BlogApplication notes
Why does EDM oil smoke and smell so much?
- Type
- Application notes
- Published
- 23 November 2026
- Prepared by
- Jonghwan Moon
- Product group
- Metalworking Fluids (MWF)
More ventilation is the usual response when EDM smoke and smell get worse, but that only clears smoke already made, and the conditions that make the smoke also raise the risk of fire. What actually lies behind it can be too little oil above the workpiece, a low flash point and high volatility, rising oil temperature, high discharge energy, or degradation and carbon build-up, and sometimes two or more at once.
Background
White smoke rises from the work tank of a die-sinking EDM machine and a smell like burnt oil spreads through the shop. Operators complain of stinging eyes or headaches, and the floor and walls around the machine gather a sticky film of oil. Running the extraction harder helps only until the same job runs again. Sparks and oil vapour meet exactly where the smoke forms, so this symptom is a health problem and a warning sign of fire as well.
Electrical discharge machining, or EDM, fills the gap between electrode and workpiece with a dielectric fluid and fires short sparks again and again, melting and vaporising metal with the heat and carrying it away. The dielectric insulates the gap until a discharge occurs, then cools it and flushes away the debris (Ho & Newman, 2003). The discharge channel reaches very high temperature and pressure, so reaction products form in the surrounding dielectric and escape above the surface as aerosols or gases (Jose et al., 2010).
The smoke is not one thing. A study analysing aerosol from die-sinking EDM found that about 69% of it was metal particles, and the samples also contained some twenty different hydrocarbons (Sivapirakasam et al., 2011). Mineral oil dielectrics are reported to form small amounts of acrolein, an eye irritant, when they break down with heat, so the smell and stinging eyes can be tied to this breakdown too (Leppert, 2018). A study that examined the same process with a structured hazard analysis concluded that EDM with hydrocarbon dielectrics is vulnerable to fire and explosion (Jose et al., 2010).
In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: measure the oil level above the machining point and the oil temperature, note the discharge settings at the time, such as current and pulse duration, along with when the oil was filled and topped up, and compare them with the oil's technical data sheet, the TDS, and the machine manual.
Hypothesis 1: oil level too low
This hypothesis comes up first when machining close to the top face of a tall mould block, when an oil level set for small parts is kept for large ones, or when oil lost to evaporation and carried off on parts has not been replaced. The same goes for a level switch left unserviced for a long time, or a machine that does not stop when the level drops during a cut. Say a tall mould block goes on in the afternoon and work starts on a shallow form in its top face. The electrode works just below the surface, and bubbles from each discharge burst at the surface, where the smoke rises.
The oil layer above the discharge acts as a cover that cools and holds hot gas and vapour from the discharge before they reach the air. A study that examined EDM with a structured hazard analysis found that a falling level or loss of oil circulation raises both fire risk and emissions, flagged a level below the discharge point as an alarming case, and recommended level sensors linked to an alarm to keep the required height above the discharge point. In the same study's measurements at high discharge energy, raising the level from 40 to 80 mm actually increased aerosol concentration at the operator's breathing zone, which the authors attributed to vapour cooling and condensing into metal particles as it passed through a deeper oil layer (Jose et al., 2010). In another study, raising the mineral oil level cut emissions of aromatic volatiles such as benzene, toluene and xylene, of chromium and nickel, and of polycyclic aromatic hydrocarbons, but emissions of aliphatic hydrocarbons rose (Evertz et al., 2006). The oil level is not a value to lower for less smoke; it is the safety height that keeps the oil from catching fire.
Measure with a rule the depth of oil above the highest machining point and compare it with the minimum height in the machine manual. Log the level before machining, during it and at the end of the shift to see how far it falls in a day. Test the level switch by actually lowering the level and checking that the machine stops. Check against the records whether the smoke thickens only on tall workpieces or top-face work.
Where the level falls short, set it for each job from the highest machining point on the workpiece and fix a top-up interval so it never drops below the manual's minimum height. Test the level switch at regular intervals and never machine with it disabled or bypassed. If the workpiece is too tall for the tank, consider moving the job to a machine with a larger tank or changing the order in which the forms are cut.
Hypothesis 2: volatile oil
When kerosene or another light oil is used instead of, or mixed into, a dedicated EDM oil, when cleaning solvent has found its way into the tank, or when smoke and smell changed right after a change of supplier or product, suspect the oil itself. Imagine the day after a can of cleaning oil from nearby was poured in to make up a shortfall. The settings are the same as yesterday, yet a solvent smell rises first when the tank lid opens, and smoke appears earlier than usual once machining starts.
The flash point is the lowest temperature at which a liquid gives off enough vapour to form an ignitable mixture with air, and it is used as an index of fire hazard. A dielectric with a low flash point gives off ignitable vapour at a lower temperature, so it carries a high fire risk in EDM, and conversely a dielectric with a high flash point reduces that risk (Jose et al., 2010). Hydrocarbon oils have long been the common dielectric for die-sinking EDM, and other dielectrics have been examined because of their environmental and health burden (Leão & Pashby, 2004). If a light oil is mixed in, the flash point of the dedicated oil can be dragged down towards that of the light oil.
Check the flash point and any volatility data for the oil in use on its TDS, and send a sample from the tank to a laboratory for flash point testing alongside new oil. The standard method for petroleum products is the Pensky-Martens closed cup test (ASTM International, 2020). Look through the top-up records for any other oil added, and see whether solvent from cleaning has a route into the tank. Note also whether the smell above the tank is sharper than that of new oil.
If the sample's flash point comes out clearly below that of new oil, drain the mixed oil, clean the tank and filter, and refill with the dedicated oil. Post the product name by the machine so top-ups use the same product only, and store cleaning oils and solvents apart. When changing oil, review a dedicated EDM product with a higher flash point with the supplier.
Hypothesis 3: oil running hot
Look at temperature when smoke grows with running time in summer, during unattended overnight runs, on machines with small tanks, or where the chiller has stopped or lost capacity. Heat also builds up during hours of roughing with a large electrode. Open up a machine that ran unattended roughing all night, and the tank walls feel hotter than usual, while the chiller fan turns but blows lukewarm air. The smoke is far thicker a few hours in than just after the start.
Heat from each discharge ends up in the oil, and when cooling cannot keep up, oil temperature rises. The hotter the oil, the narrower its margin to the flash point and the more vapour it releases. A study of EDM hazards found that a rise in dielectric temperature increases both fire risk and toxic emissions, and named a temperature above the flash point as the worst case, one that could lead to explosion. The same study saw sparks near the surface together with a raised oil temperature as a cause of fire, and noted that safety interlocks can stop machining when the dielectric reaches 15°C below its flash point (Jose et al., 2010).
Measure the oil temperature in the tank at set intervals from start to finish and match it against when the smoke thickened. If there is a chiller, check the oil temperature difference across it and whether its filter or heat exchanger is clogged. If there is a temperature cut-out, see how far its setting sits below the oil's flash point and whether the machine actually stops at that temperature.
Once temperature is confirmed, bring the cooling back first. Clean the chiller filter and heat exchanger and check the refrigerant and pump; if the temperature stays high after that, split long roughing runs with pauses or move the job to a machine with a larger tank and chiller. Set the temperature cut-out to the machine maker's guidance and the oil's flash point, and test it at regular intervals.
Hypothesis 4: high discharge energy
Suspect discharge energy when smoke thickens during roughing with peak current raised or pulse duration lengthened to save time, or when a large electrode sinks a wide area in one go. The tell-tale sign is smoke that jumps only under certain settings while the oil, level and temperature stay the same. A typical case is the week the roughing current was raised one step to meet a delivery date. Smoke drops noticeably when the job moves to finishing, and rises again when roughing resumes.
The more energy goes into each discharge, the more metal melts and vaporises and the more oil breaks down around it. In a study measuring aerosol at the operator's breathing zone in die-sinking EDM, concentration rose with higher peak current and longer pulse duration, and at 7 A and 520 µs it exceeded 5 mg/m³, the permissible exposure limit for respirable particulates. The authors warn that the habit of raising discharge energy for productivity increases both fire risk and emissions (Jose et al., 2010). In other measurements, raising the current increased every substance measured in the air (Evertz et al., 2006), and a study comparing settings through a designed experiment found peak current and pulse duration to have the strongest effect on breathing-zone concentration (Sivapirakasam et al., 2011).
Open the machining program for the smoky period and note the peak current, pulse duration and pause time, then set them beside the finishing settings that produce little smoke. Run a short cut with the same electrode and workpiece at one step lower current and see whether the smoke drops. Record the workpiece material as well: in a study comparing three materials, aerosol emission followed each material's removal rate, and constituents with low melting points made up a large share of the aerosol (Thiyagarajan et al., 2014).
With the cause narrowed to discharge energy, choose the roughing settings again with smoke and machining time weighed together. Measure the time difference between the present settings and settings with peak current one step lower and shorter pulses, and judge whether that difference is worth the smoke and fire risk. Where high energy is truly needed, hold the oil level and temperature more tightly and bring local exhaust close to the machining point.
Hypothesis 5: degraded oil
Consider degradation when the oil has not been changed for a long time, filters were not replaced on time, or the oil has turned black with sludge on the tank floor. The case is stronger when smoke and smell have worsened little by little over months rather than suddenly one day. Think of a machine whose oil was clear when first filled but is now so dark the electrode cannot be seen, with the filter pressure gauge needle sitting near the change mark. The same program now gives off a heavier smell than before.
EDM by-products include eroded metal particles, gases and aerosols, and substances formed as the dielectric breaks down with heat (Leppert, 2018). Whatever the filter does not catch stays and builds up in the oil, which breaks down a little with each discharge, adding carbon and sludge. A study that examined EDM with a structured hazard analysis found that contamination and long use of the dielectric increase emissions and raise fire risk (Jose et al., 2010). Under the same machining settings, therefore, oil that has been in service longer can give more smoke and smell.
Check the oil colour, the sludge on the tank floor, filter differential pressure and the last change date, and when the oil was first filled. Put a tank sample and new oil side by side in clear bottles to compare colour and haze, and if needed measure the sample's flash point by the same method as new oil to see whether light breakdown products have increased (ASTM International, 2020). Note whether smoke and smell drop just after a filter change or partial refill.
If degradation is indicated, fit new filters first, scoop out the sludge from the tank floor, and agree when to change the oil with the supplier. Base the change rule not on dates alone but on colour, filter pressure and machining hours together, and when changing, flush the tank and lines so no old oil remains. Shorten filter change intervals first on the machines with the heaviest workload.
Finding the cause
The five hypotheses need not be investigated all at once. Rule them out starting with what is easy to measure. Oil level and temperature take minutes with a rule and a thermometer, discharge settings are in the machining program, and top-ups and filter changes are already in the records. Items such as flash point that need a laboratory come after that.
The way the smoke appears is the next clue. Smoke that thickens only on tall workpieces or top-face work points to the oil level; smoke that grows with running time points to oil temperature; and smoke that rises in roughing and falls in finishing points to discharge energy. A sudden change after new oil or another oil was added points to flash point and volatility, while a slow worsening over months points to degradation and carbon build-up.
If that still does not settle it, run control trials that change one thing at a time: set the level to the height the machine manual recommends, run the same cut after the oil has cooled, drop the current one step, or fit new filters. Change only one thing at a time, or there is no telling which one worked. Smoke is hard to compare by eye, so record it the same way each time, with photographs from a fixed spot by the machine or readings from a simple monitor.
The final check is the air operators actually breathe. Once settings are corrected, have the industrial hygienist or a measurement service sample air at the breathing zone, to confirm that exposure is within limits and not just that the smoke is less visible. Metal particles make up a large share of die-sinking EDM aerosol (Sivapirakasam et al., 2011), so ask for the sampling to cover metals as well as oil mist.
The hypotheses can overlap. Raising discharge energy sends more heat into the oil, the oil temperature rises, and hot oil has a narrower margin to its flash point. Degraded oil with a light oil mixed in and a low level on top multiplies both smoke and fire risk. In such cases, put right the oil level and oil temperature first, as they lead straight to fire, then look again at the oil condition and discharge settings. While the safe height and temperature are not held, the effect of changing anything else cannot be compared, and the trial itself is dangerous.
Limits and cautions
Suitable oil level, upper oil temperature, discharge settings and oil change timing differ by machine, tank size, oil and workpiece, so numeric decisions follow the machine manual and the oil's TDS. The European standard EN 12957 covers safety requirements for EDM machines and their auxiliary equipment, so changing or disabling safety devices such as level monitoring or temperature cut-outs is done only with the machine maker (CEN, 2009). A review found that the way the dielectric is supplied strongly affects environmental impact, operator health and operational safety, so if smoke keeps returning, widen the review with suppliers to the process method itself (Valaki et al., 2015).
Safety matters too. EDM with hydrocarbon dielectrics carries fire and explosion risk, so keep open flames and sparks away from the machine, fit automatic fire suppression, and keep a suitable extinguisher close by (Jose et al., 2010). Follow the product's safety data sheet, the SDS, for protective equipment and ventilation, and place local exhaust close to the machining point. Never run a machine unattended if its level or temperature cut-out is not working.
Sources
- ASTM International. (2020). ASTM D93-20, Standard test methods for flash point by Pensky-Martens closed cup tester. https://www.astm.org/d0093-20.html
- European Committee for Standardization [CEN]. (2009). EN 12957:2001+A1:2009, Machine tools. Safety. Electro discharge machines.
- Evertz, S., Dott, W., & Eisentraeger, A. (2006). Electrical discharge machining: Occupational hygienic characterization using emission-based monitoring. International Journal of Hygiene and Environmental Health, 209(5), 423–434. https://doi.org/10.1016/j.ijheh.2006.04.005
- Ho, K. H., & Newman, S. T. (2003). State of the art electrical discharge machining (EDM). International Journal of Machine Tools and Manufacture, 43(13), 1287–1300. https://doi.org/10.1016/S0890-6955(03)00162-7
- Jose, M., Sivapirakasam, S. P., & Surianarayanan, M. (2010). Analysis of aerosol emission and hazard evaluation of electrical discharge machining (EDM) process. Industrial Health, 48(4), 478–486. https://doi.org/10.2486/indhealth.MS1127
- Leão, F. N., & Pashby, I. R. (2004). A review on the use of environmentally-friendly dielectric fluids in electrical discharge machining. Journal of Materials Processing Technology, 149(1–3), 341–346. https://doi.org/10.1016/j.jmatprotec.2003.10.043
- Leppert, T. (2018). A review on ecological and health impacts of electro discharge machining (EDM). AIP Conference Proceedings, 2017, 020014. https://doi.org/10.1063/1.5056277
- Sivapirakasam, S. P., Mathew, J., & Surianarayanan, M. (2011). Constituent analysis of aerosol generated from die sinking electrical discharge machining process. Process Safety and Environmental Protection, 89(2), 141–150. https://doi.org/10.1016/j.psep.2010.10.003
- Thiyagarajan, S., Sivapirakasam, S. P., Mathew, J., Surianarayanan, M., & Sundareswaran, K. (2014). Influence of workpiece materials on aerosol emission from die sinking electrical discharge machining process. Process Safety and Environmental Protection, 92(6), 739–749. https://doi.org/10.1016/j.psep.2014.01.001
- Valaki, J. B., Rathod, P. P., & Khatri, B. C. (2015). Environmental impact, personnel health and operational safety aspects of electric discharge machining: A review. Proceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture, 229(9), 1481–1491. https://doi.org/10.1177/0954405414543314