Why do forging lubricant nozzles keep clogging?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Metalworking Fluids (MWF)

Poking a blocked nozzle clear with a needle or wire and starting again is the usual response, but the lumps and residue that block it can form in the tank and lines before the liquid reaches the nozzle, and rough tools damage the orifice, so clearing alone tends to end in another blockage. What actually lies behind it can be a broken dispersion, hard dilution water, poor tank agitation, liquid drying at the nozzle tip or microbial growth, and sometimes two or more at once.

Background

The die after spraying shows bare metal along one corner. Down the row of nozzles, one gives a thin squirt and stops, and another sprays off to one side and wets the wrong place. The operator stops the press, unscrews the nozzle, pokes it with a needle and refits it, and the next shift does the same again.

A blocked nozzle costs more than the downtime. Where its share of the die gets less graphite, friction rises; in experiments, friction went up once the graphite left on the die fell below a certain amount (Mendez et al., n.d.). The report that die life doubled in an industrial process after fitting a device that gives a fixed dose at a fixed interval suggests, conversely, that a good deal can be lost when spraying wavers (Hawryluk et al., 2023). Clearing the nozzle has its own price. Cleaning with unsuitable tools damages nozzles, and an orifice worn wider passes more flow and bigger droplets at lower pressure and distorts the spray pattern (Spraying Systems Co., n.d.).

A water-based graphite lubricant is made of water, graphite, binder and additives. The water carries the graphite and helps regulate die temperature, the binder helps the graphite stick to the die and the dried film hold up, and additives such as surfactants and thickeners add performance (Quaker Houghton, 2022). Graphite particles have a large surface and attract each other strongly, so they clump readily in water, and a dispersant is used to keep them apart (Kolb et al., 2022). A nozzle blocks in two main ways: solid particles in the liquid lodge in the orifice, or the liquid evaporates and leaves solids built up inside the orifice or around its edge (Spraying Systems Co., n.d.).

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: keep the material taken out of the nozzles rather than throwing it away, log which nozzle blocked and when, with tank concentration, dilution water, tank temperature and concentrate storage records at the time, and compare them with the lubricant's technical data sheet, the TDS.

Hypothesis 1: broken dispersion

The graphite may fail to stay evenly suspended when the concentrate has been stored for a long time, kept in a hot store in summer or outdoors below freezing, or when two different lubricants have been mixed in one tank. The habit of drawing only from the top of a drum without mixing in the settled layer belongs here too. The day a drum of concentrate that wintered in an outdoor store is opened in spring and poured into the dilution tank is such a case. Rolling the drum still leaves a hard layer at the bottom, and a drop of the diluted liquid on white paper leaves small black specks behind.

A dispersion holds because the dispersant blocks the attraction between particles. Once particles clump together, the balance that kept them afloat by Brownian motion is lost and they settle under gravity, and since settling speed rises with the square of the particle radius, clumps sink much faster than single particles. The same study cites earlier reports that unstable dispersions raise the risk of nozzle clogging (Kolb et al., 2022). Storage conditions also unsettle a dispersion. One supplier's guidance calls for water-based forging fluids to be stored at 5 to 40 °C and notes that graphite products can flocculate if frozen and that high storage temperature speeds graphite settling (Quaker Houghton, 2022).

Start with a jar test. Put the tank's diluted liquid and a fresh dilution of new concentrate at the same ratio side by side in clear bottles, and over time compare how fast the top clears and the layer that builds at the bottom. If the tank sample settles noticeably faster, take the dispersion as broken. Pour some of the dilution through a fine strainer to see what grains stay behind, and check the drum's manufacturing date and the storage temperature records against the supplier's range.

Before a concentrate with a broken dispersion goes into use, settle with the supplier whether it can still be used. Keep concentrate indoors within the supplier's temperature range, use the oldest stock first, and mix the whole drum evenly before drawing from it. Do not mix different products in one tank, and empty and rinse the tank and lines when changing product.

Hypothesis 2: hard dilution water

Suspect the calcium and magnesium in the dilution water, its hardness, in plants that use well water or untreated industrial water for dilution, right after a change of water source, and on lines where a tank depleted by evaporation has been topped up with water only. Evaporation takes away only water and leaves dissolved ions behind, so a tank topped up with plain water gathers those ions over time. Picture a few weeks after a plant expansion switched the dilution water to well water: nozzles now block at noticeably shorter intervals, and a thin grey residue has settled on the tank walls and strainers.

Particles in water are kept apart by the repulsion between the electric double layers around their surfaces. As dissolved ions increase, the double layer thins, and above a certain concentration, the critical coagulation concentration, particles clump rapidly. The expression for double-layer thickness contains the square of ion charge, so divalent ions such as calcium and magnesium thin it more than the same amount of monovalent ions (Kolb et al., 2022). In research on water-mix metalworking fluids, adding hard water salts likewise made the emulsion droplets grow and the fluid less stable, and the authors explain that such conditions arise as divalent and trivalent ions accumulate over time from hard water top-ups and from workpieces. In the same study EDTA, the chelating agent commonly added, could be ineffective or highly inefficient at preventing this (Zimmerman et al., 2004). A die-casting release agent supplier recommends soft water for dilution and states that hard water can lead to nozzle plugging and build-up in the cavity, while very pure water can lead to die corrosion (Chem-Trend, n.d.).

Hardness shows up as soon as it is measured. Take the dilution water and the tank liquid separately, measure hardness by the standard titration method (ASTM International, 2017), and compare with the supplier's water requirement. If the dilution water is soft but the tank liquid is hard, ions have built up through evaporation and water top-ups. Public guidance likewise advises checking incoming water for hardness, pH and bacteria and agreeing suitable water quality with the supplier (HSE, n.d.).

If hard water looks like the cause, change the dilution water. Use softened or otherwise treated water that meets the supplier's requirement, setting the range with the supplier so it does not swing to water that is too pure. Top up the tank with diluted lubricant at the set ratio, not water alone, so ions do not accumulate, and if they already have, empty the tank and make a fresh batch. Where the water cannot be changed, ask the supplier whether a formulation tolerant of hard water exists.

Hypothesis 3: poor tank agitation

Mixing becomes a problem wherever the liquid stands still or circulates too little: where the stirrer and circulation pump are switched off at night or on holidays, where agitation is weak for the size of the tank, where long lines still carry branches that are seldom used, or where the suction sits close to the tank bottom. Say a press that stood idle for a few days under a changed production plan is started again. Only the nozzles at the end of the line to that press spit out thick lumps at the first spray, and soon one or two stop.

Graphite is heavier than water and, without stirring, settles to the bottom of the tank and the low side of the lines. Suppliers advise continuous stirring not only during dilution but in the dedicated tank before spraying, so graphite does not settle, and state that settling degrades lubricating performance (FUCHS, n.d.; Quaker Houghton, 2022). Places where flow stops also suit microbes. Public guidance says that fluid standing in sumps and pipes lets biofilm grow, so it should be kept circulating with pumps, and that dead-ends and seldom-used branches should be removed or flushed regularly (HSE, n.d.). A layer settled on the low side of a line can be swept out all at once when flow restarts and carried to the nozzles.

Take samples from the top and bottom of the tank and right before the nozzles at the end of the line, dry a set amount of each and compare the solids left. Supplier guidance likewise describes checking the dilution ratio by measuring the dried film (Quaker Houghton, 2022). If the bottom and the line end are clearly richer, mixing falls short. Confirm from records or timer settings whether the stirrer and circulation pump actually run at night and on holidays, and mark dead-ends and unused branches on the piping drawing.

The remedy is to make stirring and circulation continuous. Keep the tank stirred while in use, and add a return loop that brings the liquid back from near the nozzles so it does not stand in the lines. Remove unused branches, and flush any that must stay at a fixed interval. Raise the suction off the bottom, and check strainers and filters regularly for blockages (HSE, n.d.).

Hypothesis 4: dried-on nozzle tips

Suspect the nozzle tip in processes with long gaps between sprays, in layouts that put the nozzles close to the hot die, on nozzles that keep dripping after the spray ends, and where liquid stays in the nozzle and its short feed line during stops. Air atomising nozzles, which spray liquid mixed with air, are especially prone to this. Watch the first spray after a lunch stop: a few nozzles throw a lopsided spray, and a hard grey ring sits around the orifice at their tips.

In liquid left at the nozzle tip, the water goes first. The nozzle industry calls the build-up that evaporation leaves inside the orifice or on its outer edge, obstructing flow and degrading performance, caking or bearding, and notes that air atomising nozzles are especially sensitive to it (Spraying Systems Co., n.d.). Graphite lubricants contain a binder meant to help the dried film hold on the die (Quaker Houghton, 2022), so a layer dried at the nozzle tip may not easily redisperse in water either. Experiments also show that only part of the sprayed graphite stays on the die and the rest disperses into the air (Mendez et al., n.d.), so mist drifting around the press settling on the outside of the nozzles is worth keeping in mind.

When the blockage happens is the clue. If it clusters at the first spray after stops rather than during continuous running, the case leans towards drying at the tip. Take the nozzle out and tell apart a particle lodged inside the orifice from a ring built up around the outside of its edge. Check whether drops form and fall at the tip after spraying stops, and whether the nozzle body heats up from the die, using a thermometer rather than a hand.

If the tip is drying up, work on keeping liquid from standing in the nozzle and drying there. Stop dripping with a shut-off that cuts the liquid as the spray ends, and add a step that purges the nozzles with water or air before stops or between sprays. Move nozzles to where they take less heat from the die, or shield them. For cleaning, soak and use a soft brush instead of a needle or wire; swapping in a spare nozzle and cleaning the removed one away from the press does less harm to the orifice.

Hypothesis 5: microbial growth

Microbes find room to grow in tanks where diluted lubricant is kept for a long time, tanks in warm places, tanks without lids that let in dust and debris, and lines with low output where the liquid turns over slowly. One supplier notes that high storage temperature raises the risk of bacterial growth (Quaker Houghton, 2022). Think of opening the lid of a dilution tank left standing over the summer holiday. A sour or rotten smell rises, a slimy film clings to the surface and the tank walls, and sticky lumps are caught in the strainer before the nozzles.

Water-mix metalworking fluids are highly vulnerable to microbes, and contaminated fluids have been reported to carry 10⁴ to 10¹⁰ colony-forming units per millilitre. Microbes can build a sticky film called biofilm, and this film resists common disinfection methods (Saha & Donofrio, 2012). In a study of fungi, microbial growth together with metal chips and swarf clogged filters and left residue, and fungal contamination of machine surfaces was the norm rather than the exception (Ruiz et al., 2024). Microbes and dispersion stability are bound up with each other: metalworking fluids destabilised by hard water salts or low pH could sustain a larger microbial load (Zimmerman et al., 2004).

Check smell and appearance daily, and measure microbes with dip slides. A dip slide is a simple test: a plate coated with culture medium is dipped in the liquid, incubated, and the colonies counted. Public guidance calls for dip slides once a week and treats results at or above 10⁴ CFU/mL as microbial growth and at or above 10⁶ CFU/mL as poor control that needs immediate action (HSE, n.d.). See as well whether material from strainers and nozzles is slimy and sticky, and whether a film lines the tank walls and pipes.

When microbes are confirmed, put the management conditions right first. Public guidance says to add biocide at the supplier's recommended dose only if growth continues after measures on concentration, pH, contamination, temperature, agitation and flow have all been tried, and to drain and clean the system when contamination is heavy (HSE, n.d.). Biofilm does not go easily with chemicals alone, so scrub the tank, lines and strainers physically before refilling with fresh dilution. Cover the tank, and make only as much dilution as will be used before it stands too long.

Finding the cause

Rule them out one at a time, starting with what can be done without stopping the press. Hardness of the dilution water and tank liquid, solids at the top and bottom of the tank, and dip slides need only samples, and the stirrer timer and concentrate storage records are already on site. A jar test only needs to stand for a day or two. Pull the nozzles for a close look during a scheduled stop.

When and where the blockages happen are the next clues. If they cluster at the first spray after stops, look at drying at the tip and settling in the lines; if at the nozzles at the end of a line, look at stirring and circulation first. If they began after a change of water source, suspect dilution water hardness; if after a new drum of concentrate was opened, suspect the dispersion. If things worsened with a smell as the weather warmed or after the tank stood for a long time, look at microbes.

What comes out of the nozzle also helps narrow things down. A particle lodged inside the orifice points to lumps formed in the liquid, and a ring settled around the outer edge to solids left by evaporation (Spraying Systems Co., n.d.). Slimy, sticky lumps raise the suspicion of biofilm. If that still does not settle it, run control trials that change one thing at a time: empty the tank and make a batch with new concentrate and treated water, run the stirrer day and night, or add only a nozzle purge before stops. Change only one thing at a time, or there is no telling which one worked.

The final check is the interval between blockages. Count nozzle cleanings per shift or per set output on the same basis as before the change, and the job is done only when the figure has fallen and stays down for several weeks. On the die, confirm with photographs that the areas that used to go bare are now evenly covered.

The hypotheses can travel together. Hardness ions break a dispersion and form clumps, clumps settle faster in a poorly stirred tank, and microbes grow more readily in standing places and in a destabilised liquid. In such cases, restore the baseline first: empty and clean the tank, refill it with water that meets the supplier's requirement and new concentrate, and make stirring and circulation continuous. Then look for any remaining blockage at the nozzle tips.

Limits and cautions

Suitable dilution water hardness, dilution ratio, storage temperature, and biocide type and dose differ by lubricant, so numeric decisions follow the product's TDS and the supplier's guidance. Choose softening equipment and biocides with the supplier and the person responsible for water treatment, and do not decide alone on the floor whether a concentrate with a broken dispersion can be used again.

Safety matters too. Handle lubricants and biocides with the protective equipment set out in the product's safety data sheet, the SDS. Water-mix metalworking fluids can harm health through skin contact and through breathing in mist (OSHA, n.d.), so when cleaning a tank contaminated by microbes, wear gloves and eye protection and avoid breathing the mist. Remove or clean nozzles only with the press and the spray unit stopped and locked out, and wear eye protection when blowing out with compressed air.

Sources

  1. ASTM International. (2017). ASTM D1126-17, Standard test method for hardness in water. https://store.astm.org/d1126-17.html
  2. Chem-Trend. (n.d.). What is the recommended quality of dilution water to be used with die lubricants? [FAQ]. Retrieved November 2026. https://chemtrend.com/faq/what-is-the-recommended-quality-of-dilution-water-to-be-used-with-die-lubricants
  3. FUCHS. (n.d.). LUBRODAL F 24 W [Product information]. Retrieved November 2026. https://www.fuchs.com/de/en/product/product/148408-LUBRODAL-F-24-W/
  4. Hawryluk, M., Dudkiewicz, Ł., Marzec, J., Rychlik, M., & Tkocz, R. (2023). Selected aspects of lubrication in die forging processes at elevated temperatures—A review. Lubricants, 11(5), 206. https://doi.org/10.3390/lubricants11050206
  5. Health and Safety Executive [HSE]. (n.d.). Managing fluid quality (MW5, COSHH essentials for machining with metalworking fluids). Retrieved November 2026. https://www.hse.gov.uk/pubns/guidance/mw5.pdf
  6. Kolb, C. G., Lehmann, M., Kulmer, D., & Zaeh, M. F. (2022). Modeling of the stability of water-based graphite dispersions using polyvinylpyrrolidone on the basis of the DLVO theory. Heliyon, 8(12), e11988. https://doi.org/10.1016/j.heliyon.2022.e11988
  7. Mendez, P. F., Castro, G., & Martinez, F. (n.d.). Influence of heat transfer on the application of solid lubricant on hot dies [Author manuscript]. Colorado School of Mines. Retrieved November 2026. https://sites.ualberta.ca/~pmendez/Publications/Papers/2007_jopd_lubricant.pdf
  8. Occupational Safety and Health Administration [OSHA]. (n.d.). Metalworking fluids. U.S. Department of Labor. Retrieved November 2026. https://www.osha.gov/metalworking-fluids
  9. Quaker Houghton. (2022). Storage, preparation and dosing of forging fluid [Skill builder]. https://home.quakerhoughton.com/wp-content/uploads/2022/05/skb_Storage_Preparation_and_Dosing_of_Forging_Fluid_EN_A4.pdf
  10. Ruiz, C., von Känel, G., Burkard, S., & Küenzi, P. (2024). Fusarium spp. in metalworking fluid systems: Companions forever. Pathogens, 13(11), 990. https://doi.org/10.3390/pathogens13110990
  11. Saha, R., & Donofrio, R. S. (2012). The microbiology of metalworking fluids. Applied Microbiology and Biotechnology, 94(5), 1119–1130. https://doi.org/10.1007/s00253-012-4055-7
  12. Spraying Systems Co. (n.d.). Common spray problems. Retrieved November 2026. https://spray.com/resources/spraying-basics/spray-optimization/common-spray-problems
  13. Zimmerman, J. B., Hayes, K. F., & Skerlos, S. J. (2004). Influence of ion accumulation on the emulsion stability and performance of semi-synthetic metalworking fluids. Environmental Science & Technology, 38(8), 2482–2490. https://doi.org/10.1021/es0340477

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.