Why does paint stripper barely work?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Cleaning & Surface Prep

Reaching for a stronger product or scraping straight away is the usual response when a paint stripper barely works, but a stripper only works by soaking into the coating and swelling it, so without the conditions for that, a stronger product tends to stall the same way. What actually lies behind it can be a cross-linked coating, low temperature, solvent that evaporated before it could soak in, a thick layered coating or too short a dwell time, and sometimes two or more at once.

Background

During scheduled maintenance, paint stripper goes on an equipment cover to remove the old finish, but long afterwards the coating has only wrinkled in patches and will not come off under the scraper. After a few more applications it ends up being ground or sanded off, and working time and stripper consumption climb in the meantime. Grinding easily cuts into or heats the substrate, and the longer the hand scraping goes on, the longer the worker breathes solvent vapour.

A stripper does not dissolve the coating away; it soaks into the coating and swells it. Small solvent molecules penetrate the film quickly, and once they reach the substrate the film swells, wrinkles and blisters, releasing it from the substrate (Wollbrinck, 1993). A cured paint is a network of linked chains, so it swells rather than dissolves; swelling lowers the film's strength, and the stresses it creates crack the film and lift it away (Croll, 2010). A study that tested methylene chloride strippers on several coatings concluded that methylene chloride penetrates the film first and opens the way for the other solvents to follow (Wynne et al., 2011).

So a stripper that barely works means either that the solvent did not get far enough into the coating, or that it got in but could not swell the coating enough. Coating type, temperature, evaporation, film thickness and waiting time each change one of these two.

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: check the target coatings, working temperature and dwell time in the stripper's technical data sheet, the TDS, and compare them with a record of the coating type and thickness, that day's temperature and the time actually waited after application.

Hypothesis 1: cross-linked coating

Consider this hypothesis when stripping coatings cured by heat or reaction, such as powder-coated equipment frames, epoxy-painted floors or tank interiors, and two-part urethane topcoats. The same applies when a product sold for household or wood use is used on painted metal equipment. Think of a powder-coated steel shelf to be repainted, given a coat of stripper bought for wood. An old lacquered wooden board beside it blistered within minutes, but the shelf has only lost a little gloss and is otherwise unchanged.

The difference comes from how the coating cures. A coating that hardens as its solvent evaporates, like lacquer, has unlinked chains and redissolves in solvent, but epoxy and urethane coatings cure into a network of chemically linked chains, a cross-linked structure. A cross-linked polymer does not dissolve; it only takes up solvent and swells, and the denser the network, the less it swells (Flory & Rehner, 1943). Powder coatings include thermosetting types cross-linked by baking, which share this behaviour (Spyrou, 2012). In a comparison of consumer strippers, every product removed nitrocellulose lacquer easily, but on a metal panel with an epoxy primer and a cross-linked polyurethane topcoat, only some products had started to lift the coating after 30 minutes, and all of them needed more than 20 hours to strip it. The same report named cross-linked, powder and waterborne coatings as harder to strip (Morris & Wolf, 2006).

First establish what the coating is. Look for powder, epoxy or urethane in the equipment paint specification or delivery records, and if there are none, rub an inconspicuous spot with a cloth soaked in a strong solvent. If colour transfers and the film softens, the coating redissolves in solvent; if nothing changes, lean towards a cross-linked coating. Whether a stripper suits that coating is judged by applying it to a test piece of the same coating or a hidden spot, lifting the softened film with a plastic scraper after a set time and rating the degree of removal (ASTM International, 2022).

If the coating proves to be cross-linked, choose the stripper again to suit it. Shortlist products whose TDS names epoxy, urethane or powder coatings as targets, rate them on test pieces and use whichever strips best. If chemical removal alone cannot take the coating all the way off, consider a mechanical method such as blasting alongside it, and check whether the substrate can withstand it.

Hypothesis 2: low temperature

In unheated warehouses and on outdoor equipment in winter, on jobs that start early in the morning, and on substrates that hold a lot of heat, such as thick steel plate or large castings, suspect temperature first. Even when the air warms up around midday, a heavy steel structure stays cold for some time. A midwinter morning job on a steel cover that has been standing outside is a case in point. When the same product was used in autumn, the coating wrinkled soon after application, but today the surface is unchanged after the same time.

What slows down on a cold coating is the rate at which solvent soaks in. Diffusion of solvent in a polymer varies strongly with temperature and solvent concentration, a relationship explained through free volume, the empty space between polymer chains (Vrentas & Duda, 1977). In a cold film the chains move less, leaving fewer gaps for the solvent to squeeze into, so swelling and lifting come later. That does not make hotter always better. Environment and Climate Change Canada's code of practice for methylene chloride strippers gives 13 °C to 24 °C as the optimum ambient temperature for working with strippers and notes that methylene chloride dries more quickly on a heated surface (ECCC, 2019). Too cold and the solvent cannot get in; too hot and it may evaporate before it does.

What needs measuring is the substrate surface temperature, not the air temperature. Take the temperature of the spot to be treated with a contact thermometer and compare it with the working temperature in the TDS, then set the temperatures of good and bad stripping days side by side from the work log. On the same coating, scraping the sunny and shaded sides, or a test piece warmed indoors and a cold one outside, after the same time shows how much temperature contributes.

If temperature is the obstacle, bring the part into a warm room and apply the stripper once the substrate itself has warmed through; for equipment that cannot be moved, enclose and heat the work area or move the job to a sunny part of the day. Avoid putting a flame or hot air directly on the stripper, since it may contain flammable solvent and the solvent will evaporate before it gets into the coating. When work on a cold day cannot be avoided, allow a longer dwell time within the range the TDS sets.

Hypothesis 3: evaporated solvent

This hypothesis comes into play when working outdoors in a breeze or right in front of an extraction fan, on steel in direct sun, when spreading the stripper thinly over a large area, or when brushing it out repeatedly after application. It applies all the more to highly volatile products such as methylene chloride strippers. Take an afternoon with the big doors open for ventilation and stripper spread evenly over a large panel. Coming back later, the stripper has dried to a white crust from the edges inwards, and the coating under the dry areas is untouched.

A stripper only works while it is wet. Methylene chloride has a very high vapour pressure and leaves quickly, so wax is added to hold the solvent at the surface, and in comparison tests, methylene chloride strippers dried out much faster than lower-vapour-pressure alternatives and had to be reapplied (Morris & Wolf, 2006). The wax forms a skin that traps the solvent; brushing back and forth breaks the skin and lets the solvent escape, while thickeners also slow evaporation and lengthen contact time (Wollbrinck, 1993). Canada's code of practice likewise advises brushing the stripper on in one direction, leaving the wax seal undisturbed and covering the treated surface with chemical-resistant sheeting (ECCC, 2019).

Stay with the job and watch the surface after application. See whether spots dry or turn white from the edges before the dwell time is up, and whether coating remains only under those spots. Check the draught and sun at the work position as well. Covering one half of the same panel and leaving the other open, then scraping both after the same time, shows at once how much evaporation contributes.

If evaporation looks likely, correct the application first. Lay the stripper on generously in one direction without brushing it out again, and cover the treated surface with chemical-resistant plastic sheeting. Keep out of draughts and direct sun, but keep the ventilation going. A cover slows evaporation of the stripper but does not remove the worker's exposure to vapour, so keep ventilation and protective equipment in place while it is covered.

Hypothesis 4: thick, layered coating

On equipment repainted over many years, heavy-duty systems with primer, intermediate and topcoat built up, and surfaces where different coating types have accumulated, weigh film thickness and layering first. All the more so when the upper layers come off but the lower ones stay. A pipe support repainted in changing colours over a long period is one example. After stripper and scraping, the top two or so layers wrinkle and come away, but the scraper stops at a differently coloured layer beneath.

The whole coating lifts only when solvent passes right through it and reaches the substrate. Looking at diffusion into a flat sheet alone, the time to reach the same fraction of penetration grows with the square of the thickness, so a coating twice as thick can take about four times as long (Crank, 1975). Multiple layers create other problems too. Methylene chloride passes through overpaint into the layers beneath, but if the upper layer is cracked, the swelling force can escape sideways and the coating may not lift (Wollbrinck, 1993). Where each layer is a different coating, a stripper that suited the top may not suit the layer below. Canada's code of practice likewise notes that sanding the top clearcoat first leaves fewer layers to remove and so takes less stripper (ECCC, 2019).

Measure film thickness first. Use a magnetic or eddy-current thickness gauge for coatings on steel, and look at a knife cut through the film under a magnifier to see how many layers there are and the colour and texture of each. Record how many layers came off after the set dwell time and whether the remaining layer is the same coating as the top or a different one. Repeating the solvent rub on the remaining layer also shows whether that layer is cross-linked.

A thick, layered coating should not be taken off in one go; strip it layer by layer. Apply, remove the lifted layers and apply again, repeating as needed, and sand the top lightly to reduce the layers to be stripped. If a lower layer is a different coating, switch to a stripper that suits it, and where there are very many layers or great thickness, consider blasting as well.

Hypothesis 5: short dwell time

Suspect this hypothesis when, on a tight maintenance schedule, scraping starts a few minutes after application, when a switch to a product with a different solvent keeps the habits learned on methylene chloride products, or when dwell time is set by feel rather than by the TDS. The first week after a product change in a maintenance shop is a good example. The stripper goes on as usual and the scraper goes in shortly after, but it only skids over the coating, and the worker notes that the new product is weak.

Lifting a coating takes time for the solvent to soak in, the film to swell and the bond to break, and that time differs by product. In methylene chloride strippers, water added as an activator can reportedly cut stripping time by as much as 90%, so dwell time varies widely with the formulation (Wollbrinck, 1993). A report comparing alternatives found that methylene chloride strippers were applied several times to finish a job, whereas benzyl alcohol strippers take longer to penetrate typical coatings but, with their low vapour pressure, evaporate less, so a single application left a little longer could strip the item fully (Morris & Wolf, 2006). Scraping a coating that has not fully lifted removes only the top layer, and fresh stripper applied over it needs time again to penetrate what remains.

Compare the dwell time in the TDS with the time actually allowed. Then apply the stripper at several spots on the same surface and scrape them with a plastic scraper at staggered intervals, looking for the point at which the coating wrinkles, swells and lifts without force. Recording the time found for each coating and temperature gives a baseline for the next job.

If the dwell was too short, write product-specific dwell times into the standard work instructions and add a step to confirm lifting before scraping. For slow-penetrating products, one recommendation is to apply the stripper to several items at once and strip them in turn, so the waiting time is not lost (Morris & Wolf, 2006). Keep the treated surfaces covered so they do not dry out during the longer dwell.

Finding the cause

Start by ruling out what records and eyes can confirm straight away. The waiting time and that day's temperature are in the work log, and whether the stripper dried or crusted white is visible during the job. Dwell time, temperature and evaporation are also worth checking first because they can be changed on the very next job.

Next is the pattern of what did not come off. Coating left only at the edges or on the windward side points to evaporation, and coating left only in shade or over heavy substrate to temperature. Upper layers coming off but stopping at one particular layer suggests a thick, layered coating or a different coating in each layer. An evenly unresponsive surface points to a cross-linked coating the stripper cannot swell well, while a surface that starts to lift little by little given more time points to dwell time.

If that still does not settle it, run a control trial on the same surface. Leave one square as usual and change one thing per square: covering only on one, warming only on another, a longer dwell only on a third. Lifting the film the same way after a set time and rating the removal puts the comparison on the same footing as the standard practice for evaluating removers (ASTM International, 2022). Change several things at once and there is no telling which one worked.

The final check is to apply the changed conditions to real work. On the next part with the same coating and thickness, record whether it strips to the substrate within the set time and whether the number of applications and the amount used have fallen. The cause has been found only when those figures come down.

The hypotheses can overlap. On a cold day the solvent soaks in slowly, so a longer wait is needed, and the longer the wait, the more time an uncovered stripper has to dry. Add a thick or cross-linked coating and the time stretches further. In such cases, set the conditions that can be changed at once, such as covering and temperature, and then look again at dwell time and product, because while evaporation and temperature are unsettled, the effect of changing the product cannot be compared fairly.

Limits and cautions

A stripper's target coatings, working temperature, dwell time and application thickness differ by product, so numbers follow that product's TDS. Substrates such as aluminium, galvanised steel, plastics and composites can be damaged by some strippers, so first confirm that the product is safe on the substrate, and for items with set coating standards, such as aircraft, pressure vessels and food equipment, follow those standards and the coating specification.

Safety matters too. Methylene chloride vapour is heavier than air and can collect in hollows such as bathtubs, and in the United States a series of deaths among bathtub refinishers using methylene chloride strippers has been reported (CDC, 2012). The United States has since banned most commercial uses of methylene chloride for paint and coating removal (EPA, 2024). Alternatives carry their own health risks; N-methylpyrrolidone, for example, is classed as a reproductive toxicant (Durrani et al., 2020). Keep ventilation and the gloves, eye protection and respiratory protection the SDS specifies, and do not use strippers near ignition sources.

Sources

  1. ASTM International. (2022). ASTM D6189-97(2022), Standard practice for evaluating the efficiency of chemical removers for organic coatings.
  2. Centers for Disease Control and Prevention [CDC]. (2012). Fatal exposure to methylene chloride among bathtub refinishers: United States, 2000–2011. Morbidity and Mortality Weekly Report, 61(7), 119–122. https://www.cdc.gov/mmwr/preview/mmwrhtml/mm6107a2.htm
  3. Crank, J. (1975). The mathematics of diffusion (2nd ed.). Clarendon Press.
  4. Croll, S. G. (2010). Application of the Flory–Rehner equation and the Griffith fracture criterion to paint stripping. Journal of Coatings Technology and Research, 7(1), 49–55. https://doi.org/10.1007/s11998-009-9166-4
  5. Durrani, T., Clapp, R., Harrison, R., & Shusterman, D. (2020). Solvent-based paint and varnish removers: A focused toxicologic review of existing and alternative constituents. Journal of Applied Toxicology, 40(10), 1325–1341. https://doi.org/10.1002/jat.3979
  6. Environment and Climate Change Canada [ECCC]. (2019). Code of practice for the reduction of dichloromethane emissions from the use of paint strippers in commercial furniture refinishing and other stripping applications. Retrieved November 2026. https://www.canada.ca/en/environment-climate-change/services/canadian-environmental-protection-act-registry/publications/code-practice-reducing-dichloromethane-emissions/chapter-2.html
  7. Flory, P. J., & Rehner, J. (1943). Statistical mechanics of cross-linked polymer networks II. Swelling. The Journal of Chemical Physics, 11(11), 521–526. https://doi.org/10.1063/1.1723792
  8. Morris, M., & Wolf, K. (2006). Methylene chloride consumer product paint strippers: Low-VOC, low toxicity alternatives. Institute for Research and Technical Assistance, prepared for the California Department of Toxic Substances Control. https://www.ocf.berkeley.edu/~dshuster/MeCl/MeCl%20Reports/IRTA_PaintStrippers06.pdf
  9. Spyrou, E. (2012). Powder coatings: Chemistry and technology (3rd rev. ed.). Vincentz Network.
  10. U.S. Environmental Protection Agency [EPA]. (2024). Methylene chloride; Regulation under the Toxic Substances Control Act (TSCA). Federal Register, 89, 39254. https://www.federalregister.gov/d/2024-09606
  11. Vrentas, J. S., & Duda, J. L. (1977). Solvent and temperature effects on diffusion in polymer–solvent systems. Journal of Applied Polymer Science, 21(6), 1715–1728. https://doi.org/10.1002/app.1977.070210627
  12. Wollbrinck, T. (1993). The composition of proprietary paint strippers. Journal of the American Institute for Conservation, 32(1), 43–57. https://doi.org/10.1179/019713693806066474
  13. Wynne, J. H., Watson, K. E., Yesinowski, J. P., Young, C. N., & Clayton, C. R. (2011). Report on scientific basis for paint stripping: Mechanism of methylene chloride based paint removers, NRL/MR/6120--11-9368. Naval Research Laboratory. https://apps.dtic.mil/sti/tr/pdf/ADA552538.pdf

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.