Turning up the oil is the usual response when tool life drops after a switch to MQL, but in one production-machine trial, oil beyond a certain flow blocked the chips' way out and tool life fell instead. What actually lies behind the drop can be the wrong flow or nozzle, an unsuitable oil, chips that do not clear, heat that is not removed, or tool oil channels and coatings that do not suit MQL, and sometimes two or more at once.

Background

A line that used to run on flood coolant has been switched to minimum quantity lubrication, or MQL, and now, with the same tools and the same settings, tools need changing sooner. Drill corners wear early or the drill snaps, and hole size and finish drift before the tool reaches its expected life. Tool spend rises, the machine stops at every change, and a drill broken off inside a hole can scrap the part. The switch was made to cut coolant upkeep and waste fluid, yet more than that can be lost on tools.

Flood coolant does three jobs at once: it lubricates the cutting edge, carries heat away and washes chips out. A flood system delivers 20 to 80 litres a minute at around 20 bar, while MQL sends 10 to 100 millilitres of oil an hour as a mist in compressed air at around 4 to 6 bar (Raval et al., 2020). That much oil can lubricate, but there is almost no liquid left to carry heat and chips, so cooling and chip removal have to be shared out among the air, the tool and the cutting conditions (Weinert et al., 2004).

That does not mean MQL shortens tool life by nature. In tests turning AISI 4340 steel with carbide tools, MQL cut tool wear and surface roughness markedly compared with dry cutting, and the authors traced this to a cooler cutting zone and better contact between chip and tool (Dhar et al., 2006). If tool life has dropped, the task is to find which of the jobs flood coolant used to do has been left undone.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: lay the MQL unit's oil flow and air pressure settings, the tools and the cutting conditions beside the records from before the switch, and measure tool wear on the same basis as before so that tool life is compared on one scale.

Hypothesis 1: wrong flow or nozzle

Look at this hypothesis first on machining centres with an external mist nozzle that is re-aimed by hand at every tool change, where several tools of different lengths share one nozzle, or where the flow has been turned up on the idea that more is better. The deeper the hole, the harder it is for mist from a nozzle to reach the cutting edge, so the effect grows. Picture a line running one nozzle set for a short end mill and using it for a long drill as well. The end mill is fine, but the drill alone wears early at its corners, and a drill pulled for a look is shiny with oil on the shank while its tip is dry.

MQL oil does its work only when droplets get into the rubbing surfaces at the cutting edge. In a production-machine trial drilling cast iron with two-channel through-tool MQL, oil flow was set to 0, 15, 30 and 60 millilitres an hour; tool life rose up to 30 millilitres, did not improve beyond it, and fell for the straight-flute drill (Raval et al., 2020). The authors explain that oil past that threshold adds no lubrication but floods the cutting zone, blocks the chips' way out and keeps hot chips against the tool longer, raising its temperature. The same study notes that in drilling, where access to the cutting edge is narrow, external supply of the kind common in turning and milling works poorly, and adds that the best flow may differ from case to case. If the nozzle misses the cutting edge, no flow setting helps; the oil only ends up on the shank and the workpiece.

First see whether oil actually reaches the cutting edge. With machining stopped, compare the nozzle distance and angle for each tool against the records, then pull the tool and check whether oil marks remain on the edge and in the flutes or only the shank is shiny. Divide the oil used from the tank by running time to get the actual flow and compare it with the setting. Whenever the flow is changed, log tool life measured on the same basis alongside it.

For a nozzle problem, fix a nozzle position for each tool length and return to it at every tool change. Rather than raising the flow in one big step, choose a few steps above and below the present value, compare tool life with the same tool, and then pick. For deep holes or drills a nozzle cannot reach, review a move to through-tool supply with the machine and tool suppliers.

Hypothesis 2: unsuitable oil

Consider this hypothesis when, at the switch, neat cutting oil or another machine's lubricant was put into the MQL unit, when steel and aluminium lines share one oil, or right after a change of supplier brought in a different oil. Take a plant that put the MQL oil working well on its steel parts line into its aluminium housing line too. Tool life on the steel line is unchanged, but on the aluminium line the drills and end mills pick up aluminium on their edges and need changing sooner.

With MQL so little oil reaches the edge that performance depends on how well that oil clings to freshly cut metal and forms a film. A study that evaluated synthetic polyol esters as MQL oils looked at biodegradability, oxidation stability and cutting performance together, and reports that in cutting steel the ester and oxygen helped each other adsorb and cutting improved, whereas in cutting aluminium oxygen made cutting worse (Wakabayashi & Suda, 2008). The same oil and the same air can give different results depending on the metal being cut. Since MQL cannot cover a shortfall with volume the way flood coolant can, the oil's properties show up more directly in tool life.

Check the technical data sheet, the TDS, first to confirm that the oil in use is made for MQL, and look at its viscosity, flash point and recommended materials. Look for sticky residue or colour change in the unit's tank, filter and nozzle tip. Compare tool edges by material under a magnifier: on the aluminium line, whether metal has stuck to the edge, and on the steel line, whether the wear land is even.

If the evidence leans towards the oil, tell the supplier what material is being cut, get two or so candidate MQL oils for it, and compare tool life with the same tool under the same conditions. A plant cutting both steel and aluminium should also consider separate oils for each line. When changing oil, empty and flush the tank and lines so the old and new oils do not mix.

Hypothesis 3: chips not clearing

This hypothesis grows with holes several diameters deep, blind holes, straight-flute drills without helical flutes, and materials that form long, continuous chips. Since the flood used to push chips out, it applies above all to processes switched to MQL with tools and cycles left as they were. In drilling a deep blind hole in a steel part in one pass, the spindle load climbs as the hole gets deeper. The flutes of the withdrawn drill are packed with chips, and chips are compacted at the bottom of the hole too.

Flood coolant drives chips out of the hole under high pressure, but in MQL the oil lubricates and the compressed air has to carry the chips. In the production-machine trial above, the straight-flute drill relied on air alone to clear chips and was far more sensitive to oil flow; when chips cleared less well, hot chips stayed against the tool longer, and because MQL cools poorly, tool temperature rose and tool life fell (Raval et al., 2020). How air flow relates to chip removal in MQL drilling has been studied on its own (Stephenson et al., 2019). A study of deep-hole MQL drilling in cast iron found that heat sent into the hole wall by friction at the drill margins and by hot chips can increase thermal distortion of the workpiece, and examined the effect of raising the air pressure (Tai et al., 2013).

When withdrawing the drill, check whether the flutes are full of chips and whether chips stay packed at the hole bottom. Log spindle load or torque against depth and see whether the load rises as the hole deepens. Do not rely on the unit's gauge for air pressure; confirm that air actually comes out strongly at the tool tip, and note whether chips come out in long, unbroken strings.

If chips look like the cause, open up their way out first. Add a peck cycle that withdraws the drill at intervals, raise air pressure and air volume within what the unit allows, and keep oil flow to no more than what wets the chips. For processes with many deep holes, review drills with flutes designed for MQL with the tool supplier.

Hypothesis 4: too little cooling

This hypothesis comes to the front with materials that do not shed heat easily, such as nickel alloys, stainless steel and hardened steel, with processes that kept the high cutting speeds of the flood era, and with long uninterrupted turning cuts. A line turning stainless steel shafts has moved to MQL, but the old cutting speed chart is still on the wall. Even an insert fitted at the start of the shift goes dull within a few parts, and the edge of a removed insert looks crushed rather than evenly worn.

Flood coolant carries heat away in a large volume of liquid, but MQL mist has little cooling power (Raval et al., 2020). Tool life therefore swings most where heat is produced faster than it can be removed. In high-speed milling of hardened steel, oxygen delivered by MQL formed a protective oxide layer between chip and tool and extended tool life, but the effect was best at a particular cutting speed, and at extremely high speeds MQL was not suitable (Liao & Lin, 2007).

Set the cutting speed, feed and depth of cut now beside those of the flood era and see what was carried over unchanged. Examine worn tools under a magnifier and record whether the flank has worn evenly, the edge has been crushed, or the rake face is cratered. See whether chip colour is darker than in the flood era, measure workpiece temperature straight after machining with an infrared thermometer, and log whether dimensions drift one way through the run.

Once the cause narrows to heat, lower the cutting speed by one or two steps while keeping the feed, and compare tool life measured on the same basis together with cycle time. If the tool supplier gives recommended cutting speeds for MQL, start again from those. For a material where tool life does not recover even at lower speed, decide with the tool and machine suppliers whether to keep MQL or move that process alone to another cooling method.

Hypothesis 5: tool not built for MQL

Suspect the tool when through-coolant tools from the flood era are fitted to the MQL unit as they are, when stepped drills or combination tools with several diameters are used, when mist is fed through a high-speed spindle into the tool, or when coatings were chosen for flood conditions. A stepped drill with coolant holes from the flood era is running on an MQL spindle unchanged. The chamfer edge on the large diameter is wet with oil, but the tip of the small leading diameter is dry, and that edge alone wears first.

Mist fed into the tool has to pass through a rotating spindle and narrow channels before it reaches the edge. In high-speed spindles, centrifugal force separated oil from the mist and less mist reached the cutting zone, and a non-rotating supply mechanism suppressed this separation (Aoyama, 2002). In tools with several diameters, most of the oil left through the larger holes near the top, far from the primary cutting edge (Hughey & Stephenson, 2019). In a study measuring drill edge temperature directly, oil mist sent through the drill's oil holes lowered edge temperature compared with dry drilling, so a tool whose mist falls short of the edge loses that benefit (Ueda et al., 2007).

Coatings also perform differently under different lubrication. In a study high-speed finish-turning the nickel alloy Inconel 718 with three carbide tools carrying different coatings, the small amount of MQL oil extended the life of all three, but by different margins. The longest tool life came from a multilayer coating of TiCN, alumina and TiN under flood conditions, though the finish was poor, and under MQL the finish worsened as the worn flank roughened (Kamata & Obikawa, 2007). A tool and coating chosen under flood conditions cannot be assumed to rank the same under MQL.

With the spindle stopped, fit the tool, run mist only, and hold a plate in front to see whether mist comes evenly from each oil hole and how long it takes to start. MQL units keep critical parts inside the spindle, which makes them harder to maintain, so check the service intervals and records for the spindle-side parts as well (Filipovic & Stephenson, 2006). On the tool drawing, see whether the oil holes exit close to the cutting edge and under what lubrication the coating was specified.

Where oil channels or coating are at fault, review with the tool supplier a change to tools designed for MQL, meaning oil holes that exit close to the cutting edge and oil shared evenly between steps. Confirm with the machine supplier that the supply system suits the spindle speed. Choose the coating by trialling two or three under the same material and the same MQL conditions.

Finding the cause

Five hypotheses do not mean five separate investigations. Rule them out starting with what is easiest to check. Nozzle position, actual flow and the oil product can be checked without a long stop, and cutting conditions can be compared with the pre-switch records at once. Chips and tool edges show every time a tool is pulled, while oil channels and coatings need tool drawings and supplier data, so they come next. Tool life can only be compared on one scale. The tool-life testing standard for turning tools sets out a procedure that fixes wear criteria for tool life, so choose one criterion, such as flank wear width, and count both before and after the switch against it (ISO, 1993).

Next is the pattern of the loss. If only certain tools are short-lived, look at the route mist takes to those tools: the nozzle position, or the tool's oil channels and coating. If things get worse as holes deepen, and worse still with straight-flute drills, suspect chip evacuation. A loss on one material only, with the same oil, points to the oil type, and losses clustered in high-speed processes and heat-sensitive materials point to heat. A dry edge with only the shank wet means the oil is not reaching the edge, so look at the nozzle and oil channels before the flow.

If that still does not settle it, run control trials that change one thing at a time: re-aim the nozzle, step the flow down or up, put in another oil, add a peck cycle, or drop the cutting speed one step. Change only one thing at a time, or there is no telling which one worked. Run the trials on the same machine with the same material batch and the same tool batch so that no other difference creeps in.

After each change, count the parts or holes machined up to the set wear criterion in the same way as before the change. The job is done only when that figure approaches the flood-era tool life or the life the tool supplier gives for MQL conditions. Check as well that hole size and finish stay within tolerance to the end of tool life.

The hypotheses can overlap. Adding oil in the hope of flushing chips can block the chips' way out, and heat building up while chips stay against the tool can shorten its life (Raval et al., 2020). A nozzle that misses the edge combined with a high cutting speed leaves both lubrication and cooling short. In such cases, put right the route by which mist reaches the edge and the route by which chips leave first, then look again at the oil type and the cutting speed, because while those routes are blocked, the effect of changing oil or speed cannot be compared fairly.

Limits and cautions

Suitable oil flow, air pressure, cutting speed and coating differ by machine, tool and material, so numeric decisions follow the oil's TDS and the machine and tool suppliers' guidance. The test values above were obtained under those test conditions and should not be carried over to another process as they are. For parts with tight dimensional tolerances, thermal distortion of the workpiece matters as well as tool life, so have the quality engineer confirm measurement and release decisions.

Safety matters too. MQL mist is still a metalworking fluid aerosol, and the US National Institute for Occupational Safety and Health set its recommended exposure limit for metalworking fluid aerosols at 0.4 mg/m³ as thoracic particulate mass (NIOSH, 1998). Follow the product's safety data sheet, the SDS, for protective equipment and ventilation, and confirm that machine doors close properly and the mist collector runs. Aim nozzles or check mist output from a tool only with the spindle stopped and locked out, and wear gloves and eye protection when handling sharp tool edges.

Sources

  1. Aoyama, T. (2002). Development of a mixture supply system for machining with minimal quantity lubrication. CIRP Annals, 51(1), 289–292. https://doi.org/10.1016/S0007-8506(07)61519-4
  2. Dhar, N. R., Kamruzzaman, M., & Ahmed, M. (2006). Effect of minimum quantity lubrication (MQL) on tool wear and surface roughness in turning AISI-4340 steel. Journal of Materials Processing Technology, 172(2), 299–304. https://doi.org/10.1016/j.jmatprotec.2005.09.022
  3. Filipovic, A., & Stephenson, D. A. (2006). Minimum quantity lubrication (MQL) applications in automotive power-train machining. Machining Science and Technology, 10(1), 3–22. https://doi.org/10.1080/10910340500534258
  4. Hughey, E., & Stephenson, D. A. (2019). Oil delivery balancing and priming for multi-diameter minimum quantity lubrication tooling assemblies. Procedia Manufacturing, 34, 343–348. https://doi.org/10.1016/j.promfg.2019.06.172
  5. International Organization for Standardization [ISO]. (1993). ISO 3685:1993, Tool-life testing with single-point turning tools. https://www.iso.org/standard/9151.html
  6. Kamata, Y., & Obikawa, T. (2007). High speed MQL finish-turning of Inconel 718 with different coated tools. Journal of Materials Processing Technology, 192–193, 281–286. https://doi.org/10.1016/j.jmatprotec.2007.04.052
  7. Liao, Y. S., & Lin, H. M. (2007). Mechanism of minimum quantity lubrication in high-speed milling of hardened steel. International Journal of Machine Tools and Manufacture, 47(11), 1660–1666. https://doi.org/10.1016/j.ijmachtools.2007.01.007
  8. National Institute for Occupational Safety and Health [NIOSH]. (1998). Criteria for a recommended standard: Occupational exposure to metalworking fluids (DHHS (NIOSH) Publication No. 98-102). Centers for Disease Control and Prevention. https://www.cdc.gov/niosh/docs/98-102/
  9. Raval, J. K., Stephenson, D. A., & Tai, B. L. (2020). Effect of oil flow rate on production through-tool dual channel MQL drilling. In Proceedings of the ASME 2020 International Manufacturing Science and Engineering Conference (Vol. 1, V001T05A007). ASME. https://doi.org/10.1115/MSEC2020-8375
  10. Stephenson, D. A., Hughey, E., & Hasham, A. A. (2019). Air flow and chip removal in minimum quantity lubrication drilling. Procedia Manufacturing, 34, 335–342. https://doi.org/10.1016/j.promfg.2019.06.171
  11. Tai, B. L., Stephenson, D. A., & Shih, A. J. (2013). Workpiece temperature during deep-hole drilling of cast iron using high air pressure minimum quantity lubrication. Journal of Manufacturing Science and Engineering, 135(3). https://doi.org/10.1115/1.4024036
  12. Ueda, T., Nozaki, R., & Hosokawa, A. (2007). Temperature measurement of cutting edge in drilling: Effect of oil mist. CIRP Annals, 56(1), 93–96. https://doi.org/10.1016/j.cirp.2007.05.024
  13. Wakabayashi, T., & Suda, S. (2008). Practical performance and action mechanism of ester lubricants in minimal quantity lubrication machining. Journal of the Japan Petroleum Institute, 51(3), 134–142. https://doi.org/10.1627/jpi.51.134
  14. Weinert, K., Inasaki, I., Sutherland, J. W., & Wakabayashi, T. (2004). Dry machining and minimum quantity lubrication. CIRP Annals, 53(2), 511–537. https://doi.org/10.1016/S0007-8506(07)60027-4

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.