Pouring in more concentrate or more water whenever the central tank drifts out of range is the usual response, but as long as what leaves the system and what enters it stay the same, the concentration is pushed the same way again. What actually drives it can be water evaporation, a wrong top-up ratio, drag-out on chips and parts, an unstable automatic mixer or selective depletion of components, and often two or more at once.
Background
Log the refractometer readings on a central tank feeding coolant to many machines, and a concentration that sat at the top of the range last week has slipped towards the bottom this week. The person in charge adds concentrate when it is low and water when it is high, yet a few days later it is pushed the same way again. When a central tank goes off, every machine on it cuts under the same wrong conditions, so as the concentration wanders, problems such as tool life, rust, foam and odour spread across many machines at once.
Keeping concentration within range is the centre of fluid management in its own right. Among ways to keep microbial growth down, a public safety agency lists operating the system at the correct concentration and keeping makeup water quality adequate (OSHA, n.d.), and the UK safety regulator advises measuring concentration with a refractometer and pH every week and following the supplier's recommended levels (HSE, n.d.). A professional society's journal names concentration as the most important test because fluid systems are never static (Canter, 2011).
The principle behind drifting concentration is a mass balance, an account of what leaves and what enters. Evaporation removes only water and so raises concentration, while what leaves on chips, parts and exhaust air takes tank fluid away at its existing concentration. Research on grinding likewise reports that a relevant share of cutting fluid is lost through drag-out on chips and workpieces, evaporation and exhaust air (Madanchi et al., 2015). Depending on the concentration of the top-up that fills the gap, the tank goes up or down. Since a fluid's chemistry also changes over its service life (Brinksmeier et al., 2015), the account must also allow for the possibility that the refractometer reading and the amount of working components actually in the fluid do not match.
In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: for two or three weeks, record tank level, concentration and temperature at the same time every day, together with how much water, concentrate and premix went in that day, then compare the log with the recommended range and the refractometer factor in the coolant's technical data sheet, the TDS.
Hypothesis 1: evaporating water
If concentration climbs steadily, suspect evaporation first, especially in a hot season, when tank temperature runs high, when lower output means less leaves on chips and parts, and over holidays when machines stand but circulation and cooling keep running. The log for the first week after the summer shutdown is a good example. The pumps ran while production stopped, the low tank was filled with premix as usual, and the refractometer reading starts well above where it was before the break.
Evaporation raises concentration because only water leaves and the concentrate components stay behind. UK guidance notes that water-mix fluids evaporate in use and become more concentrated, so top-ups should only be made with fluid below the recommended concentration (HSE, n.d.). US guidance likewise says a low sump level indicates fluid loss or water evaporation, and that if the fluid is too strong, water should be added to bring it back (OSHA, n.d.). The link most often missed is the top-up. Fill the volume lost to evaporation with premix at the recommended concentration, and since what left was water but what came in carried concentrate, the concentration steps up with every top-up.
To single out evaporation, lay the records side by side. See whether concentration rises on low-output days and hot days, and count what share of the top-up volume was premix and what share plain water. Log tank temperature alongside shop temperature, and look at whether the tank lid stands open and whether the chiller is actually holding the fluid temperature down. As water evaporates, minerals dissolved in it such as calcium and magnesium stay behind and build up, and the more concentrated they become, the faster the problems appear (OSHA, n.d.). So measuring the hardness of makeup water and tank fluid, and seeing whether the tank's hardness climbs over time, gives a separate gauge of how much water has gone.
If evaporation turns out to be the main cause, the answer is to change how the tank is topped up. Set the top-up concentration below the recommended range, and fill with plain water or very lean fluid on days when concentration is high. Cover the tank and channels to cut evaporation, and plan circulation separately for shutdowns. Where hardness keeps rising, review treatment of makeup water with the supplier.
Hypothesis 2: wrong top-up ratio
For a tank topped up by hand, see whether concentration jumps in steps on the days of top-ups. Typical conditions are a change of person each shift, concentrate poured by eye or counted in buckets, concentrate added straight into the tank without first being mixed with water, and a mixing chart that does not reflect the supplier's refractometer factor. Take a plant where the day shift pours in a drum of concentrate because the reading is low and the night shift fills up with water because the next morning's reading is high: the concentration graph saws up and down and the average settles nowhere.
US guidance calls for topping up with premix made from concentrate and pure water at the manufacturer's recommended concentration, and stresses that proper mixing procedures are critical to fluid life; its checklist asks whether additions are controlled by a coordinator and recorded on a log sheet (OSHA, n.d.). Concentrate poured straight into the tank circulates as a rich slug until it mixes, and a sample drawn then can read higher or lower than the truth. Converting the refractometer reading into concentration is another easy place to go wrong. An analog refractometer reads in Brix, a sugar scale, which must be converted to concentration with the factor or chart the supplier provides, and manufacturers recommend calibrating the instrument before each use (Canter, 2011). Leave out the factor or use another product's, and the tank is fine but the number is wrong, and the amounts poured to chase that number then knock the tank off.
Where human hands are involved, the records give the answer. Lay the date, time, person and amounts of water and concentrate for each top-up over the concentration graph and see whether the jumps line up with top-ups. Check the refractometer's zero with distilled water, and confirm that the conversion factor in use matches the current product's TDS. Also have two people measure the same sample separately and see how far their readings differ.
With the top-up procedure narrowed down as the cause, set the rule that top-ups are made with premix only, and stop pouring concentrate in directly. Post a chart beside the tank giving water and concentrate amounts for the target concentration so the result is the same whoever does it, and have one person or one crew handle top-ups and record them on a log sheet. Recheck the refractometer factor whenever the product changes, and train everyone who measures in the same method.
Hypothesis 3: drag-out losses
If concentration falls and the fall is worse at high output, the fluid that chips and parts carry away comes to mind first. Typical cases are a new part with many deep holes or pockets, chips that break fine and soak up fluid, chips hauled off without being drained, and high-pressure nozzles that raise mist and exhaust losses. In the month a new housing part arrives, every part goes on to the washer with fluid sitting in its holes, the bottom of the chip cart is awash, and because the tank is topped up only with plain water each day, the concentration slips a little each week.
Fluid that leaves on chips and parts removes tank fluid at its existing concentration, so on its own it does not change the concentration. What moves the concentration is what fills the gap. Top up to the level with plain water, and the concentrate that chips and parts carried away is never replaced, so concentration falls. Grinding research reports that drag-out on chips and workpieces, evaporation and exhaust air account for a relevant share of cutting fluid loss, and that the exhaust share depends on process settings (Madanchi et al., 2015). So when output or parts change, the same top-up habit produces a quite different concentration. It is also why systems that drift up and systems that drift down can sit in the same plant: the balance between evaporation and drag-out differs from system to system.
Drag-out can be measured by catching it. Take a few parts straight after machining and collect the fluid until they stop dripping, or weigh them straight after machining and again once fully drained to find how much each part carries off. Scoop a set volume of chips and measure the fluid squeezed out. Multiply these by daily output, compare with the daily top-up volume in the log, and you can estimate what share of the top-up is drag-out. Also check the records for whether concentration falls further on high-output days.
The remedy runs along two lines. One is to cut what leaves: tilt parts or blow them off so fluid in the holes drains back towards the tank, drain or centrifuge chips to recover fluid, and if mist and exhaust losses have grown, review nozzle pressure and exhaust settings. The other is to put back the concentrate that leaves: set the top-up concentration to match the ratio of drag-out to evaporation, and measure that ratio again whenever output or parts change.
Hypothesis 4: unstable mixer
In a system that leaves top-ups to an automatic mixer, split the records by time of day and see whether concentration jumps about even within a single day. Typical conditions are plant water pressure that changes through the day, a blocked concentrate suction line or filter, a nearly empty concentrate drum, a discharge hose that has been lengthened, and a mixer serviced without its setting being rechecked. With the same mixer and the same setting, fluid caught at the outlet in the morning, when other processes draw heavily on the water supply, and in the evening, when water use has dropped, can read noticeably differently on the refractometer.
A venturi proportioner draws up concentrate by the suction water creates as it passes through a narrow throat, so when the incoming water pressure and flow change, the amount of concentrate drawn changes with them. A patent for a proportioning dispenser states the aim of accurate dilution over a wide range of incoming water pressures, and explains that a pressure regulator ahead of the eductor, holding pressure steady, gives more consistent dilution (Dalhart, 2014). If the suction line blocks or the drum runs dry so the mixer draws air instead of concentrate, it delivers water only, and a tank filled with it quietly goes lean. A mixer tends to be treated as a device set once and forgotten, but its outlet concentration moves with the conditions under which water and concentrate enter it.
Measure a mixer at its outlet, not in the tank. Catch outlet fluid in the morning, afternoon and evening, read it on the refractometer, and note the water pressure at the time. If outlet concentration moves with the time of day and tracks water pressure, the mixer is responsible. Inspect the concentrate suction line, filter, check valve and the amount left in the drum, and confirm the mixer setting against the service records. Measuring separately how much concentrate the mixer used and how much premix it delivered over a set period gives the real mixing ratio as a number.
Where outlet concentration followed water pressure or the time of day, fix the incoming water pressure first. Fit a pressure regulator ahead of the mixer, put the suction line and filter on the checklist for regular cleaning, and mark drum levels so drums are changed before they run dry. In a plant with large swings in water pressure, review with the supplier a type of mixer less affected by pressure, and whatever the type, keep measuring outlet concentration at intervals.
Hypothesis 5: selective depletion
Consider this hypothesis when the refractometer reads within range yet rust, foam or poor tool life increase, and when adding more concentrate only lifts the number without fixing the problem. It shows up when much slideway or hydraulic oil leaks into the tank, when microbes grow and the fluid smells, in systems topped up with hard water, and in systems not recharged for a long time. Picture a tank that has run for years on top-ups without ever being fully changed. Oil floats on the surface, the refractometer always reads within range, and the supplier's laboratory analysis comes back showing a marked shortfall of certain components.
A water-miscible coolant is a mixture of many components, emulsifiers, corrosion inhibitors, EP additives, biocides and amines among them, and they do not deplete at the same rate. A professional society's journal points out that because components deplete at different rates, the real concentration becomes close to a guess (Canter, 2011). The routes are many. Tramp oil that leaks in feeds microbes and at the same time extracts key components (OSHA, n.d.), and in experiments inoculated with field cutting fluid, aerobic microbes consumed key components and lowered pH and corrosion protection, while fungal mycelium that grew later flocculated the effective components and reduced lubricity and stability (Shen et al., 2025).
Hardness plays a part too. In tests that accelerated ageing with a calcium salt, the emulsion went through droplet coalescence and creaming to complete separation (Glasse et al., 2012). The trouble is that the refractometer cannot tell these changes apart. Concentration is commonly measured by refractometer or titration; refractometer readings are affected by tramp oil, while titration needs qualified laboratory staff and time (Wahrendorff et al., 2021).
The key to checking is to measure the same sample two ways. Alongside the refractometer reading, measure alkalinity or oil content by the titration method the supplier specifies, and see whether the two agree. Titrating oil content has also been studied as an automated method (Grossi & Riccò, 2017). A refractometer reading within range with a low titration value signals that working components have been depleted. Measure tramp oil content, microbial count, pH and the hardness of makeup water and tank fluid together, and have the supplier's laboratory analyse the composition against new fluid. Always draw samples from the same point and below the surface, so floating oil does not get in.
Once selective depletion is confirmed, pouring in more concentrate will not solve it. Stop the tramp oil leaks and remove oil with a skimmer or separator, and if microbes have multiplied, tackle the cause of that first. Replace depleted components with additives the supplier recommends, but if the damage is extensive, drain the system, clean it and recharge it. US guidance likewise states that when testing shows additions are no longer effective, the system should be drained, cleaned and recharged (OSHA, n.d.). From then on, do not rely on the refractometer alone; add periodic titration or laboratory analysis.
Finding the cause
First see which way, and in what pattern, the concentration moves. A steady rise points to evaporation combined with premix top-ups, and a steady fall to drag-out combined with plain-water top-ups. Steps on each top-up day point to the manual top-up ratio, and swings by time of day within a single day point to the automatic mixer. If the number is right but rust, foam, odour or tool life worsen, look for components depleted where the refractometer cannot see.
Next, clear away what is easy to measure. Checking the refractometer zero and conversion factor takes minutes, and two people measuring the same sample can be done on the spot. Mixer outlet concentration needs only three readings a day, and overlaying the top-up records on the concentration graph can be done in the office. Splitting the account between drag-out and evaporation, titration and laboratory analysis take longer, so they come after.
Balancing the mass account is the strongest check. Take the total water and concentrate added over the logged period, the change in tank level, and the concentration at start and finish, and work out how much concentrate went in and how much remains in the tank. Concentrate missing from the tank compared with what went in has left as drag-out or been consumed; the volume shortfall against everything added, minus the fluid lost to drag-out, is what evaporated. If the account will not balance, suspect unrecorded top-ups or the mixer's real ratio again.
After a fix, confirm it with a comparison. Change only one thing, the top-up method or the mixer conditions, and log concentration for two or three weeks at the same time, place and method as before. It is settled only when concentration holds within range without being pushed to one side. Change several things at once and there is no telling which one worked.
The hypotheses tend to appear together. A system may rise from evaporation in summer and fall from drag-out in a month of heavy production, and with mixer instability on top, the graph grows more confusing still. In such cases put the measurement right first, because the rest of the account only works when the refractometer factor, the sampling method and the mixer outlet concentration can be trusted. Then set the top-up concentration to match the ratio of evaporation to drag-out, and finally confirm by titration whether components have been depleted separately.
Limits and cautions
Recommended concentration ranges, refractometer factors and titration methods differ by product, so numeric decisions follow the coolant's TDS and the supplier's guidance. Refractometer readings can depart from the truth in fluid carrying tramp oil or in aged fluid, so a number within range is not proof that the fluid is healthy. Composition analysis and microbial assessment belong to the supplier or a laboratory, and whether to drain and recharge is decided on their results.
A word on safety and health. Handle concentrate and additives with the protective equipment set out in the product's safety data sheet, the SDS. Coolant soaked into clothing can become far more concentrated than intended as the water evaporates, so change wet workwear promptly (OSHA, n.d.). Breathing coolant mist can cause lung diseases such as occupational asthma, and skin contact can cause dermatitis, so maintain local exhaust ventilation and skin protection (HSE, n.d.). Clean tanks and take samples only with pumps and conveyors stopped and locked out.
Sources
- Brinksmeier, E., Meyer, D., Huesmann-Cordes, A. G., & Herrmann, C. (2015). Metalworking fluids—Mechanisms and performance. CIRP Annals, 64(2), 605–628. https://doi.org/10.1016/j.cirp.2015.05.003
- Canter, N. (2011, March). Monitoring metalworking fluids. Tribology & Lubrication Technology. Society of Tribologists and Lubrication Engineers. https://www.stle.org/files/TLTArchives/2011/03_March/Cover_Story.aspx
- Dalhart, M., Sr. (2014). Dispenser with inline pressure regulator (U.S. Patent No. 8,813,789). U.S. Patent and Trademark Office. https://patents.google.com/patent/US8813789B2/en
- Glasse, B., Fritsching, U., Koch, T., de Paiva, J. L., & Guardani, R. (2012). Turbidimetric spectroscopy for the evaluation of metalworking fluids stability. Tribology Transactions, 55(2), 237–244. https://doi.org/10.1080/10402004.2011.653871
- Grossi, M., & Riccò, B. (2017). An automatic titration system for oil concentration measurement in metalworking fluids. Measurement, 97, 8–14. https://doi.org/10.1016/j.measurement.2016.11.014
- Health and Safety Executive [HSE]. (n.d.). MW5: Managing fluid quality (COSHH essentials for machining with metalworking fluids). Retrieved November 2026. https://www.hse.gov.uk/pubns/guidance/mw5.pdf
- Madanchi, N., Winter, M., & Herrmann, C. (2015). Cutting fluid drag-out and exhaust air in grinding processes: Influence on the eco-efficiency. Procedia CIRP, 29, 329–334. https://doi.org/10.1016/j.procir.2015.02.054
- Occupational Safety and Health Administration [OSHA]. (n.d.). Metalworking fluids: Safety and health best practices manual. U.S. Department of Labor. Retrieved November 2026. https://www.osha.gov/metalworking-fluids/manual
- Shen, Y., Zhang, W., Wu, L., Dong, Y., Guo, G., Dong, L., & Guo, Z. (2025). Microbial proliferation deteriorates the corrosion inhibition capability, lubricity, and stability of cutting fluid. Frontiers in Microbiology, 16, 1522265. https://doi.org/10.3389/fmicb.2025.1522265
- Wahrendorff, P., Stefanakis, M., Steinbach, J. C., Allnoch, D., Zuber, R., Kapfhammer, R., Brecht, M., Kandelbauer, A., & Rebner, K. (2021). Simultaneous determination of droplet size, pH value and concentration to evaluate the aging behavior of metalworking fluids. Sensors, 21(24), 8299. https://doi.org/10.3390/s21248299