KALTECKOREA

BlogApplication notes

Why did a part catch fire when heated after penetrating oil?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Maintenance Aids

Penetrating oil is often taken for an oil that does not catch fire easily and is heated with a torch straight after spraying, but besides oil the can may also hold solvent and propellant gas that ignite readily. What actually lies behind the fire can be flammable solvent and propellant, solvent that has not yet evaporated, liquid pooled in gaps, poor ventilation or spraying onto a hot surface, and sometimes two or more at once.

Background

A rusted flange bolt will not budge, so it gets a generous spray of penetrating oil, and when it still will not turn, the nut is heated with a torch. A few seconds later flames rise round the bolt, spread under the flange and catch the liquid that dripped onto the floor. Even when the fire stays small, the worker can suffer burns to hands and face, nearby cables, hoses and insulation are damaged, and clearing up after extinguishing and investigating the cause push back the whole maintenance schedule.

When a liquid burns, what burns is not the liquid itself but the vapour from its surface. The flash point is the lowest temperature at which a liquid gives off enough vapour near its surface to form an ignitable mixture with air, and a liquid whose flash point is below the surrounding temperature always gives off enough vapour to ignite (HSE, 2015). Heating a liquid raises its vapour pressure, so the vapour concentration above it reaches the lower flammable limit, the leanest mixture that will ignite, sooner (Drysdale, 2011). A torch is both the heat that increases this vapour and the ignition source that lights it.

So a fire during heating means one of two things, or both: enough vapour or gas to ignite was already there when heating began, or the heating turned leftover liquid into vapour. What was left, and how much, is what separates the hypotheses.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: check the ingredients, flash point and type of propellant in the product's safety data sheet, the SDS, then hear from the worker when and how much was sprayed, when heating began, and what the ventilation and surroundings of the work spot were like, and write it down in time order.

Hypothesis 1: flammable contents

This hypothesis is the first to catch out anyone who thinks of penetrating oil as oil and nothing else. An aerosol penetrant often holds, together with a thin oil that works its way into rust, a solvent that thins it so it creeps into gaps and a propellant gas that pushes it out of the can. Think of a mechanic freeing rusted bolts on an exhaust manifold. Assuming that oil is harmless, he sprays the bolts and puts the torch to them at once.

Looking inside the can, what ignites readily is not so much the oil as what surrounds it. Light hydrocarbons such as propane, butane and isobutane are widely used as aerosol propellants, and they are flammable and need careful handling (EPA, n.d.). In air, butane starts to ignite at just 1.6% by volume and propane at 2.1% (NIOSH, n.d.-a; NIOSH, n.d.-b). The globally harmonised system for classifying and labelling chemicals divides aerosols according to their flammable components and other criteria, and requires flammable aerosols to carry a warning not to spray them onto an open flame or other ignition source (UN, 2023). Even if the oil itself has a high flash point, once the gas and solvent catch fire, the flame passes on to the oil.

Start with the label and the SDS. Check whether the can carries the flame pictogram and a hazard statement for an extremely flammable or flammable aerosol, whether the ingredients table in the SDS lists propane, butane or petroleum solvents, and what flash point is given under physical and chemical properties. The flash point in an SDS is usually a standard test value measured by heating the liquid in a closed cup, so products can be compared on the same basis (ASTM International, 2026).

Once the product turns out to be a flammable aerosol, rework any sequence that puts it together with heating. Either leave penetrant off bolts that will be heated and try to free them with heat and cooling alone, or, if penetrant has been used, heat only after checking everything covered below: drying, pooled liquid, ventilation and surface temperature. Where heating is routine in maintenance, review with the supplier whether to keep a separate, less flammable product.

Hypothesis 2: solvent not yet gone

Look at this hypothesis when heating starts right after spraying, when the solvent is slow to evaporate on a cold day or in a shaded corner, and when a surface still glistening wet is heated as it is. The scene goes like this. Short of time, a mechanic sprays five bolts in turn, comes back to the first, and puts the torch straight onto a nut that is still wet. A faint blue flame flares up round the nut.

The vapour is the problem. While sprayed liquid dries, the solvent turns to vapour and lingers just above the surface, and with a low-flash-point solvent this vapour reaches an ignitable concentration even at room temperature. Guidance from the UK Health and Safety Executive adds that a liquid below its flash point can still be readily ignited when spread as a thin film over a surface (HSE, 2015). The torch's heat drives off the remaining solvent all at once, adding to the vapour, and since vapour pressure climbs steeply as temperature rises, the time to reach an ignitable concentration shrinks accordingly (Drysdale, 2011).

Before heating, see whether the surface is still wet and whether there is a strong smell of solvent. To confirm it in numbers, measure right around the work point with a portable combustible gas detector; such measurements should be made both before and during hot work (CSB, 2010). Check the solvent's flash point and evaporation properties in the SDS, and find in the work record how long passed between spraying and the start of heating.

The remedy is a wait built into the sequence. Set the waiting time from the product's SDS and TDS, but do not rely on time alone: wipe off remaining liquid with a dry cloth and confirm with a gas detector that the area round the work point is clear before applying the flame. Keep the detector running during heating and have an extinguisher within reach. Avoid spraying several bolts at once and heating them in turn, since the neighbouring bolts are still wet while one is being heated; finish spraying, waiting, checking and heating for one bolt before moving to the next.

Hypothesis 3: pooled liquid

Generously sprayed penetrant pools in thread gaps, between flanges, in recesses round bolt heads and in supports under the part, and it soaks into nearby insulation and rags left on the floor. On one flange, liquid sprayed on the upper bolts has run down and lies glinting between the heads of the lower ones. After the upper nut has been heated for a while, the heat spreads through the flange, white smoke rises from the pooled liquid below, and flames come up from underneath.

Pooled liquid, unlike a thin film, becomes a reservoir that gives off vapour for a long time. HSE guidance warns that even apparently empty containers may hold small amounts of unseen liquid at the bottom or in crevices and seams, and that heavy residues can give off flammable vapour when heated. The same guidance notes that liquid spilt onto absorbent material such as clothing or packaging can be readily ignited below its flash point (HSE, 2015). Once alight, the pooled liquid keeps giving off vapour and burns as a pool fire, so it does not go out easily even after the torch is taken away (Drysdale, 2011).

Before heating, look below rather than above. Check for liquid pooled in recesses under the work point, between flanges, in supports and on the floor, where the runs lead, whether nearby insulation has darkened with soaked-in liquid, and whether rags left close by have taken up liquid. After a fire, where the scorching is heaviest is a clue; if the area below the heated spot is more burnt than the spot itself, suspect that pooled liquid flared up.

If pooled liquid looks like the cause, cut the amount sprayed first, placing only what each bolt needs with the extension tube. Before heating, soak up pooled liquid with absorbent pads, remove or cover wet insulation, and lay a fire blanket under the work point. Collect soaked rags and pads in a metal bin with a self-closing lid and empty it at least daily (HSE, 2015).

Hypothesis 4: poor ventilation

In enclosed spaces such as pits under equipment, the insides of tanks and ducts and the space behind machine guards, and in workshops with the doors shut for winter, sprayed gas and vapour cannot disperse and they gather. A mechanic may go down into the pit under a conveyor, spray a number of bolts one after another, then put the torch to the first bolt right there. The flame does not stay round the bolt but races across the floor of the pit.

Vapour heavier than air is at the heart of this hypothesis. Taking air as 1, the relative density of butane gas is 2.11 and that of propane 1.55, so both are heavier than air (NIOSH, n.d.-a; NIOSH, n.d.-b). Flammable liquid vapours are also heavier than air and, unless dispersed, collect in low areas; if they ignite there, the flame can travel back along the vapour to its source, the liquid (HSE, 2015). In a bulletin by the US Chemical Safety Board summarising eleven hot work accidents around tanks, no gas testing was done before or during the work in seven of them (CSB, 2010).

The gas detector gives the answer. Measure not only round the work point but at the lowest spots, such as the floor of the pit, drains and under guards, and keep measuring while the work goes on. Use a calibrated detector, handled by someone trained to use it (CSB, 2010). Also record where air comes in and goes out, whether a fan or extraction was running, and whether doors and windows were open.

In an enclosed space, do not combine spraying and heating. Remove the part and heat it in the open, or draw air out of low spots with portable fans and extraction so that air also moves through the low areas where heavy vapour can gather. Start heating only after gas readings have fallen below the site's limit, following the hot work permit procedure.

Hypothesis 5: spraying hot parts

This covers spraying again when a heated bolt still will not come free, spraying bolts on exhaust pipes, moulds or steam lines that have only just stopped, and spraying penetrant to cool a heated nut. A common example: a nut heated for a long time with the torch will not move, so the worker sets the torch down for a moment and sprays the still-hot nut again. A burst of white vapour rises the instant it is sprayed, and beside the nut that vapour turns into flame.

A hot surface can itself become the ignition source. Liquid that touches it turns to vapour at once and forms a dense cloud, and liquid released as a spray or mist forms an ignitable mixture even below its flash point (HSE, 2015). A study of more than a thousand tests of fuels on a hot surface reported that ignition is not set by a single temperature but appears as a probability, and that the temperature at which ignition occurs half the time is closely tied to the fuel's autoignition temperature (Davis et al., 2006). The can itself is also at risk: aerosol containers carry a warning that they may burst if heated and an instruction not to expose them to temperatures above 50 °C (UN, 2023).

Retrace the work sequence at the moment of the fire. Ask the worker whether spraying came before heating or during or just after it, and measure with an infrared thermometer how hot the same part gets just after operation. Compare that value with the autoignition temperature in the SDS, but since hot-surface ignition happens with a probability, do not conclude that a lower temperature is safe. Also check whether the can was left next to the torch or hot parts.

Write a rule into the work sequence that penetrant is never sprayed during heating or onto hot surfaces. If it must be reapplied, wait until the part has cooled enough, and meanwhile keep the can away from the torch and hot parts. Schedule work on bolts of equipment that has just been running for after it has cooled.

Finding the cause

After a fire, write down the time sequence before memories fade. Recording what was sprayed, when and how much, when heating began and where the flame was first seen narrows several of the five hypotheses straight away. Asking what was left where at that moment, rather than whose fault it was, is what brings out the real sequence. Then move on to checking the SDS, examining the scorch marks, and measuring gas and temperature at the same spot.

Where the flame first appeared and what it looked like are the first clues. A faint flame flaring round the heated nut points to solvent that had not dried or to gas from the can; heavier scorching below the work point points to liquid pooled in gaps and on the floor. Flame that spread widely along the floor points to vapour gathered in low spots and to ventilation, and fire at the moment of spraying points to spraying onto a hot surface.

Next is the time gap. The shorter the gap between spraying and heating, the larger the share of solvent that had not evaporated; if there was a proper wait and fire still broke out, look harder at pooled liquid or vapour left in an enclosed space. If the same product has been used without trouble in the open, the ventilation of the spot becomes the deciding point.

Do not run tests that recreate the fire. Instead, confirm by adding pre-heating checks one at a time from the next job on. After spraying, measure the work point and low spots with a gas detector to see when the reading falls, compare readings before and after wiping up pooled liquid, and measure and record the part temperature. The final check is that, when the work follows the agreed sequence, readings stay below the limit throughout heating.

The hypotheses often overlap. Spraying a can of flammable gas and solvent generously inside a pit and heating at once puts the can's contents, undried solvent, pooled liquid and poor ventilation to work together. In such cases, rather than picking one cause, layer the measures: first remove the largest fuel sources, pooled liquid and gathered vapour, then add waiting and measuring, and finally revisit the choice of product.

Limits and cautions

Flash point, flammable range, autoignition temperature and waiting time differ by product, so take numbers from that product's SDS and TDS. For a fire that injured someone or seriously damaged equipment, preserve the scene and leave the investigation to the site safety lead and fire investigation specialists; hot work on equipment that has held flammable material, such as tanks and pipework, follows the site's hot work permit and gas testing procedures.

Move combustibles round welding, cutting and heating work at least 35 feet, about 10.7 m, away where practicable; where they cannot be moved, cover and protect them and post a fire watch, and keep watching for at least half an hour after the work ends to catch smouldering fires (OSHA, n.d.). Wear a face shield and heat-resistant gloves while using a torch, keep aerosol cans in a cool place away from the work point, and never pierce or burn cans, even empty ones.

Sources

  1. ASTM International. (2026). ASTM D93-26, Standard test methods for flash point by Pensky-Martens closed cup tester. https://webstore.ansi.org/standards/astm/astmd9326
  2. Davis, S., Chavez, D., & Kytomaa, H. (2006). Hot surface ignition of flammable and combustible liquids (SAE Technical Paper 2006-01-1014). SAE International. https://doi.org/10.4271/2006-01-1014
  3. Drysdale, D. (2011). An introduction to fire dynamics (3rd ed.). Wiley. https://doi.org/10.1002/9781119975465
  4. Health and Safety Executive [HSE]. (2015). Safe use and handling of flammable liquids (HSG140, 2nd ed.). https://www.hse.gov.uk/pubns/books/hsg140.htm
  5. National Institute for Occupational Safety and Health [NIOSH]. (n.d.-a). NIOSH pocket guide to chemical hazards: n-Butane. Retrieved November 2026. https://www.cdc.gov/niosh/npg/npgd0068.html
  6. National Institute for Occupational Safety and Health [NIOSH]. (n.d.-b). NIOSH pocket guide to chemical hazards: Propane. Retrieved November 2026. https://www.cdc.gov/niosh/npg/npgd0524.html
  7. Occupational Safety and Health Administration [OSHA]. (n.d.). 29 CFR 1910.252, General requirements: Welding, cutting, and brazing. U.S. Department of Labor. Retrieved November 2026. https://www.osha.gov/laws-regs/regulations/standardnumber/1910/1910.252
  8. U.S. Chemical Safety and Hazard Investigation Board [CSB]. (2010). Seven key lessons to prevent worker deaths during hot work in and around tanks (Safety bulletin). https://www.csb.gov/assets/1/20/csb_hot_work_safety_bulletin_embargoed_until_10_a_m__3_4_10.pdf
  9. U.S. Environmental Protection Agency [EPA]. (n.d.). Substitutes in propellants. Significant New Alternatives Policy program. Retrieved November 2026. https://www.epa.gov/snap/substitutes-propellants
  10. United Nations [UN]. (2023). Globally Harmonized System of Classification and Labelling of Chemicals (GHS) (10th rev. ed.). https://unece.org/transport/dangerous-goods/ghs-rev10-2023

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.