Switching to a different topcoat is the usual response when a recoat peels, but how well two coats hold together depends largely on the state of the lower coat's surface at the moment of recoating, so unless that state is put right the new product tends to peel as well. What actually lies behind it can be a missed recoat window, amine blush, contamination between coats, incompatible coatings or skipped sanding, and sometimes two or more at once.

Background

Some time after maintenance painting on a steel structure or a piece of plant, the topcoat lifts like a thin skin. Picked at with a fingernail, it comes away in large flakes, and underneath, the lower coat shows with its colour and gloss intact. Repainting now means stripping all the loose film and feathering the edges, so the job is bigger than the first time, and meanwhile the lower coat alone has to provide the weather and chemical resistance the topcoat was there for. In an immersed coating such as a tank lining, blisters can hold the contents and leach them into the next load, or a delaminated coating can contaminate what the tank holds, adding contamination to the cost of repainting (Bannister et al., 2022).

Two coats hold together in two main ways. In one, solvent and resin from the topcoat penetrate a little into the surface of the lower coat and the polymers of the two layers entangle; in the other, the topcoat flows into the valleys of a rough surface and keys mechanically. Between epoxy layers, strong adhesion is thought to need some interdiffusion so that the crosslinked structure continues across the interface (Bannister et al., 2022), and a rough surface can strengthen an interface by enlarging the contact area and providing mechanical keying (Packham, 2003). Either way, it starts only once the topcoat has evenly wetted the surface beneath.

So intercoat failures fall into two groups: at the moment of recoating, the surface of the lower coat was in no state to accept the topcoat, or the two coatings were a combination that could not entangle or key in the first place. An over-hard surface, a white film on the surface, dust and oil, mismatched solvents and gloss left untouched all lead into one of these two, so which interface failed and how the flakes look narrow the cause sharply.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: keep the peeled flakes, and lay the minimum and maximum recoat intervals in both products' technical data sheets, the TDS, beside the job records of painting dates, air temperature, humidity and surface temperature.

Hypothesis 1: recoat window missed

Look at this hypothesis first when a primer or intermediate coat was applied and the topcoat then fell behind schedule. Typical cases are members shop-primed and shipped to site, members left a long time outdoors in the sun, and surfaces where hot weather sped up the cure. Suppose primed steel sat in the yard for a few weeks while assembly was delayed. The surface looked clean and still glossy, so the topcoat went straight on, yet some time later the topcoat comes off those members in long strips like tape. Other members painted the same day are sound.

The trouble is that the lower coat keeps curing as time passes. As two-part epoxies and moisture-cure urethanes cure, crosslinking tightens and the surface becomes hard and smooth, leaving less room for topcoat solvent to penetrate and for the two layers to entangle. In a study of the interface between two epoxy layers, the topcoat penetrated deeper into the lower layer the shorter the overcoating interval and the lower the lower layer's cure temperature (Bannister, 2023). Exceeding the recoat window can cause intercoat adhesion problems, notably with coal tar epoxies and moisture-cure urethanes. The first coat of a coal tar epoxy can cure very hard and glossy within hours, and some moisture-cure urethanes must be recoated within 24 hours, with urethane topcoats applied between 24 hours and a month or more liable to disbond. Among epoxies, polyamide-cured types recoat comparatively well even after long periods (USACE, 1995).

Begin with the dates. Compare the time between applying the lower coat and applying the topcoat with the maximum recoat interval in the TDS, and if that value is listed by temperature, read the line matching the actual temperatures over that period. Check against the job records whether the failures cluster in members or areas that stood longest, and compare the gloss and hardness of the remaining lower coat with places recoated on time with the same product. If the back of the flakes is smooth and the lower coat still shows its as-applied gloss, that is a sign the two layers barely entangled.

Where the window has been exceeded, prepare the surface as the TDS directs. Usually that means roughening by sanding or a light sweep blast, and with products such as coal tar epoxy that develop exudate and an oxidised layer, removing those as well. Where the supplier allows, a slow-evaporating strong solvent can be used to swell the surface and help entanglement (USACE, 1995). From the next job on, put the maximum recoat interval into the schedule so a warning goes out before it is reached, and where long waits cannot be avoided, choose a coating with a long recoat window.

Hypothesis 2: amine blush

This hypothesis comes to the front when an amine-cured epoxy was applied on a humid day, in the evening or early morning when dew forms easily, or in a poorly ventilated tank or confined space. The same goes for applying straight after mixing the two parts, or for cold weather that slows the cure. Picture a first epoxy coat applied inside a tank late on a monsoon-season afternoon, and next morning the surface is hazy in patches. To keep to schedule the second coat went straight on top, and around commissioning the second coat lifts in that area only.

The hazy film is a product of the curing agent and the air. With small amine curing agents, some unreacted amine can be squeezed out to the film surface during crosslinking, and when that amine reacts with carbon dioxide in the air it forms blush, a hazy white colouration. This film is water soluble and must be wiped or washed off before the next epoxy coat (USACE, 1995). One study explains that the amine, being less compatible with the rest of the epoxy system, tends to migrate to the surface before cure, meets moisture and carbon dioxide there and forms a white carbamate layer that becomes a weak boundary to which the next coat cannot properly adhere (Bannister et al., 2022). In the same study, a longer induction time, the wait between mixing and application, markedly reduced the carbamate layer at 80% relative humidity but had no measurable effect at 40% and below. On surfaces with heavy carbamate, the second coat barely penetrated the first (Bannister, 2023).

The state of the first coat before recoating is the strongest clue. Ask the painters whether there were hazy patches, a white film or a surface that felt less than smooth, and on peeled areas look for white residue on the back of the flakes and on the exposed lower surface. In the job records, compare the relative humidity when the first coat went on, the margin between surface temperature and dew point, and the wait between mixing and application with the TDS conditions. If failures cluster only in areas painted on humid days with the same product, blush is a reasonable suspect.

Wash or wipe any remaining blush off with clean water and let the surface dry completely before the next coat. Prevention starts with cure conditions. Keep to the induction time in the TDS, and when humidity or surface temperature is out of range, postpone painting or bring conditions into range with dehumidification and heating. Many formulators require an induction time of 15 to 30 minutes after mixing, and amine adduct curing agents, pre-reacted with some resin to enlarge the molecule, were developed to reduce the tendency to blush (USACE, 1995). Where blush keeps recurring, review products using such curing agents with the supplier.

Hypothesis 3: contaminated interface

This hypothesis turns on what settled between coats. It applies when grinding, blasting or welding went on nearby after the first coat, inside plants that use silicone release agents or lubricants, near coasts or roads treated with de-icing salt, and when dew formed on the surface overnight. Chalky powder on an epoxy surface after long outdoor exposure to sunlight belongs here too. Say pipe grinding took place in the same area the day after the first coat, and nobody wiped the surface before the topcoat. A sweep of the palm picks up fine grey dust, and some time later the topcoat in that area lifts, its back feeling gritty.

For the topcoat to bond it must first wet the surface beneath, and a liquid spreads evenly only when its surface tension is below the critical surface tension of the solid (Zisman, 1964). If a thin low-energy film such as oil or silicone is present, the paint cannot wet the lower coat and merely rests on that film, so it pulls back into round spots, or, even where it looks bonded, parts at that film under load. In tests where steel was contaminated with silicone before priming and painting, tensile adhesion strength fell by 68% and the failure moved from within the paint to the interface between paint and steel (Anderson et al., 2012). The same study found that solvent wiping improved adhesion but rarely brought it back to the original level.

Dust and powder do harm in a different way. Dust, dirt, dry spray and overspray reduce adhesion between coats and leave porosity in the next coat, so surface cleanliness must be checked right before recoating, and oil and water carried in the compressed air also cause adhesion defects and fisheyes (USACE, 1995). Water-soluble salts left at the interface are another matter. A coating acts as a membrane that lets water through but holds salts back, so water gathers where salt sits, osmotic pressure raises blisters and adhesion falls (Morcillo, 1999). Overnight dew forms a water film at the interface by itself and also holds airborne salt and dust in place.

Look for contamination by eye and hand first. Sweep the surface with a palm or a white cloth to see whether powder comes off, and check the back of the flakes under a magnifier for dust particles or round fisheye marks. Where a drop of water beads up instead of spreading, a low-energy film can be suspected. Check for salts by sticking on a patch and dissolving them out with water, as in the standard extraction used on steel surfaces (ISO, 2020), then measuring the conductivity of that water. Judge condensation by measuring air temperature, relative humidity, dew point and surface temperature to see whether dew could form at the time of painting (ISO, 2017). Also look in the work log for what was going on nearby around then.

If contamination is the cause, make cleaning right before recoating a fixed step. Brush and blow off dust and overspray, and wipe oil and silicone with clean cloths dampened with solvent, changing them often so the contamination is not spread around. Remove chalked epoxy and salts by methods such as pressure washing with detergent, then let the surface dry. Separate silicone-using processes from the painting area, fit oil and water separators on the compressed-air line, and before painting blow air onto white paper to check that no oil or water marks it. Postpone painting whenever dew can form.

Hypothesis 4: incompatible coatings

Suspect this hypothesis when maintenance painting goes ahead without knowing what the existing coating is, when products from different suppliers are mixed, or when a specification change altered only the type of topcoat. A two-part coating with strong solvents applied over an oxidatively dried alkyd on old plant is an example often cited. An outdoor pipe run that had always been painted with alkyd is recoated in this year's maintenance with a two-part urethane. Shortly after application, the surface in some sections wrinkles and swells, and scraping there brings up softened lower coat along with the topcoat.

A little swelling of the lower coat by topcoat solvent helps entanglement, but too much softens the lower coat until it lifts. A polymer dissolves in solvents whose solubility parameters are close to its own, and a crosslinked polymer swells instead of dissolving (Hansen, 2007). So the same solvent may only just soften the skin of a tightly crosslinked epoxy while penetrating deep into a coating that is weak against it, causing wrinkles and lifting. Incompatible coating systems can soften and lift the existing coating or adhere poorly to it. If the existing coating has little integrity, it may fail to withstand the weight and stress imposed as the new coat cures and come away with it, so maintenance coatings with low shrinkage on curing are the better choice (USACE, 1995).

Identify the existing coating first. Find earlier painting records and specifications, and if there are none, send a flake to the supplier or a laboratory to determine its type. Then check compatibility with a test patch, applying the new system to a small area of the actual surface. Follow the standard practice for the patch (ASTM International, 2021), let it go through a season if possible, and otherwise leave it at least a few weeks before inspecting for lifting, wrinkling, other signs of incompatibility and adhesion (USACE, 1995). On areas already peeled, see whether lower coat came away on the flakes and whether the lower surface has softened or wrinkled.

If the combination proves incompatible, tell the supplier what the existing coating is and get a system that can go over it. Matching to one supplier's system is simplest; if that is not possible, use the weaker-solvent topcoat or intermediate coat the supplier recommends. Do not paint over lower coat that has already softened; remove it down to a sound layer. Where the affected area is large, weigh full removal and repainting against overcoating, costs included.

Hypothesis 5: sanding skipped

This hypothesis comes with any recoat over a hard, glossy surface. Typical cases are repair paint over stoved factory-finished parts, maintenance painting over an old coating that still has its gloss, topcoats over epoxy past its recoat window, and jobs where sanding was skipped to keep to schedule. A case in point is a scratch on a glossy stoved panel covered with repair paint after degreasing only, with no sanding. It looked smoothly covered, but when inspection cut through it and pulled tape, only the repair coat lifted, cleanly.

A smooth surface offers no valleys for the topcoat to key into, and a hard one gives solvent no way in. With keying and entanglement both blocked, all that holds the two layers is weak attraction at the interface, so when a knock or a temperature swing puts load on it, the coat tends to part along that face. Roughness on scales from microns down to nanometres can strengthen an interface, not only by enlarging the contact area but because it brings energy-dissipating processes in the coating into play when the bond is stressed (Packham, 2003). Glossy, hard or smooth existing coatings may need roughening for adhesion, by hand or power-tool sanding, until the gloss is gone and the surface is visibly rough (USACE, 1995).

Whether sanding was done stays written on the surface. Under a low-angle light, check the exposed lower coat for sanding scratches, or for gloss left exactly as it was before painting. If sanded and unsanded areas are mixed, compare which side the peeling favours. Confirm whether the work instruction listed a sanding step and abrasive grade, and whether it was actually carried out. If doubt remains, sand one part of the same surface, leave another as it is, paint both with the same product and compare adhesion.

Once the lower coat proves to have gone unsanded, make sanding until the gloss has gone evenly a mandatory step before recoating. Match the abrasive grade to the TDS and the film thickness, and after sanding brush and wipe off the dust so the problem does not turn into one of contamination. On large areas, a light sweep blast is also used instead of sanding to roughen and clean the surface in one pass. Around repairs, sand well into the surrounding coating so the new paint finishes on a roughened surface.

Finding the cause

Five hypotheses do not mean five separate investigations. Rule them out starting with what can be checked on paper. Recoat intervals and the temperature, humidity and dew point at the time of painting need only the job records and the TDS, and whether the two products are a compatible pair can be settled from the specification and the supplier. Surface inspection and adhesion testing come after that.

The first clues are the back of the flakes and the exposed surface. If both are smooth and the lower coat keeps its gloss, suspect an over-cured or unsanded surface; white residue points to blush; dust particles or round fisheye marks point to contamination. If lower coat has come away on the flakes and the exposed surface is soft or wrinkled, the evidence leans towards incompatible coatings. Look at where the peeling sits as well: clustered on members that stood longest, check the recoat window first; on areas painted on humid days, blush; near grinding or welding work, contamination.

Next, measure which interface is weak. In the tape test, where cuts are made and tape is applied and pulled, a multicoat system may fail between coats, so the test shows which interface is weak rather than adhesion to the substrate (ASTM International, 2023). The pull-off test, which bonds a metal dolly to the coating and pulls it straight off, records whether the break is between coats, within a coat or in the dolly adhesive, and so reveals the weakest link in the system (ISO, 2023; USACE, 1995). If the break always falls between the same two coats, all five hypotheses converge on that one interface.

If that still does not settle it, run control trials. Divide the same surface into small areas: one left as it is, one washed with water only, one solvent-wiped only, one sanded only and one washed and sanded, and paint them all with the same product under the same conditions. After a set period, measure adhesion the same way in each, and which treatment made the difference becomes clear. Change only one thing per area, or the result cannot be read.

The hypotheses can overlap. Epoxy left outdoors for a long time may be past its recoat window, chalked by sunlight and covered with dust and salt as well. In such cases keep to the order of removing contamination first and roughening second. Preparing an existing coating for overcoating likewise means washing and wiping off dirt, chalk and oil, then sanding glossy surfaces (USACE, 1995). After changing the preparation, measure adhesion again the same way as in the trials; the job is done only when the break has moved from the interface into a coat.

Limits and cautions

Minimum and maximum recoat intervals, induction times, application temperature and humidity, and the degree of sanding all differ by coating type and formulation, so numeric decisions follow the product's TDS and the supplier's guidance. Adhesion values do not predict a coating's service life, and a coating with somewhat lower adhesion can still protect for a long time if it stays intact (USACE, 1995). For immersed coatings such as tank linings, or for safety-related structures, do not decide on repainting from floor judgement alone; get the supplier and a coating inspector to confirm.

Safety matters too. For coatings containing solvents, amine curing agents or isocyanates, follow the product's safety data sheet, the SDS, for protective equipment and ventilation, and enter confined spaces such as tanks only with ventilation and gas monitoring in place. Before sanding or blasting an old existing coating, first confirm it contains no hazardous constituents, and control dust with extraction and respiratory protection. Collect solvent-soaked cloths in a lidded metal container so they cannot catch fire.

Sources

  1. Anderson, G. L., Stanley, S. D., Young, G. L., Brown, R. A., Evans, K. B., & Wurth, L. A. (2012). The effects of silicone contamination on bond performance of various bond systems [Preprint]. NASA Technical Reports Server, Document ID 20120016452. https://ntrs.nasa.gov/citations/20120016452
  2. ASTM International. (2021). ASTM D5064-16a(2021), Standard practice for conducting a patch test to assess coating compatibility. https://store.astm.org/d5064-16ar21.html
  3. ASTM International. (2023). ASTM D3359-23, Standard test methods for rating adhesion by tape test. https://store.astm.org/d3359-23.html
  4. Bannister, C. C. (2023). The influence of stoichiometry and cure conditions on surface and interfacial properties of epoxy resin barrier coatings [Doctoral thesis, Durham University]. https://etheses.durham.ac.uk/id/eprint/15377/
  5. Bannister, C., Guy, A., Mihaylova, R., Orgill, J., Burg, S. L., Parnell, A., & Thompson, R. L. (2022). The influence of ambient cure chemistry and stoichiometry on epoxy coating surfaces. RSC Advances, 12(44), 28746–28754. https://doi.org/10.1039/d2ra05067f
  6. Hansen, C. M. (2007). Hansen solubility parameters: A user's handbook (2nd ed.). CRC Press.
  7. International Organization for Standardization [ISO]. (2017). ISO 8502-4:2017, Preparation of steel substrates before application of paints and related products — Tests for the assessment of surface cleanliness — Part 4: Guidance on the estimation of the probability of condensation prior to paint application. https://www.iso.org/standard/58061.html
  8. International Organization for Standardization [ISO]. (2020). ISO 8502-6:2020, Preparation of steel substrates before application of paints and related products — Tests for the assessment of surface cleanliness — Part 6: Extraction of water soluble contaminants for analysis (Bresle method).
  9. International Organization for Standardization [ISO]. (2023). ISO 4624:2023, Paints and varnishes — Pull-off test for adhesion. https://www.iso.org/standard/83350.html
  10. Morcillo, M. (1999). Soluble salts: Their effect on premature degradation of anticorrosive paints. Progress in Organic Coatings, 36(3), 137–147. https://doi.org/10.1016/S0300-9440(99)00036-3
  11. Packham, D. E. (2003). Surface energy, surface topography and adhesion. International Journal of Adhesion and Adhesives, 23(6), 437–448. https://doi.org/10.1016/S0143-7496(03)00068-X
  12. U.S. Army Corps of Engineers [USACE]. (1995). Painting: New construction and maintenance (EM 1110-2-3400). Department of the Army.
  13. Zisman, W. A. (1964). Relation of the equilibrium contact angle to liquid and solid constitution. In F. M. Fowkes (Ed.), Contact angle, wettability, and adhesion (Advances in Chemistry, Vol. 43, pp. 1–51). American Chemical Society. https://doi.org/10.1021/ba-1964-0043.ch001

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.