BlogApplication notes
Why does mould grow on silicone joints in food plants and clean rooms?
- Type
- Application notes
- Published
- 23 November 2026
- Prepared by
- Jonghwan Moon
- Product group
- Sealants & Damping
Wiping mouldy silicone joints white with chlorine bleach is the usual response, but if the mould has grown into the joint, or the water, food and shelter it needs are still there, the stains tend to come back. What actually lies behind them can be spent fungicide, water standing in the joint, soil that feeds the mould, gaps and defects in the joint, or cleaning agents that do not suit the sealant, and several can act together.
Background
In a food plant washroom, black spots appear one by one on the silicone joint where wall meets floor, or on the joints between clean room panels, then spread along the line. Chlorine bleach fades them for a while, but before long they are back in the same place. In a food plant, mould can lead to product contamination and findings at hygiene inspections, and in a clean room it breaks the requirement that exposed surfaces be smooth, impervious and unbroken (Health Canada, 2023). Sealant colonised by mould discolours and loses tensile strength and adhesion, and can lose its ability to keep water out (Ahn et al., 2024).
Mould needs water, food and somewhere to settle and hold on. Almost any indoor material that meets excess moisture can grow mould and bacteria (WHO, 2009). With synthetic polymer materials, what fungi attack is held to be not the polymer itself so much as ingredients mixed into it, such as plasticisers, lubricants, stabilisers and colourants (ASTM International, 2021). That is why sealants for places that stay wet contain fungicide (Ahn et al., 2024).
Mould on a silicone joint first grows in soil on the surface and, given time, grows into the sealant. One sealant manufacturer separates the stage where mould grows only in organic deposits on the surface from the stage where it has grown into the sealant, and says the latter calls for the sealant to be cut out (Otto-Chemie, n.d.). A stain that will not wipe off may not be a surface problem alone.
In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: mark the mouldy joints on a plan, confirm when they were sealed and whether the product is a fungicidal grade, then compare the cleaning and disinfecting agents, strengths and contact times in the sanitation procedure with the sealant's technical data sheet, the TDS.
Hypothesis 1: spent fungicide
Even a sealant with fungicide in it does not stay protected for ever. If mould has started to spread evenly along every joint a few years after sealing, particularly in washrooms hosed down often with hot water or in floor joints that are always wet, start with this hypothesis. Think of the floor joints in a beverage filling room. They were clean in the first year, but some years on black spots began to spread evenly along them, while the joints round a drain in the same room, resealed last year, are still white.
A Korean study comparing six silicone sealants explains that fungicide which works by leaching out of the sealant takes the sealant's mould resistance with it as it leaves over time (Ahn et al., 2024). In the same study, an oxime-cure sealant with fungicide lost resistance after four weeks in water at 50 degrees, ending at about the level of the same sealant without fungicide, while the alkoxy-cure fungicidal sealant changed little after immersion. Another study of fungicides in silicone sealants proposed comparing ratings before and after underwater leaching to estimate how much protection is lost over the service life (de Buyl & Gastaldi, 2004). The more often a joint meets water, the faster the fungicide leaves it, leaving a joint that looks sound but no longer resists mould.
Finding in the installation records whether the product was a fungicidal grade, and when it went in, comes first. Mould spread evenly over old joints and absent from recently resealed ones puts weight on this hypothesis. Mould that is not concentrated at a particular height or spot but spread over every joint that often gets wet is another clue. Photographing the joints in one area grouped by year of sealing makes the comparison easier.
Fungicide cannot be topped up later, so once it is judged spent, cut the sealant out and reseal. The standard for assessing fungal growth on sealant surfaces includes a condition after 28 days in water at 50 degrees (Ahn et al., 2024; ISO, 2021), so ask the supplier for results under that condition for the new product. There is also a study finding one method of the standard on microbial action on plastics well suited to judging antifungal performance in sanitary settings (de Buyl & Gastaldi, 2004; ISO, 2019).
Hypothesis 2: standing water
When mould spots gather in a band along one stretch rather than over the whole joint, suspect a place where water lingers. That means joints where wall meets floor, around drains, where dew forms on cold pipes and chiller walls, and low spots that stay wet after washing. In a washroom on the evening after sanitation, the floor water has been squeezed away, yet a thin line of water along the joint at the foot of the wall is still there the next morning. The black spots line up at exactly that height.
Water is the key to controlling mould. Wet areas must be dried within 24 to 48 hours to prevent mould, and unless the water problem is fixed, mould that has been cleaned off is likely to return (EPA, n.d.). A review of microbes in water-related indoor spaces finds that places with liquid water always present, such as plumbing, sinks and drains, support active fungal growth, and that constantly humid air also helps airborne fungi grow (Novak Babič et al., 2020). The food plant rule that drip or condensate from fixtures, ducts and pipes must not contaminate food follows the same logic (FDA, n.d.).
A few hours after cleaning, walk round to see whether water is left on the mouldy joints, and overlay the mould locations and the wet spots on one plan. Pour a little water on the floor to see whether it runs properly to the drain, and for cold pipes or walls measure surface temperature and the room dew point to see whether conditions allow condensation. Check too whether the joint surface has sunk into a hollow that holds water.
Once water proves to be the cause, fix the water path before the sealant. Add squeegeeing and drying the floor and joints after washing to the sanitation procedure, and shorten drying time with ventilation and dehumidification. Insulate pipes that sweat, and correct the fall of floors where water pools. Finish resealed joints with a smooth surface so that water runs off rather than lingering.
Hypothesis 3: soil feeding mould
Where organic matter is left on the joint surface, around lines that spatter food, on walls reached by steam carrying fat and sugar, or where soap and detergent have dried, soil becomes food for mould. On the wall beside a sauce filling line, the black spots gather only in joints at the height of the spatter marks, and rubbing them by hand leaves a sticky film.
Mould at first grows only in organic deposits built up on the sealant surface, such as personal care products, soap residue and skin flakes, and once established it grows into the sealant (Otto-Chemie, n.d.). The review of water-related indoor spaces holds that soaps and shampoos give a scaffold for biofilm, the sticky layer microbes build for themselves, and support alkali-tolerant fungi that break down detergent ingredients (Novak Babič et al., 2020). In a food plant, spattered product and fat do the same job. For as long as soil remains, mould can feed on it before the fungicide in the sealant reaches it.
Wipe the joint with a white cloth to see whether a sticky film or residue comes off, and mark whether the mould sites match the height of spatter or steam. If film still comes off straight after cleaning, the present method is not removing all the soil. Bleach may only lighten a stain for a while, so scrub with detergent instead: if the stain comes off, the mould is still on the surface; if it does not, it may have grown in.
If soil is the food, cleaning comes before disinfection. Keep to the order of removing soil with detergent, rinsing and only then disinfecting, and clean more often where product spatters regularly. Removing stains while they are still on the surface stops them growing in, so log black spots early at inspections and deal with them. Cut out and reseal joints where the mould has spread inside.
Hypothesis 4: gaps and joint defects
Where sealant has come away from the wall or floor, the surface is torn, or bubbles and underfilled spots were left during application, the space inside becomes a refuge that cleaning and disinfection cannot reach. Floor joints struck by forklifts or trolleys, spots scraped often, and joints where new sealant was run over old are typical. A joint that shows only a few mould spots from outside can turn out, when its edge is pressed with a knife point, to have lifted off the wall, with the gap behind it black and wet.
A review of why Listeria persists in food plants concluded that it is not down to special strains but to harbourage sites, shelters created by unhygienic design or damaged materials, where the bacteria find good growth conditions, and that such sites are hard to eliminate (Carpentier & Cerf, 2011). The conclusion concerns bacteria, but a gap that keeps water and food and that cleaning solution cannot reach offers mould the same conditions. That is why the sterile manufacturing rules require exposed clean room surfaces to be unbroken, with no recesses that are hard to clean (Health Canada, 2023). The food plant rules likewise require floors, walls and ceilings built so they can be cleaned properly and kept in good repair (FDA, n.d.).
Run a knife point or thin spatula along the joint edges to find where the sealant has lifted, and cut a little away at those spots to see whether the inside is wet or mouldy. A torch held at a low angle shows tears, bubble holes and open lines against the substrate clearly. Mark on the plan, too, whether the damage lines up with the routes of trolleys and equipment.
Patch repairs tend to leave gaps behind, so cut the sealant out completely in the mouldy stretch, clean and dry the substrate, and reseal. Follow the standard guide for the sequence of substrate preparation, primer, backer and tooling (ASTM International, 2025). Not sealing over a mouldy surface is also a principle in public guidance on mould (EPA, n.d.). Fit guards where equipment strikes, so the joint is not torn again.
Hypothesis 5: wrong cleaning agents
Joints in food plants and clean rooms take chlorine disinfectants, peracetic acid, quaternary ammonium compounds, alcohol, hot water and high-pressure washing every day. After a change of disinfectant or a rise in strength, in areas where disinfectant is left on without rinsing, and on sites that aim pressure jets straight at the joints, do not overlook this hypothesis. Suppose that some months after a clean room switched to a new disinfectant, the joints round door frames wiped every day turned rough, and mould spots began to appear along that roughened texture.
Cleaning and disinfecting agents affect mould by two routes. One runs through the sealant. A manufacturer of sealants used in clean room and food plant joints states that solutions such as hydrogen peroxide, sodium hypochlorite, peracetic acid and alcohols are generally compatible with fully cured sealant, yet advises against prolonged or continuous exposure and asks for rinsing as the instructions direct (Pecora, 2020). The standard test that immerses sealant in liquid does not, in its standard form, look at acids or alkalis, so the effect of an actual chemical can only be known from a modified test (ASTM International, 2020). The other route runs through the microbes. Oxidising chemicals such as bleach and hydrogen peroxide narrow microbial diversity, yet some microbes survive even rigorous sanitation, and mechanical forces and chlorination are thought to select for biofilm-forming species (Novak Babič et al., 2020).
From the sanitation procedure, find the chemicals in use, their strengths, contact times, whether they are rinsed off and when they were changed, and set these against when the mould increased. Compare by fingertip the joint surfaces in heavily and lightly disinfected areas for softening, tackiness or roughness. Soaking specimens of the same sealant in the chemicals now in use and comparing their hardness and surface with fresh specimens reveals what the chemicals do.
When the chemicals and the sealant look mismatched, the first step is to give the sealant supplier the list of chemicals in use and get compatibility confirmed in writing. Clean room surfaces must withstand repeated application of cleaning, disinfectant and sporicidal agents (Health Canada, 2023), so choose a resealing product with data from tests in the actual chemicals. Keep disinfectants to the set strength and contact time, rinse where required, and check the product label for effectiveness against mould.
Finding the cause
Before investigating five hypotheses separately, rule out what can be seen. Marking the mould on a plan and overlaying where water lingers, where soil spatters and where equipment strikes can be done in a single site inspection. The installation records and the sanitation procedure are already on paper.
The pattern of the mould is the first clue. A band along the height of a water line points to standing water, spots gathered at spatter height to soil that feeds mould, and growth starting at lifted edges or tears to gaps in the joint. Mould spread evenly over joints some years old while newly sealed ones stay clean suggests spent fungicide, and an increase that started in heavily disinfected areas after a change of chemicals suggests the cleaning agents.
Next, check whether the stain scrubs off with detergent. Mould growing in surface deposits can be cleaned away, but mould that has grown into the sealant means cutting the sealant out (Otto-Chemie, n.d.). If it wipes off, fix water, soil and cleaning method first; if not, replace the joint and look to the fungicide and to gaps for why the mould got so deep.
If that still does not settle it, run control trials that change one thing at a time. In one area, reseal some joints with a new fungicidal sealant and, for others, only add squeegeeing and drying after washing. Afterwards, photograph at fixed intervals and compare how long the mould takes to reappear. Compare candidate products beforehand by their results in the test for fungal growth on sealant surfaces (ISO, 2021).
The hypotheses can overlap. Where water stands, soil stays with it; a lifted gap holds both water and soil; and sealant kept long in water loses its fungicide too (Ahn et al., 2024). In such cases, put water and gaps right first, refine the cleaning method, and then replace the sealant, because if water and gaps remain, a new fungicidal sealant will go the same way.
Limits and cautions
Fungicide type and content, and disinfectant strength and contact time, differ by product, so numeric decisions follow the product's TDS, the chemical label and the site's validated sanitation procedure. For sealant used near food-contact surfaces, confirm food-contact suitability, and for clean rooms the requirements of the relevant grade, with the quality team. If mould has spread widely or the inside of walls or insulated panels appears wet, replacing the sealant will not finish the job, so have a facilities specialist inspect it.
Safety matters too. When cutting out mouldy sealant, wet it first so spores are not released, and wear a mask, gloves and eye protection. Do not mix chlorine disinfectants with other cleaners, and for every chemical follow the product's safety data sheet, the SDS, for protective equipment and ventilation. When replacing sealant in a production area, enclose the work zone so that cure by-products and debris cannot reach product, and finish cleaning and disinfection before restarting.
Sources
- Ahn, M.-S., Choi, S.-H., Lee, K.-H., & Nah, C. (2024). Assessment of fungal growth resistance in silicone sealants according to test methods. Journal of the Korea Institute of Building Construction, 24(1), 43–53. https://doi.org/10.5345/JKIBC.2024.24.1.043
- ASTM International. (2020). ASTM C1247-20, Standard test method for durability of sealants exposed to continuous immersion in liquids. https://store.astm.org/c1247-20.html
- ASTM International. (2021). ASTM G21-15(2021)e1, Standard practice for determining resistance of synthetic polymeric materials to fungi. https://store.astm.org/g0021-15r21e01.html
- ASTM International. (2025). ASTM C1193-25, Standard guide for use of joint sealants. https://store.astm.org/c1193-25.html
- Carpentier, B., & Cerf, O. (2011). Review: Persistence of Listeria monocytogenes in food industry equipment and premises. International Journal of Food Microbiology, 145(1), 1–8. https://doi.org/10.1016/j.ijfoodmicro.2011.01.005
- de Buyl, F., & Gastaldi, H. (2004). Insights into the use of biocides in silicones sealants: Test methods and durability aspects. In Durability of building and construction sealants and adhesives (pp. 228–251). ASTM International. https://doi.org/10.1520/STP12566S
- Health Canada. (2023). Annex 1 to the Good manufacturing practices guide: Manufacture of sterile drugs (GUI-0119): Premises, equipment, utilities and personnel. Retrieved November 2026. https://www.canada.ca/en/health-canada/services/drugs-health-products/compliance-enforcement/good-manufacturing-practices/guidance-documents/gmp-guidelines-annex-1-manufacture-sterile-drugs-0119/premises-equipment.html
- International Organization for Standardization [ISO]. (2019). ISO 846:2019, Plastics: Evaluation of the action of microorganisms. https://www.iso.org/standard/74599.html
- International Organization for Standardization [ISO]. (2021). ISO 21265:2021, Building and civil engineering sealants: Assessment of the fungal growth on sealant surfaces. https://www.iso.org/standard/70339.html
- Novak Babič, M., Gostinčar, C., & Gunde-Cimerman, N. (2020). Microorganisms populating the water-related indoor biome. Applied Microbiology and Biotechnology, 104(15), 6443–6462. https://doi.org/10.1007/s00253-020-10719-4
- Otto-Chemie. (n.d.). Causes for mould attack. Retrieved November 2026. https://www.otto-chemie.com/en/otto-anti-mould/causes-for-mould-attack
- Pecora Corporation. (2020). Pecora joint sealant chemical compatibility: Cleaning agents, degreasers and detergents (Technical Bulletin #213). https://www.pecora.com/wp-content/uploads/pdfs/PEC-213-Pecora-Joint-Sealant-Chemical-Compatibility-Cleaning-Agents-7-7-2020-mdm.pdf
- U.S. Environmental Protection Agency [EPA]. (n.d.). A brief guide to mold, moisture and your home. Retrieved November 2026. https://www.epa.gov/mold/brief-guide-mold-moisture-and-your-home
- U.S. Food and Drug Administration [FDA]. (n.d.). 21 CFR 117.20, Plant and grounds. Code of Federal Regulations. Retrieved November 2026. https://www.ecfr.gov/current/title-21/section-117.20
- World Health Organization [WHO]. (2009). WHO guidelines for indoor air quality: Dampness and mould. WHO Regional Office for Europe. ISBN 9789289041683. https://pubmed.ncbi.nlm.nih.gov/23785740/