Why does thermal oil flash point fall and the pump cavitate?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Heat Transfer & Cooling

Repairing the pump or topping up the oil is the usual response when thermal oil loses flash point and the pump starts to shake, but if the oil now holds more components that boil easily, or the suction side is short of pressure, the shaking returns even after the pump is fixed. What actually lies behind it can be light ends from thermal cracking, water that got in, a blocked expansion tank vent or a low tank level, solvents or other foreign fluids mixed in, or running too hot, and sometimes two or more at once.

Background

The circulation pump sounds as if gravel were rolling through it, the discharge pressure gauge needle trembles, and the heater outlet temperature swings. An oil analysis report received around the same time shows a flash point well below that of the fresh oil. The two symptoms look unrelated, but they can share a root: the oil now holds more components that boil easily, or conditions at the pump suction have made the oil more likely to boil.

Left alone, the losses are large. In a pump where bubbles collapse, the impeller erodes and the vibration goes on, and if the pump vapour-locks and circulation stops, the heater tubes can overheat within a very short time. The easily boiling components also leave through the vents as flammable vapour that can start a fire outside the system (Ennis, 2009). These light ends are flammable liquids with properties similar to petrol, and when too much builds up they can damage equipment or, released to atmosphere, cause a fire or explosion (HDI, 2019).

Flash point is the lowest temperature at which vapour from a liquid mixes with air to form a mixture that can ignite (HDI, 2019). The flash point of a liquid made of several components is set by the vapour pressure each one contributes, so mixing in a component with a high vapour pressure drags it down (Liaw et al., 2002). The pump faces the same vapour pressure problem. When pressure at the impeller inlet drops to the oil's vapour pressure, the oil boils on the spot and forms bubbles, which collapse as they move into higher pressure and cause noise, vibration, loss of head and erosion; this is cavitation. The margin of suction pressure over vapour pressure is the net positive suction head, NPSH, and that margin shrinks when the vapour pressure rises or the suction pressure falls (Gülich, 2020).

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: set the fresh oil's flash point and boiling range from the oil's technical data sheet, the TDS, beside the current analysis, and line up the records of pump suction pressure, expansion tank level and temperature, and heater outlet temperature with the times the pump shook.

Hypothesis 1: cracked light ends

This hypothesis gains weight in a system where the oil has not been changed for a long time and has only been topped up as it went down, where there is no device or routine for drawing off light ends, or where the heater has a local hot spot somewhere. Say a plant has received an analysis report every year and seen the flash point edging down, but let it pass because it stayed within limits. Then one summer the pump started to sound rough, and an oily smell that had not been there before now hangs around the expansion tank vent.

When heat breaks the oil's long molecules, short-chain fragments, the light ends, form along with gases such as hydrogen. Light ends lower the flash point and the autoignition temperature, and if they are not drawn off they gather as vapour in the system and cause vapour locking that blocks circulation (Ennis, 2009). The standard thermal stability test sorts breakdown products by weight into low boilers that boil below the fresh oil's initial boiling point, gases such as hydrogen and methane, high boilers and so on (ASTM International, 2020b). Because light ends have a high vapour pressure, whatever amount is mixed into the oil pulls the mixture's flash point down, and for the same reason they are the first to boil at the pump suction.

Flash point is comparable only when measured the same way. In-service oil is usually tested in the Pensky-Martens closed cup, a standard that covers both new and in-use lubricating oils (ASTM International, 2020c). Measure the amount of light ends against fresh oil by simulated distillation (Gamble, 2023), and look at the trend of flash point and light ends year by year. One risk engineering guideline treats light ends above 3% as excessive (HDI, 2019).

If the finding is that light ends have built up, give them a way out. Light ends must be boiled off at set intervals or sent out by an automatic separation step, and the collected condensate must be handled as a petrol-like flammable liquid, with the point where it is collected managed as an explosion hazard area (HDI, 2019). In a system that runs hot enough for fast breakdown, continuous flash distillation of a small side stream is another option (Ennis, 2009). Drawing them off alone only lets them build up again, though, so look at the same time for the condition behind the cracking, such as film or operating temperature.

Hypothesis 2: water in the oil

Water shows up most readily after maintenance. It gets in when pipework washed with water is not fully dried, when water from an exchanger test is left behind, when rain seeps into top-up drums stored outdoors, and when a tube leaks in a steam or cooling water exchanger on the process side. A system being heated up again after maintenance reaches the boiling point of water, and the pipework crackles like water dropped into a chip pan while the pump pressure swings widely.

A thermal oil system runs above the boiling point of water, so any water that gets in turns to steam inside the system. Water dissolves slightly in most thermal oils, fresh oil already contains a trace, drums stored outdoors can hold much more, and drums have been found with free rainwater in them. Water boiling all at once can overpressure the expansion tank and other components, large amounts cause vapour locking, and if the pump vapour-locks, the heater coil can overheat within a very short time (Ennis, 2009). A pump with vapour at its suction cannot deliver its head through an impeller built for liquid alone, and it shakes (Gülich, 2020). Water does not burn and so does not pull the flash point down; if the flash point is unchanged but the pump shakes only during warm-up, the weight shifts towards this hypothesis.

Measure water by Karl Fischer titration; in high-temperature thermal oil service, water must be kept low (Gamble, 2023). Draw samples at the same point and cool them first, so the water does not flash off and results stay comparable. During warm-up, log whether the crackling and pump pressure swings start near the boiling point of water and die down after a while. Search the maintenance records for jobs that used water, check where top-up drums were stored, and see whether any exchanger has process steam or cooling water flowing at higher pressure than the oil side.

Water has to be boiled out slowly. Heat at low fire with a bypass flow through the expansion tank to let the steam out; one recommendation is to close the bypass only after the water is gone and the system has stayed above 110 °C for at least an hour (Ennis, 2009). Another guideline says to keep boiling out until no further pressure swings appear with the whole system heated (HDI, 2019). From then on, keep drums indoors, dry the system with hot air after any maintenance that used water, and repair leaking exchangers.

Hypothesis 3: tank vent or level

The expansion tank takes up the oil's changes in volume, but it is also the exit through which light ends, water and gases leave the system, and the height that supplies pressure to the pump suction. Exit and height both falter when the vent line or condenser narrows with oily residue, when the screen fitted over the vent outlet clogs, when the bypass flow to the tank is closed too early, and when leaks or light end draw-off have dropped the tank level. Imagine the level gauge sitting lower than usual, with the pump sounding rougher on the days the tank level is lowest.

Light ends cause vapour locking if not properly vented, and the expansion tank is designed to stay unlagged and below system temperature so that it acts as a condenser in normal operation (Ennis, 2009). The tank's low level limiter guards against the system running dry and also keeps enough suction pressure at the circulation pump (HDI, 2019). In synthetic fluid systems at solar power plants, venting cut the hydrogen dissolved in the oil by 10 to 75%, and in a model, simply bringing the oil to equilibrium with the gas in the vessel vapour spaces lowered the hydrogen concentration sharply (Jung & Spenke, 2022). When the way out is blocked, what should have left stays in the system and boils at the pump suction.

Much of the checking can be done on a walk round. See whether the vent line, condenser and vent screen are open, and whether liquid collects in the condensate pot and, if so, since when it has grown. Set tank level and temperature beside pump suction pressure and the times the pump noise rose, and check whether gas comes out of the bleed valves at the system's high points. Gas trapped at high points can also damage pumps and overheat heater tubes (Ennis, 2009).

Restore the exit and the height together. Clean blocked vent lines and condensers, run the vent as a fully welded line to a safe point outdoors, keep ignition sources away from its outlet and the condensate collection point, and screen it against rain and insects (HDI, 2019). Set cold and hot reference levels for the tank and hold them, topping up only into the cold tank. Close the start-up bypass only after water and light ends have been driven off (Ennis, 2009).

Hypothesis 4: foreign fluids

If the flash point dropped in one step rather than gradually, suspect something that came in from outside first. This covers a system flushed with a solvent such as acetone to dissolve hardened residue and not fully drained afterwards, a leaking process exchanger letting in light process material such as a solvent or monomer, and top-up with a different oil of lower flash point. Consider a first week back after cleaning in which the vent smells of solvent, the pump starts to shake, and a sample taken that week shows a flash point far below the last analysis.

The flash point of a liquid mixture can be calculated from the vapour pressures of its components and how they mix. In a study that compared such a model with measurements, mixtures far from ideal behaviour sometimes showed a flash point lower than that of either pure component (Liaw et al., 2002). So a low flash point liquid left behind drags the flash point of the whole charge towards its own, in step with the amount left, and that high vapour pressure component boils first at the pump suction and invites cavitation. Flushing solvent must be drained and the system rinsed with water to remove what remains before recommissioning, and leftover cleaning fluid also speeds up oil degradation (Ennis, 2009).

Begin by matching the timing. Check in the records whether the drop in flash point coincides with cleaning, a top-up or process-side maintenance, and analyse a fresh oil sample and the current oil together in the same laboratory. A peak absent from the fresh oil appearing below its boiling range in simulated distillation or gas chromatography may be the foreign material, and identifying it calls for a compositional analysis. The test items for judging whether an in-service heat transfer fluid can stay in use are set out in a standard (DIN, 2000). Consider a leak test on any exchanger where the process side runs at higher pressure than the oil side.

Once a foreign fluid is confirmed, cut off its source and decide what to do with the oil. Repair the leaking exchanger, write solvent draining, water rinsing and drying into the cleaning procedure, and label top-up stock so that only the same product is used. When the amount is large or the material unknown, review replacement with the supplier, and until then assess separately the risk if oil with a lowered flash point leaks out.

Hypothesis 5: running too hot

When the set point went up with a product change, when the system runs unpressurised close to the oil's initial boiling point, or when the process suddenly takes less heat and the outlet temperature jumps, look at the operating point itself. In a plant that raised its set point for a new product in autumn, the pump noise grows each late afternoon when the outlet temperature peaks for the day and settles down at night.

Vapour pressure climbs steeply with temperature, so at the same suction pressure, the hotter the oil, the smaller the NPSH margin and the closer the pump comes to cavitation (Gülich, 2020). A heat transfer installation can use oil above its initial boiling point, but the safety requirements and tests covering that condition are set out separately in the standard for heat transfer installations (DIN, 2015). High temperature also adds light ends. In a study of a synthetic fluid, hydrogen from breakdown rose with temperature and with time (Jung & Senholdt, 2020). Running hot thus works along two paths at once, cutting the suction margin straight away and slowly lowering the flash point as light ends build up.

Overlay the times the pump shook with the outlet temperature and pump suction pressure records, and this hypothesis shows itself quickly. If the shaking comes and goes with the temperature peaks, the operating point is the place to look. Then compare the peak operating temperature with the TDS maximum and boiling range, and compare the NPSH margin calculated from the oil's vapour pressure at that temperature with the pump maker's required NPSH. Check also whether there is a monitor that warns when suction pressure falls too far (HDI, 2019).

The operating point offers two levers: the temperature and the suction margin. One guideline keeps the maximum operating temperature at least 30 K below the oil's maximum permitted feed temperature (HDI, 2019). If the temperature cannot come down, review with the designer ways to raise suction pressure, such as the height and level of the expansion tank or pressurising it with inert gas, and weigh up with the supplier a change to an oil with a higher boiling range. Light ends that have already built up at high temperature must be drawn off before the flash point recovers.

Finding the cause

Start with one sample and a few records. Measure flash point and water on the same sample, and overlay the times the pump shook on outlet temperature, suction pressure and expansion tank level. The vent line and condensate pot can be inspected without stopping the plant, so look at them the same day. These three easy checks rule out several of the five hypotheses early.

Next is the shape of the symptom. A flash point that slips a little each year with light ends growing alongside points to cracked light ends, and a drop in one step right after cleaning or a top-up points to a foreign fluid. A sound flash point with the pump shaking only during warm-up near the boiling point of water suggests water; shaking that follows the temperature peaks suggests running too hot; and shaking concentrated on days of low tank level or a blocked vent suggests the expansion tank.

If that does not settle it, change one thing at a time. Lower the outlet temperature one step and listen for a change in pump noise, clear a blocked vent and boil out with the bypass flow to the tank, or fill the tank to its reference level. Only one change at a time shows which one worked, and afterwards measure flash point and suction pressure again by the same method as before.

The final check is laboratory analysis. Compare the amount and boiling distribution of light ends with fresh oil by simulated distillation, and add the tests needed by following the standard guide for choosing tests on in-service heat transfer fluids (ASTM International, 2020a). The job is done only when, after light ends are drawn off or the cause is fixed, the flash point moves back towards that of fresh oil and pump suction pressure and noise stay steady even as temperature rises.

The five hypotheses can arrive tangled together. High operating temperature makes light ends, a system with blocked venting cannot let them out so they build up, and water or solvent left after maintenance cuts an already narrow suction margin once more. In such cases restore the vent path and tank level first, lower the operating temperature, then draw off light ends and analyse the oil again, because while there is no way out, easily boiling components build up again whatever else is fixed.

Limits and cautions

Flash point, boiling range, maximum operating temperature and control values for light ends and water differ by oil, so numeric decisions follow the oil's TDS and the supplier's criteria, and required NPSH follows the pump maker's data. Flash point values differ by test method, so compare only values measured the same way. Design changes that add pressure, changes to tank height and oil replacement are decided with the designer under the standard for heat transfer installations and local regulations.

Oil with a lowered flash point is more dangerous when it leaks. In a system run above its initial boiling point with a flash point below 220 °C, part of any leaking oil evaporates, and a large leak can take a room to the lower explosive limit (HDI, 2019). While the cause is being found, check the shaking pump's seal for leaks often, because hot oil sprayed from pump seals has led to significant fires (Ennis, 2009). Cool samples before drawing them, and around vent outlets and when handling condensate, wear the protective equipment set out in the product's safety data sheet, the SDS, and keep ignition sources away.

Sources

  1. ASTM International. (2020a). ASTM D5372-20, Standard guide for evaluation of hydrocarbon heat transfer fluids. https://store.astm.org/d5372-20.html
  2. ASTM International. (2020b). ASTM D6743-20, Standard test method for thermal stability of organic heat transfer fluids. https://store.astm.org/d6743-20.html
  3. ASTM International. (2020c). ASTM D93-20, Standard test methods for flash point by Pensky-Martens closed cup tester. https://store.astm.org/d0093-20.html
  4. Deutsches Institut für Normung [DIN]. (2000). DIN 51529:2000-11, Testing of mineral oils and related products – Testing and evaluation of used heat transfer fluids. https://www.dinmedia.de/en/standard/din-51529/21165384
  5. Deutsches Institut für Normung [DIN]. (2015). DIN 4754-1:2015-03, Heat transfer installations working with organic heat transfer fluids – Part 1: Safety requirements, test. https://www.dinmedia.de/en/standard/din-4754-1/225280007
  6. Ennis, T. (2009). Safety in design of thermal fluid heat transfer systems. In Hazards XXI (IChemE Symposium Series No. 155, pp. 162–169). Institution of Chemical Engineers. https://www.icheme.org/media/9653/xxi-paper-025.pdf
  7. Gamble, C. (2023, August 1). Facts at your fingertips: In-service heat-transfer-fluid testing. Chemical Engineering. https://www.chemengonline.com/facts-at-your-fingertips-in-service-heat-transfer-fluid-testing/
  8. Gülich, J. F. (2020). Centrifugal pumps (4th ed.). Springer. https://doi.org/10.1007/978-3-030-14788-4
  9. HDI Global SE [HDI]. (2019). Risk engineering guideline: Heat transfer oil systems. HDI Risk Consulting. https://www.hdi.global/globalassets/_local/international/downloads/group_heat-transfer-oil-systems/20190305_403-hrc-reg130gb_-heat_transfer_oil_systems.pdf
  10. Jung, C., & Senholdt, M. (2020). Comparative study on hydrogen issues of biphenyl/diphenyl oxide and polydimethylsiloxane heat transfer fluids. AIP Conference Proceedings, 2303, 150009. https://doi.org/10.1063/5.0028894
  11. Jung, C., & Spenke, C. (2022). Hydrogen monitoring and control in the heat transfer fluid of parabolic trough plants. AIP Conference Proceedings, 2445, 100003. https://doi.org/10.1063/5.0085825
  12. Liaw, H.-J., Lee, Y.-H., Tang, C.-L., Hsu, H.-H., & Liu, J.-H. (2002). A mathematical model for predicting the flash point of binary solutions. Journal of Loss Prevention in the Process Industries, 15(6), 429–438. https://doi.org/10.1016/S0950-4230(02)00068-2

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.