KALTECKOREA

BlogApplication notes

Why does honing miss the bore finish?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Metalworking Fluids (MWF)

Changing stones or resetting pressure and time is the usual response when a honed bore misses its finish, but if the honing oil the stones work in stays the same, the miss tends to come back. What actually lies behind it can be the wrong oil viscosity, swarf recirculating through coarse filtration, loaded stones, low oil flow or a changing oil temperature, and sometimes two or more at once.

Background

A cylinder block or hydraulic cylinder bore is honed, the profilometer goes in, and the reading falls outside the drawing range. Some days it is too rough with deep scratches; other days it is too smooth and the cross-hatch looks faint. The machine and the stones have not changed, yet the values differ between morning and afternoon and from bore to bore.

Bores out of range must be re-honed or scrapped, and extra measurement and rework lengthen the cycle. The bigger loss comes after assembly. The valleys of the honing pattern are where oil is held and made to flow, and the parameter for valley depth stands for oil retention, heat removal and room for wear debris (Buj-Corral et al., 2019), so when it drifts, friction, wear and leakage at rings, pistons and seals can change.

Honing presses stones radially against the bore wall while the tool rotates and strokes up and down, so the abrasive grains cut fine grooves that cross one another (Klocke, 2009). The grains remove very small chips, and the honing oil lubricates and cools between them and washes chips out of the stone pores. The ability to wash chips out has been reported to depend on the fluid type, its viscosity and its surface tension (Grosse et al., 2015). So the finish is set not only by stones and pressure but also by the condition of the oil the stones work in.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: record the finish values of the out-of-range bores with the time of honing and the spindle number, and compare the oil temperature and filter pressure drop at the time with the honing oil's technical data sheet, the TDS, and the machine settings.

Hypothesis 1: wrong oil viscosity

Look at viscosity after a change of honing oil supplier or grade, when hydraulic or slideway oil from the machine leaks into the honing oil tank, and when the material being honed has changed but the oil has not. A case in point is a line that honed only cast iron blocks taking on steel sleeves as well. Cast iron bores still land within range, but the steel sleeves vary widely in finish, and long, thin chips cling to the stone face.

Viscosity governs how well the honing oil washes chips out of the stone pores. A paper on honing fluids finds that low viscosity and low surface tension help flush the pores, and it also cites earlier work finding that low-viscosity honing oil suits materials that make short, broken chips, with viscosity rising as chips get longer (Grosse et al., 2015). In the same paper, honing cast iron with a polymer dilution gave a higher removal rate and lower roughness than a mineral honing oil, but that came from changing the whole fluid type, not viscosity alone. Viscosity moves a long way with temperature, so comparisons must always use values at the same temperature (ASTM International, 2020).

The first check is the kinematic viscosity of the oil in use. Measure a tank sample and new oil at the same reference temperature by the standard method and compare both with the TDS value (ISO, 2020). If the used oil is noticeably thicker or thinner than new oil, suspect another oil mixing in, and check the records for a tank level that rises regardless of output or for more frequent top-ups of the hydraulic system. Grouping finish values by material shows which material the viscosity does not suit.

If another oil mixing in is the cause, stop the leak first and replace part or all of the oil until viscosity is back within the TDS range. On a line with mixed materials, choose a viscosity grade to suit the chip form with the honing oil supplier again, and if needed split materials across machines. After changing viscosity, measure the finish again with stones and pressure unchanged, so the effect of viscosity can be seen on its own.

Hypothesis 2: coarse filtration

Suspect filtration on finishing passes with fine-grit stones, in cast iron work that throws off much fine graphite and iron, and in systems where filters are changed late or a blocked filter lets oil past through its bypass valve. Average roughness has barely moved, yet a few bores show one or two unusually deep scratches running along the stroke. Around then, the filter pressure gauge needle sits near the change mark, and grey, mud-like sediment lies thick on the tank floor.

Fine particles that escape filtration ride the pump back to the cut, where they behave like a third abrasive caught between stone and bore, wearing tools and degrading the surface (Khan et al., 2021). Grains in the stone are held by the bond and cut only so deep, but particles carried in the oil are not held; pressed under the stone, they roll or drag, and if they are larger than the stone's grit they can leave scratches deeper than the intended grooves. Graphite dust from cast iron and grains shed from the stones join them.

Begin by drawing oil downstream of the filter and looking at it. Stand it in a clean bottle and see whether anything settles, and when figures are needed, measure cleanliness with the standard method that expresses particle counts as size-graded codes (ISO, 2021). Check the pressure drop across the filter, the change dates and any sign that the bypass valve has opened. If deep scratches cluster just before filter changes and fall away just after, filtration is the cause.

Set the filter rating again to match the finishing stone's grit, and change filters when the pressure drop reaches a set value. Arrange an alarm for an open bypass valve, add a magnetic separator for ferrous work, and give the tank a section from which sediment can be drawn off. Remove floor sediment whenever the oil is changed, or the fresh oil is dirty from the start. Cast iron lines, with much graphite dust and shed grain, load filters heavily, so keep filter change records alongside output and set the change interval from them.

Hypothesis 3: loaded stones

Loading tends to appear with dense, fine-grit stones, with soft materials whose chips stick readily, and at the low pressures of the finishing stage. It also follows a decision to stretch the dressing interval. A typical pattern: over the day, bores grow steadily smoother and the cross-hatch fades, while the time to remove the same stock creeps up. Pull a stone and its face shines in patches, as if metal had been smeared onto it.

A stone keeps cutting only while dull grains break away and fresh ones are exposed. This balance, in which dull grains take enough force to pull out of the bond and the bond wears with them to reveal new grains, is called the self-sharpening of the stone (Mahlfeld & Dröder, 2023). When the balance fails, chips mixed with oil fill the stone pores. In one experiment, roughness and removal rate generally rose with grit size and grain density, but once the stone loaded, grains pushed the material aside instead of cutting it and roughness and removal rate fell together (Buj-Corral et al., 2019). So a loaded stone makes the bore too smooth, and the valleys tend to turn shallow.

Looking at the stone face under a magnifier is quickest. Sharp, standing grains with even marks where others have pulled out mean a healthy stone; smoothly worn grains and pores filled with metal mean loading. Log the stock removed and the time per cycle, and see whether the drop in roughness lines up with the drop in removal rate. The same study reports that changes in the acoustic emission signal during honing can reveal loading (Buj-Corral et al., 2019), so if such monitoring is fitted, read its record too.

Dress a loaded stone to open a fresh face, and reset the dressing interval to the finish trend. If it keeps happening, choose with the stone supplier a bond and grain density that suit the material, and look at honing oil viscosity and flow as well, so the pores are flushed. Finish honing is sensitive to small changes in pressure (Buj-Corral et al., 2021), so change pressure one step at a time.

Hypothesis 4: low oil flow

Flow tends to fall short when nozzles are half blocked with chips, when nozzle aim has shifted during a tool change, and when pressure has fallen because of a worn pump or a blocked filter. Shapes where oil struggles to get in and out, such as blind bores and deep bores, make it worse. Think of a multi-spindle machine where the bores from one spindle alone miss the finish, and the oil stream from that spindle's nozzle alone comes out thin and broken.

The amount of oil and the way it is supplied change the result in their own right. A study of friction, cooling and lubrication in grinding found that not only the fluid type and composition but also the supply method shape the process and its results, with flow in the nozzles and in the contact zone as the key (Brinksmeier et al., 1999). In honing, too, short flow can leave chips less well flushed from the stone pores, so loading may come sooner (Grosse et al., 2015), and heat tends to stay in the contact zone. A review of honing research notes that lowering part temperature during honing leads to a better surface finish and smaller shape deviation (Sender & Buj-Corral, 2023).

Measure the oil actually delivered at each spindle. Catching it in a container for a set time and weighing it or reading the volume will do, and note the pressure gauge reading ahead of the nozzle too. Look at nozzle bores and aim, and confirm that the stream points where stone meets bore. Checking the records for out-of-range bores clustering on one spindle or on blind-bore shapes shows whether flow is the likely cause.

Clean blocked nozzles, re-aim them and bring the flow back to the value the machine builder and the TDS recommend. A flow meter or pressure switch ahead of the nozzle that alerts when supply drops means the next shortfall is caught before the finish drifts. For shapes where oil pools, such as blind bores, look at supplying oil through the tool.

Hypothesis 5: oil temperature

Watch temperature on machines with no oil cooler or a small tank, in midsummer, and on Monday mornings starting with oil left cold over the weekend. On some days, for the first few hours after start-up, finish and diameter drift little by little and settle only by the afternoon. With the same program and the same stones, the first parts of the morning and the afternoon parts form separate groups of readings.

Temperature changes both the oil and the machine. The viscosity of petroleum oils falls as temperature rises (ASTM International, 2020), so cold oil is thick and warm oil thin, and the flushing power and stone contact conditions seen above shift through the day. Warmed honing oil and machining heat have been shown to expand the honing head almost uniformly, affecting the accuracy of diameters set by in-process automatic sizing (Yokoyama et al., 1990). The part sits in the same oil and warms with it, which fits reports that lowering part temperature during honing improves finish and form (Sender & Buj-Corral, 2023).

Log oil temperature at the tank and at the nozzle by the hour, and set the finish and diameter readings for the same times alongside. Measure the temperature of parts taken to the gauge room as well, to confirm whether they were measured before cooling. If morning and afternoon readings split and the gap tracks oil temperature, temperature is the cause. If a cooler is fitted, check the temperature difference across it and its set point to confirm it is working. Without a cooler, first find out how far the oil temperature swings over a day.

Once temperature is confirmed, the answer is to hold the oil within a set temperature band. Fit a cooler or a larger one, and on cold mornings circulate the oil and load the first part only after it reaches the set temperature. Measure parts after they have settled to gauge room temperature, and on machines with automatic sizing, recalibrate once temperature is stable.

Finding the cause

The five hypotheses need not all be tackled from the start. Rule out first what can be seen without stopping the machine. Oil temperature, filter pressure drop and the oil stream at the nozzles can be checked in passing, and finish records already exist. What needs samples pulled or laboratory work, such as viscosity, cleanliness analysis and stone inspection, comes after. When gathering records, log the bores within range as well as those outside it, or there is nothing to compare against.

First look at the direction of the miss. If bores grow too smooth, valleys turn shallow and removal slows as well, suspect loaded stones and oil that fails to flush chips, meaning viscosity and flow. If finish is too rough or mixed with deep scratches, look first at swarf that escaped filtration. Always measure with the same parameters and the same filter settings, and for plateau-honed surfaces split peaks, core and valleys using the values taken from the material ratio curve (ISO, 1996).

Next is when and where it happens. Misses on one spindle only point to that spindle's nozzle and flow; a split between morning and afternoon points to oil temperature; a cluster just before filter changes points to filtration; and a start on the day oil or material changed points to viscosity. A saw-tooth trend that improves after dressing and then slowly worsens points to stone loading.

If that still does not settle it, run control trials that change one thing at a time. Hone a few test bores with the same stones right after fitting a new filter, right after dressing, right after changing to fresh oil and in the afternoon once temperature is stable, and compare the finish. Change only one thing at a time, or there is no telling what worked. Afterwards, look again at the spread of readings with the same parameters and sample size as before, and the job is done only when the share within range has recovered.

The hypotheses overlap. Dirty oil from coarse filtration fills the stone pores faster, low flow brings on loading sooner and leaves heat behind, and high temperature lowers viscosity and shifts the flushing conditions again. In such cases, put the oil side right first, meaning cleanliness, flow, temperature and viscosity, and then reset stones and pressure, because while the oil is unsettled the effect of a stone change cannot be compared fairly.

Limits and cautions

Suitable finish specifications, honing oil viscosity, filter rating, flow and temperature differ by material, stone, machine and part duty, so numeric decisions follow the drawing, the honing oil's TDS and the machine and stone suppliers' guidance. Finish parameters change with the instrument's filter and evaluation length, so first make sure supplier and customer measure under the same conditions. For functional surfaces such as engine or hydraulic parts, judge form and cross-hatch angle as well as finish together with the quality engineer.

Safety matters too. Use protective equipment for honing oil as the product's safety data sheet, the SDS, directs, and limit skin contact with metalworking fluids and breathing in their mist (NIOSH, 1998). Change filters and stones or clean nozzles only after the machine is fully stopped and locked out, and clear oily floors and rags at once to prevent slips and fires.

Sources

  1. ASTM International. (2020). ASTM D341-20, Standard practice for viscosity-temperature equations and charts for liquid petroleum or hydrocarbon products.
  2. Brinksmeier, E., Heinzel, C., & Wittmann, M. (1999). Friction, cooling and lubrication in grinding. CIRP Annals, 48(2), 581–598. https://doi.org/10.1016/S0007-8506(07)63236-3
  3. Buj-Corral, I., Álvarez-Flórez, J., & Domínguez-Fernández, A. (2019). Effect of grain size and density of abrasive on surface roughness, material removal rate and acoustic emission signal in rough honing processes. Metals, 9(8), 860. https://doi.org/10.3390/met9080860
  4. Buj-Corral, I., Rodero-de-Lamo, L., & Marco-Almagro, L. (2021). Optimization and sensitivity analysis of the cutting conditions in rough, semi-finish and finish honing. Materials, 15(1), 75. https://doi.org/10.3390/ma15010075
  5. Grosse, T., Winter, M., Baron, S., Hoffmeister, H.-W., Herrmann, C., & Dröder, K. (2015). Honing with polymer based cutting fluids. CIRP Journal of Manufacturing Science and Technology, 11, 89–98. https://doi.org/10.1016/j.cirpj.2015.09.001
  6. International Organization for Standardization [ISO]. (1996). ISO 13565-2:1996, Geometrical product specifications (GPS) — Surface texture: Profile method; Surfaces having stratified functional properties — Part 2: Height characterization using the linear material ratio curve.
  7. International Organization for Standardization [ISO]. (2020). ISO 3104:2020, Petroleum products — Transparent and opaque liquids — Determination of kinematic viscosity and calculation of dynamic viscosity.
  8. International Organization for Standardization [ISO]. (2021). ISO 4406:2021, Hydraulic fluid power — Fluids — Method for coding the level of contamination by solid particles.
  9. Khan, T., Broderick, M., & Taylor, C. M. (2021). Investigating the industrial impact of hydraulic oil contamination on tool wear during machining and the development of a novel quantification methodology. The International Journal of Advanced Manufacturing Technology, 112(1–2), 589–600. https://doi.org/10.1007/s00170-020-06370-y
  10. Klocke, F. (2009). Manufacturing processes 2: Grinding, honing, lapping. Springer. https://doi.org/10.1007/978-3-540-92259-9
  11. Mahlfeld, G., & Dröder, K. (2023). Performance and wear of diamond honing stones. Machines, 11(4), 502. https://doi.org/10.3390/machines11040502
  12. National Institute for Occupational Safety and Health [NIOSH]. (1998). Criteria for a recommended standard: Occupational exposure to metalworking fluids (DHHS (NIOSH) Publication No. 98-102). https://doi.org/10.26616/NIOSHPUB98102
  13. Sender, P., & Buj-Corral, I. (2023). Influence of honing parameters on the quality of the machined parts and innovations in honing processes. Metals, 13(1), 140. https://doi.org/10.3390/met13010140
  14. Yokoyama, K., Kobayashi, K., & Ichimiya, R. (1990). Analyses of thermal and elastic deformations of honing head. Journal of the Japan Society for Precision Engineering, 56(8), 1513–1518. https://doi.org/10.2493/jjspe.56.1513

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.