Why is the oil film applied before stamping so uneven?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Metalworking Fluids (MWF)

Opening the valve further is the usual response to dry patches on blanks, but that tends to flood some areas while the dry ones stay dry. What actually makes the film uneven can be a worn, clogged felt roller, spray lost as overspray and mist, viscosity that drifts with temperature, an application rate not tied to line speed, clogged or worn nozzles, or a spray width that does not match the blank, and sometimes two or more at once.

Background

Pull a few blanks just before they enter the press and hold them at an angle to the light. On some, oil has run to one edge and beaded there; on others the middle looks dry and hardly anything comes off on a fingertip. The blanks come from the same coil, yet the front and back differ, and every few parts the formed piece shows scoring or a split at a drawn corner. Blanks with too much oil drip on the way and leave pools on the floor, and add load to cleaning in the next process.

Stamping lubricant controls how much metal flows in from the blank holder, spreads strain over the punch, and reduces galling, where metal sticks to the die, and scoring (WorldAutoSteel, n.d.-b). In drawbead tests, lubrication lowered the friction coefficient, and a heavy-duty stamping lubricant cut frictional resistance to less than half that of dry conditions (Trzepieciński et al., 2019). So where oil is missing, friction rises in that spot alone and metal flow changes. In tests on zinc-coated sheet, areas with no lubricant at all led to sample fracture, and above 1 g/m² adding more oil brought little further reduction in friction (WorldAutoSteel, n.d.-a). Short areas invite defects, and flooded areas only use more oil.

Roller applicators such as felt rollers and spray systems are the common ways to oil blanks. Roller coaters are limited by blank size and need flat steel, while spray systems are less limited by part shape and size, though high-viscosity lubricants can be hard to spray (WorldAutoSteel, n.d.-b). Whatever the method, the oil on the blank is the oil delivered per unit time divided by the area of blank passing in that time. If any one of the amount delivered, the share that reaches the blank, or the speed and width of what passes changes, the film changes with it.

In such cases the technical team sets up the six hypotheses below and rules them out one by one. The start is always the same: cut samples from a few blanks at set positions across the width, measure the film by weighing before and after wiping the oil off, and compare the applicator settings, oil temperature and line speed at the time with the lubricant's technical data sheet, the TDS.

Hypothesis 1: worn, clogged felt

This hypothesis belongs to lines running felt rollers past their change interval, to material with plenty of scale and iron fines, to blanks with burrs that tear at the felt, and to the first run after a stop long enough for the roller to dry out. The same goes for feed holes that carry oil into the roller and have narrowed with residue. Shine a torch on a worn felt and this is what shows: the middle pressed flat and glazed, the edges fluffed up, and dark stripes wound round the roller here and there.

Felt is a porous material that soaks up oil and gives it up on contact with the blank. The speed at which liquid soaks into a porous material follows the equation for capillary flow, slowing as the pore radius gets smaller and the liquid's viscosity gets higher (Washburn, 1921). Where iron fines and hardened oil fill the pores, that part takes up less oil and gives less to the blank, and the same goes for areas pressed dense. One equipment supplier explains that as the felt wears, oil becomes particularly short in some spots, and operators worried about defects open the valve further, so too much oil ends up being used. The same source notes that fibres shed by deteriorating rollers can cause defects of their own, and that oil soaked into a roller gathers at its bottom by gravity, leaving less at the top of the roller, the part that touches the underside of the sheet (Fuso Seiki, 2019).

Begin by taking the roller out. Look for glazed bands, fluffing, torn areas and dark stripes, and line their positions up across the width with the dry bands on the blanks. Measure film weight on the blank separately on the top and underside, at the left, centre and right, and compare. If the underside is always lighter, suspect supply to the lower roller; if only certain bands are light, suspect the felt at that position. Check the oil feed holes and strainer for blockage as well.

If the felt proves to be the cause, base the change rule on condition rather than time. Replace it once glazed bands or fluffing pass a set level, and pass the feed oil through a strainer so iron fines do not reach the felt. Deal with heavy burrs on blanks first, and after a long stop wet the roller thoroughly before starting production. If the sheet is not flat or blank sizes change often, a spray system in place of rollers is worth considering.

Hypothesis 2: overspray and mist

Check whether oil scatters before it reaches the blank where air atomising nozzles break the oil up with compressed air, where the air pressure is set high, where nozzles sit far from the sheet, or where a thin oil is sprayed through tips chosen for a thicker one. Say the line moved to air atomising only recently. The floor and machine guards around the applicator turn glossy, a faint haze drifts under the lights, and the blanks are wet only in the middle and dry at the edges.

An air atomising nozzle mixes compressed air into the oil, breaks it into small droplets and spreads them to a set width. If the droplets are too fine, they drift sideways before reaching the sheet, or hit it too hard and bounce off, becoming overspray that soils the surroundings and the workers. The same source explains that setting the air pressure as low as possible makes the droplets coarser so they settle softly (Fuso Seiki, 2019). A nozzle supplier's guidance runs the same way: a tip suited to a heavy oil will overspray by nearly 60% with a thinner one, and raising the nozzles to cover the blank causes excessive mist, so keep the height as low as will cover the target (Spraying Systems Co., 2026). Oil that drifts away is missing from the film, and since how much drifts varies with draughts and air pressure, the film varies too.

Compare what stays on the sheet with what is used. Take the oil the applicator used over a set time, divide by the blank area that passed in that time, and set the result against the film actually measured on cut samples; the share that never reached the sheet comes out as a number. Check air pressure, nozzle height and tip type against the supplier's recommendations, and note by eye how fast oil builds up on the floor and guards and how much haze hangs around the spray.

If a large share is drifting away, make the droplets coarser and the distance shorter. Lower the air pressure to what is needed for even coverage, bring the nozzles closer to the sheet, and choose tips again to suit the viscosity and flow of the oil now in use. Review with the supplier whether nozzles that spray by liquid pressure alone, without air, could be used. Capture drifting mist with local exhaust so it does not reach the workers.

Hypothesis 3: viscosity drift

Suspect viscosity at the first run of winter in a poorly heated plant, on summer afternoons when the oil tank picks up heat from the press or the sun, at the turn of the seasons, and whenever the film differs between morning and afternoon on the same settings. Picture the line on a summer afternoon: the tank thermometer reads higher than in the morning, and on the same settings the oil on the blanks spreads thinner and wider, some of it running to the edges.

The viscosity of petroleum oils falls as temperature rises, and standard equations and charts give the viscosity at any temperature in a range from two measured values (ASTM International, 2020). When viscosity changes, every stage of the applicator changes with it. The rate at which oil soaks into felt is inversely related to viscosity, so cold oil wets the roller slowly, and in a spray, higher viscosity resists break-up and gives larger droplets (Washburn, 1921; Lefebvre & McDonell, 2017). On the sheet, thinned oil spreads wider and runs more easily. The same carries on inside the press: as die temperature rises, lubricant viscosity can fall and the friction coefficient rise (WorldAutoSteel, n.d.-b).

Measure oil temperature at the tank and just before the applicator a few times over a day, and log it alongside film weight measured at the same times. If the film follows the temperature up and down, the case lies here. Use the viscosities at two temperatures given in the TDS to estimate how much viscosity changes across the working temperature range, and check the oil storage area and any heat sources near the tank as well.

The most direct remedy is to hold the oil temperature steady. Keep oil indoors, move or shield the tank from heat sources, and if needed hold a set temperature with a temperature controller. On cold mornings, start production only once the oil has reached that temperature. Where temperature is hard to hold, choose with the supplier an oil whose viscosity changes less with temperature, and reset the applicator for each season.

Hypothesis 4: rate not tied to speed

The rate falls out of step with speed when the applicator keeps delivering a fixed flow while line speed changes with part number, coil and feeder settings, and when acceleration, deceleration, stops and restarts are frequent. It applies all the more to applicators whose flow is set by hand on a needle valve. Suppose the line was run a step faster after a part change while the oil setting stayed as it was. The film on the blanks becomes visibly thinner, while during a slow trial run oil had pooled at the end of every blank.

Since the oil on the blank is the oil delivered divided by the area passing, doubling the speed at a constant flow halves the film. A nozzle supplier advises matching flow rate to conveyor speed, and explains that switching nozzles on and off very rapidly to change flow almost instantly with line speed keeps the pressure, and so the droplet size and spray angle, constant, giving even coverage over a wide range of flow rates. The same source notes that automated on and off control eliminates the drips that cause quality problems (Spraying Systems Co., 2026). Adjusting flow by changing pressure, by contrast, changes droplet size and spray pattern along with it. Blanks from acceleration and deceleration, and from just before a stop and just after a restart, differ from the rest because of this mismatch.

The check is to set the speed record beside the film weight. From the same coil, pick blanks from the steady-speed section, the acceleration and deceleration sections and just after a restart, measure their film, and match it to the line speed at the time. See whether the applicator controller actually receives a line speed signal and, if it does, whether it is set to change flow with speed. A table of speed and applicator settings by part number shows mismatched combinations at once.

If the two are running apart, tie them together. Feed the line speed signal to the applicator controller so flow follows speed; if that is not possible, set applicator settings for each part number's speed in the work standard and change them whenever the speed changes. Make the applicator stop when the line stops, and check the film separately on the first few blanks after a restart.

Hypothesis 5: clogged, worn nozzles

Suspect the nozzles one by one where oil is fed without a strainer, where open tanks let debris in, where tips have gone a long time unchanged, and where blocked nozzles have habitually been poked clear with wire. Imagine an applicator with several nozzles spraying side by side, where a long dry band runs along the blanks under just one nozzle. Under the nozzle next to it, the oil is if anything piled on heavily.

Nozzles fail in two directions. Unwanted solid particles blocking the orifice reduce flow and disturb the spray pattern, while gradual erosion of nozzle material enlarges the orifice and internal passages, raising flow and droplet size, lowering pressure and distorting the pattern. Damage from unsuitable cleaning tools also degrades performance (Spraying Systems Co., n.d.). Wear is hard to see. In a paper on nozzle wear, a worn tip that looked no different from a new one sprayed 30% over capacity, and worn flat fan nozzles developed streaks and heavier flow in the centre of the pattern while the effective spray angle narrowed (Barber, n.d.). A blocked nozzle leaves its band dry and a worn one floods its band, so stripes form on the blank.

Catch each nozzle's output for the same time, measure it, and compare it with a new nozzle or the catalogue flow. The same paper advises collecting and measuring rather than trusting the eye, which cannot see wear, and checking spray angle with a protractor and pattern width with a rule (Barber, n.d.). Pass a sheet of card or paper under the spray once and the band pattern shows blocked and worn nozzles together. Look at what is caught in the strainer ahead of the nozzles too.

Base nozzle replacement on measurement, not on looks. Replace a nozzle once its flow departs from a new one's by more than a set margin, put a strainer ahead of the nozzles to catch debris, and keep the tank covered. Soak blocked nozzles and clean them with a soft brush instead of wire, and swap in a spare tip so the removed one can be dealt with off the line. Set the inspection interval from the measurement records.

Hypothesis 6: spray width off blank

This hypothesis fits where blank width changes with part number but the number, spacing and height of the nozzles stay the same, where wide-angle tips are used on narrow blanks, and where nozzle height has been changed by hand over time. A narrow blank passing under a row of nozzles set up for a wide one is such a case. The outer nozzles spray the conveyor beyond the blank, and faint bands remain on the blank at each seam between nozzles.

The width one nozzle covers is set by spray angle and height, and when several nozzles cover a wide blank, neighbouring sprays have to overlap by the right amount or the seams go bare. A nozzle supplier's guidance says some tips must overlap the adjacent pattern by 20 to 30% for even coverage, and that a narrow target calls for a narrow-angle tip rather than rotating a tip to narrow it. It states that rotating tips raises lubricant use by 30 to 70%, and advises covering a wide target with a wide-angle tip or more nozzles, since raising the nozzles to widen coverage causes excessive mist (Spraying Systems Co., 2026). Oil that lands beyond the blank never reaches it, seams with too little overlap go dry, and places with too much overlap flood. For a roller applicator, the same logic is why roller width has to suit blank width (WorldAutoSteel, n.d.-b).

Pass card under the spray to see the covered width and the seams, and compare that width with each part number's blank width. Measuring film separately at the blank edges, at the seams and directly under the nozzles shows in numbers whether overlap is short or excessive. Check whether the number of nozzles switched on, their height and tip angle are recorded for each part number, and whether the record matches what is actually set.

Set spray conditions separately for each part number. Switch off nozzles that fall outside the blank, and set the height and spacing of the rest so neighbouring sprays overlap by the amount the supplier recommends. Keep narrow-angle tips for narrow blanks, and write these conditions into the part changeover procedure so they change with every changeover.

Finding the cause

There is no need to look at all six at once. Rule out the easy measurements first. Each nozzle's output and a single card's spray bands take minutes, and oil temperature and line speed are in the records. Cutting a few blanks and weighing the film comes next, and taking the roller out is fitted into a scheduled stop.

The shape of the unevenness is the next clue. Stripes running along the blank point to the nozzle or felt at that position, or to the seams between nozzles. If the whole width thickens and thins together, look at conditions that act on the whole applicator, such as line speed or oil temperature. A difference between top and underside points to the supply to the upper and lower rollers or nozzles, and dry edges with glossy surroundings point to overspray and spray width.

Look at timing as well. Differences between morning and afternoon or across seasons point to temperature and viscosity; problems that began after a part change point to speed and spray width settings; and a slow decline over weeks points to felt or nozzle wear. If that still does not settle it, run control trials that change one thing at a time: measure the film again with one nozzle replaced, with new felt, with the oil temperature held, and with the line speed held.

The final check is the spread of film weight measured the same way. Measure at the same positions across and along the blank, top and underside, as before the change, see whether the gap between the heaviest and lightest spots has narrowed, and count scoring and splits on formed parts over the same period. The job is done only when the figures have recovered and stay there.

The hypotheses can be entangled. Oil that warms and thins drifts more from the same tip, a worn nozzle passes more flow and upsets settings matched to speed, and a roller with its valve opened further makes flooded and dry areas both worse. In such cases, put right first the conditions that act on the whole applicator, oil temperature and flow matched to line speed, and then look one by one at causes that differ by position, such as nozzles, felt and spray width, because while the overall conditions are unsettled, differences between positions cannot be compared fairly.

Limits and cautions

Suitable film weight, oil temperature, air pressure, nozzle height and overlap differ by steel type and surface coating, part shape, lubricant and applicator, so numeric decisions follow the lubricant's TDS and the equipment supplier's guidance. Changing the film weight can also affect later processes such as welding, bonding and painting, so confirm any change of standard with the people responsible for those processes.

Safety matters too. Handle the lubricant with the protective equipment set out in the product's safety data sheet, the SDS. Metalworking fluids can harm health through skin contact and through breathing in mist (OSHA, n.d.), so extract around the spray and clean oily floors straight away to prevent slips. Remove rollers or work on nozzles only with the line and applicator stopped and locked out, and wear eye protection when handling compressed air.

Sources

  1. ASTM International. (2020). ASTM D341-20, Standard practice for viscosity-temperature equations and charts for liquid petroleum or hydrocarbon products. https://store.astm.org/d0341-20.html
  2. Barber, J. (n.d.). How to pre-empt a significant profit drain: Nozzle wear [White paper WP106]. Spraying Systems Co. Retrieved November 2026. https://www.spray.com/-/media/dam/industrial/usa/sales-material/white-paper/wp106_preempt_nozzle_wear.pdf
  3. Fuso Seiki. (2019). A thorough comparison of 3 ways to apply lubricant when stamping! [Technical column]. https://fusoseiki.co.jp/en/column/solutions/172.html
  4. Lefebvre, A. H., & McDonell, V. G. (2017). Atomization and sprays (2nd ed.). CRC Press. https://doi.org/10.1201/9781315120911
  5. Occupational Safety and Health Administration [OSHA]. (n.d.). Metalworking fluids. U.S. Department of Labor. Retrieved November 2026. https://www.osha.gov/metalworking-fluids
  6. Spraying Systems Co. (2026). Precision spray lubrication systems: Solutions for metal fabrication & forming [Bulletin No. 685C]. https://www.spray.com/en-za/-/media/dam/industrial/usa/sales-material/product-market-bulletin/b685a_lubrication_systems.pdf
  7. Spraying Systems Co. (n.d.). Common spray problems. Retrieved November 2026. https://spray.com/resources/spraying-basics/spray-optimization/common-spray-problems
  8. Trzepieciński, T., Kubit, A., Slota, J., & Fejkiel, R. (2019). An experimental study of the frictional properties of steel sheets using the drawbead simulator test. Materials, 12(24), 4037. https://doi.org/10.3390/ma12244037
  9. Washburn, E. W. (1921). The dynamics of capillary flow. Physical Review, 17(3), 273–283. https://doi.org/10.1103/PhysRev.17.273
  10. WorldAutoSteel. (n.d.-a). Coating friction. AHSS Application Guidelines. Retrieved November 2026. https://ahssinsights.org/coatings/coating-friction/
  11. WorldAutoSteel. (n.d.-b). Lubrication. AHSS Application Guidelines. Retrieved November 2026. https://ahssinsights.org/forming/tooling/lubrication/

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.