KALTECKOREA

BlogApplication notes

Why do refrigeration expansion valves and capillary tubes keep clogging?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Equipment/Service Lubricants

Clearing the valve or fitting a new capillary is the usual response to a blockage, but if whatever blocked it keeps forming or arriving from elsewhere in the circuit, the new part tends to clog in the same place. What actually blocks the narrow passage can be wax from mineral oil, frozen moisture, acid and sludge from oil breakdown, oxide scale and debris left from installation, or broken-down desiccant, and often two or more at once.

Background

The compressor runs without a break, yet the cold store will not pull down. The suction gauge sits lower than usual, and heavy frost forms only at the expansion valve outlet or the end of the capillary tube. With refrigerant unable to pass the narrow passage properly, too little reaches the evaporator and cooling capacity falls, and a hermetic compressor cooled by suction gas tends to run hotter. If the store warms up, stored goods may have to be thrown away, and replacing a blocked part means recovering the refrigerant and opening the pipework, so repair cost and downtime grow together.

Expansion valves and capillary tubes are the narrowest passages in a refrigeration circuit and the point where refrigerant pressure and temperature fall at once. Anything dissolved or suspended in the oil that circulates with the refrigerant, if it solidifies on cooling or settles where flow slows, usually lodges here. A study that used accelerated tests to examine capillary clogging in air conditioners divided the process into four stages. In outline, sludge forms inside the compressor, the oil carries it to the capillaries or expansion valves, and once separated from the refrigerant it deposits on the inner walls of the passage (Taira et al., 1998).

A blockage forms in one of two ways. Either a solid forms in the refrigerant and oil as they cool, or a solid formed or introduced elsewhere in the circuit is carried along and lodges. The first kind often clears once things warm up, while the second leaves debris you can hold when the part is opened. This difference alone narrows the cause a good deal.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: keep the blocked part and the filter drier ahead of it, log when the blockage appeared with the operating pressures and temperatures at the time and any recent repairs or oil top-ups, and compare them with the refrigeration oil's technical data sheet, the TDS, and the equipment installation guidance.

Hypothesis 1: wax from mineral oil

Look at this hypothesis first in mineral-oil machines with very low evaporating temperatures, such as blast freezers and ultra-low-temperature stores. It applies especially when the compressor has been topped up with a general-purpose mineral oil rather than a refrigeration oil, when a refrigeration oil graded for higher temperatures has been used, or when the set point has been lowered. Picture a freezer compressor topped up during maintenance from whatever drum of mineral oil was to hand. A few weeks later, evaporating pressure sags only during the coldest night-time running; raising the set point in the day seems to bring the flow back, and the same thing happens again at night.

Mineral oil contains wax components that stay dissolved while warm and come out as solids when cold. The standard test for this property of refrigeration oil is the floc point test: a mixture of 10% oil and 90% refrigerant is cooled under set conditions, and the highest temperature at which wax or other solids first precipitate is the floc point. The same standard notes that wax deposited in a system is known to clog capillary tubes and make expansion valves stick, and it uses R-12 as the test refrigerant because it stays mixed with oil at low temperature; with a less miscible refrigerant such as R-22, the oil separates before the floc point is reached (ASHRAE, 2013). The temperature at which a cluster of wax crystals first appears in the oil alone is measured separately as the cloud point (ASTM International, 2023). Since the oil carried in the refrigerant first reaches its coldest at the outlet of the expansion device, precipitated wax tends to build up around there.

Check the maintenance records first for any recent top-up or oil change, and whether the oil used was the grade the compressor maker specifies. Match the operating records to see whether the blockage appears only at the lowest evaporating temperature and eases when the temperature rises, and look inside the blocked valve or a cut section of capillary for white or yellowish waxy residue. Send a sample of the oil in service to a laboratory for cloud point and floc point, and compare the results with the TDS values and the lowest evaporating temperature of the equipment.

If wax is indicated, the first step is to change to a refrigeration-grade oil suited to the lowest evaporating temperature of the equipment. Mixed oil tends to linger if only part is drained, so change it following the compressor maker's procedure, and clean or replace the expansion valve and capillary where wax has built up. To keep it from returning, label the top-up oil grade for each machine and do not store it alongside mineral oils meant for other uses.

Hypothesis 2: frozen moisture

Moisture tends to get in after the circuit has been opened and closed. Typical cases are pipework left open for a long time during a compressor or component change, refrigerant charged without a proper vacuum, top-ups from an oil container left open, and a leak in the evaporator or suction line that draws air in. Say a compressor was changed on site on a rainy day, the vacuum was pulled in a hurry and the refrigerant charged. For the first few hours it cools well, then frost gathers at the expansion valve outlet and suction pressure drops sharply, and after a stop and restart it runs normally again for a while.

Refrigerant and oil can hold a certain amount of water in solution, but water beyond that limit separates out. The moment refrigerant falls below freezing as it passes the expansion device, the free water freezes, and the ice narrows or blocks the expansion valve, the capillary tube or the evaporator inlet. Beyond ice, moisture can lead to corrosion of metals and to acid formation, so refrigerant systems control it separately with driers and evacuation (ASHRAE, 2018). Because ice melts when the machine stops and warms, the blockage tends to build while running and clear after a rest. Polyol ester oil, POE, the ester-based synthetic, dissolves more water than mineral oil and forms acid by hydrolysis when it meets water, so water that gets in can lead to acid as well as ice (Cartlidge & Schellhase, 2003).

The easiest check is the colour of the moisture indicator on the liquid line sight glass. When it is blocked, wrap the expansion valve body in a warm cloth; if flow returns soon after, ice is strongly suspected. If an oil sample can be drawn, measure its water content by Karl Fischer titration, the standard method, and compare it with the oil supplier's recommended value (ASTM International, 2025). Match the repair records to see whether the blockage began after the date the circuit was opened.

If moisture is the cause, recover the refrigerant, fit a new filter drier, and pull a deep vacuum for long enough to draw the water out. Driers are rated for water capacity and flow capacity under standard conditions, so choose a rating that suits the refrigerant and the size of the equipment (AHRI, 2009). Use top-up oil, POE above all, straight from a sealed container, and never reuse oil from an opened drum. Find and seal any low-side leak that could draw air in before pulling the vacuum.

Hypothesis 3: acid and sludge

Suspect residue from oil breakdown in equipment where the compressor has run hot for a long time or moisture has remained in the circuit. Typical cases are machines that came through a summer with clogged condensers and high discharge temperatures, machines that ran short of refrigerant with superheated suction gas for long periods, and machines using HFC refrigerant with POE. One such scene is a chilled display cabinet that ran all summer with dust matted on its condenser fins and is opened at the autumn service. A thin brown, sticky film coats the inner wall of the cut capillary inlet, and the oil drawn from the compressor is darker than new and smells sour.

Over long service, refrigerant or oil breaks down little by little and acid builds up. In older chlorine-based refrigerant and mineral oil systems the trouble was strong mineral acids, hydrochloric and hydrofluoric, from thermal breakdown of the refrigerant, but in HFC and POE systems the POE meets water and hydrolyses back to organic acids with five to nine carbon atoms and alcohols. These organic acids are much weaker and less corrosive, but over long periods they react with metals to form metal salts, which tend to accumulate in narrow places such as capillary tubes. How fast acid forms depends on the ester's structure, moisture, temperature, the acid already present and metals (Cartlidge & Schellhase, 2003).

Heat pushes the same way. In tests running reciprocating and rotary compressors on HFC-134a and POE, capillary sludge increased with compressor temperature, and the sludge from the rotary compressor was a tar-like substance. The authors concluded that desiccant and high temperature can break down and polymerise ester oil into such tar (Yamamoto et al., 1996). The accelerated tests mentioned earlier reproduced clogging by raising oil temperature and refrigerant flow for the same reason (Taira et al., 1998).

Measuring the oil's acid number, the amount of potassium hydroxide needed to neutralise one gram of oil, is the core check. Laboratories use standard methods such as colour-indicator titration (ASTM International, 2022), and on site acid test kits give quick semi-quantitative results. For mineral oil and chlorine-based refrigerant systems, 0.05 mg KOH/g has served as the action level, based on analysis of 700 used oils, but there is no industry consensus yet for POE systems, where the value is expected to be higher (Cartlidge & Schellhase, 2003). So for POE systems, watch the trend against earlier values from the same machine. Look at oil colour and smell and at the discharge temperature records too.

With acid and sludge identified, remove the source of heat first. Clean the condenser and set the charge and superheat to bring discharge temperature down, then change the oil and filter drier and replace the capillary or expansion valve. Measure the acid number again over the following weeks to months to confirm the lower value holds. If it climbs again, heat may still be high or moisture may remain, so go back over the discharge temperature and the moisture checks.

Hypothesis 4: installation debris

If clogging began right after new installation or pipe repair, look at what was left in the circuit during the work. This covers pipe brazed without nitrogen flowing, cut tube ends left with burrs, tube stacked on site without caps, leftover flux and machining oil from component manufacture. Consider an expansion valve inlet strainer that blocks a few days after a unit is connected to new pipework and commissioned. Pulled out, the strainer holds dark, scale-like flakes tangled with shiny metal fragments.

When copper tube is heated to brazing temperature, the oxygen left inside oxidises the inner surface and forms an oxide layer. Systems such as refrigeration and air-conditioning pipework need an inert gas flowing during brazing to push the oxygen out of the tube, which keeps oxide from forming on the inner surface. The copper tube handbook's model specification calls for a continuous purge of oil-free dry nitrogen during brazing, kept up until the joint is cool to the touch (CDA, 2019). Oxide formed without nitrogen can break off in flakes as refrigerant and oil flow, and those flakes and metal fines follow the flow to the narrowest point. Process chemicals such as residual oils make matters worse. Where such residues are present, metal salts from oil breakdown accumulate more readily in capillaries (Cartlidge & Schellhase, 2003), and in reciprocating compressor tests the cleanliness of the circuit governed sludge formation (Yamamoto et al., 1996).

The evidence is the debris itself. Open the blocked strainer, the expansion valve inlet screen and the inlet side of the removed filter drier, and look for dark flakes, metal fragments and hardened flux. Check the records for whether blockages cluster in a short period after commissioning and fall off afterwards, and ask the installer whether nitrogen was flowing during brazing and whether tube ends were capped in storage. If a cut section of pipe is available, see whether its inner surface has turned black and flaky.

Once installation debris is confirmed, clean the blocked screens, fit a new filter drier and run for a while so the remaining fragments collect in the drier. If a lot has been caught, change it once more. For future work, write the nitrogen purge method and flow rate into the brazing procedure, store tube with its ends capped, and deburr cut ends so the swarf does not fall inside.

Hypothesis 5: broken-down desiccant

Look at the desiccant if the blockage sits just downstream of the filter drier and that drier has been in service a long time or is mounted where it shakes hard. Examples are a drier hung unsupported on a line that carries compressor vibration, a drier reused rather than replaced at a repair, and a drier that has held moisture or acid for long enough to reach its limit. One example is a capillary blocked just past a drier left in place for years, where cutting the inlet reveals a pale powder caked together with oil.

A drier is packed with desiccant, porous beads that soak up water, and the refrigerant leaves its water behind as it passes between them. When beads rub together or break, fine dust forms, and if that dust gets past the screen at the drier outlet it lodges in the narrow passage right behind. In tests that analysed capillary sludge, the sludge from the reciprocating compressor was mainly desiccant and metal dust, and with the rotary compressor the presence or absence of desiccant governed sludge formation (Yamamoto et al., 1996). The drier rating standard rates water capacity and flow capacity (AHRI, 2009), so the water capacity on a rating sheet says nothing about whether the desiccant will hold together without breaking up.

Look for fine white or grey powder at the outlet of the removed drier and at the capillary inlet just behind it. Sorting the debris into hard flakes like oxide scale, sticky deposits like sludge or fine powder like desiccant separates this hypothesis from its neighbours. Confirm from the records and on site when the drier was last changed, how it is supported and how much it vibrates, and whether it suits the refrigerant and oil, and if needed cut the drier open to see whether the beads have broken.

If desiccant dust turns up, do not reuse the drier; fit a new one with a water capacity rating suited to the refrigerant and equipment size, and confirm with the supplier that its outlet filtration is adequate. Mount the drier firmly so compressor vibration does not reach it directly, and make changing it whenever the circuit is opened part of the maintenance standard. Replace the blocked capillary so no powder remains.

Finding the cause

Five hypotheses do not call for five sets of tests. Rule them out starting with what can be seen without opening the equipment. The moisture indicator on the sight glass, the pressures and temperatures in the operating records, and the dates of oil top-ups and repairs in the maintenance records can all be checked today. Oil analysis and dismantling come after that.

The shape of the symptom is the first fork. If the blockage builds while running and clears after a stop or when warmed, it is a solid formed by cooling, that is ice or wax. Between the two, suspect ice first if it began after the circuit was opened and the moisture indicator reads wet, and wax if it appears only at the lowest evaporating temperature after a recent oil top-up. If it does not clear with a rest and keeps getting worse, a solid has been carried in, and the part has to be opened to see the debris.

Debris sorts itself by appearance. Dark flakes and metal fragments point to installation debris, fine white or grey powder to desiccant, and a brown sticky film or tar to sludge from oil breakdown. For sludge, confirm the part played by heat and moisture from the oil acid number and the discharge temperature records; for installation debris, see whether blockages clustered just after commissioning. If appearance does not settle it, send the debris to a laboratory for analysis.

Settle any remaining doubt with control trials that change one thing at a time. Replace only the filter drier first, then change the oil to the right grade. Change two things at once and there is no telling which one worked. Afterwards, record the time until the next blockage, suction pressure and discharge temperature on the same basis as before the change, and treat the job as finished only when that interval has grown long enough.

The causes often interlock. Leftover moisture can turn to ice, but it also hydrolyses POE into acid (Cartlidge & Schellhase, 2003), and high temperature together with desiccant can turn ester oil into tar (Yamamoto et al., 1996). So when ice and sludge appear together, remove the moisture first, then look at the source of heat and the oil condition. While moisture remains, acid and sludge keep forming even after the oil and drier are changed, so the effect of those changes cannot be compared fairly.

Limits and cautions

Oil grade, control values for moisture and acid number, drier size and vacuum time differ by refrigerant, oil, compressor and equipment, so numeric decisions follow the oil's TDS and the compressor and equipment makers' guidance. Contamination from a compressor motor burnout calls for a separate clean-up procedure, and if clogging keeps recurring without a clear cause, hand it to a refrigeration specialist and a laboratory.

Handling refrigerant involves certification and regulation. In the United States, intentionally venting refrigerant while servicing refrigeration and air-conditioning equipment is prohibited and technicians must be certified (EPA, n.d.), and elsewhere the local regulations and qualifications apply. Recover the refrigerant and confirm pressure before opening pipework, and on equipment with flammable refrigerant, remove the refrigerant completely and ventilate before any hot work. Acidic oil can harm skin and eyes, so wear gloves and eye protection as the safety data sheet, the SDS, directs.

Sources

  1. Air-Conditioning, Heating, and Refrigeration Institute [AHRI]. (2009). ANSI/AHRI Standard 710 (I-P), Performance rating of liquid-line driers. https://www.ahrinet.org/search-standards/ahri-710-i-p2009-performance-rating-liquid-line-driers
  2. American Society of Heating, Refrigerating and Air-Conditioning Engineers [ASHRAE]. (2013). ANSI/ASHRAE Standard 86-2013, Methods of testing the floc points of refrigeration grade oils. https://webstore.ansi.org/standards/ashrae/ansiashraestandard862013
  3. American Society of Heating, Refrigerating and Air-Conditioning Engineers [ASHRAE]. (2018). Control of moisture and other contaminants in refrigerant systems. In ASHRAE handbook: Refrigeration (Chapter 7). ASHRAE.
  4. ASTM International. (2022). ASTM D974-22, Standard test method for acid and base number by color-indicator titration. https://store.astm.org/d0974-22.html
  5. ASTM International. (2023). ASTM D2500-23, Standard test method for cloud point of petroleum products and liquid fuels. https://store.astm.org/d2500-23.html
  6. ASTM International. (2025). ASTM D6304-25, Standard test method for determination of water in petroleum products, lubricating oils, and additives by coulometric Karl Fischer titration. https://store.astm.org/d6304-25.html
  7. Cartlidge, D., & Schellhase, H. (2003). Using acid number as a leading indicator of refrigeration and air conditioning system performance (Final Report ARTI-21CR/611-50060-01). Air-Conditioning and Refrigeration Technology Institute. https://digital.library.unt.edu/ark:/67531/metadc786951/
  8. Copper Development Association [CDA]. (2019). The copper tube handbook. https://www.copper.org/applications/plumbing/cth/brazed-joints/cth_7brzjts_purge.php
  9. Taira, S., Oonuma, Y., Yamakawa, K., & Yajima, R. (1998). Accelerated evaluation of capillary clogging in HFC air conditioners. In Proceedings of the 1998 International Refrigeration Conference at Purdue. Purdue University. https://iifiir.org/en/fridoc/accelerated-evaluation-of-capillary-clogging-in-hfc-air-conditioners-17325
  10. U.S. Environmental Protection Agency [EPA]. (n.d.). Stationary refrigeration and air conditioning. Retrieved November 2026. https://www.epa.gov/section608
  11. Yamamoto, T., Yamamoto, T., Simizu, Y., Nakayama, Y., & Takizawa, K. (1996). Consideration of sludge formation in HFC-134a/polyol ester oil refrigeration system. Transactions of the Japan Society of Refrigerating and Air Conditioning Engineers, 13(2), 167–173. https://doi.org/10.11322/tjsrae.13.167

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.