BlogApplication notes
Why do heavy metals exceed discharge limits?
- Type
- Application notes
- Published
- 23 November 2026
- Prepared by
- Jonghwan Moon
- Product group
- Water & Waste Treatment
Adding more alkali or coagulant is the usual response when effluent metals exceed the limit, but metal that stays dissolved and metal that escapes as solids have different causes, so more chemical alone rarely settles it. What actually lies behind it can be a precipitation pH that does not suit every metal, complexing agents holding metals in solution, incomplete reduction of hexavalent chromium, weak coagulation and settling, or solids carried over the clarifier, and sometimes two or more at once.
Background
The routine effluent test report arrives showing copper, nickel or zinc above the limit. Nothing unusual was logged, and the treated water looked clear, yet the figure sits above the line. Exceeding a discharge limit brings regulatory action and the cost of putting it right, and raising chemical doses without knowing the cause pushes up both chemical and sludge disposal costs. Heavy metals can harm aquatic life once discharged, so the very reason the plant exists is at stake.
The backbone of heavy metal treatment is chemical precipitation. Alkali is added to turn dissolved metal ions into insoluble hydroxides, the small particles are gathered with coagulant and polymer and settled in a clarifier, and only clear water leaves. For cost, performance and simplicity, precipitation is still regarded as the most favourable option at industrial scale (Blais et al., 2008). How soluble the resulting metal compounds are, however, depends on pH, and most are least soluble on the alkaline side (EPA, 2000).
So metal stays in the effluent in one of two ways: it never becomes solid and leaves dissolved, or it becomes solid but fails to settle and leaves suspended in the water. An unfiltered sample also picks up the metal inside particles, so both routes push the figure up. The performance of a precipitation system is judged by how well suspended solids are removed, and when solids removal falls short, metal concentrations come out high as well (EPA, 1983).
In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: split one effluent sample in two, analyse one as taken and the other after filtering to separate dissolved metal from total metal, and compare the reaction tank pH, chemical doses and flow records from the day of the exceedance with the treatment chemicals' technical data sheets, the TDS, and the design conditions.
Hypothesis 1: wrong precipitation pH
When several metals enter one reaction tank and only one of them exceeds the limit, look at pH first. It happens especially when a new plating line starts sending a different metal into the wastewater, when the reaction tank pH setpoint was fixed long ago and never revisited, and when hydroxide deposits coat the pH electrode so it reads something other than the real value. Think of a plant that takes nickel plating and zinc plating rinses into one reaction tank. Nickel has stayed within the limit for months, but zinc keeps crossing the line, while the reaction tank pH recorder always sits near the same setpoint.
The key is that each metal is least soluble at a different pH. Metal hydroxide solubility changes with pH, and the suitable pH for precipitation depends both on the metal to be removed and on whether it is bound as hydroxide, carbonate or sulphide, so treatment conditions have to be set case by case (EPA, 2000). The suitable pH for hydroxide precipitation is generally between 8.8 and 9.3 but varies with the composition of the waste, and some metals, such as lead and silver, settle better as compounds other than hydroxides (EPA, 1983). More awkward still, some metal hydroxides are amphoteric. They dissolve in acid and dissolve again in strong alkali, so in wastewater carrying several metals the best pH for one metal can put another back into solution (Pohl, 2020). If the reaction tank runs at a single pH, the metal that settles least well at that value stays in the effluent.
Checking begins with measuring pH properly. Calibrate the reaction tank electrode with standard buffers and take a separate reading inside the tank with a handheld meter to see whether it agrees with the recorder. Then divide real wastewater into several jars, set each to a slightly different pH, run them through the same coagulation and settling, and filter the supernatant to measure dissolved concentration metal by metal. The resulting curve of pH against metal concentration shows which metal remains at the current setpoint and whether any pH band brings every metal within the limit. This kind of jar test, comparing coagulation conditions side by side, has a standard procedure (ASTM International, 2019).
If a pH band exists where every metal meets the limit, move the setpoint to the middle of it and set and keep intervals for cleaning and calibrating the electrode. If no such band exists, stop trying to remove everything at once and consider two-stage precipitation: settle and separate some metals at one pH, then readjust pH to remove the rest. Sulphide precipitation is another option. Metal sulphides are not amphoteric, so they can remove metals to low concentrations over a wide pH range (Fu & Wang, 2011). Either way, run jar tests on real wastewater before making the change.
Hypothesis 2: complexed metals
When pH is right and the treated water is clear but filtered samples still show high metal, suspect complexing agents. A complexing agent wraps around a metal ion and holds it in solution, and such agents are common in electroless plating baths, printed circuit board etchants and cleaners. This hypothesis moves to the front right after a change of cleaner or plating chemical supplier, or when rinses from electroless plating or etching lines mix into the general wastewater. Picture the month after a new alkaline cleaner came into use. Reaction tank pH and chemical doses are as before and the clarifier supernatant is clear, yet copper in the effluent creeps upward.
Keeping metal from settling is exactly what a complexing agent is for. Wastewater from electroless plating, immersion plating, etching and printed circuit board manufacture carries metal tied up by complexing agents, which works against the precipitation that most metal removal methods rely on. Complexing agents such as phosphates, tartrates, EDTA and ammonia reduce metal removal by hydroxide precipitation, and rinses after etchants based on ammonium hydroxide and ammonium chloride carry copper bound to ammonia (EPA, 1983). The bond between metal and complexing agent can be stronger than the pull towards forming a hydroxide, so adding more alkali leaves the metal still bound. Methods for removing bound metals therefore usually break the complex first, or make another metal take its place, before precipitating, and oxidation, replacement and coprecipitation, sulphide precipitation and adsorption have all been studied (Zhu et al., 2019).
The easiest clue is the difference between filtered and unfiltered samples. If the two are almost equal and dissolved metal is high, the metal is in the water, not in particles. If, in jar tests, raising pH well above normal barely lowers dissolved metal, the case leans towards complexing agents. Collect the safety data sheets, the SDS, for the cleaners, plating baths and etchants in use, look for ingredients such as EDTA, citrates, tartrates and ammonia, and measure ammonia nitrogen in the effluent too. Matching the rise in metal against the times when each line's rinse comes in narrows down the source.
Once the cause narrows to complexing agents, separate the flows first. Collect complexed metal wastewater apart from other streams, treat it separately, and give it its own solids separation, such as a membrane filter or a high-pH clarifier. To support hydroxide precipitation, consider ferrous sulphate treatment, which adds iron ions so the metals settle with them, or sulphide precipitation (EPA, 1983). Decide which chemical and how much with jar tests on that wastewater. Also discuss with the supplier whether a cleaner without complexing agents could be used, weighing cleaning quality alongside.
Hypothesis 3: chromium not reduced
When chromium exceeds the limit, the reduction step is the first place to look, all the more at a plant with processes that use hexavalent chromium, such as chrome plating, chromate conversion or chromic acid etching. Hexavalent chromium does not settle as a hydroxide as it is, so a separate reduction tank converts it to trivalent chromium before precipitation. Problems are likely when an extra line has increased the chromium rinse flow but the reduction tank and chemical pump are unchanged, when the reducing agent tank has run dry or the pump has clogged, and when calibration of the pH or oxidation-reduction potential electrodes has slipped. In the first busy season after an expansion, chromium rinse arrives nonstop and water from the reduction tank joins the other streams straight away.
Hexavalent chromium is highly toxic and dissolves and moves readily in water, whereas trivalent chromium is less toxic and can be settled as a hydroxide, so reduction is the first step of treatment (Barrera-Díaz et al., 2012). Reducing agents such as sulphur dioxide, sodium bisulphite, sodium metabisulphite and ferrous sulphate pass electrons to hexavalent chromium and turn it into trivalent chromium, which then leaves with the other metals by alkaline precipitation. The reaction favours low pH: a pH of 2 to 3 is normal for complete reduction, and above pH 5 the reaction is slow. Oxidising agents such as dissolved oxygen and ferric iron use up the reducing agent first and interfere with reduction, and the process is controlled by pH and oxidation-reduction potential, or ORP (EPA, 1983). If incompletely reduced water passes to the clarifier, the remaining hexavalent chromium will not settle however well pH is set, and it leaves in the effluent still dissolved.
Taking a sample at the reduction tank outlet and measuring hexavalent chromium separately is the quickest check. If hexavalent chromium makes up a large share of total chromium in the effluent, the reduction step is the cause; if most of it is trivalent, reduction worked and the leak is in precipitation or solids separation. Calibrate the reduction tank pH and ORP electrodes, check them again with handheld meters against the recorded values, and look as well at the reducing agent tank level, pump output, recent chromium rinse flow and residence time in the reduction tank.
The core of the remedy is a layout that finishes reduction before chromium wastewater mixes with anything else. Set the pH and ORP setpoints from the reducing agent supplier's recommended range and jar tests, and if chromium rinse flow has grown, recalculate whether residence time is enough and enlarge the reduction tank or chemical feed capacity. Put reducing agent stock and the pump on the daily checklist, and confirm hexavalent chromium at the reduction tank outlet at fixed intervals.
Hypothesis 4: weak floc settling
A cloudy clarifier supernatant with high metal only in unfiltered samples suggests the metal has become solid but has not clumped into coarse particles. It shows up after a change in the type or dose of coagulant or polymer, when the polymer solution has been kept too long or the way it is made up has changed, when mixing after polymer addition is so strong that it breaks the clumps apart, and when the wastewater has changed so the old doses no longer fit. Looking into the flocculation tank, tiny pinpoint particles drift in the water without gathering into larger clumps, and cloudy water carries on as far as the overflow weir at the end of the clarifier.
Metal hydroxides tend to form first as very small colloidal particles that do not settle well on their own, so coagulating agents are added to help them settle. Once alkali has set the precipitation pH, a polymer coagulant gathers the insoluble metal compound particles into coarse clumps, or floc, that settle rapidly by gravity (EPA, 1983, 2000). Aluminium and iron coagulants act in two ways. Positively charged hydrolysis products neutralise the negative charge on particles, or, at higher doses, an amorphous hydroxide precipitate sweeps particles up and enmeshes them. Which one dominates depends on pH and dose (Duan & Gregory, 2003). Organic polymers are widely used to grow floc by bridging particles with their long chains or by neutralising charge, and which polymer suits depends on the water and its particles (Bolto & Gregory, 2007). If any of these goes wrong, the metal becomes solid yet passes through the clarifier as small suspended particles.
Jar tests show the cause most clearly. Take water just past the reaction tank, add coagulant and polymer at several dose steps, run rapid mixing, slow mixing and settling times matched to the plant in the same way for each jar, and compare floc size, settling speed, and supernatant turbidity and metal concentration (ASTM International, 2019). If the jar at the current dose is worst while jars at other doses settle clear, the dose is the problem; if only the jar using freshly made polymer improves, the condition of the polymer solution is. On the floor, also check the make-up date and concentration of the polymer solution, the actual output of the chemical pumps and the speed of the flocculation tank mixer.
If coagulation is confirmed, reset the doses to the condition that settled clearest in the jar tests. More is not better, and overdosing can reduce treatment effectiveness (EPA, 2000). Make up polymer solution at the supplier's recommended concentration and ageing time, and use it within a set period. After polymer addition, keep mixing gentle so the floc is not broken, and repeat jar tests whenever the wastewater composition changes to keep the doses right.
Hypothesis 5: solids carry-over
Sometimes jar tests settle well while solids and metal are both high at the actual clarifier outlet. Then the problem lies in the clarifier and what follows it rather than in the chemicals. Typical cases are treating a weekend's stored wastewater all at once or flow rising above design after rain, a broken sludge withdrawal pump or a lengthened withdrawal interval, and no filter after the clarifier. Say a plant has turned the flow right up on a Monday morning to empty its holding tank. The sludge layer has risen almost to the clarifier surface, and pieces of brown floc ride over the weir with the outgoing water.
A clarifier gives floc time to sink to the bottom while water passes slowly through. When flow rises, that time shortens, and if bottom sludge is not withdrawn on time, the sludge layer rises and pushes even settled floc towards the outlet. Solids removal is a reliable indicator of how a precipitation system is performing, and insufficient solids removal can result in high metal concentrations. That is why a filter is placed after the clarifier to polish out suspended solids, such as metal hydroxides that did not settle, and it also acts as a safeguard for the discharge when something goes wrong in the clarifier (EPA, 1983). The metal in floc is already solid, so in this case dissolved metal is low and only unfiltered metal is high.
Measure turbidity or suspended solids in the clarifier outlet water and set filtered and unfiltered metal from the same sample side by side. Measure the height of the sludge layer with a sludge blanket sampler, a long tube that brings up a sample from top to bottom, and check the flow records for whether flow on the day of the exceedance went beyond the design range and whether any sludge withdrawals were missed. Where effluent turbidity is logged continuously, overlaying the times turbidity rose with flow and withdrawal times can reveal the cause.
The remedy starts with evening out the flow into the clarifier. Use a holding tank to release surges gradually, and set the treatment flow within the clarifier's design range. Set the sludge withdrawal interval by layer height, and keep a standby withdrawal pump. If there is no filter, such as a sand filter, after the clarifier, consider installing one, and logging effluent turbidity continuously with an alarm on any rise allows action before the limit is breached.
Finding the cause
Five hypotheses do not mean five separate investigations. The first fork is the comparison of dissolved and total metal described in the background. High dissolved metal means the metal never became solid, so look at the chemistry: pH, complexing agents and chromium reduction. Low dissolved metal with high total metal means it became solid but was not removed, so look at coagulation and the clarifier. This one analysis cuts the field of search roughly in half.
The next clue is which metal exceeded. If only chromium did, measure hexavalent chromium at the reduction tank outlet first. If only one or two of several metals exceed and changing pH changes which one, the precipitation pH does not suit the metals; if a particular metal such as copper or nickel rises in dissolved form after a change of cleaner or plating chemical, suspect complexing agents. If every metal rises together along with suspended solids, solids escaping is more likely than the chemistry of any one metal.
If that still does not settle it, run control jar tests on the same wastewater. Set out jars that change only pH in steps, jars that change only coagulant and polymer dose, and jars with a chemical added to break complexes, changing one thing at a time so it is clear what made the difference. If the jars settle clear but solids leave only in the plant clarifier, the cause is flow and sludge management, not chemicals.
The hypotheses can overlap. Raising pH further to pull out metal held by complexing agents can redissolve amphoteric metals, and adding more chemical makes more sludge and loads the clarifier harder. In such cases put the chemistry right first, by separating flows and completing reduction, then reset coagulation doses, and finally adjust clarifier flow and sludge withdrawal, because while an earlier stage is unsettled, the effect of changing a later one cannot be compared fairly.
After the fix, measure dissolved and total metal again by the same method over several days, covering the times when wastewater composition changes. Do not stop at one result within the limit; the job is done only when the limit holds under the conditions that caused the exceedance before.
Limits and cautions
Discharge limit parameters, values and analytical methods differ by country, region, industry and permit conditions, so decisions follow the applicable regulations, the permit and results from an accredited laboratory. Suitable precipitation pH, chemical doses and reduction conditions vary with wastewater composition, so set them from the treatment chemicals' TDS and jar tests on real wastewater. If complexed or mixed metal wastewater keeps exceeding the limit, equipment changes may be needed, so review it with a water treatment design specialist.
Safety matters too. Hexavalent chromium can cause cancer in people and harms the skin and airways, so use protective equipment and ventilation that limit exposure when handling chromium wastewater and the reduction tank (OSHA, n.d.). With sulphide precipitation, toxic hydrogen sulphide can form if pH drops below about 8, so hold pH and ventilate the treatment tanks (EPA, 1983). Acids, alkalis and reducing agents are corrosive, so wear protective equipment according to each product's SDS and do not store acids and reducing agents together.
Sources
- ASTM International. (2019). ASTM D2035-19, Standard practice for coagulation-flocculation jar test of water. https://store.astm.org/d2035-19.html
- Barrera-Díaz, C. E., Lugo-Lugo, V., & Bilyeu, B. (2012). A review of chemical, electrochemical and biological methods for aqueous Cr(VI) reduction. Journal of Hazardous Materials, 223–224, 1–12. https://doi.org/10.1016/j.jhazmat.2012.04.054
- Blais, J.-F., Djedidi, Z., Ben Cheikh, R., Tyagi, R. D., & Mercier, G. (2008). Metals precipitation from effluents: Review. Practice Periodical of Hazardous, Toxic, and Radioactive Waste Management, 12(3), 135–149. https://doi.org/10.1061/(ASCE)1090-025X(2008)12:3(135)
- Bolto, B., & Gregory, J. (2007). Organic polyelectrolytes in water treatment. Water Research, 41(11), 2301–2324. https://doi.org/10.1016/j.watres.2007.03.012
- Duan, J., & Gregory, J. (2003). Coagulation by hydrolysing metal salts. Advances in Colloid and Interface Science, 100–102, 475–502. https://doi.org/10.1016/S0001-8686(02)00067-2
- Fu, F., & Wang, Q. (2011). Removal of heavy metal ions from wastewaters: A review. Journal of Environmental Management, 92(3), 407–418. https://doi.org/10.1016/j.jenvman.2010.11.011
- Occupational Safety and Health Administration [OSHA]. (n.d.). Hexavalent chromium. U.S. Department of Labor. Retrieved November 2026. https://www.osha.gov/hexavalent-chromium
- Pohl, A. (2020). Removal of heavy metal ions from water and wastewaters by sulfur-containing precipitation agents. Water, Air, & Soil Pollution, 231(10), 503. https://doi.org/10.1007/s11270-020-04863-w
- U.S. Environmental Protection Agency [EPA]. (1983). Development document for effluent limitations guidelines and new source performance standards for the metal finishing point source category. Office of Water Regulations and Standards. https://www.epa.gov/sites/default/files/2015-10/documents/metal-finishing_dd_1983.pdf
- U.S. Environmental Protection Agency [EPA]. (2000). Wastewater technology fact sheet: Chemical precipitation (EPA 832-F-00-018). Office of Water.
- Zhu, Y., Fan, W., Zhou, T., & Li, X. (2019). Removal of chelated heavy metals from aqueous solution: A review of current methods and mechanisms. Science of the Total Environment, 678, 253–266. https://doi.org/10.1016/j.scitotenv.2019.04.416