Cleaning again with stronger chemicals is the usual response when a cleaning fails, but if the cleaning does not match what is on the membrane, stronger chemicals bring nothing back and tend only to damage the membrane. What actually makes cleaning fall short can be a cleaning agent that does not suit the foulant, cleaning conditions short on temperature, pH, time or flow, cleaning that comes too late, fouling that ordinary cleaning barely removes, or acid and alkali cleanings in the wrong order, and often two or more at once.
Background
An RO unit is stopped for half a day, chemicals are circulated and it is restarted, yet normalised permeate flow comes back only about halfway and differential pressure barely moves. A few weeks later the same symptom calls for another cleaning, and the interval between cleanings keeps shrinking. Each cleaning costs chemicals, lost production and spent solution disposal, and if performance never returns, membrane replacement follows.
Cleaning works only when two things are right together. The cleaning agent must react chemically with what makes up the fouling layer and break its bonds, and mass transfer must be enough for the agent to get into the layer and for loosened foulant to leave it into the flow (Elimelech, 2005). If the chemistry does not fit, longer time or higher flow does little, and even with the right chemistry, too little heat or time leaves the reaction unfinished. Whether a cleaning worked is judged by whether normalised operating values have returned to their values at start-up (Hydranautics, 2017).
Fouling on a working membrane is seldom only one of mineral scale, organic matter, colloids or biofilm; it is usually a mixture (Jiang et al., 2017). So depending on what has built up, and which chemicals were used, in what order and how thoroughly, the same chemical works in one unit and fails in another.
In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: take the chemicals, order, temperature, pH, time and flow from the cleaning log, set them beside normalised permeate flow, salt passage and stage differential pressure before and after each cleaning, and gather the evidence of what the foulant actually is.
Hypothesis 1: wrong cleaning agent
The typical case is a unit that has used one cleaning agent ever since it was installed while the raw water changed. The same applies when a new source is blended in, the pretreatment coagulant is changed, organic matter in the raw water rises with the season, or one general-purpose cleaner is expected to handle every cleaning. Imagine a plant that used hard groundwater and has started blending in treated wastewater for reuse. Cleaning is still a single acid cleaning as before, and the face of the first-stage elements is coated in slippery slime.
Each foulant yields to different chemistry. Acid dissolves calcium carbonate and metal oxides such as iron, while organic matter and biofilm come off with high-pH cleaning plus detergent or chelating agent. EDTA, a chelating agent that binds metals, is used to lift colloids, organics, biological matter and sulfate scale (Hydranautics, 2017). The difference showed clearly in fouling layers where calcium bridges organic molecules into a tightly linked layer. In one study, cleaning such a layer with EDTA or an anionic surfactant brought permeate flow back well, while sodium hydroxide alone at pH 11 under the same conditions brought it back poorly and left substantial adhesion between foulants (Elimelech, 2005).
Before choosing a cleaner, find out what has built up. Open the feed end of a pressure vessel and look at the face of the first element: a slimy or gel-like layer points to biological or organic matter, reddish-brown to iron. Analysing the first spent cleaning solution for metals and organic carbon against a fresh batch gives an estimate of what dissolved. The feed water analysis, the filter pads from fouling index tests and the deposits left on cartridge filters are clues of the same kind (DuPont, 2021).
Match the cleaner to the foulant type that turns up: for calcium-bridged organics, an alkaline cleaning with chelating agent or surfactant; for iron and calcium carbonate, an acid cleaning; for mixed fouling, both in sequence. If the picture is unclear, pull one element and trial-clean it with several cleaners; specialist firms offer this testing (Hydranautics, 2017). Running the unit briefly after each cleaning step and logging the values leaves evidence of which chemical worked for the next cleaning.
Hypothesis 2: conditions too mild
Here the cleaner is right but the conditions are weak. A cleaning tank left in an unheated spot in winter, solution made with cold water and no heater, pH set once and never measured again, recirculation cut short to meet a production schedule, and a small cleaning pump driving every stage at once all lead to this hypothesis. Look at a cleaning tank in the corner of a pump room in winter: the solution, made straight from mains water, is cold to the hand, and its pH was measured only once, right after mixing. After an hour of recirculation the solution is cloudier than at the start.
Temperature is among the conditions that matter most. Raising the same EDTA solution from 20 to 40 °C sharply increased cleaning efficiency, explained by faster diffusion of the agent into the fouling layer together with faster reaction. Where the chemical reaction was unfavourable, on the other hand, longer cleaning did not raise efficiency much, and higher flow helped only when the agent reacted well with the foulant (Elimelech, 2005). pH moves during cleaning too. Dissolving foulant pulls the solution's pH, so manufacturers' guidance is to readjust it if it shifts by more than 0.5 units and to make up fresh solution when it turns cloudy or discoloured (Hydranautics, 2017; DuPont, 2021).
Pushing conditions harder has its limits. Cleaning efficiency is set jointly by the type and concentration of cleaner, pH, temperature, time and flow (Al-Amoudi & Lovitt, 2007), and the pH range a membrane tolerates narrows as temperature rises. Cleaning at extremes of pH and temperature may work better but can shorten membrane life through hydrolysis, so the manufacturer also limits exposure time at those limits (Hydranautics, 2017). In tests cleaning nanofiltration membranes with caustic soda, some membranes showed widened pores and higher salt passage (Simon et al., 2013).
If the cleaning log has no numbers, start recording them at the next cleaning. Measure solution temperature and pH at the start and end of each step, and note cleaning flow per stage, recirculation time and soak time. If temperature fell short, fit a heater to the cleaning tank and warm the solution to a target within the manufacturer's range, and clean one stage at a time so each gets a suitable flow. Alternate soaking and recirculation, readjust pH midway, and judge the effect by whether recovery improves when the same cleaning is repeated with only the conditions changed.
Hypothesis 3: cleaning too late
This hypothesis often applies to units cleaned only at scheduled shutdowns, units whose operating data are not normalised, and units left alone until output falls short. An example is a unit where high-pressure pump pressure has been raised bit by bit to hold output. For months the operating screen showed permeate flow on target, and cleaning was booked only when the pump had no more pressure to give.
Fouling usually progresses, and unless caught early it can impair performance badly within a short time (Hydranautics, 2017). One manufacturer advises cleaning when normalised permeate flow drops 10%, normalised salt passage rises 5 to 10%, or normalised differential pressure rises 10 to 15%. The same manual notes that waiting longer may mean cleaning no longer restores performance, and that membranes then foul faster so the time between cleanings shortens (DuPont, 2021). For biofilm, the difference has been seen in images. A study following cleaning by magnetic resonance imaging found that cleaning an early-stage biofilm removed more biomass than cleaning a biofilm that had grown longer (Creber et al., 2010).
While pressure is raised to hold permeate flow, the deposit keeps thickening. In spiral-wound elements, biofilm grows on the feed spacer, narrowing the feed channel and raising differential pressure (Vrouwenvelder et al., 2009), and biofilm that is not fully removed regrows quickly from what remains (DuPont, 2021). That is why a late cleaning that removes only part of the deposit shortens the time to the next cleaning.
Trace back on the normalised trend when the cleaning trigger was crossed. If cleaning came well after the trigger, and each cleaning recovers to a slightly lower level with the gaps getting shorter in a staircase pattern, this hypothesis is likely. If only measured permeate flow was being watched, normalise it using the pump pressure and temperature records to expose the hidden decline (ASTM International, 2019).
If late cleaning is the cause, the first measure is to turn the trigger into an alarm. Build normalisation into the control system so it signals when a cleaning trigger is crossed, and recover output by cleaning rather than by pushing pressure higher. A deposit that is already thick will not come off in one go, so consider repeating the right cleaning two or three times under proper conditions, or pulling the elements for cleaning outside the unit.
Hypothesis 4: hard-to-remove fouling
When no cleaning brings much recovery, suspect that the deposit itself does not dissolve under ordinary cleaning. That happens with silica-rich groundwater treated at high recovery, with barium or strontium in the raw water, with oil getting into the feed, and with overdosed cationic polymer coagulant in pretreatment. Picture a unit on silica-rich groundwater whose last-stage permeate flow falls little by little. Acid and alkaline cleanings in turn leave the operating values much as before, and the last element, once pulled, feels heavy in the hands.
The reason these foulants resist lies in their make-up. Barium and strontium sulfate scales are particularly hard to dissolve, silica scale is very difficult to remove by traditional chemical cleaning, and fouling by polyelectrolytes from pretreatment is often hard to clear as well (Hydranautics, 2017). Concentrated silica polymerises or binds with metal hydroxides into a hard layer on the membrane, so the response leans on preventing it by controlling recovery and pH rather than on cleaning (Milne et al., 2014). Organics adsorbed on the membrane surface, such as oil, are also very hard to remove, and some, such as heating oil, cannot be cleaned off (DuPont, 2021).
What has built up becomes certain only once an element is opened. Pull the last element, compare its weight with a new one, and send it for autopsy to analyse the crystal form and elemental make-up of the deposit. Check how much silica or barium came out in the spent cleaning solution, and from the feed analysis and recovery, calculate how far silica and barium sulfate exceed their solubility in the concentrate. If oil or coagulant is suspected, check the feed for oil and review the coagulant dosing record.
For such fouling, agree a dedicated cleaning with the membrane manufacturer or a specialist cleaning firm, and replace elements that still do not recover. More important is keeping it from forming again. If silica or sulfate is the cause, reset recovery and antiscalant; if oil, add oil separation to pretreatment; if coagulant, hold the dose to the minimum and adjust it as the feed changes.
Hypothesis 5: acid and alkali order
Look at this hypothesis where acid cleaning always comes first by habit, where scale removal is the first thought even with biofilm or organic fouling present, and where rinsing between cleaning steps has been cut back. Say a unit with rising differential pressure in its first stage is cleaned with acid first, as usual. Differential pressure climbs further while the acid circulates, and even after the alkaline cleaning that follows, the unit ends up worse than before.
Order matters because acid dissolves some foulants but makes others set harder. One manufacturer strongly recommends alkaline cleaning as the first step and acid first only when the membrane is known to carry calcium carbonate or iron oxide alone. When acid cleaners react with silica, organics such as humic acids, or biofilm, performance can decline further; an alkaline cleaning afterwards sometimes restores it, but often an extreme cleaning outside the guidelines becomes necessary (DuPont, 2021). Another manufacturer likewise says membranes fouled with oil or biological matter should not be cleaned at low pH first because that matter congeals, and notes that the wrong choice of chemical or order of introduction can make fouling worse (Hydranautics, 2017).
Check the order and the rinses between steps in the cleaning log. Where the unit was run briefly and logged after each step, the most direct evidence is whether differential pressure or permeate flow got worse after the acid step. Without such records, confirm in reverse whether organics or biofilm were present, from a slimy layer on the face of the first element or from organic carbon in the spent cleaning solution.
The fix is in the order: rewrite the cleaning procedure as alkali first, acid second. Taking one manufacturer's sequence as an example: rinse with permeate, clean at high pH, rinse with permeate until the pH on the concentrate side falls below 8.5, clean at low pH, then rinse again (Hydranautics, 2017). Use acid first only when the deposit is clearly calcium carbonate or iron alone. For fouling already set by acid, repeat the alkaline cleaning under proper conditions, and if some remains, consult the membrane manufacturer rather than attempting cleaning outside the guidelines alone.
Finding the cause
The easiest evidence is records that already exist. The cleaning log's chemicals, order, temperature, pH and time, together with normalised trends, show without stopping the unit whether conditions fell short, how long after the trigger cleaning came, and whether acid went first. Identifying the foulant comes next, and pulling an element for autopsy comes last.
Which value fails to return points the way. If differential pressure stays high after cleaning, something such as biofilm or particles is still lodged in the feed channels, so look at the choice of cleaner, whether conditions were sufficient and whether alkali went first. If differential pressure recovered but permeate flow alone falls short, suspect a thin adsorbed layer of organics or a hard-to-reverse layer such as silica. If salt passage actually rose after cleaning, examine membrane damage separately from fouling.
Location is a clue too. Poor recovery in the first stage points first to biological matter, organics, colloids and iron; poor recovery in the last stage, to scale and silica. If only un-normalised permeate flow was watched, suspect late cleaning first and check whether each cleaning recovers to a lower step than the last.
If records do not settle it, run comparison trials. Run the unit briefly after each cleaning step to measure which step brought recovery, repeat the same cleaning with only the conditions changed, and trial-clean one pulled element with different cleaners. The final check is an autopsy of one lead and one tail element; once it shows what remains on the membrane, it is clear whether to change the cleaning, change pretreatment and recovery, or replace elements.
The hypotheses often overlap. Using the wrong cleaner in cold solution on a layer thickened by late cleaning cuts recovery further, and organics set by acid first can look like hard-to-remove fouling. So first carry out one proper cleaning: a cleaner matched to the foulant, alkali first, at sufficient temperature and time within the manufacturer's range. What remains after that is fouling that ordinary cleaning cannot remove, or membrane damage, and that is when to decide on autopsy and replacement.
Limits and cautions
Cleaning pH and temperature limits, soak times, cleaning triggers and permissible cleaners differ by membrane and element type, so numbers follow the membrane manufacturer's data, and only proprietary cleaners confirmed for that membrane are used. Extreme cleaning outside the guidelines, cleaning of special foulants such as silica or barium sulfate, and autopsies are arranged with the membrane manufacturer or a specialist firm. Polyamide membranes are damaged by chlorine, so never use water with residual chlorine in the cleaning tank or for rinsing.
Safety matters too. For cleaning acids and alkalis, chelating agents, surfactants and non-oxidising biocides, follow each product's safety data sheet, the SDS, for protective equipment and ventilation; add chemicals to water gradually to dissolve them, and never mix different chemicals in one tank. Heated solutions and pipework can burn, so confirm that hoses and piping can take the temperature, pressure and pH. Neutralise spent cleaning solution and dispose of it in line with local discharge limits.
Sources
- Al-Amoudi, A., & Lovitt, R. W. (2007). Fouling strategies and the cleaning system of NF membranes and factors affecting cleaning efficiency. Journal of Membrane Science, 303(1–2), 4–28. https://doi.org/10.1016/j.memsci.2007.06.002
- ASTM International. (2019). ASTM D4516-19a, Standard practice for standardizing reverse osmosis performance data. https://store.astm.org/d4516-19a.html
- Creber, S. A., Vrouwenvelder, J. S., van Loosdrecht, M. C. M., & Johns, M. L. (2010). Chemical cleaning of biofouling in reverse osmosis membranes evaluated using magnetic resonance imaging. Journal of Membrane Science, 362(1–2), 202–210. https://doi.org/10.1016/j.memsci.2010.06.052
- DuPont Water Solutions. (2021). FilmTec reverse osmosis membranes technical manual (Form No. 45-D01504-en, Rev. 8).
- Elimelech, M. (2005). Chemical cleaning of organic-fouled reverse osmosis membranes (Desalination and Water Purification Research and Development Program Report No. 109). U.S. Department of the Interior, Bureau of Reclamation. https://www.usbr.gov/research/dwpr/reportpdfs/report109.pdf
- Hydranautics. (2017). Foulants and cleaning procedures for composite polyamide RO membrane elements (Technical Service Bulletin TSB107.25). https://membranes.com/tsb107
- Jiang, S., Li, Y., & Ladewig, B. P. (2017). A review of reverse osmosis membrane fouling and control strategies. Science of the Total Environment, 595, 567–583. https://doi.org/10.1016/j.scitotenv.2017.03.235
- Milne, N. A., O'Reilly, T., Sanciolo, P., Ostarcevic, E., Beighton, M., Taylor, K., Mullett, M., Tarquin, A. J., & Gray, S. R. (2014). Chemistry of silica scale mitigation for RO desalination with particular reference to remote operations. Water Research, 65, 107–133. https://doi.org/10.1016/j.watres.2014.07.010
- Simon, A., McDonald, J. A., Khan, S. J., Price, W. E., & Nghiem, L. D. (2013). Effects of caustic cleaning on pore size of nanofiltration membranes and their rejection of trace organic chemicals. Journal of Membrane Science, 447, 153–162. https://doi.org/10.1016/j.memsci.2013.07.013
- Vrouwenvelder, J. S., Graf von der Schulenburg, D. A., Kruithof, J. C., Johns, M. L., & van Loosdrecht, M. C. M. (2009). Biofouling of spiral-wound nanofiltration and reverse osmosis membranes: A feed spacer problem. Water Research, 43(3), 583–594. https://doi.org/10.1016/j.watres.2008.11.019