Changing the oil and cleaning the tubes is the usual response when thermal oil turns black and the heater tubes coke up, but if the condition that spoiled the oil stays, the new charge tends to spoil early too. What actually lies behind it can be a high film temperature from low flow, oxidation by air at the expansion tank, running past the oil's temperature limit, contamination that got in, or frequent starts and stops, and sometimes two or more at once.

Background

When a thermal oil heater is opened for maintenance, the tube bores carry a hard black layer, and the oil circulating in the system has lost its clear colour and turned dark. The burner has to fire harder to hold the same outlet temperature, and the flue gas temperature creeps up as well. A coked tube cannot pass heat on to the oil inside, so the tube wall runs hot, and if left alone the tube can rupture and spray oil into the firebox, starting a fire (Ennis, 2009; HDI, 2019).

The losses do not stop at fuel. Spoiled oil thickens and carries less heat, and its debris blocks filters and gets into pump seals and bearings. In the end the plant has to stop to replace the whole charge and clean the tubes, and if the old oil and debris are not fully removed then, the fresh oil spoils early as well (Ennis, 2009).

Thermal oil is organic, so heat and oxygen change its molecules. Excess heat breaks long molecules into light ends with low boiling points, and the broken pieces link up again into heavy ends with high boiling points. Heavy ends raise the viscosity and cut heat transfer, and they stick to hot tube walls, turn tarry and finally harden into a solid carbon layer, that is, coke (Ennis, 2009). Oxygen from the air takes another route and forms acids and sludge (Aguilar et al., 2010). The thermal load on the oil is judged less by the bulk oil temperature than by the temperature of the thin oil film against the tube wall, the film temperature, and the spot with the highest film temperature is where the load is highest (HDI, 2019).

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: look up the maximum bulk and film temperatures in the oil's technical data sheet, the TDS, and set the operating records for heater outlet temperature, circulation flow and heater inlet pressure, together with the latest oil analysis, beside them for comparison.

Hypothesis 1: low flow

When less oil flows through the heater, the tube walls run hotter at the same firing rate. This happens when the strainer ahead of the pump slowly fills with debris, when the pump impeller is worn, when added users or throttled valves change the pipework resistance, and when one pass of a multi-pass heater gets less than its share of flow. Picture a plant where the strainer's differential pressure gauge has been creeping up for months, but nobody has touched it because the outlet temperature looks normal. The burner runs longer than usual at high fire to hold that temperature, and when the heater is opened for maintenance, thick coke scrapes out of only a few of the tubes.

The heat passing from tube wall to oil equals the convective heat transfer coefficient times the temperature difference between wall and oil, and in turbulent tube flow that coefficient rises with velocity (Bergman et al., 2011). If the burner sends the same heat while the velocity falls, the wall-to-oil temperature difference widens as the coefficient shrinks, so the film temperature rises even when the outlet temperature does not. In a multi-pass heater with uneven flow, the starved tubes overheat, and the carbon layer that forms where it overheats blocks heat and drives the wall hotter still (Ennis, 2009). Fouling studies on crude oil exchangers likewise find that reaction fouling speeds up with wall temperature and is held back by flow shear, and threshold models are used to find combinations of wall temperature and shear at which little fouling forms (Wilson et al., 2017).

Confirm low flow with numbers. Compare a flow meter reading, if there is one, with the design flow; if not, look at the pressure difference across the pump and the temperature rise across the heater. A larger temperature rise at the same firing rate means less oil is flowing. A rise in heater inlet pressure can mean the heater tubes are partly blocked, a fall can mean a blocked strainer upstream or a pump fault, and a rise in flue gas temperature can signal that the tubes are taking up less heat (Ennis, 2009). In a multi-pass heater, set the outlet temperature of each pass side by side to see whether any pass is starved.

Once low flow shows up, restoring the flow comes first. Clean the strainer, check pump performance, and if valves or users have changed, set the system to deliver the design flow again. Balance the flow between passes. Check too that a minimum flow safeguard is fitted to shut down the burner and pump when flow drops below a set value, and that it actually works (HDI, 2019). Tubes that already carry coke will not clear just because the flow is back, so decide on a cleaning method at the same time.

Hypothesis 2: air oxidation

The expansion tank takes up the extra volume as the oil heats, and it usually sits at the highest point of the system with a vent line open to atmosphere (HDI, 2019). Oxidation becomes a problem when the oil in that tank is both in contact with air and hot. That is the case when the vapour space is not blanketed with an inert gas such as nitrogen, when part of the circulating flow passes through the tank so its oil runs close to system temperature, and when the tank itself is wrapped in insulation. Open the expansion tank on a summer inspection day and a brown skin floats on the oil, a sticky black band runs along the oil line on the wall, and scraping the bottom brings up mud-like sludge.

Hydrocarbons react with oxygen faster the hotter they are. Radicals formed by heat or metals meet oxygen and become peroxides, the peroxides split and form new radicals so the chain carries on, and at the end acids appear along with large tangled molecules that thicken the oil and settle out as sludge (Aguilar et al., 2010). Oxygen in a heat transfer system makes degradation excessive, so air must be kept out; for that reason the expansion tank is designed not to run at system temperature and to be blanketed with nitrogen that displaces oxygen. Tarry material formed this way also travels with the flow to the heater, where it can stick to hot tube walls, block heat and in time harden into a carbon layer (Ennis, 2009).

Oxidation leaves its mark on the analysis report. An acid number above that of fresh oil points to oxidation or acidic contamination; check whether viscosity and insolubles have risen with it (Gamble, 2023). On site, measure the expansion tank temperature during operation and compare it with system temperature, check whether the piping routes circulating flow through the tank, and confirm that nitrogen supply and tank pressure are live. Photograph the brown skin and sludge in the tank to compare at the next inspection.

With the cause narrowed to oxidation, cut off at least one of air and heat. Blanket the vapour space with nitrogen, keep the tank out of the main circulation so its oil stays cool rather than reaching system temperature, and strip any insulation from the tank (Ennis, 2009). For oil with a high acid number and insolubles, decide with the supplier whether to filter it or bring replacement forward, and from then on measure the same items regularly to see whether the trend has turned.

Hypothesis 3: too hot for the oil

Every oil has a temperature it can withstand. A plant approaches that limit when the heater set point goes up to raise output, when process conditions change but the oil chosen for a lower temperature stays, and when a different grade is used for top-up. Say a plant raised the outlet temperature a little when it added another dryer, and about six months have passed. The routine analysis shows the flash point down and the viscosity up, and more black grains are turning up in the strainer than before.

Thermal cracking happens even without oxygen. Heat breaks molecular chains into light and heavy ends together, and since more heavy ends make degradation faster in a self-accelerating way, one recommendation is to replace the oil once heavy ends exceed 10% by weight (Ennis, 2009). How heavy material becomes coke has been studied in detail with petroleum residue. In those experiments, coke formed when reacted heavy molecules could no longer stay dissolved in the oil and separated out as a second, hydrogen-poor liquid phase (Wiehe, 1993).

The limit is not a sharp line. The maximum bulk and film temperatures an oil supplier quotes mean the oil stays stable for one year under those conditions, so one guideline sets the actual maximum operating temperature at least 30 K below the permitted maximum bulk temperature (HDI, 2019). Laboratory thermal stability tests likewise show how much breaks down at a set temperature and time, without fixing the temperature at which breakdown begins (ASTM International, 2020b). In a study of a synthetic fluid used in solar power plants, hydrogen from breakdown rose with temperature and with time, and field samples after five and ten years of service followed the same trend (Jung & Senholdt, 2020).

Pull the peak heater outlet temperatures and how long they lasted from the operating records, and compare them with the TDS maximum. Film temperature is hard to measure directly, so check in the heater maker's design data where the peak film temperature occurs and how high it is, and read the tube skin thermocouple records if there are any. In the oil analysis, use simulated distillation to see how far light and heavy ends have grown compared with fresh oil, and lay the flash point and viscosity trends beside them (Gamble, 2023). Light ends move the flash point and heavy ends move the viscosity, so when both have worsened together, the weight shifts towards thermal cracking.

Running past the limit leaves two ways out: change the operating point or change the oil. Look with the process side at whether lowering the set point can restore the margin, and if the high temperature is a must, review a switch to an oil made for that temperature with the supplier. Oil with heavy build-up of light and heavy ends is either reclaimed by distillation or replaced, and on replacement the old oil must be drained completely and the system cleaned, or the new oil will spoil early (Ennis, 2009).

Hypothesis 4: contamination

A thermal oil system is closed, but maintenance and the process bring other substances in. Cleaning solvent, water or pickling acid can be left behind after pipework repairs, a leaking tube in a process exchanger can let process material across to the oil side, and top-up drums stored outdoors can take in rain, or an oil of unknown make-up can go in as top-up. Suppose a reactor jacket gasket is replaced and the plant restarts, and soon after, the oil turns noticeably darker and unfamiliar debris starts collecting in the strainer.

Thermal oil itself is barely corrosive, so corrosion in the system usually starts from contaminants such as leftover cleaning fluid or process fluid that has leaked in. Such contamination can have a large effect on oil degradation, and fresh oil also spoils early if cleaning solutions were not fully flushed out or old oil was left in the system (Ennis, 2009). Acidic material raises the acid number, but oxidation raises it too, so telling the two apart needs the timing and the other test items as well (Gamble, 2023). Metal dissolved by corrosion can also act as a catalyst that speeds up hydrocarbon oxidation (Aguilar et al., 2010).

The first clue is timing. Check the records for whether the change in the oil sped up suddenly after maintenance, a restart, a top-up or a suspected process-side leak. Then send a fresh oil sample and the current oil to the same laboratory and compare viscosity, acid number, water, insolubles and flash point side by side. The test items for judging whether an in-service heat transfer fluid can stay in use are set out in a standard (DIN, 2000). Components or water absent from the fresh oil mean contamination, and water can be a trace of leakage from the process side (Ennis, 2009). Exchangers where the process side runs at higher pressure than the oil side are places where process material can cross over, so consider a leak test there.

Once contamination is confirmed, close the way in first. Repair leaking exchangers; after maintenance, drain cleaning fluids completely, rinse with water and dry the system before filling with oil; and do not store top-up drums outdoors. For oil that is already contaminated, choose by severity: filter light cases through media that withstand the operating temperature, and for heavy cases strip the light and heavy ends by distillation or replace the charge (Ennis, 2009).

Hypothesis 5: start-stop cycling

In a plant that shuts the heater down and restarts it every weekend or holiday, a process that ramps temperature up and down with every batch, or a site where power cuts sometimes stop the pump without warning, the oil can take a heavy thermal load at each start and stop. A typical scene is Monday morning. To meet the production start time, the system that cooled over the weekend is heated at full burner firing. Another is a power cut. The circulation pump has stopped, but the heater's refractory and tubes still hold their heat.

Heating a cold system in a hurry pushes the film temperature at the tube wall past its limit before the bulk oil has warmed. In one loss case, preheating after a weekend shutdown was run at maximum firing instead of the prescribed lowest setting, the permitted film temperature was exceeded and coke formed locally in the heater, and the resulting hot spot ruptured a tube (HDI, 2019). The warning that ramping up temperature to finish heating quickly drives film temperatures too high makes the same point (Ennis, 2009). In a heater whose pump has stopped, the remaining heat goes straight into oil that is no longer moving and can overheat it where it sits.

What happened at start-up is held in the burner management system and temperature logs. Find there at what firing rate and for how long the burner ran at start-up, how fast the outlet temperature rose, how long the burner took to go out after a power cut or pump stop, and how the outlet temperature moved afterwards. At maintenance, see whether coke is concentrated in the tubes of the hottest firing zone, and check whether the oil analysis worsened particularly in periods with many starts.

Damage from starts and stops is curbed first by writing the procedure down. Start a cold system at low fire and raise the temperature in steps while confirming circulation, and keep the pump running after the burner goes out until the heater has cooled. Where heat left in the heater could degrade the oil or damage the heater when the pump stops, one guideline calls for emergency cooling that runs on backup power (HDI, 2019). If stops cannot be avoided, weigh up with the heater maker whether keeping the oil circulating at a low temperature over the weekend would be better.

Finding the cause

Five hypotheses do not mean searching all five at once. Operating records and oil analysis can be checked without stopping the plant, so look at them first. Flow, heater inlet pressure, peak outlet temperature and start-up records are already in the control system, and oil samples must be drawn at the same point under the same conditions every time for results to be comparable (HDI, 2019). Inspect the tube interiors when the plant is down anyway.

The shape of the analysis report gives the direction. A rising acid number with viscosity and insolubles rising alongside leans towards air oxidation, while a falling flash point with growing heavy ends leans towards thermal cracking, from running past the temperature limit or from a hot film. Water or components absent from fresh oil point to contamination, and a sudden change after a particular maintenance job or top-up points to that job. The standard guide for choosing tests on in-service heat transfer fluids sets no pass limits, so judge against fresh oil values and the supplier's criteria (ASTM International, 2020a).

Where the coke sits is a clue too. A tube short of flow overheats in that spot alone (Ennis, 2009), so if coke is concentrated in a few tubes or one zone, look first at what heated that spot, such as flow distribution or hurried start-ups. If it is spread evenly through the heater, suspect the oil itself first: oxidation, operating temperature or contamination.

If that still does not settle it, run control trials that change one thing at a time. Clean the strainer to restore flow, blanket the expansion tank with nitrogen, or switch start-ups to low fire, then see over the following analyses whether the rate of increase in acid number, viscosity, and light and heavy ends has slowed. Only one change at a time shows which one worked, and since oil changes slowly, judge by the trend across several results rather than a single value. The final check is the tube inspection at the next shutdown, to see whether coke has built up again in the cleaned tubes.

The hypotheses feed one another. Heavy ends raise viscosity and cut heat transfer, that raises the film temperature and speeds degradation, and the coke that builds up heats the spot further (Ennis, 2009). Sludge from oxidation can block the strainer, cutting flow and turning into a film temperature problem. In such cases put flow and temperature right first, close off the routes for air and contamination, and only then decide whether to replace the oil, because while flow and temperature are unsettled, fresh oil is likely to spoil again.

Limits and cautions

Maximum bulk and film temperatures, flow and replacement criteria differ by oil and heater, so numeric decisions follow the oil's TDS and the heater maker's guidance, and plant design and safety devices follow the standard for heat transfer installations and local regulations (DIN, 2015). Hard coke is removed by methods that require dismantling, such as high-pressure water jetting, mechanical cleaning or burning out with steam and air, so leave it to the heater maker and specialist contractors (Ennis, 2009), and get tube thickness and damage assessed by an inspection body.

Heat transfer systems almost always run above the oil's flash point, and oil soaked into insulation degrades over time and can start a fire inside the lagging, so repair leaks at once and replace soaked insulation (Ennis, 2009). When handling oil or drawing samples, wear the protective equipment set out in the product's safety data sheet, the SDS, draw samples cooled through a closed sample cooler, and carry out hot work such as welding only after the section has been drained and purged with inert gas (HDI, 2019).

Sources

  1. Aguilar, G., Mazzamaro, G., & Rasberger, M. (2010). Oxidative degradation and stabilisation of mineral oil-based lubricants. In R. M. Mortier, M. F. Fox, & S. T. Orszulik (Eds.), Chemistry and technology of lubricants (3rd ed., pp. 107–152). Springer. https://doi.org/10.1023/b105569_4
  2. ASTM International. (2020a). ASTM D5372-20, Standard guide for evaluation of hydrocarbon heat transfer fluids. https://store.astm.org/d5372-20.html
  3. ASTM International. (2020b). ASTM D6743-20, Standard test method for thermal stability of organic heat transfer fluids. https://store.astm.org/d6743-20.html
  4. Bergman, T. L., Lavine, A. S., Incropera, F. P., & DeWitt, D. P. (2011). Fundamentals of heat and mass transfer (7th ed.). John Wiley & Sons.
  5. Deutsches Institut für Normung [DIN]. (2000). DIN 51529:2000-11, Testing of mineral oils and related products – Testing and evaluation of used heat transfer fluids. https://www.dinmedia.de/en/standard/din-51529/21165384
  6. Deutsches Institut für Normung [DIN]. (2015). DIN 4754-1:2015-03, Heat transfer installations working with organic heat transfer fluids – Part 1: Safety requirements, test. https://www.dinmedia.de/en/standard/din-4754-1/225280007
  7. Ennis, T. (2009). Safety in design of thermal fluid heat transfer systems. In Hazards XXI (IChemE Symposium Series No. 155, pp. 162–169). Institution of Chemical Engineers. https://www.icheme.org/media/9653/xxi-paper-025.pdf
  8. Gamble, C. (2023, August 1). Facts at your fingertips: In-service heat-transfer-fluid testing. Chemical Engineering. https://www.chemengonline.com/facts-at-your-fingertips-in-service-heat-transfer-fluid-testing/
  9. HDI Global SE [HDI]. (2019). Risk engineering guideline: Heat transfer oil systems. HDI Risk Consulting. https://www.hdi.global/globalassets/_local/international/downloads/group_heat-transfer-oil-systems/20190305_403-hrc-reg130gb_-heat_transfer_oil_systems.pdf
  10. Jung, C., & Senholdt, M. (2020). Comparative study on hydrogen issues of biphenyl/diphenyl oxide and polydimethylsiloxane heat transfer fluids. AIP Conference Proceedings, 2303, 150009. https://doi.org/10.1063/5.0028894
  11. Wiehe, I. A. (1993). A phase-separation kinetic model for coke formation. Industrial & Engineering Chemistry Research, 32(11), 2447–2454. https://doi.org/10.1021/ie00023a001
  12. Wilson, D. I., Ishiyama, E. M., & Polley, G. T. (2017). Twenty years of Ebert and Panchal—What next? Heat Transfer Engineering, 38(7–8), 669–680. https://doi.org/10.1080/01457632.2016.1206407

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.