KALTECKOREA

BlogApplication notes

Why are we using so much release agent?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Release & Process Aids

Mixing the concentrate leaner or switching products is the usual response when release agent use climbs, but only part of what is sprayed onto a hot die stays as a film, so unless the place where the rest escapes is found, use rarely comes down. What actually lies behind it can be spraying on idle cycles, overspray and mist from air atomising, unmanaged dilution, clogged or worn nozzles, a die running too hot, or hand spraying that varies by operator, and sometimes two or more at once.

Background

Each time the die opens, the spray head comes down, leaves a white fog and goes back up. Liquid pools on the floor under the die, and a sticky film builds up inside the cell guards and on top of the machine. Concentrate drums are being changed ever more often while output stays the same, and purchasing wants to know why so much release agent is going in.

The loss does not stop at the price of concentrate. Liquid that fails to stay on the die becomes wastewater that adds to treatment costs, makes the floor slippery and hangs in the air as mist that operators breathe in. Longer spraying also lengthens the cycle. When the die is cooled too far or the spray runs too long, forging suffers from the die chilling the workpiece, and die casting can show defects such as cold shuts, where metal streams fail to fuse (Mendez & Powell, 2008).

In die casting and forging, a release agent builds a parting film between casting and die, insulates the die from the molten metal, protects the die face from oxidation, and cools the die as its water evaporates (Sabau et al., 2007). The concentrate is usually diluted with water and sprayed onto the hot die, and once the water has evaporated, what remains forms a thin film. Yet the amount that actually stays on the die is small compared with the amount sprayed, and how much stays depends on heat transfer at the die surface (Mendez & Powell, 2008). So a consumption problem calls first for asking where the spray goes, not how much is sprayed.

In such cases the technical team sets up the six hypotheses below and rules them out one by one. The start is always the same: divide the concentrate used over a set period by the number of good shots to get use per shot, and set it beside the dilution and spray conditions in the release agent's technical data sheet, the TDS, and the values actually set on the cell.

Hypothesis 1: idle-cycle spraying

When a spray programme is tied to the die-open signal, it sprays just the same on cycles that run without metal. That happens while a die is being warmed up after a change, when the melt supply stops and the cell runs on standby, when scrap shots are thrown away and the cell restarts, and when spray time is fixed even though the die is already well covered. Picture a lunch changeover when a furnace problem stopped the metal, yet the cell kept opening and closing the die and spraying on its own. On return, the die face is wet and glistening, and the floor below is awash.

With no metal coming in, nothing puts heat into the die, while the release agent keeps cooling it as it evaporates (Sabau et al., 2007). As the die face cools, more of the spray fails to evaporate and stays liquid. A study that divides deposition into stages explains that on a very hot die the spray simply flies off, within a suitable temperature band the solids stick with no liquid left, and once the die face has cooled to around the boiling point of water, liquid running down washes off even the film already laid. The same study adds that industrial practice tries to shorten the first stage and avoid the washing stage altogether (Mendez & Powell, 2008). Spray on an idle cycle adds no film and ends up on the floor and in the wastewater. Taking the next shot on a cooled die also adds the risk of defects such as cold shuts.

Setting two numbers against each other shows it. From the machine records, pull the spray count and the actual casting shot count for the same period and look at the gap, then compare concentrate use divided by spray count with concentrate use divided by good shots. A wide gap means idle-cycle spraying is driving use up. Check which programme the cell runs during warm-up and standby, and watch whether liquid pools under the die meanwhile.

Where idle cycles are the cause, tie spraying to the actual casting signal. Skip spraying on cycles without metal, and give warm-up and restart their own spray programme set to the TDS and the supplier's advice. Reset fixed spray times to what it takes to cover the die, and set the cell to stop itself when standby runs long.

Hypothesis 2: air overspray and mist

Look at this hypothesis when air pressure is set high on twin-fluid nozzles, which break the liquid up with compressed air, when air was turned up to reach deep ribs or the inside of cores, or when the spray head sits far from the die. The same applies when supply air pressure has changed and nobody has touched the regulator. When fog lingers long after the cell door opens, and a thin layer of release agent has settled on the duct inlet and nearby machines, this side is worth suspecting.

In a twin-fluid nozzle, air tears the liquid into drops, and the more air there is relative to liquid, and the faster it moves, the smaller the drops (Lefebvre & McDonell, 2017). Small drops carry little momentum, so rather than flying straight to the die they ride the air currents and scatter in and around the cell. Near a hot die, the smaller the drop, the more likely its water evaporates before it arrives, and the solids that should stick are then dispersed into the air (Mendez & Powell, 2008). Data on paint spray guns show that conventional guns atomising with compressed air have a transfer efficiency, the share of sprayed material that lands on the target, of about 20 to 40%, so most becomes overspray, while high-volume low-pressure guns with slower air bounce back less and transfer more (EPA, n.d.-a). Release agent is not paint, but in both cases much of the air-broken liquid misses its target.

Read the air pressure gauge at the head against the setting, and see whether the ratio of air to liquid pressure lies within the TDS or the equipment manual. Measure spray distance and angle at the actual head position. Photograph where the fog drifts during spraying and how much settles on guards and machines outside the die, so that conditions before and after adjustment can be compared. Drop the air pressure one step for a few shots and watch whether the film still forms evenly and sticking does not increase.

If overspray is the finding, find the lowest air pressure that still covers the die and fix it there, and reset the head to sit closer to the die and point more squarely at its face. Rather than reaching deep features with stronger air, give them a nozzle aimed at that spot. On heads that use separate air for spraying and for blowing off, check that the two do not overlap in time and blow the film away.

Hypothesis 3: unmanaged dilution

Dilution drifts when concentrate and water are mixed by eye in a tank, when an automatic mixer's setting slips or water pressure changes, when a different person mixes on each shift, and when nobody measures the mixed concentration. The day after a night shift pours concentrate roughly and tops up with water, castings start sticking on a few dies and spray time gets lengthened. After that, even once the concentration is back, the longer spray time stays.

One model explains the film left on the die by three things: the share of active content in the liquid, the amount of liquid reaching the die and the part of it that actually sticks (Mendez & Powell, 2008). A lean mix lays a thinner film for the same spray time, so castings stick more easily, and the floor usually makes up the difference by spraying longer. A rich mix builds more film than needed and uses that much more concentrate. Either way, the process is uneven while concentration wanders, and industry guidance likewise notes that water-based release agents need accurate, consistent dilution and that loose control of it makes the process inconsistent (Cross, 2023). This also covers cases where the real reason for higher concentrate use is not the concentration but spray time added because of it.

Draw a sample of the mixed liquid from the tank and from the end of the line, and measure concentration by the method the supplier recommends. Measuring several times a day and at each shift change shows how far it swings. If there is a mixer, read the concentrate and water flowmeters together, and check that the ratio of concentrate to water used over a period matches the set dilution. Look in the records for when and why spray time settings were changed.

If dilution is drifting, take mixing out of people's hands. Use a proportioning mixer to hold the set ratio, measure and log concentration at least once a day, and decide who does what when it leaves the range. Once concentration is under control, bring the spray time that was added along the way back down towards the TDS basis.

Hypothesis 4: clogged or worn nozzle

Nozzle holes wear with long use, and release agents that carry solids dry and harden at the nozzle tip. Where nozzles have run for years with no replacement rule, where heads parked near a hot die dry out at every break, or where blocked holes are routinely cleared with wire, nozzle condition may be what is pushing use up. A test spray from the head shows one nozzle putting out a thin, twisted stream, another throwing coarse drops, and the rest looking fine. Sticking turns up exactly where that nozzle is meant to cover.

As a nozzle's hole and inner passages wear and widen, flow usually rises, pressure may drop, the pattern turns irregular and the drops grow larger. A nozzle maker's guide shows that a worn tip spraying 30% over its rated flow could not be told from a new one by eye, and only liquid collected over a set time revealed the difference. The same guide lists caking, dried solids left on the inside or around the orifice as liquid evaporates, among the common faults (Barber, n.d.). A worn nozzle sprays more than needed, and a clogged one leaves its spot uncovered so castings stick there. The floor then lengthens spray time for the whole head to fill one spot, and the healthy nozzles spray more as well.

Looking is not enough, so collect and measure. At a set pressure, catch each nozzle's output for a fixed time, weigh it or measure its volume, and compare it with a new nozzle or the maker's table. A short burst onto a plate or sheet of paper shows the pattern, revealing streaks or a lopsided spray. Check the tip and the rim of the hole for dried residue as well.

A maintenance rule keeps nozzle trouble from recurring as often. Replace a nozzle when its collected flow differs from a new one by more than a margin the plant has set, and always keep spares of the same size. Clean holes by the method the supplier recommends rather than with wire, and when production stops, flush the head with water so agent does not dry inside the nozzles. After changing nozzles, take back the spray time that was added for one spot.

Hypothesis 5: die too hot

A die runs hot after cycle time has been cut, at spots where heat gathers such as thick bosses or the area near the gate, when cooling channels have narrowed with scale, and when cooling water warms up in summer. A typical scene: sticking appears only around the thick sections rather than over the whole die, and when spray hits that spot it sizzles and drops leap back off. The operator then sprays that spot longer or adds spray time to the whole head.

A drop landing on a very hot surface floats on a layer of vapour formed beneath it, so it cannot wet the surface and skids or bounces away. This is the Leidenfrost effect, and the vapour layer also blocks heat transfer between drop and surface (Quéré, 2013). The temperature at which it starts, the Leidenfrost point, varies with the liquid's properties, surface roughness and surface contamination, and whether a drop striking a hot surface sticks, rebounds or breaks up depends on the surface temperature and the speed of impact (Bernardin & Mudawar, 1999; Liang & Mudawar, 2017). In one test under die casting conditions, water spray entered film boiling, where a vapour film covers the surface, above about 350 °C, and the Leidenfrost temperature of a diluted release agent was found to be above 350 °C (Sabau et al., 2007). While the die face sits in this range, the release agent cannot stick and acts only as coolant, so what is sprayed before the die has cooled enough to take a film flies off without sticking.

Die temperature shows only when measured. An infrared thermal camera shot of the die face just before and just after spraying shows where it runs hot and how far spraying cools it, and researchers studied release agent spraying this way alongside heat flux sensors (Sabau & Dinwiddie, 2008). Measure inlet and outlet water temperature and flow for each cooling circuit to find blocked or weak ones, and check the records for whether a die change or a cycle cut coincides with the rise in use. Film the spots where drops leap off during spraying and match them against the thermal image.

When a hot die is behind it, the key is to stop the release agent doing the cooling water's job. Clean clogged cooling channels, restore circuits short of flow, and review added die cooling at hot spots with whoever designs the dies. If a film still has to form at high temperature, ask the supplier whether an agent suited to higher die temperatures is available. Once die temperature is steady, try bringing spray time down again.

Hypothesis 6: uneven hand spraying

Where operators hold a spray gun, as in gravity or low-pressure casting and rubber and plastics moulding, the person is the spray system. Use splits by person when operators change at each shift, when many are new, and when someone who once had castings stick has taken to spraying generously. Two shifts may run the same die, yet one empties the container visibly faster. One operator stands well back and sweeps long passes, another works close and sprays in short bursts.

Film thickness is set by spray conditions such as spray pressure and the speed at which drops strike, how well the liquid adheres or is washed off, and the flow of cooling water and air (Sabau et al., 2007). Hand spraying varies distance, angle, time and the number of overlapping passes from person to person, so there are as many sets of conditions as there are operators. From farther away, more of the spray misses its target, and spraying one spot too long cools the die until liquid runs, as described earlier. Painting data put numbers on the effect of technique. Taking a conventional gun's transfer efficiency as 40%, switching to a high-volume low-pressure gun was estimated to give 49%, and adding proper spray technique 61% (EPA, n.d.-b). The same equipment, in other words, transfers very different shares depending on who uses it and how.

Start by splitting use by shift and by person. Issue concentrate or mixed liquid by weight to each shift, or log the container level at each changeover, and the difference shows as a number. If there is one, film each operator spraying for a short clip and compare distance, angle, time and order. Logging on the same sheet which shift and which spot had sticking shows where the habit of generous spraying began.

If the spread between people is large, make spraying a standard. Write a work standard for each die with the spraying order, distance and time, illustrated, and take as the basis the method of the operator who uses least without sticking, then train everyone on it. Guns can be fitted with metered output or a timer, and where volumes justify it, consider moving to automatic spraying.

Finding the cause

There is no need to dig through all six at once. Rule them out starting with what can be confirmed in numbers without stopping the line. The gap between spray count and shot count, the mixed concentration and use by shift come out of records and simple measurements alone. Collected flow per nozzle can be measured in a short stop, and die thermal imaging and cooling circuit checks come after that.

The shape of the leak is the first clue. If liquid pools under the die and the die face is wet, look at idle-cycle spraying or overlong spraying that cools the die until the film washes off. If fog fills the cell and film builds on guards and ducts, suspect air overspray or spray leaping off a hot die, and if sticking always comes at the same spot, suspect the nozzle that covers it or heat at that spot. If use splits by shift or by person, look first at hand spraying or dilution control.

When the same sign points two ways, add an observation that separates them. With heavy fog, if drops can be seen leaping off the die face during spraying and the thermal image shows that spot hot, die temperature is the likelier cause; if fog spreads before the spray even reaches the die, air pressure is. When sticking sits at one spot, look at heat if that nozzle's collected flow is normal, and at the nozzle if it is not.

If that still does not settle it, run control trials that change one thing at a time. Drop air pressure one step, replace one suspect nozzle with a new one, switch off idle-cycle spraying, or change to a mix set to the target concentration. Change only one thing at a time, and compare before and after on the same basis: concentrate use per good shot and the number of sticking cases. The job is done only when use falls and sticking does not rise.

The hypotheses overlap easily. When a hot die will not take a film, air and spray time get turned up; the extra air brings overspray, and the extra time over-cools other parts of the die until the film washes off. A single clogged nozzle can also raise spraying for the whole head. In such cases, first put right the conditions under which a film forms, such as die temperature and nozzle condition, and then bring spray time and air pressure down. Cutting spray while those conditions are unsettled raises sticking and spraying climbs again, round and round.

Limits and cautions

Dilution, spray time, air pressure and a suitable die temperature differ by release agent, alloy, die and equipment, so numeric decisions follow the product's TDS and the equipment supplier's guidance. While cutting back spraying, watch casting quality, including sticking, soldering and cold shuts, and go back to the earlier setting if quality wavers. Changing the die cooling design or moving to a different release agent is a decision for the die designer and the supplier together.

Safety matters too. For release agent concentrate and the mixed liquid, follow the product's safety data sheet, the SDS, for protective equipment and ventilation. Foundry guidance on spray coating advises spraying smaller castings under extraction, using spray equipment that makes as little mist as possible, and keeping people without protective equipment out until spraying has ended and the mist has cleared (HSE, 2022). Pooled liquid on the floor causes slips, so clean it up at once, and treat wastewater in line with local rules. Inspect or clean nozzles only after the equipment is fully stopped and locked out, and take care against burns near a hot die.

Sources

  1. Barber, J. (n.d.). How to pre-empt a significant profit drain: Nozzle wear. Causes, detection and corrective action strategies (White paper WP106). Spraying Systems Co. Retrieved November 2026. https://www.spray.com/-/media/dam/industrial/usa/sales-material/white-paper/wp106_preempt_nozzle_wear.pdf
  2. Bernardin, J. D., & Mudawar, I. (1999). The Leidenfrost point: Experimental study and assessment of existing models. Journal of Heat Transfer, 121(4), 894–903. https://doi.org/10.1115/1.2826080
  3. Cross, M. (2023, October 23). Optimizing fluids and equipment for consistent die casting performance. EUROGUSS 365. https://www.euroguss.de/en/euroguss-365/2023/expert-knowledge/optimizing-fluids-and-equipment-for-consistent-die-casting-performance
  4. Health and Safety Executive [HSE]. (2022). FD12: Spray coating a large casting (open workshop). COSHH essentials for foundries. https://www.hse.gov.uk/pubns/guidance/fd12.pdf
  5. Lefebvre, A. H., & McDonell, V. G. (2017). Atomization and sprays (2nd ed.). CRC Press. https://doi.org/10.1201/9781315120911
  6. Liang, G., & Mudawar, I. (2017). Review of drop impact on heated walls. International Journal of Heat and Mass Transfer, 106, 103–126. https://doi.org/10.1016/j.ijheatmasstransfer.2016.10.031
  7. Mendez, P. F., & Powell, A. C. (2008). Influence of heat transfer on the application of solid lubricant on hot dies. Scripta Materialia, 59(7), 784–787. https://doi.org/10.1016/j.scriptamat.2008.06.014
  8. Quéré, D. (2013). Leidenfrost dynamics. Annual Review of Fluid Mechanics, 45, 197–215. https://doi.org/10.1146/annurev-fluid-011212-140709
  9. Sabau, A. S., & Dinwiddie, R. B. (2008). Characterization of spray lubricants for the high pressure die casting processes. Journal of Materials Processing Technology, 195(1–3), 267–274. https://doi.org/10.1016/j.jmatprotec.2007.05.021
  10. Sabau, A. S., Hatfield, E. C., Dinwiddie, R. B., Kuwana, K., Viti, V., Hassan, M. I., & Saito, K. (2007). Assessment of computer simulation software and process data for high pressure die casting of magnesium (ORNL/TM-2007/41). Oak Ridge National Laboratory. https://info.ornl.gov/sites/publications/files/Pub8532.pdf
  11. U.S. Environmental Protection Agency [EPA]. (n.d.-a). Automotive refinishing industry isocyanate profile, Chapter 6: Control technology. Design for the Environment. Retrieved November 2026. https://www.epa.gov/sites/default/files/2015-06/documents/isocyanate_profile_chapter_6.pdf
  12. U.S. Environmental Protection Agency [EPA]. (n.d.-b). HVLP spray guns in the auto refinishing shop: A success story. Design for the Environment. Retrieved November 2026. https://19january2021snapshot.epa.gov/sites/static/files/2014-01/documents/auto_refinishing_hvlp_success_story.pdf

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.