BlogApplication notes
Why does transformer oil gas analysis show acetylene and hydrogen?
- Type
- Application notes
- Published
- 23 November 2026
- Prepared by
- Jonghwan Moon
- Product group
- Equipment/Service Lubricants
Acetylene and hydrogen in a transformer oil gas analysis are easily taken at once as proof of internal arcing, but the same gases can come from a past event, the tap changer, the oil itself or the sampling as well as from a fault in progress, so one value cannot settle the cause and the rate of increase must be read with it. What actually lies behind them can be arcing, partial discharge, stray gassing oil, tap changer leakage, sampling or lab error, or residual gas from a past fault, and sometimes two or more at once.
Background
The routine insulating oil analysis report arrives, and the acetylene column, empty last time, now shows a number, with hydrogen up as well. The transformer looks normal from outside and no protection relay has operated. The operations team asks whether it must come off line now or can be watched until the next analysis.
Both choices are costly. If acetylene keeps rising, a high-energy arc may be active inside the transformer, and running on can end in a tank rupture that spreads burning oil over a wide area (USBR, 2003). If instead the cause lay in the tap changer or the sample, taking a large transformer out and opening it wastes the outage and the cost. So the first task is to find where the numbers on the report came from.
Insulating oil and paper break down and give off gas under electrical and thermal stress, and which gases form, and how much, depends on the energy and temperature at the spot. The international guide uses this gas make-up to sort faults into partial discharge, low-energy and high-energy discharges, and overheating in three temperature bands (IEC, 2022). In a review of inspected faults, partial discharges in gas produced mainly hydrogen, often in large amounts, while small breakdowns in oil produced relatively more acetylene (Duval, 2002). Acetylene above a few ppm points to high-energy arcing, but a very hot thermal fault at 500°C or more can also make trace amounts (USBR, 2003).
When this report comes in, the technical team sets up the six hypotheses below and eliminates them one by one. The first check is always the same: set this result beside earlier analyses of the same transformer, and line it up with the sampling point and date, the laboratory, and any load changes, lightning, faults or maintenance in between.
Hypothesis 1: arcing
Arcs form where the current path has deteriorated. Typical spots are loosened lead connections, worn tap selector contacts, weakened insulation between turns, and conductors shifted by a through-fault, and they can show up in high-load seasons or after a short-circuit event. The picture for this hypothesis is acetylene appearing for the first time in a routine analysis, then a resample a few weeks later showing acetylene, hydrogen and ethylene all higher.
At an arc the oil is briefly heated to very high temperatures, its hydrocarbon chains break, and the fragments recombine as hydrogen and acetylene. Acetylene stands out among the gases formed at such high energy, so the international guide separates low-energy from high-energy discharges by gas ratios such as acetylene to ethylene and methane to hydrogen (IEC, 2022). In a review of inspected cases, high-energy discharges were confirmed by molten copper or extensive winding damage, and low-energy discharges such as tracking and small arcs also produced enough gas to be picked up readily by analysis (Duval, 2002).
The rate matters more than the value. Once acetylene appears, sample weekly, or daily if needed, to see whether new acetylene is forming. If it is not increasing and the level stays below the guide's highest condition, operation can continue, but a steady rise means an arc is active inside (USBR, 2003). Read the fault type from gas ratios and the triangle chart together; ratio-based interpretation codes were drawn up for this purpose (Rogers, 1978). Electrical tests such as winding resistance and turns ratio, checked tap position by tap position, help narrow down where the arc is.
If acetylene is rising, whether to keep operating is decided with transformer specialists and the manufacturer. One public-sector guide advises taking the unit out of service if acetylene rises by more than 10 ppm a month (USBR, 2003), and each operator should set its own criteria from published guides and expert advice. Once the cause has been found and repaired by internal inspection, treat the oil and establish a new baseline.
Hypothesis 2: partial discharge
Partial discharge is small discharges repeating in one part of the insulation without the whole of it breaking down. It forms readily in voids in the paper, bubbles left by incomplete vacuum filling, damp insulation and sharp edges where the electric field concentrates, and it is a suspect in newly installed or refilled transformers too. Picture a transformer refilled not long ago, where hydrogen alone climbs noticeably, methane follows a little, and acetylene barely shows.
Corona-type partial discharges in gas are tiny, around 10 to 30 pC, but they run for long periods across large volumes of paper and so produce a great deal of hydrogen, which analysis picks up readily. The same review notes that sparking discharges in oil and corona-type discharges in gas are chemically very different, that larger discharge amplitudes pull the gas make-up towards low-energy discharge, and that partial discharges become harmful when they damage the paper or create bubbles in the oil (Duval, 2002). So when a hydrogen-dominated result begins to pick up small amounts of acetylene, it is worth asking whether the discharges are growing.
A result dominated by hydrogen first has to be split between partial discharge and low-temperature gassing of the oil. Separate triangle charts for low-temperature faults, drawn with hydrogen, methane and ethane, were proposed so that these two fall into different zones (Duval, 2008). The next step is to confirm with electrical or acoustic partial discharge measurement whether discharges are really present and roughly where. If moisture is a candidate, measure the water content of the oil as well.
Once partial discharge is confirmed, the path depends on its cause. Bubbles or moisture can be reduced by vacuum degassing and drying the oil; a defect in the insulation structure calls for agreeing the scope of repair with the manufacturer. Either way, follow hydrogen and acetylene trends more closely than usual, and if acetylene starts rising too, move on to the judgement for arcing.
Hypothesis 3: stray gassing oil
Oil can give off gas at ordinary operating temperatures with no fault present. Look at this hypothesis for new transformers, transformers whose oil has been replaced with new oil, and oil dosed with a metal passivator against corrosive sulphur. Think of a newly commissioned transformer whose hydrogen rises a little at each analysis for some months, then stops climbing and levels off.
This is called stray gassing. Some oils give off mainly hydrogen and methane the first time they are heated below 300°C, rising to a plateau set by the oil type, typically 5 to 250 ppm, after which heating them again produces no more. The same review relates this behaviour to the refining technique and reports that it stops after some months in service or after heat treatment of the oil (Duval, 2002). The standard test method defines it as gas formed in the oil from heating, contamination or both, and explains that some severely hydrotreated oils and contaminated oils can give off gas at lower temperatures than expected and so suggest a fault that is not there (ASTM International, 2020).
One study found that oils of different molecular structures gave different gas patterns in stray gassing tests (Tomita & Ito, 2019), and in accelerated ageing of oil and paper at 130°C, oil containing a metal passivator showed rising hydrogen, carbon monoxide and carbon dioxide (Gao et al., 2021). The gases stray gassing mainly gives, however, are hydrogen and methane, so where acetylene also appears, check separately whether another hypothesis overlaps.
The check runs along two lines, records and testing. Look at when the oil was changed, whether a passivator was added, and whether the hydrogen trend levels off at a plateau. A standard test that heats a sample of the oil in service at 120°C for a long period and measures the gas formed, under both dry air and dry nitrogen, shows the oil's own tendency (ASTM International, 2020). See also whether the result falls in the stray gassing zone of the low-temperature triangle chart (Duval, 2008). If the oil is confirmed as the source, record that and its plateau as the basis for later interpretation, and decide with the oil supplier whether heat treatment or an oil change is needed.
Hypothesis 4: tap changer leakage
An on-load tap changer that breaks current in oil makes a small arc at every tap change, so the oil in its compartment normally contains acetylene. Where the tap changer compartment sits inside the main tank and the seal between them ages, that oil or gas can pass into the main tank, so look at this hypothesis for older transformers and distribution transformers with frequent tap operations. A case in point is a substation transformer that changes taps often, where acetylene in the main tank creeps up while the other hydrocarbons barely move.
In gas terms, a tap changer's normal current breaking is a low-energy discharge that makes mainly acetylene, so interpreting tap changer oil has to allow for this large background of gas (Duval, 2002). That is also why a separate guide covers gas analysis of these compartments alone (IEEE, 2016). In a study of 175 transformers at one distribution operator, assessed against the guides and expert judgement, 26 were found to have main tank oil contaminated by tap changer gases (Bustamante et al., 2020). Read from the main tank result alone, this acetylene easily looks like arcing.
The most direct check is to draw separate samples from the main tank and the tap changer compartment on the same day and compare them. See whether the main tank acetylene trend moves with the tap operation count, and whether the two conservator levels move in opposite directions, a sign of oil passing from one to the other. Existing interpretation methods were not designed to single out this contamination, so methods adding a contamination zone to the triangle and pentagon charts have been proposed (Bustamante et al., 2024).
Once a leak path is confirmed, repair the seals and barrier following the tap changer maker's procedure. After the repair, degas the main tank oil to clear the gas that came across, set a new baseline, and analyse again at the usual interval. Until the repair, note the contamination alongside every main tank interpretation so changes in acetylene are not mistaken for arcing.
Hypothesis 5: sampling or lab error
A gas analysis is the number from one bottle of sample, so if that bottle does not truly represent the inside of the transformer, the result is off too. This is especially so when the person or point sampling changes, a bubble gets into the syringe, delivery is delayed, or the laboratory or gas extraction method changes. An example is a report the month after a new person took over sampling, with several gases jumping at once, while a resample the same week came back at the usual values.
Gas in oil divides between the oil and any gas it touches according to an equilibrium set by Henry's constants, and dissolved gas molecules move by diffusion, to an extent that depends on the gas and the temperature (Riedmann et al., 2022). So if a bubble forms in the syringe or the oil is exposed to air for long, gas moves into the bubble, and conversely oil left over from another sample or in the sampling line can add gas that was not there. In the laboratory, gas is extracted by vacuum extraction, stripping with a carrier gas or headspace partitioning and then measured by gas chromatography (IEC, 2023), so a change of method or equipment can give different values for the same oil.
The rule is never to diagnose from a single analysis, since a sample can be mishandled or mislabelled in the field or the laboratory (USBR, 2003). Resample a doubtful result from the same point following the set procedure, and if possible split it into two for the same laboratory. Log oil temperature, sampling point, whether the syringe held a bubble, and dispatch and analysis dates, and confirm that the laboratory follows the standard method for measuring dissolved gases by gas chromatography (ASTM International, 2017).
If the cause lies with sampling, the remedy is to fix the procedure. Set out the sampling point and order, the volume of oil to flush to waste and how to handle the syringe on one procedure sheet, and when the job changes hands, sample together during the handover. Keep the laboratory and method unchanged where possible; if they must change, send samples to both over an overlap period to measure the difference before joining up the trend.
Hypothesis 6: residual old gas
Gas in oil does not vanish as soon as its cause has gone. Look at this hypothesis after one-off events such as a nearby lightning strike, a through-fault, an earlier internal fault, or welding done with oil in the tank. In a transformer that suffered a through-fault last year, acetylene may sit at nearly the same value over several analyses. The other gases hardly move either.
A one-off arc from a nearby lightning strike or a high-voltage surge can also make a small amount of acetylene, and if no new acetylene forms afterwards, the remaining value may simply be the trace of that event. Welding with oil in the tank can make gas from the heat, so samples before and after the welding are needed to tell which gases came from it (USBR, 2003). How long residual gas stays depends on the transformer's design. One analysis notes that in free-breathing transformers, gas can escape or dissolve over time and shift the basis for interpretation (Riedmann et al., 2022).
The key is the shape of the trend. A jump right after an event followed by a flat or slowly falling line can be read as residual gas; a fresh rise is taken to mean new gas is forming. The US guide likewise asks for the change and the rate of increase to be read alongside the value itself (IEEE, 2019). Noting the dates of events such as lightning, through-faults, welding and oil treatment beside the results makes this judgement much easier.
If the gas is judged residual, record its value as the new baseline and measure later changes against it. If residual gas keeps clouding interpretation, the oil can be degassed and a fresh baseline set. Either way, analyse a few more times at shorter intervals than usual to confirm that the trend has truly stopped before going back to the normal schedule.
Finding the cause
The six hypotheses need not all be checked at once. Clear them starting with what can be done without taking the transformer off line. The very first step is to resample by the set procedure and see whether the result repeats; next come event and maintenance records, a sample from the tap changer compartment, and the history of oil changes and additives. Electrical tests and internal inspection come after that.
The shape of the gas make-up points to the cause. A result led by hydrogen, with a little methane and hardly any acetylene, comes down to partial discharge or stray gassing of the oil, and a history of new oil or passivator weighs towards the oil. Acetylene rising together with hydrogen and ethylene suggests arcing, while acetylene alone rising with tap operations suggests oil from the tap changer. Acetylene sitting flat after an event suggests residual gas, and values that do not repeat on resampling point to sampling and analysis.
Next comes time. One field guide holds that a sudden increase and the rate of gas generation matter more for judging a transformer than the accumulated amount (USBR, 2003). Shorten the analysis interval to suit the suspected hypothesis, and log tap operation counts, load and oil temperature in the same table to see what the increase moves with. If stray gassing is suspected, run the standard heating test on the same oil as a control.
The final check is to use interpretation methods side by side and back them with electrical tests. Read the international guide's ratio method and triangle (IEC, 2022), the low-temperature triangle charts (Duval, 2008) and the US guide's concentration and rate criteria (IEEE, 2019) together, and confirm that they point the same way. If they point to arcing and the rise continues, move on to partial discharge measurement, winding resistance and turns ratio tests, and internal inspection if needed.
The hypotheses can overlap. A new arc can add to acetylene that came from the tap changer or remained from a past event, and stray gassing of the oil can mask hydrogen from small partial discharges. In such cases, take the known share, residual gas or gas from the tap changer, as the baseline and read only the increase above it. While the baseline is unsettled, do not call a small increase either a fault or normal; shorten the interval and keep watching.
Limits and cautions
Gas concentration limits, rate criteria and analysis intervals differ with the transformer's type, age, size, oil preservation system and the operator's own criteria, so numeric decisions follow the international and US guides, the transformer manufacturer and specialist advice. If acetylene is rising, do not wait for the next routine analysis; decide on continued operation with a specialist at once. The above assumes mineral insulating oil, and interpretation can differ for other insulating liquids such as esters (Duval, 2008).
Sampling an energised transformer carries risks of electric shock, burns and oil spills, so it is for trained staff keeping to set safety clearances and procedures. Handle the oil with gloves and eye protection as its SDS requires, and clean up spills at once. Acetylene and hydrogen are flammable, so keep ignition sources away when drawing gas from a gas-collecting relay.
Sources
- ASTM International. (2017). ASTM D3612-02(2017), Standard test method for analysis of gases dissolved in electrical insulating oil by gas chromatography. https://store.astm.org/d3612-02r17.html
- ASTM International. (2020). ASTM D7150-13(2020), Standard test method for the determination of gassing characteristics of insulating liquids under thermal stress. https://store.astm.org/d7150-13r20.html
- Bustamante, S., Manana, M., Arroyo, A., Laso, A., & Martinez, R. (2020). Determination of transformer oil contamination from the OLTC gases in the power transformers of a distribution system operator. Applied Sciences, 10(24), 8897. https://doi.org/10.3390/app10248897
- Bustamante, S., Martinez Lastra, J. L., Manana, M., & Arroyo, A. (2024). Distinction between arcing faults and oil contamination from OLTC gases. Electronics, 13(7), 1338. https://doi.org/10.3390/electronics13071338
- Duval, M. (2002). A review of faults detectable by gas-in-oil analysis in transformers. IEEE Electrical Insulation Magazine, 18(3), 8–17. https://doi.org/10.1109/MEI.2002.1014963
- Duval, M. (2008). The Duval triangle for load tap changers, non-mineral oils and low temperature faults in transformers. IEEE Electrical Insulation Magazine, 24(6), 22–29. https://doi.org/10.1109/MEI.2008.4665347
- Gao, S., Zhang, G., Zeng, X., Ke, T., & Liu, Y. (2021). Investigation on the effects of Irgamet 39 on stray gassing generation in the insulating oil. In 2021 IEEE Electrical Insulation Conference (EIC) (pp. 614–617). IEEE. https://doi.org/10.1109/EIC49891.2021.9612302
- Institute of Electrical and Electronics Engineers [IEEE]. (2016). IEEE guide for dissolved gas analysis in transformer load tap changers (IEEE Std C57.139-2015). https://doi.org/10.1109/IEEESTD.2016.7464235
- Institute of Electrical and Electronics Engineers [IEEE]. (2019). IEEE guide for the interpretation of gases generated in mineral oil-immersed transformers (IEEE Std C57.104-2019). https://doi.org/10.1109/IEEESTD.2019.8890040
- International Electrotechnical Commission [IEC]. (2022). IEC 60599:2022, Mineral oil-filled electrical equipment in service – Guidance on the interpretation of dissolved and free gases analysis.
- International Electrotechnical Commission [IEC]. (2023). IEC 60567:2023, Oil-filled electrical equipment – Sampling of free gases and analysis of free and dissolved gases in mineral oils and other insulating liquids – Guidance.
- Riedmann, C., Schichler, U., Häusler, W., & Neuhold, W. (2022). Online dissolved gas analysis used for transformers – possibilities, experiences, and limitations. e & i Elektrotechnik und Informationstechnik, 139(1), 88–97. https://doi.org/10.1007/s00502-022-00992-8
- Rogers, R. R. (1978). IEEE and IEC codes to interpret incipient faults in transformers, using gas in oil analysis. IEEE Transactions on Electrical Insulation, EI-13(5), 349–354. https://doi.org/10.1109/TEI.1978.298141
- Tomita, H., & Ito, T. (2019). Effect of molecular structures of insulating oil on stray gassing. In 2019 IEEE 20th International Conference on Dielectric Liquids (ICDL) (pp. 1–4). IEEE. https://doi.org/10.1109/ICDL.2019.8796698
- U.S. Bureau of Reclamation [USBR]. (2003). Transformer diagnostics (Facilities Instructions, Standards, and Techniques Volume 3-31). U.S. Department of the Interior. https://www.usbr.gov/power/data/fist_pub.html