KALTECKOREA

BlogApplication notes

Why do parts stored outdoors rust first where rain hits?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Corrosion Prevention

Re-coating with the same preventive or throwing a cover over the stack is the usual response to rust on parts stored outdoors, but unless the type of film and the time water stays on the metal change, rain, sun, dew and salt still have a way past the film. What actually lies behind the rust can be a thin film washed by rain, a film damaged by sun and heat, dew under the cover, spots where water collects, salt in the air or protection that runs out before storage ends, and sometimes two or more at once.

Background

Parts stacked in the yard because the warehouse is full are uncovered after a few weeks, and red rust has spread over the top faces and along the streaks where rain ran down. The undersides of the same parts, and the side the cover protected well, are still clean. Stripping rust and re-protecting becomes routine work, rust on machined or fitting faces spoils dimensions and finish until parts are scrapped, and shipments slip.

Atmospheric corrosion of steel proceeds while the surface is wet, and how much happens depends heavily on how long the surface stays wet. It is also well established that repeated wetting and drying drives corrosion (Alcántara et al., 2017). Rust therefore starts where water lands most often and stays longest. A rust preventive's job is to keep that water and air off the metal, and where the film thins, is damaged, or is outlasted by the water, that is where it gives way first.

Outdoor storage is a very different setting from indoors. Parts take rain and sun directly, dew forms as temperatures swing between day and night, and near the coast the air carries salt. A preventive and packaging chosen with an indoor store or shelf in mind may never have been tested to hold up under these conditions.

In such cases the technical team sets up the six hypotheses below and rules them out one by one. The start is always the same: check the preventive's technical data sheet, the TDS, for whether it is meant for outdoor storage and for how long it protects, then record the storage period, how the stack is covered and supported, the distance from the sea and the weather over that time, and match these against where the rust appeared.

Hypothesis 1: rain-washed film

Look at this hypothesis first when parts coated with a thin oil made for indoor use are put outside uncovered, when yard storage stretches through a rainy season, and when parts have broad upward faces and edges where rain runs down. Behind the plant, a pallet of sheet steel brackets coated with a thin oil sits in the yard. After the rainy season, rust has bloomed on the top faces of the uppermost brackets and along the streaks running down from their edges, while the brackets below, shielded from rain by the parts above, are almost unchanged.

Preventives are designed with different film types and thicknesses for different uses. The specification for solvent-cutback preventives separates a hard film for metals exposed outdoors for long periods from soft films for long indoor protection or only limited outdoor use, and tests the hard-film grade at a film thickness of about 100 μm against half that or less for the soft-film grades (DoD, 1993). Leaving an indoor soft film or thin oil for long where rain lands and runs therefore uses that film outside the range it was designed for. Where the film has weakened, rain leaves the surface wet for longer, and in a cyclic corrosion test that included rainfall, steel corroded at very high rates right after rain (Katayama et al., 2021).

Start with where the rust is. Rust on top faces, at edges where rain drips and along run-down streaks, with the less-rained faces clean, fits this hypothesis. On the same part, rub a finger or blotting paper over a rust-free area and over the edge of a rusting area to compare how much film is left, and if film thickness can be measured, compare the two readings. Check too whether the TDS describes the preventive as for indoor or short-term use.

If washed-off film is the cause, switch to a water-resistant preventive such as an outdoor hard film or wax type, apply it evenly at the thickness the TDS recommends, and give edges and corners where rain runs a second pass. Where a cover can be used, keep rain off the parts directly, but manage the moisture under the cover as well, as the hypothesis on dew shows. Before re-coating, deal with the remaining film and any rust first.

Hypothesis 2: sun and heat damage

The question of whether the film can stand sun and heat arises wherever metal temperatures climb high: a yard in full summer sun, south-facing faces, the space under a black cover. Steel pipe protected in spring and left in the yard all summer is a case in point. By autumn the film on the upper half that faced the sun has lost its sheen or left run marks, and the rust is concentrated there, while the film on the shaded lower half is still tacky.

There are two ways sun and heat damage a film. One is flow. Soft films are specified for limited outdoor use only where metal temperatures do not rise high enough to make the film flow, while the hard-film grade must have a flow point of at least 80 °C and is the only grade put through accelerated weathering (DoD, 1993). The other is ultraviolet light and oxidation. In NASA tests comparing many corrosion preventive compounds, one week of ultraviolet exposure alone degraded the films of many products heavily, so their protection had collapsed before any salt fog was applied. The same report notes that petroleum oils oxidise slowly over time (Calle et al., 2012). Once a degraded film cracks or peels, rain and dew reach the metal through the gaps.

The first check is to compare the sunny and shaded faces side by side. If the film on the sunny side shows run marks, a dull hardened surface, fine cracks or peeling, and the rust is concentrated there, this hypothesis gains weight. Measure the metal surface temperature on a clear afternoon with a contact thermometer and compare it with the service temperature or flow point in the TDS, or put one coated coupon in the sun and one in the shade and compare them after a few weeks.

Where only the sun-facing film has suffered, switch to an outdoor hard film with a high flow point that has passed weathering tests. Shade the stack with a light-coloured or reflective cover that still lets air through, and move it into shade or under a roof where possible. For storage that runs through summer, schedule a mid-term check of the film and re-coat only the damaged faces.

Hypothesis 3: dew under the cover

This hypothesis comes to mind when a waterproof cover is pulled down to the ground to keep rain out, in spring and autumn when clear nights alternate with warm days, and on earth floors where ground moisture rises under the cover. Take the day a heap of machine parts was wrapped tightly in plastic sheeting against autumn rain, its edges weighed down with stones. Two weeks later, droplets cling to the inside of the cover, and the top faces that touched it are spotted with drop-shaped rust, though not a drop of rain got in.

Rust under a cover comes from temperature changes, not rain. Guidance on open storage explains that the fairly rapid temperature changes such material goes through make moisture condense on it, and that moisture not carried off by adequate ventilation will damage the stores (DLA, 1994). At night the metal and cover cool, and once the surface falls below the dew point of the air, water condenses; under a cover with no airflow it barely dries even by day, so the surface stays wet for longer. The standard for judging condensation risk before painting treats the probability as low only when the steel surface is at least 3 °C above the dew point (ISO, 2017b). In transit or storage, moisture carrying salt can also be trapped under a cover and cause corrosion (AGA, 2014).

Before lifting the cover, look for droplets on its inner face and for spot-like rust where the cover touched or where water could have dripped. Measuring air temperature, relative humidity and metal surface temperature around sunrise and working out the gap to the dew point shows how often condensation is likely, and a small temperature and humidity logger left under the cover keeps several days of records. Check as well whether the cover reaches the ground and whether there is a vent at the top.

Once condensation under the cover is confirmed, change the cover so it keeps rain off but lets air through. The guidance recommends, where possible, a gap of 12 to 18 inches, about 30 to 45 cm, between the bottom of the cover and the ground, bringing the cover down only to the top of the dunnage, and an opening in the upper part of the stack cover arranged so that rain and snow cannot get in (DLA, 1994). Keep the cover from touching the metal directly, and raise the supports so ground moisture does not rise into the stack. Even under a cover, use a preventive that can withstand condensation.

Hypothesis 4: water traps

Water lands and stays put in channels left open-side up, upward flanges and dished faces, stacked plates and pipes, and parts set straight on the ground or on wet timber supports. A walk round the yard the morning after rain brings this hypothesis into view. Everything else has dried, yet rainwater stands in the bottoms of channel sections lying with the groove up, the gaps between stacked plates are still wet, and the rust is heaviest in exactly those places.

Spots where water collects stay wet long after their surroundings have dried, and since time of wetness governs corrosion, rust grows fastest there. The design standard for steel structures recommends avoiding troughs, ledges and hollows that hold water and deposits, providing drainage holes where needed, and allowing free circulation of air; narrow gaps between overlapping surfaces draw water in by capillary action and hold it (ISO, 2017a). Moisture rising from the ground and rain splashing up add water by the same route. That is why the guidance on open storage sets the height of supports according to the ground surface (DLA, 1994).

A few hours after rain, walk the yard marking every place where water still stands, and see whether those places match where the rust is heaviest. Record which way parts are stacked, how high the supports are and what they are made of, and whether the ground beneath drains well. Lift a few of the stacked plates or pipes and check whether the faces between them are rustier than the outer faces.

When standing water and heavy rust coincide, start by changing how parts are stacked. Lay channels and dished parts open side down or sideways, tilt plates and pipes slightly so water runs off one way, and put spacers between overlapping faces so air can pass. Following the guidance, raise supports at least 3.5 inches, about 9 cm, on well-drained paved ground and 8 inches, about 20 cm, on gravel, and on poorly drained ground keep them 10 inches, about 25 cm, above the highest possible water level (DLA, 1994). Use dry timber for the supports.

Hypothesis 5: salt in the air

Close to the sea, in coastal plants, port yards or hilltop sites in the sea wind, the air brings salt even without rain. Roadside yards where de-icing salt is spread in winter are similar. Sometimes a protection method that served an inland plant for years is carried over unchanged to a new plant by the coast. With the same preventive and the same storage, rust appears within weeks, and it is looser than the rust seen inland, flaking off easily.

In marine atmospheres, salinity and steel corrosion fall off exponentially with distance from the sea. The same study found that high salinity produced coarser, less protective rust (Alcántara et al., 2015). Sea salt draws in moisture and wets the surface even at low humidity. Under sodium chloride, iron starts to corrode at around 70% relative humidity, and the magnesium chloride in sea salt forms a water film at a far lower 35%. The same review notes that rain also rinses contaminants off surfaces, so chloride builds up more on faces that see less rain (Alcántara et al., 2017). On the coast, then, rust can appear under eaves and on undersides as well as on rain-washed faces.

First record the distance from the sea, the prevailing wind and whether de-icing salt is used in winter. Salt can be measured as a deposition rate over a set period by the wet candle method in the standard for measuring atmospheric corrosivity parameters (ISO, 2012b). A simpler check is to wash a rusted face and a clean face with purified water and compare the chloride in the two rinses. The corrosivity category of an atmosphere is set from the first-year corrosion of standard metal specimens or from environmental data such as temperature, humidity, sulphur dioxide and chloride deposition (ISO, 2012a). If rust has formed evenly on less-rained faces as well as on rain-washed ones, lean towards salt.

When salt deposition reads high, choose the preventive and storage method again to suit that corrosivity category. Avoid spots open to the sea, give priority to roofed storage that blocks the sea wind, and before protecting, wash salt off the surface with clean water and dry it completely. For coastal storage, pick an outdoor preventive with salt spray test results and inspect more often than inland.

Hypothesis 6: protection too short

This hypothesis applies when parts meant to stay a few weeks are still in the yard months later because of a changed delivery date or a delayed installation, when a preventive chosen for short-term shipping is left to cover long storage, and when there is no schedule for inspection and re-coating during storage. Consider a pile of structural members whose site installation has been put back. For the first few weeks they are clean; after a few months rust spots start to appear one by one on the rain-facing surfaces, and before long rust has spread across those faces.

A preventive's protection period is set by film type, thickness and environment, and it has an end. The specification tests the grades differently: the hard film goes through salt spray and accelerated weathering, while the soft films go through humidity and shed storage tests under a roof (DoD, 1993). In other words, a soft film's results say nothing about its life in storage exposed to rain and sun. In real beachside exposure, too, the degree of protection varied widely between products, and the ranking differed between steel, stainless steel and aluminium alloys (Calle et al., 2012). As the film slowly thins and ages, the faces taking the most rain and sun reach the limit first, so rust at the end of the protection life also starts there.

Write down side by side the date of protection, the storage period first planned and the actual storage period, and check the protection period in the TDS and whether the conditions behind it were indoor or outdoor. If rust appeared around the time actual storage passed the TDS protection period, this hypothesis fits. Coupons protected on the same day by the same method and kept beside the stack, taken out at set intervals, give a direct measure of how long the film lasts on site.

If protection life is the problem, write it into the storage plan. When storage looks set to run long, switch to a long-term outdoor preventive, and give the supplier the storage period and environment so a suitable product can be chosen. Material stored in the open needs closer attention than material indoors (DLA, 1994), so set an inspection interval and re-coat thinning or damaged faces before rust appears.

Finding the cause

There is no need to investigate all six hypotheses separately. Rule them out starting with what records and one walk round the yard can confirm. The TDS's intended use and protection period, the protection date and the storage period are on file, and stacking direction, supports, cover arrangement and distance from the sea can be seen. Surface temperature, dew point and salt measurements take days to weeks, so they come next.

Where the rust sits is the best clue. Rust gathered on top faces and run-down streaks points to washed-off film; rust on the sunny side, with film that has run or hardened, points to sun and heat. Droplets inside the cover and spot rust where it touched suggest dew, and heavy rust where water stands after rain or between overlapping faces suggests water traps. Rust spread evenly onto less-rained undersides and under eaves leans towards salt, and rust that held off for the first months and came only after storage ran past plan leans towards protection life.

If that still does not settle it, run control trials with coupons. Protect pieces of the same steel sheet on the same day, then place one where rain falls, one under a roof, one under a ventilated cover and one under an unventilated cover, and add a pair coated with an outdoor preventive. Only one condition should differ at a time, or there is no telling what made the rust worse.

The final check is real storage. Carry the revised preventive and storage method through the next storage period, recording the same spots with photographs at set intervals. The job is done only when no rust returns, after rain and right up to the end of the planned storage period.

The hypotheses often overlap. Film damaged by sun is washed off more easily by rain, coastal salt lowers the humidity at which a water film forms, and where water collects the film's life ends sooner. In such cases, first fix what shortens the time water stays on the metal, the cover and ventilation, the stacking direction and the supports, then revisit the film type and protection period. While long wet periods remain, no preventive can be compared fairly with another.

Limits and cautions

Film thickness, protection period, service temperature and re-coating interval differ by product and by the corrosivity category of the site, so figures follow the product's TDS and supplier data. For long storage near the sea or in heavily polluted areas, and for precision-machined or safety-related parts, do not settle the method on floor judgement alone; measure the environment and decide with a corrosion specialist or the supplier. Whether deeply rusted parts can still be used follows the quality engineer and the customer specification.

Safety matters too. For solvent-cutback preventives, follow the product's safety data sheet, the SDS: keep away from ignition sources and use protective equipment and ventilation, and follow the SDS for rust removers as well. When lifting covers and restacking members, watch for collapse and use lifting equipment, and do not stand on rain-wet covers or timber supports, which are slippery.

Sources

  1. Alcántara, J., Chico, B., Díaz, I., de la Fuente, D., & Morcillo, M. (2015). Airborne chloride deposit and its effect on marine atmospheric corrosion of mild steel. Corrosion Science, 97, 74–88. https://doi.org/10.1016/j.corsci.2015.04.015
  2. Alcántara, J., de la Fuente, D., Chico, B., Simancas, J., Díaz, I., & Morcillo, M. (2017). Marine atmospheric corrosion of carbon steel: A review. Materials, 10(4), 406. https://doi.org/10.3390/ma10040406
  3. American Galvanizers Association [AGA]. (2014). A guide to minimizing and treating wet storage stain on hot-dip galvanized steel. https://galvanizeit.org/uploads/publications/Wet_Storage_Stain_On_Galvanized_Steel.pdf
  4. Calle, L. M., Montgomery, E., Kolody, M., Curran, J., Back, T., & Balles, A. (2012). Environmentally friendly corrosion preventative compounds: Final report. NASA Kennedy Space Center. https://ntrs.nasa.gov/citations/20160009024
  5. Defense Logistics Agency [DLA]. (1994). Joint service manual for storage and materials handling. DLAM 4145.12, TM 38-400, NAVSUP PUB 572, AFMAN 23-210, MCO 4450.14.
  6. Department of Defense [DoD]. (1993). MIL-PRF-16173E, Corrosion preventive compound, solvent cutback, cold-application. U.S. Department of Defense.
  7. International Organization for Standardization [ISO]. (2012a). ISO 9223:2012, Corrosion of metals and alloys — Corrosivity of atmospheres — Classification, determination and estimation. ISO.
  8. International Organization for Standardization [ISO]. (2012b). ISO 9225:2012, Corrosion of metals and alloys — Corrosivity of atmospheres — Measurement of environmental parameters affecting corrosivity of atmospheres. ISO.
  9. International Organization for Standardization [ISO]. (2017a). ISO 12944-3:2017, Paints and varnishes — Corrosion protection of steel structures by protective paint systems — Part 3: Design considerations. ISO.
  10. International Organization for Standardization [ISO]. (2017b). ISO 8502-4:2017, Preparation of steel substrates before application of paints and related products — Tests for the assessment of surface cleanliness — Part 4: Guidance on the estimation of the probability of condensation prior to paint application. ISO.
  11. Katayama, H., Kiyoizumi, K., Shitanda, I., Itagaki, M., Tsutsumi, Y., & Murase, Y. (2021). Influence of rainfall on atmospheric corrosion behavior of carbon steel. Tetsu-to-Hagane, 107(12), 1004–1010. https://doi.org/10.2355/tetsutohagane.TETSU-2021-063

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.