KALTECKOREA

BlogApplication notes

Why did cooling performance drop after raising glycol concentration?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Heat Transfer & Cooling

It is easy to assume more glycol means more safety, but as concentration rises, the same equipment carries and passes on less heat, so a step taken against freezing can cut cooling performance. What actually drags performance down can be lower specific heat and conductivity, higher viscosity and laminar flow, reduced pump flow, more glycol than needed, or fouling and ageing, and sometimes two or more at once.

Background

With winter coming and freezing a worry, the glycol concentration in a process cooling loop was raised. A few days later, the coolant supply temperature will not come down to set point, the chiller runs without a break, and the process side leaving the heat exchanger is warmer than before. Nothing in the equipment changed, only the coolant, which makes it all the more puzzling.

When cooling falls short, temperature-sensitive processes drift in quality, and production has to slow down or the chiller runs longer, which costs more energy. In a system with spare design capacity, the capacity lost to glycol may go unnoticed, but in one already running near its design load, glycol can make matters worse, and the difference shows on the hottest days (Dow, 2008).

Coolant does two jobs: it loads heat and carries it, and it takes heat in and hands it over across the walls of heat exchangers. The first depends on flow and specific heat, the second on the heat transfer coefficient of the fluid film near the wall, which is set by thermal conductivity, viscosity and the state of the flow (Bergman et al., 2011). As the concentration of an aqueous glycol solution rises, its specific heat and thermal conductivity fall and its viscosity rises, and the viscosity gap widens as temperature drops (Bohne et al., 1984; Melinder, 2007). Raising concentration changes both jobs at once.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: measure the actual concentration with a refractometer scaled for the glycol in use, set supply and return temperatures, flow and pressures either side of the pump beside the records from before the concentration was raised, and compare them with the coolant's technical data sheet, the TDS, and the equipment's design conditions.

Hypothesis 1: weaker heat transport

This hypothesis comes first when glycol is put into a water-only loop for the first time, when concentration is raised in one large step, and when the coolant is changed while flow is left as it was. Take a process cooling loop filled with glycol for the first time in autumn: the flowmeter reads as before, but the temperature difference between supply and return across the load has widened, and the process outlet creeps up a little each afternoon.

The heat a coolant carries is the product of mass flow, specific heat and temperature difference (Bergman et al., 2011). A fluid with lower specific heat must warm up more to carry the same heat at the same flow, so the return runs hotter and the chiller and exchangers work at less favourable temperatures. Handing heat over suffers too. The film coefficient shrinks as thermal conductivity falls, and the conductivity of ethylene glycol and water mixtures falls as the glycol share rises (Sun & Teja, 2003). Propylene glycol moves the same way with different numbers, so calculations should use the property tables for the glycol actually in use (Melinder, 2007).

Confirm it with numbers. From the present flow and temperature difference, and specific heat and density at the actual concentration and operating temperature, calculate the heat the load actually receives, and run the same calculation on the records from water or the previous concentration for comparison. If the calculated loss of capacity is close to the loss actually seen, property change alone explains it; if the real loss is much worse, another hypothesis is also at work.

If property change explains it, the remedy is to use only as much as needed. The coolant supplier recommends a concentration giving a freezing point about 3°C below the lowest expected temperature, and states that the less glycol used, the higher the relative heat transfer efficiency (Dow, 2008). If capacity still falls short, review with the designer raising flow to narrow the temperature difference or adding heat exchanger area.

Hypothesis 2: laminar flow

In systems run at low temperature, in small-bore tubes or narrow plate heat exchanger channels, and in systems turned down to low flow at part load, ask whether the state of the flow has changed. Suppose the supply temperature was lowered to chill the product further, and the concentration raised along with it, yet the lower the supply temperature goes, the wider the approach between the two sides of the exchanger becomes, and the process side does not cool as expected.

Whether flow in a tube is turbulent or laminar is set by the Reynolds number, velocity times tube diameter divided by kinematic viscosity. In a smooth tube, flow becomes laminar below about 2300, and a band above that is transitional (Bergman et al., 2011). In laminar flow the fluid slides along the wall in layers without mixing, so the heat transfer coefficient falls well below its turbulent value, and in the transitional band the coefficient swings widely with Reynolds number (Gnielinski, 2010). As noted above, the viscosity of aqueous glycol climbs steeply as the glycol share rises and the temperature falls, so raising concentration and lowering temperature cut the Reynolds number from both sides at once. The supplier's design data also say the turbulent correlation should be used only above a Reynolds number of 10,000, so applying it to a system that has dropped below that overstates the coefficient (Dow, 2008).

What needs checking is the Reynolds number at the actual operating point. Calculate it from the flow per tube or channel, the channel dimensions, and viscosity at the actual concentration and the lowest operating temperature. Repeat the calculation for conditions before the concentration was raised, and it shows whether flow that used to be turbulent has dropped into the transitional or laminar range. Asking the exchanger maker to rerate performance at today's conditions is another good check.

If flow has slipped towards laminar, work on restoring the Reynolds number. Bringing concentration down to what is needed is the most direct step; if that is not enough, review with the exchanger maker changing the number of passes or raising flow to lift velocity. At very low temperatures, viscosity can climb so high that operation becomes impractical without larger pumps (Dow, 2008), so for processes that need such temperatures, choosing with the supplier a coolant whose viscosity rises less is another option.

Hypothesis 3: reduced flow

When pumps and piping are unchanged but now circulate a stronger, more viscous fluid, suspect that flow has dropped. On the morning round the day after the concentration went up, the flowmeter sits lower than before, the pump motor current is slightly higher if anything, and the valve on the most distant load is wide open.

Centrifugal pump curves are usually tested on water. With a liquid more viscous than water, the same pump's head, flow and efficiency fall below the water curve and its power draw rises, and a guideline exists for estimating real performance by applying correction factors to the water curve (Hydraulic Institute, 2021). The piping resists more as well. Pipe friction losses grow as Reynolds number falls, and in laminar flow the friction factor is inversely proportional to Reynolds number (Bergman et al., 2011). With the pump curve lower and the system curve higher, the operating point where they cross moves to a lower flow, and less flow makes the widening temperature difference and falling Reynolds number described above worse still.

Do not rely on the installed flowmeter alone; measure flow once more by an independent method, such as a clamp-on ultrasonic flowmeter. Record the differential pressure across the pump and the motor current, plot the operating point on a viscosity-corrected pump curve, and check the pressure drop across strainers too. If the operating point has been pushed well to the left of the curve, reduced flow is part of the loss.

With low flow confirmed, clean clogged strainers and rebalance the valves first. If flow is still short, review a change of pump speed or impeller with the pump supplier on the basis of a viscosity correction, and at root bring the concentration back to what is needed to lower viscosity. When upsizing a pump, check the motor power as well.

Hypothesis 4: excess glycol

Sometimes the actual concentration is higher than people think. That happens when a little more concentrate is added before each winter, when only water evaporates from an open expansion tank and leaves the glycol behind, when top-ups are made with concentrate, when an ethylene glycol scale is read for propylene glycol or the other way round, and when the first fill was not mixed well and has layered. A loop that has had a little concentrate added every winter for several years reads well above the design concentration when checked with a refractometer.

The freezing point does not keep falling as concentration rises. The solid–liquid phase diagram of ethylene glycol and water is especially complex in the 55 to 85 weight percent range, enough that two laboratories measured it again independently, and a hydrate of glycol and water in a 1:1 ratio was identified at 77.5 weight percent (Cordray et al., 1996). The coolant supplier also says it is rarely necessary to go above 50 to 55 percent glycol in water, while for corrosion protection it asks for at least 25 to 30 percent (Dow, 2008). Within that span, every bit of excess adds only freeze margin that is never needed while enlarging the losses in the three hypotheses above: lower specific heat and conductivity, higher viscosity and less flow.

Checking starts from an accurate concentration. Take samples from several points in the loop and read them on a refractometer matched to the glycol type, and send them for laboratory analysis if readings disagree. Look up the freezing point for that concentration in the coolant TDS and compare it with the lowest temperature expected on site to see how much margin is left. Reconcile the top-up records with how much concentrate has been drawn from stock.

If the loop is too strong, drain some off and refill with good-quality water to bring it back to target. Make top-ups with a solution premixed to the target concentration, and check whether the expansion tank is a closed type that limits evaporation. Posting the target concentration, the minimum temperature it was based on and the date it was measured near the loop keeps the habit of adding concentrate every year from coming back.

Hypothesis 5: fouling and ageing

If performance slid gradually over months rather than dropping exactly when the concentration was raised, look at the coolant itself and the exchanger surfaces. Candidates are coolant left unchanged for a long time, loops that often see high temperatures or air ingress, loops topped up with a different product or automotive antifreeze, and loops diluted with hard water. Open the strainer on a loop whose coolant has not been changed in years and black sludge is caught in it, and a sample drawn off is dark and smells burnt.

Glycol ages too. All glycols form organic acids as they break down, the breakdown is faster with oxygen and heat, and the acids lower pH and promote corrosion (Dow, 2008). In tests on aqueous glycol, acidic breakdown products formed under every condition, with the most degradation when copper was present in aerated solution (Rossiter et al., 1985). When corrosion products and sludge build up on exchanger walls, the layer adds one more resistance to heat flow, and such fouling lowers heat transfer, raises pressure loss and becomes a major operating cost (Müller-Steinhagen et al., 2011).

A sample's appearance and smell are the first clues. The supplier's guide treats a black or dark grey colour, an oily layer on top, a burnt smell and heavy sludge as signs that replacement may be needed, and asks for pH to be held between 8 and 10, with fluid below 7 replaced (Dow, 2008). For the exchanger, check the operating records for whether the approach temperature and pressure loss have both grown over the months. Ask the laboratory to analyse pH, inhibitor level, organic acids and metals together.

Where sludge and fouling are found, clean the exchanger surfaces first. Flush the system, refill with inhibited industrial glycol at the required concentration, and do not use automotive antifreeze or other products for top-ups, because silicate-bearing antifreeze can form silicate gel that cuts both flow and heat transfer (Hercamp & Hudgens, 1985). Seal off where air gets in, and set the replacement interval by regular analysis.

Finding the cause

Start with what the instruments can show. Concentration, supply and return temperatures, flow and pressures either side of the pump can all be measured today without stopping the plant. Coolant analysis and exchanger inspection follow.

The shape of the decline splits the paths. A step drop at exactly the moment the concentration was raised points to the glycol itself: properties, laminar flow, reduced flow or excess concentration. Within that group, a wider temperature difference at unchanged flow points first to specific heat and conductivity, lower flow to the pump operating point, and a loss that grows markedly at lower temperatures to laminar flow. A gradual slide over months, with pressure loss rising alongside, points to fouling and ageing.

Calculation is itself a good comparison test. Recompute Reynolds number and heat duty with properties at the actual concentration and temperature and the measured flow; if the predicted capacity matches what is seen, the drop is explained by the physics of glycol. If the real figure is clearly worse than predicted, something outside the calculation is at work, such as fouled exchanger surfaces or a misread flow. Bear in mind that the smaller film coefficient governs heat transfer, so in an exchanger where the process side carries most of the resistance, changing the coolant has little effect (Dow, 2008).

After that, change one thing at a time. Bring concentration down to target and log supply temperature and heat duty at the same load for several days; if capacity is still short, move on to the pump and strainers, and finally to cleaning the exchangers. The job can be called done once supply temperature has been seen to hold set point at design load in the hottest part of the year.

The hypotheses feed one another. Excess concentration lowers specific heat and conductivity and raises viscosity, which cuts flow, and less flow lowers the Reynolds number further, pushing towards laminar flow. A fouling layer on top removes whatever margin is left. In such cases, put concentration right first, then flow, and finally the exchanger surfaces, because while concentration is unsettled, the effect of changing anything else cannot be compared fairly.

Limits and cautions

The required concentration depends on the lowest site temperature, how much piping is exposed outdoors and whether ice crystals can be tolerated, so numeric decisions follow the freezing point tables in the coolant TDS and the designer's judgement. Lowering concentration also lowers freeze protection, so for systems with outdoor coils or piping that stands idle in winter, recheck the minimum temperature before diluting. Propylene glycol and ethylene glycol differ in properties, so do not borrow one's tables for the other, and leave rerating of chillers and exchangers to their makers.

Safety matters too. Ethylene glycol can do harm when inhaled, swallowed or in contact with skin and eyes (NIOSH, n.d.), so wear gloves and eye protection as the product's safety data sheet, the SDS, requires. In systems that could touch food or drinking water, use only coolants approved for that purpose. Collect drained coolant in lidded containers and dispose of it under local rules.

Sources

  1. Bergman, T. L., Lavine, A. S., Incropera, F. P., & DeWitt, D. P. (2011). Fundamentals of heat and mass transfer (7th ed.). Wiley.
  2. Bohne, D., Fischer, S., & Obermeier, E. (1984). Thermal conductivity, density, viscosity, and Prandtl-numbers of ethylene glycol-water mixtures. Berichte der Bunsengesellschaft für physikalische Chemie, 88(8), 739–742. https://doi.org/10.1002/bbpc.19840880813
  3. Cordray, D. R., Kaplan, L. R., Woyciesjes, P. M., & Kozak, T. F. (1996). Solid-liquid phase diagram for ethylene glycol + water. Fluid Phase Equilibria, 117(1–2), 146–152. https://doi.org/10.1016/0378-3812(95)02947-8
  4. Dow Chemical Company [Dow]. (2008). Engineering and operating guide for DOWTHERM SR-1 and DOWTHERM 4000 inhibited ethylene glycol-based heat transfer fluids (Form No. 180-01190-0208). https://cdn.shopify.com/s/files/1/0299/3356/8138/files/DOWTHERM_SR-1_Inhibited_Ethylene_Glycol_Heat_Transfer_Fluid_Engineering_and_Operating_Guide.pdf
  5. Gnielinski, V. (2010). G1 Heat transfer in pipe flow. In VDI e.V. (Ed.), VDI heat atlas (2nd ed., pp. 691–700). Springer. https://doi.org/10.1007/978-3-540-77877-6_34
  6. Hercamp, R. D., & Hudgens, R. D. (1985). Silicate gelation in heavy-duty diesel engine cooling systems (SAE Technical Paper 852327). SAE International. https://doi.org/10.4271/852327
  7. Hydraulic Institute. (2021). ANSI/HI 9.6.7-2021, Rotodynamic pumps: Guideline for effects of liquid viscosity on performance. https://www.pumps.org/wp-content/uploads/2022/01/9.6.7d.pdf
  8. Melinder, Å. (2007). Thermophysical properties of aqueous solutions used as secondary working fluids [Doctoral thesis, KTH Royal Institute of Technology]. ISBN 978-91-7178-707-1.
  9. Müller-Steinhagen, H., Malayeri, M. R., & Watkinson, A. P. (2011). Heat exchanger fouling: Mitigation and cleaning strategies. Heat Transfer Engineering, 32(3–4), 189–196. https://doi.org/10.1080/01457632.2010.503108
  10. National Institute for Occupational Safety and Health [NIOSH]. (n.d.). Ethylene glycol. NIOSH Pocket Guide to Chemical Hazards. Retrieved November 2026. https://www.cdc.gov/niosh/npg/npgd0272.html
  11. Rossiter, W. J., Jr., Godette, M., Brown, P. W., & Galuk, K. G. (1985). An investigation of the degradation of aqueous ethylene glycol and propylene glycol solutions using ion chromatography. Solar Energy Materials, 11, 455–467. https://doi.org/10.1016/0165-1633(85)90016-4
  12. Sun, T., & Teja, A. S. (2003). Density, viscosity, and thermal conductivity of aqueous ethylene, diethylene, and triethylene glycol mixtures between 290 K and 450 K. Journal of Chemical & Engineering Data, 48(1), 198–202. https://doi.org/10.1021/je025610o

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.