KALTECKOREA

BlogApplication notes

Why is a formed-in-place gasket so hard to take apart without damage?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Adhesives

Reaching for a longer pry bar or an abrasive disc is the usual response when a formed-in-place gasket will not let go, but that dents the flange and spoils its flatness, so the next assembly tends to leak. What actually makes the joint hard to open can be the wrong strength grade, a very thin layer, a layer that has cured further or swollen in oil over long service, the wrong removal method and tools, or a soft or rough face material, and often two or more at once.

Background

The bolts on a gearbox cover are all out for a service, yet the cover stays stuck to the housing and will not move. A screwdriver twisted in the seam chips the aluminium edge, and once the cover is finally off, scraping the old gasket from both faces takes a long time. At reassembly, the faces show scratch lines and dents here and there.

Dents and scratches that run across the face become paths for oil to escape after the next assembly. The face may need remachining or the part may need replacing, and the service takes that much longer. A vehicle maker's service bulletin warns that grinding off old gasket with abrasive pads removes metal quickly and spoils flatness, and that the grit is too fine for the oil filter to catch and can lead to early engine bearing failure (General Motors, 2024).

Formed-in-place gaskets for flanges come in two main kinds. Anaerobic sealants, which cure when air is shut out and they touch an active metal face, are used on rigid flanges; RTV silicones, which react with moisture in the air and cure to a rubber, are used on flexible flanges such as pressed covers and oil pans. Both cure while stuck to the two faces, so taking the joint apart means overcoming that grip, and anaerobic flange sealants are meant to come apart easily when a cleavage load wedges the joint open (Henkel, n.d.-b). For the same area, a bonded joint is weaker under cleavage or peel than under shear, because the load is concentrated on a very small area at the edge of the joint (Petrie, 2007). Taking the joint apart is therefore a matter of putting the right wedging force in the right place, and when that force goes elsewhere, the flange is damaged instead of the gasket.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: find the assembly record of which product went on that joint and when, compare it with the product's technical data sheet, the TDS, and keep the remaining gasket on both faces of the removed part rather than scraping it off straight away.

Hypothesis 1: wrong strength grade

Look at this hypothesis first on joints where some other product to hand was used instead of the specified flange sealant. Typical cases are a high-strength anaerobic meant for threadlocking or retaining put on a flange, a supplier change that brought in a product with a similar name but a different grade, and an anaerobic put on a thin cover meant for RTV. Say the maintenance shop ran out of the specified sealant and assembled a pump cover with another anaerobic product from the shelf. Months later all the bolts are out, but the cover sits on the housing as if it were one piece, and a spatula blade will not enter the seam.

Anaerobic products share a chemistry but differ in purpose and cured strength from one product to the next. The standard specification divides single-component anaerobic adhesives into groups by purpose, such as threadlocking, sealing and retaining, and within each group into classes by strength and grades by viscosity (ASTM International, 2016). An anaerobic flange sealant is made to add enough structural strength to cut micromovement between the parts while still coming apart under a cleavage load, and RTV seals moving covers by stretching like rubber (Henkel, n.d.-b). When a high-strength grade cures across the whole flange face, a wedge driven into the edge of the joint may not start a crack in the layer at all, and the force can bear first on the softer flange edge.

Confirm the product used first. Gather the assembly record, the label on any container left on site and the purchase records, and set the purpose and strength grade of the product actually applied beside those of the product specified for that joint. The layer left on the removed faces is a clue too. A hard, glassy film spread widely that a fingernail cannot dent is cured anaerobic, while a layer that stretches and tears like rubber is RTV. If RTV was specified and a hard film turns up, the product was changed.

If the grade is the cause, go back to the specified product at reassembly, and change the service instructions and shelf stock so that joints opened in service get only flange grades made to be taken apart. When a substitute is unavoidable, check in the TDS first that its purpose group and strength class match. For a part already stuck with a high-strength product, do not force it by twisting; follow the removal method in that product's TDS. One manufacturer advises that threadlocking anaerobics that will not yield to hand tools be heated to roughly 230 to 315 degrees Celsius to soften them and separated before they cool (Henkel, n.d.-a).

Hypothesis 2: very thin layer

This hypothesis shows itself on rigid flanges where two smoothly machined faces are clamped hard together. Typical joints are split gearbox housings, the bedplate to crankcase joint and pump housings, all tightened until metal nearly touches metal. Imagine opening, years later, a joint between two finely finished aluminium housing halves that were tightened to the specified torque. With every bolt out, no gap shows along the seam, there is nowhere to push even a thin blade, and the fitter ends up tapping a screwdriver into the seam.

A formed-in-place gasket is liquid at assembly, so surface roughness and clamping pressure set the thickness of the cured layer. According to one manufacturer's design guide, rough faces with a surface roughness Ra of 3.0 μm or more reach metal-to-metal contact regardless of pressure, while on smooth faces of Ra 0.3 μm or less the sealant forms an adhesive layer that gets thinner as clamping pressure rises. The same guide notes that real metal-to-metal contact does not exceed 25 to 35% of the area even on the most carefully finished faces, and that anaerobic sealants cure through gaps of only 0.1 to 0.25 mm, depending on the product (Henkel, n.d.-b). Most of the flange face is thus covered by a very thin, fully cured layer. In a study testing three adhesives at thicknesses of 0.2, 0.5 and 1 mm, lap-shear strength was higher the thinner the bond line (da Silva et al., 2006). A thin layer spread over a wide area grips hard and leaves no gap for a wedge, so the force of a lever lands on the metal at the edge of the joint.

Check on the removed faces. See whether the remaining layer is thin enough to be clear and spread evenly over the whole face, and whether metal shows through around the bolts. Find the specified roughness for the flange face on the drawing or in the machining record, and check against the assembly record that the bolts were not tightened above the specified torque. Look as well for pry lugs, recesses or jacking screw holes built into the housing for disassembly. If such features exist and the seam was still twisted open, the way the tools are handled needs looking at too.

If the layer is too thin for a wedge, the answer is to provide places to apply force. The same guide recommends designing in two or more pry lugs or recesses per joint, and where space is tight, using the bolt holes as jacking screw holes. Where no such features exist, as on pressed covers sealed with RTV, it describes driving a thin spatula, sharpened on its front and side edges, into the seam with light hammer taps and working it round the joint, a method that causes little to no surface damage (Henkel, n.d.-b). Ban twisting a screwdriver or chisel in the seam.

Hypothesis 3: long time in service

On equipment assembled long ago, equipment that has run hot without a break and flanges that have sat in oil, suspect what time has done to the layer. A joint that came apart easily when opened as a trial just after assembly but will not budge at an overhaul years later fits this case. A typical scene is lifting the cover off a gear reducer at its overhaul after several years in service. The sealant at the outer edge is hard and stuck fast, while on the inner, oil side it is swollen and soft, tearing apart and staying on both faces in pieces.

A formed-in-place gasket does not finish curing on the day of assembly. Moisture-cure silicone cures from the outside in; water that passes through the layer already cured goes on to cure the next layer, so the cured depth grows with the square root of time (Comyn et al., 1998). The middle of a wide flange keeps curing slowly for that much longer. Anaerobic sealant is set off by ions on the metal face, and in a study comparing cure on copper and on iron, the sealant cured fully on copper within hours at room temperature but did not finish curing on iron, where the model predicted a very long time to near-complete cure at room temperature (Abenojar et al., 2024). A joint on iron faces can therefore keep curing a little further while in service. In the same study, though, the strength of screws on iron barely changed after six hours, so on the anaerobic side time may add little to the grip. The oil side goes another way. In a test that soaked RTV silicone in hot engine oil, its hardness fell by about 30% and its volume swelled by about 20% (Herman & Donaldson, 2020). A swollen, softened layer does not come away cleanly but tears and stays behind, so scraping takes longer and the face has more chances to be damaged.

The first check is to find the assembly date, the running hours since and the running temperature in the records and set them against the cure time in the TDS. On the removed faces, see whether the layer differs between the outer edge and the inside. A hard outer edge with a swollen, soft oil side points to long exposure to oil and heat, and an anaerobic film is best compared for hardness with the film from a joint on the same equipment opened soon after assembly. Comparing in the service records how hard recently assembled and long-assembled joints on the same equipment were to open brings out the effect of time.

Allow more time for the older joints. For silicone, wet the exposed edge of the seam with a gasket remover that the TDS or the service instructions allow, let it soak briefly and then work a blade in; for anaerobic, follow the removal method in the product's TDS. Lift torn pieces on the oil side with a non-metallic scraper, and cover open ports so no pieces fall into the housing. For equipment run under harsh conditions, review the choice of a grade suited to the oil and temperature with the supplier.

Hypothesis 4: wrong removal method

Damage to the face usually happens at the hands of disassembly and cleaning. Expect it when the service is rushed, when the seam is twisted open with a screwdriver, when the old gasket is ground off with an abrasive disc or wire brush on a power tool, and when a steel scraper is held upright against the face. Take a rushed job where the cover was twisted open with a screwdriver and the remaining sealant was ground off the face with an abrasive disc on an air tool. The face shines, but swirl marks run in every direction, and the cover edge is dented in two or three places by the screwdriver tip.

One vehicle maker's service bulletin warns of exactly this scene. Abrasive pads can remove about 0.2 mm of metal in some 15 seconds, rounding the surface and spoiling its flatness so that oil, coolant and air leak, and the grit and metal particles can ruin engine bearings early. The same bulletin calls for a new razor-blade scraper held as parallel to the face as possible or a plastic scraper, for spraying on a cleaner and letting it soak for several minutes before lifting the material, and notes that how the face feels matters more than how it looks (General Motors, 2024). A cleaner works because silicone takes up solvent and swells. In a study that soaked silicone rubber in many solvents, the degree of swelling tracked the solvent's solubility parameter (Lee et al., 2003). A swollen layer holds the face less firmly and comes away even under a soft blade, so there is less need to scrape hard.

Read the shape of the damage first. Dents at the edge of the seam are where it was twisted open, swirl marks running every way are the trace of a rotary abrasive tool, and straight lines across the face are the marks of a scraper held upright. Lay a straightedge on the face and measure flatness with feeler gauges, and run a fingernail across the face to find any line that catches. Ask the fitters which tools are in the toolbox, what the service instructions say to use, and what they actually use.

Once tool marks confirm it, set working rules first. Use no abrasive discs, abrasive pads or wire brushes on the gasket faces of parts that see lubricant. Soak old gasket with a cleaner and lift it with a non-metallic scraper or with a fresh blade held parallel to the face, and plug oil passages and open ports during the work so no debris gets in. Open joints with the pry lugs or jacking screws provided, and build these rules into the service instructions and the toolbox kit. Where a face is already damaged, measure flatness and scratch depth and judge them against the part maker's limits.

Hypothesis 5: soft or rough face

This hypothesis shows most clearly when the two mating faces are of different materials. Typical joints are an aluminium cover on a cast iron block, a plastic cover on a steel housing, and sealant laid on rough, unmachined cast faces. Picture a joint between a cast iron block and an aluminium cover sealed with anaerobic sealant. Once apart, the sealant stays hard on the iron side and resists scraping, while the aluminium side has picked up deep marks from only a few passes of the scraper.

How firmly a face grips the sealant depends on its material and roughness. Before it cures, an adhesive flows into the fine valleys and pores of the surface, and once cured it is locked into them mechanically (Kinloch, 1987). Anaerobic sealant starts to cure from radicals formed when transition metal ions on the face, such as iron or copper, break down a peroxide (Raftery et al., 1997). One manufacturer's design guide states that greater roughness increases surface area and bond strength, and advises activators or heat on less active faces such as stainless steel, low-copper aluminium and anodised coatings (Henkel, n.d.-b). Rough cast iron or steel faces therefore grip the sealant hard, and an anaerobic layer on them cures more completely. Cast aluminium and plastics, on the other hand, are softer than steel tools, so when a strongly gripping joint is forced open or scraped, the softer side is damaged first.

Confirm the material and finish of both faces from the drawing and the parts themselves. Setting side by side which face the remaining sealant clings to and which face carries the damage shows at once whether the gripping side and the damaged side differ. If anaerobic sealant was used, look in the assembly record for whether an activator went on the less active face; a film that is hard only on the active side and soft on the other shows the material difference in the cure.

If the face material is making things worse, use only non-metallic scrapers on the softer face and soak the cleaner first into the side where the sealant stays firmly attached. Apply the separating force through lugs or jacking screws on the harder part so the edge of the softer part never acts as a fulcrum. Where the design can be changed, review the specified face roughness and the product grade with the sealant supplier, and put the disassembly features on the harder part.

Finding the cause

The five hypotheses need not be investigated all at once. Clear first what the records can clear. Which product and grade went on and when, and how long the unit has run since, are in the assembly and service records, and which tools were used to open and clean the joint can be learned by asking the fitters. Examining the faces and the remaining layer comes next.

Next, read what the removed faces say. Recording whether separation happened within the sealant layer or at the boundary between sealant and face, using the standard designations of failure patterns, makes later comparison easy (ISO, 2022). A wide, thin, hard glassy film points to the strength grade or a very thin layer; a swollen, torn layer on the oil side points to long service and oil exposure; sealant left on one face with the damage on the other points to the face material. Dents and swirl marks point by themselves to the removal method.

If that still does not settle it, run a control trial. Apply the specified product and the product actually used to separate pairs of test pieces with the same material and finish as the real parts, cure them under the same conditions, then part them with the same spatula and compare the effort needed and the damage to the faces. If the tools are suspect, change only the tools from the next disassembly and compare the outcome. Change only one thing at a time, or there is no telling what made the difference.

The final check is the faces before reassembly. Measure flatness with a straightedge and feeler gauges, feel for any line that catches, and make sure no old gasket remains thick enough to hold the faces apart. The cause has been put right only when the reassembled joint opens without damage, by the specified method, at the next service.

The hypotheses can overlap. When a high-strength grade goes into a joint whose layer is thin because smooth faces were clamped hard, and that joint then runs for years in heat and oil, the reasons it resists opening stack up. Trying to free such a joint with a stronger tool only damages the softer face. Put right the grip and the place to apply force first, through the product grade and the disassembly features, and then match the tools and method.

Limits and cautions

Cure time, disassembly temperature, allowable gap and face roughness differ by product and part, so numeric decisions follow the product's TDS and the equipment maker's service instructions. Where the face of a pressure-bearing joint or a safety-related part is damaged, do not decide on floor judgement alone whether to remachine or replace it; get the equipment maker's limits and a machining specialist's confirmation.

Safety matters too. For gasket removers and cleaning solvents, follow the product's safety data sheet, the SDS, for protective equipment and ventilation. The solvents named for cleaning off cured residue include methylene chloride (Henkel, n.d.-a), which OSHA regards as a potential occupational carcinogen (OSHA, n.d.). When heat is used to separate a joint, first clear residual oil and fuel in and around the part and any combustibles nearby, and handle hot parts with heat-resistant gloves. Support heavy covers and housings before separating them so they cannot drop suddenly.

Sources

  1. Abenojar, J., López de Armentia, S., del Real, J. C., & Martínez, M. A. (2024). Kinetic study of anaerobic adhesive curing on copper and iron base substrates. Materials, 17(12), 2886. https://doi.org/10.3390/ma17122886
  2. ASTM International. (2016). ASTM D5363-16, Standard specification for anaerobic single-component adhesives (AN). https://store.astm.org/d5363-16.html
  3. Comyn, J., Day, J., & Shaw, S. J. (1998). Kinetics of moisture cure of silicone sealants. The Journal of Adhesion, 66(1–4), 289–301. https://doi.org/10.1080/00218469808009970
  4. da Silva, L. F. M., Rodrigues, T. N. S. S., Figueiredo, M. A. V., de Moura, M. F. S. F., & Chousal, J. A. G. (2006). Effect of adhesive type and thickness on the lap shear strength. The Journal of Adhesion, 82(11), 1091–1115. https://doi.org/10.1080/00218460600948511
  5. General Motors. (2024). Use of surface conditioning disks when cleaning gasket sealing surfaces and/or reused parts (Service Bulletin 00-06-01-012N). Copy published by the U.S. National Highway Traffic Safety Administration. https://static.nhtsa.gov/odi/tsbs/2024/MC-11006670-0001.pdf
  6. Henkel. (n.d.-a). Anaerobic adhesives: Frequently asked questions. Retrieved November 2026. https://next.henkel-adhesives.com/us/en/support/faqs/products-and-technologies/anaerobic-adhesives.html
  7. Henkel. (n.d.-b). Leak-free flanges: A Loctite design guide. https://dm.henkel-dam.com/is/content/henkel/Gasketing%20Design%20Guide-Final_LR
  8. Herman, J., & Donaldson, K. (2020). Experimental investigation on the impact of engine oil on RTV silicone (SAE Technical Paper 2020-01-5002). SAE International. https://doi.org/10.4271/2020-01-5002
  9. International Organization for Standardization [ISO]. (2022). ISO 10365:2022, Adhesives — Designation of main failure patterns. https://www.iso.org/standard/80800.html
  10. Kinloch, A. J. (1987). Adhesion and adhesives: Science and technology. Chapman and Hall. https://doi.org/10.1007/978-94-015-7764-9
  11. Lee, J. N., Park, C., & Whitesides, G. M. (2003). Solvent compatibility of poly(dimethylsiloxane)-based microfluidic devices. Analytical Chemistry, 75, 6544–6554. https://doi.org/10.1021/ac0346712
  12. Occupational Safety and Health Administration [OSHA]. (n.d.). Methylene chloride. U.S. Department of Labor. Retrieved November 2026. https://www.osha.gov/methylene-chloride
  13. Petrie, E. M. (2007). Handbook of adhesives and sealants (2nd ed.). McGraw-Hill. ISBN 9780071479165
  14. Raftery, D., Smyth, M. R., & Leonard, R. G. (1997). Investigations into the cumene hydroperoxide-based cure chemistry of anaerobic adhesives. International Journal of Adhesion and Adhesives, 17(4), 349–352. https://doi.org/10.1016/S0143-7496(97)00029-8

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.