716.html
  7. Jose, M., Sivapirakasam, S. P., & Surianarayanan, M. (2010). Analysis of aerosol emission and hazard evaluation of electrical discharge machining (EDM) process. Industrial Health, 48(4), 478–486. https://doi.org/10.2486/indhealth.MS1127
  8. Liu, S., Okada, A., & Kitamura, T. (2024). Fundamental study on dielectric oil viscosity for high-performance wire EDM. The International Journal of Advanced Manufacturing Technology, 135(7–8), 3451–3461. https://doi.org/10.1007/s00170-024-14693-3
  9. Lonardo, P. M., & Bruzzone, A. A. (1999). Effect of flushing and electrode material on die sinking EDM. CIRP Annals, 48(1), 123–126. https://doi.org/10.1016/S0007-8506(07)63146-1
  10. Schumacher, B. M. (1990). About the role of debris in the gap during electrical discharge machining. CIRP Annals, 39(1), 197–199. https://doi.org/10.1016/S0007-8506(07)61034-8
  11. Takeuchi, H., & Kunieda, M. (2007). Relation between debris concentration and discharge gap width in EDM process. International Journal of Electrical Machining, 12, 17–22. https://doi.org/10.2526/ijem.12.17
  12. Wong, Y. S., Lim, L. C., & Lee, L. C. (1995). Effects of flushing on electro-discharge machined surfaces. Journal of Materials Processing Technology, 48(1–4), 299–305. https://doi.org/10.1016/0924-0136(94)01662-K

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.