BlogApplication notes
Why does coolant go bad again days after adding biocide?
- Type
- Application notes
- Published
- 23 November 2026
- Prepared by
- Jonghwan Moon
- Product group
- Water & Waste Treatment
Adding more biocide is the usual response when coolant turns, but unless the biocide reaches the places where microbes live at a high enough level for long enough, the smell is back within days. What actually lies behind it can be the wrong dose or timing, biofilm shielding the microbes, fungi or mycobacteria the biocide barely touches, biocide spent on tramp oil and dirt, pH too high for the biocide to last, or dead legs in the pipework the biocide never reaches, and often two or more at once.
Background
A sour or rotten-egg smell rises from the tank, biocide goes in, and for a day or two the smell settles and the fluid looks clear. A few days later the smell is back, a slimy film coats the tank wall again, and the dipslide is once more crowded with colonies. More biocide goes in, and the interval between doses keeps shrinking.
The repeated cycle costs more than biocide. Coolant with microbial growth brings complaints about smell and skin problems, tends to lead to rust and emulsion splitting, and finally stops the machines while the fluid is dumped and the tank cleaned. Systems running water-mix fluids can become contaminated with harmful bacteria, and breathing in their mist can cause lung diseases such as occupational asthma and hypersensitivity pneumonitis, so managing fluid quality is managing workers' health (HSE, 2021).
Biocide kills only when, dissolved in the water, it reaches the microbes and holds a certain level for a certain time. Microbes floating in the fluid fall away fairly easily, but those stuck to surfaces or sitting where the biocide cannot reach survive and repopulate the new fluid. In a study that followed a system for six months after it was drained, cleaned and recharged, the fresh fluid had no countable bacteria, yet about 6.9 million cells per mL were counted after 12 hours and about 360 million after three months, and the authors concluded that standard cleaning methods fall short (Veillette et al., 2004).
In such cases the technical team sets up the six hypotheses below and rules them out one by one. The start is always the same: put the dates and amounts of biocide added, the concentration and pH before and after, and the dipslide results on one sheet, and compare them with the recommended dose and working pH range in the biocide's technical data sheet, the TDS.
Hypothesis 1: wrong dose or timing
Start with this hypothesis where biocide goes in only when the fluid smells, where the amount is set from the tank gauge alone, or where a whole drum is poured into one spot and left. In a central system feeding several machines, the system volume includes the fluid circulating in the pipes and machines, so a dose worked out from the tank alone easily falls short. On a Friday afternoon, told that the fluid smells, an operator pours a drum of biocide into a corner of the tank and goes home. The pump stands idle over the weekend, and on Monday morning the fluid from the machine nozzles still smells at first start-up.
There is a reason a single dose does not last. Biocide breaks down little by little in the fluid, so the level on the day of dosing falls day by day. Isothiazolone biocides used in metalworking fluids broke down by hydrolysis in alkaline fluid, and the authors judged that high-pH fluids need periodic additions (Barman & Preston, 1992). Dosing heavily does not settle it either. In a year-long study of a large central tank, Pseudomonas bacteria held above 100 million per mL even though large quantities of biocide were added (Mattsby-Baltzer et al., 1989). Biocide dumped in one spot reaches nowhere else until it mixes, and microbes that survive where the level is too low multiply again while the biocide fades.
The dosing record comes first. Check whether it shows when, how much and where biocide went in, and whether the amount was worked out from the whole volume, including the fluid in pipes and machines. Then take dipslides one, three and seven days after dosing and plot when counts drop and when they climb again; that puts a number on how long the biocide holds. If the supplier has a method for measuring residual biocide, measure it on the same days.
If the record is blank or the dose fell short, hand dosing over to a schedule and measurements rather than to the smell. The UK Health and Safety Executive advises adding biocide only when bacteria keep growing after concentration, pH, tramp oil, metal contamination, temperature, agitation and flow have been put right, using only the supplier's recommended dose, and where practicable dosing with a dispensing system at a point of high turbulence (HSE, 2021). Recalculate the amount from the whole volume, schedule the next dose ahead of the day counts start to climb, and dose while the pump is running.
Hypothesis 2: shielded by biofilm
Suspect biofilm when a slimy film coats the tank wall, the underside of the chip conveyor or the constantly wet surfaces inside the machine. It is more likely in machines where only the fluid has been changed for years without cleaning the system, and where the tank walls are hard to reach. The tank has fresh fluid and a dose of biocide, yet a gloved finger run along the inside wall comes away with a brown, sticky film.
Biofilm is a community of microbes stuck to a surface and living inside a sticky polymer they make themselves, the extracellular polymeric matrix. The matrix holds the microbes to the surface and protects them from harmful substances outside (Flemming & Wingender, 2010). In metalworking fluid systems, antimicrobial components and fluid type stopped new biofilm from forming but had little effect on biofilm already established (von Känel et al., 2025). A study of 69 machines in ten plants likewise found that bacterial counts in the fluid and the size of biofilm populations did not change with whether the fluid contained biocide (Trafny et al., 2015). That is why, even when biocide thins out the microbes in the fluid, cells shed from the film on the walls fill it again within days.
Look for biofilm first by eye and by hand. When the fluid level is down or during cleaning, check the tank wall, under the chip conveyor, grooves inside the machine and the inside of nozzles and hoses for slimy film or clumps. Wipe the film with a swab and press it onto a dipslide, take a dipslide of the fluid on the same day, and compare the two to see whether the microbes are concentrated on the walls rather than in the fluid. Logging how many days it takes counts to climb after a fluid change is another clue.
If film is visible, more biocide will not solve it. Before draining, add the system cleaner the supplier recommends and circulate it for the set time; after draining, remove the remaining film and deposits with brushes and tools, rinse, and then refill. The plant study above also concluded that controlling biofilm takes good management of the delivery system and hygiene of the machines, even with fluids that contain biocide (Trafny et al., 2015). After cleaning, start controlling concentration and tramp oil straight away, before film can settle again.
Hypothesis 3: fungi or mycobacteria
If biocide clears bacterial colonies from the dipslide but cotton-like clumps float on the fluid and filters and nozzles block with slimy masses, look at fungi rather than bacteria. Where one class of biocide has been used for years, also suspect mycobacteria, a group of bacteria that stands up well to biocides. Picture a filter housing opened in late summer, its screen covered in a greyish, jelly-like mass, while that week's dipslide shows an almost empty bacterial side.
Each biocide works on a different range of organisms. That is why the standard practice for selecting biocides for metalworking fluids asks for the target organisms, efficacy and chemical compatibility with the fluid to be weighed up (ASTM International, 2022). Moulds isolated from in-use metalworking fluids were mostly of the genus Fusarium, and the effect of fungicides was limited and depended on the chemistry of the fluid (Ruiz et al., 2024). In tests on mycobacteria, the organism was 2 to 1,600 times more resistant than Pseudomonas to formaldehyde-releasing, isothiazolone and phenolic biocides, and more resistant still in used fluid or alongside Pseudomonas (Selvaraju et al., 2011). When a biocide aimed at bacteria clears out the competition, hardy groups like these can stay behind and fill the gap.
Begin by reading the two sides of the dipslide separately. A common dipslide has one side for bacteria and the other for moulds and yeasts, so do not call the fluid clean from the bacterial side alone. Take a little of the clumps from filters, nozzles and the tank edge and look under a microscope for the threadlike hyphae of mould. Mycobacteria are hard to pick up with ordinary culture, so if they are suspected, send samples to a laboratory that can run genetic tests or dedicated culture.
If mould is seen, choose with the supplier a biocide that includes a fungicidal component or a separate fungicide, and since the effect depends on the fluid, test it in the fluid actually in use before deciding. If mycobacteria are confirmed, switch to a biocide with efficacy data against them and clean out the biofilm they live in at the same time. The authors of the mycobacteria tests likewise concluded that efficacy should be tested more rigorously before and during biocide use (Selvaraju et al., 2011).
Hypothesis 4: spent on oil and dirt
In machines where hydraulic or slideway oil leaks and a layer of oil covers the fluid, in tanks with fine iron particles and chips settled on the bottom, and in tanks that take in foreign matter such as washing fluid or food scraps, the biocide may be going somewhere other than the microbes. Imagine an old machining centre whose tank is evenly covered in brown oil, with the skimmer switched off for weeks. The day after biocide goes in, the oil layer is unchanged and the fluid beneath it smells again.
Biocide does not deal only with microbes. Isothiazolone biocides oxidise thiols, compounds that carry sulphur, and as the reaction goes on they turn into a ring-opened form (Collier et al., 1990). Because the killing action is tied to reactions like these, a fluid full of things to react with uses up the biocide before it reaches the microbes. Oil takes components away by another route. A model that used oil-water partition coefficients to calculate how tramp oil draws metalworking fluid components into the oil and lowers their level in the water was used to set how often and how much of the depleted components to add back (Eppert et al., 2003). A biocide that dissolves readily in oil can be held in the oil layer the same way, leaving less to reach the microbes living in the water.
Measure the tramp oil first. Stir the tank, let a sample stand in a graduated cylinder and read the share of oil that floats to the top, or use the method the supplier recommends. The UK Health and Safety Executive advises checking tramp oil weekly and keeping it below 2% (HSE, 2021). Also look at chips and fines settled on the tank bottom, whether skimmers and filters are working, and where oil is leaking in. If the drop in counts after dosing is noticeably smaller in tanks with more tramp oil, that is grounds to suspect consumption.
If consumption looks like the cause, clear the oil and debris before adding more biocide. Remove tramp oil with skimmers, mobile oil coalescers or vacuum units, and take out fines with centrifuges or filters, or with magnetic separators for ferrous material. Repair the leaking seals and lines to stop the oil getting in, and cover the tank so that food and other foreign matter stay out. Once the fluid is clean, reset the dose and see whether the same amount now holds for more days.
Hypothesis 5: pH too high
Check the pH range in which the biocide holds up when a fresh charge was mixed rich and started at high pH, or after alkaline booster was added to lift a pH that had fallen as microbes grew. A case in point is a tank where, on hearing that the pH had dropped, someone added alkaline booster and poured biocide into the same spot on the same day. The fluid stays clear that week, and from the middle of the next week it smells again.
A biocide has a pH range in which it holds up chemically. The active ingredient of an isothiazolone biocide for metalworking fluids was stable in acidic media but broke down faster as pH rose in alkaline media, with half-lives of about 47 days at pH 8.5, 23 days at 9.0, 3.3 days at 9.6 and 2 days at 10 (Barman & Preston, 1992). The same study judged this biocide suitable for metalworking fluids at pH 8.5 or below. A rise of just over one pH unit can cut the biocide's life from weeks to days. For the same reason, selecting a biocide includes a separate test of whether it holds up chemically in that fluid (ASTM International, 2022).
pH only means something when it is read against the dosing dates. Measure with a calibrated pH meter rather than test strips, and record the value before and after biocide dosing and after any alkaline booster. Compare those values with the working pH range in the biocide's TDS, and see whether the number of days until the smell returned was shorter when pH was high. Check that the pH and hardness of the make-up water meet the supplier's recommendations as well.
If the fluid's pH stays above the biocide's range, there are two routes: switch to a different class of biocide that holds up at that pH, or keep the current one and shorten the dosing interval to match its half-life. Do not add alkaline booster and biocide in the same spot on the same day; dose the biocide once the booster has mixed in evenly. When falling pH calls for booster, do not just fix the number with alkali either; look at concentration and counts together and first find what pulled it down.
Hypothesis 6: dead legs in the pipes
Look at this hypothesis in systems with places where fluid never flows or flows only now and then: branch lines to idle machines, pipe behind closed valves, filter housings and backwash lines, and pipes left sealed at one end after equipment was moved. Think of the day a machine on a central system restarts after standing for weeks. The first fluid out of its nozzles is cloudy and smells, and after that the dipslide results for the central tank climb again.
Fluid carrying biocide cannot get into places with no flow, and in the standing fluid microbes build biofilm. The UK Health and Safety Executive says that when a supply system is built or modified, points of low or no flow should be avoided: bottlenecks, dead ends, lengths of pipe sealed at one end so fluid cannot flow through, and dead legs, fittings fluid passes only infrequently; dead ends should be removed, and dead legs too where reasonably practicable, or else flushed regularly, for example weekly (HSE, 2021). Microbes grown in such places are washed into the main flow when flow returns and reseed freshly treated fluid. The six-month tracking study also confirmed that residual microbes can quickly repopulate new fluid even after cleaning and recharging (Veillette et al., 2004).
Start by spreading out the piping drawing and marking which routes always carry flow and which branches do not. Go through closed valves, branches to idle machines, filter housings and backwash lines one by one, collect the first fluid out of each separately, note its smell and cloudiness, and take a dipslide. If the branch reads higher than the tank fluid on the same day, that is the seed. Also look for records of counts rising after a particular machine was restarted.
Cut out sealed ends, and either disconnect unused branches from the system or flush them on a fixed schedule. Before reconnecting a machine that has stood for a long time, drain and clean its own tank and pipes separately. When cleaning the whole system, open every valve so the cleaner reaches each branch, and open and wipe filter housings and backwash lines too. When laying or changing a system, choose a layout with no places where flow stops from the start.
Finding the cause
There is no need to investigate all six hypotheses at once. Rule them out starting with what is easy to measure. The dosing record and total system volume, pH against the biocide TDS, and the amount of tramp oil can all be checked within a day. Places that need hands and eyes, such as tank walls, filters and pipe branches, come next, and laboratory work to identify the organisms comes last.
The shape of the symptom points the way. If the pattern is the same each time, clean straight after dosing and climbing again a few days later, look at what makes the biocide vanish early: too low a dose, high pH, or consumption by tramp oil and dirt. If the trouble returns soon even after a fresh charge, biofilm on the walls or dead legs are seeding it. Low bacterial counts with floating clumps and blocked filters suggest mould, and a rise after a particular machine restarts points to the branch feeding it.
Use fast measurements alongside accurate ones. The test method for adenosine triphosphate, ATP, in metalworking fluids shows the total amount of microbial life in minutes without culture, but it cannot tell bacteria from fungi (ASTM International, 2021). So plot a daily ATP curve from the day of dosing, and identify the organisms with both sides of the dipslide and the laboratory. A control trial helps too. Split fluid from the same tank into two containers, remove the tramp oil and bring the pH into range in one, add the same dose of biocide to both, and compare the day on which counts start climbing again. Change only one thing at a time, or there is no telling which change worked.
Set the finish line in numbers. By the UK Health and Safety Executive's guide, dipslide results of 10,000 CFU per mL or more indicate microbial growth, and 1,000,000 CFU per mL or more indicate poor control, which normally means draining and cleaning the system (HSE, 2021). The job is done only when, after the fix, results stay below 10,000 and the dosing interval returns to the one in the TDS.
The hypotheses often overlap. High pH and an underdose produce the same pattern of biocide running out early, and biofilm and dead legs reseed each other. In such cases, put tramp oil and pH right first, clear biofilm and dead legs with a system clean, and only then reset the biocide type and dose, because while the fluid is dirty and film remains, no biocide's effect can be compared fairly.
Limits and cautions
Biocide type, dose, working pH range and compatibility with other additives differ by product and by coolant, so numeric decisions follow the TDS of the biocide and the coolant and the supplier's guidance. Biocides are subject to registration and approval schemes in most countries, so use them only for the approved purpose and within the approved amount. Identifying organisms, mycobacteria in particular, is laboratory work, and laying or reworking a system is decided with the equipment supplier.
Safety matters too. Handle neat biocide with protective equipment such as gloves and goggles, following the product's safety data sheet, the SDS, and a dispensing system cuts down contact with the concentrate. Respiratory diseases such as hypersensitivity pneumonitis and asthma, as well as dermatitis, have been reported in workers exposed to metalworking fluids (NIOSH, 1998), so consider respiratory protection for jobs that raise a lot of mist, such as tank cleaning, and refer any worker with a cough or breathlessness to an occupational health professional.
Sources
- ASTM International. (2021). ASTM E2694-21, Standard test method for measurement of adenosine triphosphate in water-miscible metalworking fluids. https://store.astm.org/e2694-21.html
- ASTM International. (2022). ASTM E2169-22, Standard practice for selecting antimicrobial pesticides for use in water-miscible metalworking fluids. https://store.astm.org/e2169-22.html
- Barman, B. N., & Preston, H. G. (1992). The effects of pH on the degradation of isothiazolone biocides. Tribology International, 25(4), 281–287. https://doi.org/10.1016/0301-679X(92)90065-U
- Collier, P. J., Ramsey, A., Waigh, R. D., Douglas, K. T., Austin, P., & Gilbert, P. (1990). Chemical reactivity of some isothiazolone biocides. Journal of Applied Bacteriology, 69(4), 578–584. https://doi.org/10.1111/j.1365-2672.1990.tb01551.x
- Eppert, J. J., Rajagopalan, N., DeVor, R. E., & Kapoor, S. G. (2003). Modeling the effect of tramp oil contamination on selective component depletion in metalworking fluid systems. Journal of Manufacturing Science and Engineering, 125(1), 85–94. https://doi.org/10.1115/1.1537259
- Flemming, H.-C., & Wingender, J. (2010). The biofilm matrix. Nature Reviews Microbiology, 8(9), 623–633. https://doi.org/10.1038/nrmicro2415
- Health and Safety Executive [HSE]. (2021). MW5: Managing fluid quality. COSHH essentials for machining with metalworking fluids. Retrieved November 2026. https://www.hse.gov.uk/pubns/guidance/mw5.pdf
- Mattsby-Baltzer, I., Sandin, M., Ahlström, B., Allenmark, S., Edebo, M., Falsen, E., Pedersen, K., Rodin, N., Thompson, R. A., & Edebo, L. (1989). Microbial growth and accumulation in industrial metal-working fluids. Applied and Environmental Microbiology, 55(10), 2681–2689. https://doi.org/10.1128/aem.55.10.2681-2689.1989
- National Institute for Occupational Safety and Health [NIOSH]. (1998). Criteria for a recommended standard: Occupational exposure to metalworking fluids. DHHS (NIOSH) Publication No. 98-102. Centers for Disease Control and Prevention. https://www.cdc.gov/niosh/docs/98-102/
- Ruiz, C., von Känel, G., Burkard, S., & Küenzi, P. (2024). Fusarium spp. in metalworking fluid systems: Companions forever. Pathogens, 13(11), 990. https://doi.org/10.3390/pathogens13110990
- Selvaraju, S. B., Khan, I. U. H., & Yadav, J. S. (2011). Susceptibility of Mycobacterium immunogenum and Pseudomonas fluorescens to formaldehyde and non-formaldehyde biocides in semi-synthetic metalworking fluids. International Journal of Molecular Sciences, 12(1), 725–741. https://doi.org/10.3390/ijms12010725
- Trafny, E. A., Lewandowski, R., Kozłowska, K., Zawistowska-Marciniak, I., & Stępińska, M. (2015). Microbial contamination and biofilms on machines of metal industry using metalworking fluids with or without biocides. International Biodeterioration & Biodegradation, 99, 31–38.
- Veillette, M., Thorne, P. S., Gordon, T., & Duchaine, C. (2004). Six month tracking of microbial growth in a metalworking fluid after system cleaning and recharging. Annals of Occupational Hygiene, 48(6), 541–546. https://doi.org/10.1093/annhyg/meh043
- von Känel, G., Steinmann, L. Y., Mauz, B., Lukesch, R., & Küenzi, P. (2025). It is useless to resist: Biofilms in metalworking fluid systems. Life, 15(6), 890. https://doi.org/10.3390/life15060890