Adding a demulsifier additive is the usual response when water will not separate, but such additives give uneven results and can even increase emulsion. What actually holds the water can be accumulated oxidation products, grease or preservative that got in, detergents, microbial growth, weak purification or short residence time, and two or more can act together.

Background

The sight glass on the turbine oil reservoir is milky, and opening the tank bottom drain yields only a little water. The purifier runs nonstop, yet the water figure in the oil analysis report barely comes down. Water finely dispersed in the oil causes corrosion and cannot act as a lubricant, so it is a state to avoid in turbine oil (Kamal, 2013). Oil that holds water also changes in how it lubricates and carries heat away, and when that water reaches the bearings and control system, shaft stability and control can suffer (Winslow et al., 2005).

Water in oil takes three forms: dissolved water that cannot be seen, emulsified water spread as very small droplets, and free water that collects separately at the bottom. Most industrial oils are made to release water so that free water can be drained from the system (Holdmeyer, 2022). In a steam turbine, water keeps entering in small amounts through steam passing the shaft gland seals, cooler leaks, plant cleaning, wet makeup oil and condensation of moisture from the air. The water level in the system settles where input and output are equal, and output is set by the oil's water-shedding ability and the purification equipment. So if water creeps up with no new leak, the oil's water separability may have worsened or the purification equipment may have lost efficiency (Kamal, 2013).

How readily an oil releases water is measured with the water separability test. Oil and water are stirred together, and the test records how many millilitres separate as oil, water and emulsion layer, and how long that took (ASTM International, 2021). An oil with good water separability breaks cleanly from water in the reservoir so the water at the bottom can be drained, but this property breaks down when there is too much water or when polar contaminants and impurities are present (Kamal, 2013). Polar substances are those whose molecules carry an uneven charge, so they get along with both water and oil.

In such cases the technical team sets up the six hypotheses below and rules them out one by one. The start is always the same: measure water separability and water content on a reservoir sample and a new oil sample side by side, compare them with the values in the oil's technical data sheet, the TDS, and match the time water stopped separating against the records of makeup, maintenance, cleaning and purification equipment.

Hypothesis 1: oxidation products

This hypothesis comes to mind first with oil left unchanged for years, a system that has run with high bearing temperatures, or a turbine whose oil has darkened and where varnish has started to come up. Systems that carried a lot of water for long periods belong here too. Picture a steam turbine running on the same oil for several years. When the oil was new, a small cooler leak left water pooled at the tank bottom where it was easy to drain; this year a similar leak leaves the sight glass cloudy for days.

Oil reacts with oxygen to form sludge, resin-like material and acids, and the reaction speeds up when metal contaminants and water are present (Hong & Jang, 2023). One study oxidised a turbine oil at 150 °C with a copper catalyst and blown air, then ran the water separability test: the emulsion layer left after 30 minutes grew from 7 mL in oil oxidised for 2.5 hours to 64 mL in oil oxidised for 15 hours, and viscosity rose with it (Nimr et al., 2026). The same study explains that polar oxidation products such as resins, asphaltenes and acids agglomerate and hold water droplets in the oil. A large amount of oxidation products can worsen water separability, and an industry report notes that highly refined Group II and III base oils retain water separability less well than Group I (TMI Staff, 2014).

Checking begins with the trend in the numbers. Put the in-service water separability results beside the new oil value and earlier results, and see whether they worsened gradually over years. Oxidation products that float in the oil without dissolving are measured with membrane patch colorimetry, or MPC, a test that ages the oil under set conditions, filters it through a fine membrane and measures how deep the colour left behind is (ASTM International, 2025b). If water separability and MPC have worsened together while the oil has darkened, this hypothesis gains weight.

If oxidation products look responsible, purification that strips out polar material can be reviewed with the supplier. Varnish removal units typically improve water separability, but the results have been reported as not consistent (TMI Staff, 2014). For heavily oxidised oil, cleaning the system and changing the oil under the guide for turbine lubrication systems is the surer path (ASTM International, 2023a). Manage bearing temperature and water together so the new oil does not go the same way.

Hypothesis 2: grease or preservative

If water stopped separating after maintenance, ask what went into the system at that time. Typical cases are grease applied to bearing housing joints or seals, new parts or pipe spools stored under a preservative coating and assembled without wiping, and a system filled with preservative oil for a long shutdown and then started without cleaning. Suppose spare parts taken from the store at an overhaul were assembled with preservative still on them, and every joint face was given a generous coat of grease. A few days after restart, with no cooler leak, the cloudiness in the sight glass refuses to clear.

Both carry molecules that wedge themselves between water and oil. The thickener that stiffens a grease is usually a soap of a metal such as lithium, aluminium, sodium or calcium, and a soap molecule has a strongly polar head and a hydrocarbon tail that gets along with oil (Van Rensselar, 2017). Preservative oils commonly contain barium, calcium or sodium sulfonates. These polar compounds are there to wet the metal surface and drive water off it, and sodium sulfonate is used to make preservatives that emulsify in water (McGuire, 2016). When molecules that hold water at one end and oil at the other settle at the oil-water boundary, droplets cannot merge, and sulfonate detergents of the same structure have been reported to destroy water separability at very low concentrations (TMI Staff, 2014).

The first clue is the date. Match the day water separability or the sight glass worsened against records of maintenance, part replacement and long shutdowns, and identify the grease and preservative used at the time. Elemental analysis of the in-service oil beside the new oil can reveal metals the new oil does not contain. Calcium is not normally in turbine oil formulations, so its appearance points to contamination (Malcolm, 2015). Depending on the grease and preservative, lithium, barium or sodium can also be clues. If a sample from the new oil drum passes the water separability test and only the reservoir sample fails, the material entered inside the system.

If only a little got in, decide with the supplier whether purification and a partial change will carry the oil. If water separability has collapsed, clean the system and change the oil under the flushing guide (ASTM International, 2023a). To stop a repeat, wipe preservative off new parts before assembly, apply grease thinly and only where it is needed, and flush a system that was laid up with preservative oil before starting it.

Hypothesis 3: detergent ingress

Look at this hypothesis when water separability collapses after the tank was wiped with a cleaner or the system was flushed, after a top-up from a drum or hose used for another oil, or after an engine oil or other oil containing detergent went in by mistake. Take a turbine whose reservoir was cleaned with a detergent cleaner at an overhaul, rinsed and filled with new oil. The first analysis shows a water separability result far below the TDS value, although the oil has only just gone in.

A well-known culprit is alkylbenzene sulfonate detergent. With a strongly polar sulfonate head and a tail that gets along with oil, this molecule can stay in the system after a flush and destroys water separability at very low concentrations. Calcium as calcium alkylbenzene sulfonate can affect water separability values at levels of 3 ppm, and some field tests found problems at even lower levels (TMI Staff, 2014). Another oil containing detergent does much the same when it is mixed in. Mixing incompatible oils can degrade water separability, foam inhibition, oxidation stability and rust protection, and can form precipitates that plug filters and passages (ASTM International, 2020).

Start with the records. Match the day water separability worsened against cleaning, flushing and top-up records, and identify the cleaner, the makeup oil, and the drums and hoses used. If elemental analysis shows calcium the new oil does not contain, suspect that another product got in. Introduction of a product with different additives is named as a common root of such results (Malcolm, 2015). Here too, testing a new oil drum sample beside a reservoir sample shows whether the material entered inside the system or came with the oil supplied.

Topping up with demulsifier additive to compensate is widely discouraged. Such additives often fail and have been reported to increase emulsion instead (TMI Staff, 2014). Once detergent residue is confirmed, flush the system again and change the oil under the flushing guide (ASTM International, 2023a). From then on, agree with the supplier which cleaners may be used on the turbine system, mark drums and hoses for turbine oil only, and if another oil must be mixed in, test the compatibility of the mixture first (ASTM International, 2020).

Hypothesis 4: microbial growth

Suspect microbes in systems where water lingers, in tanks and pipework with many slow-flow corners, and in equipment that stood idle for a long time. Steam turbines, and hydro turbines even more so, are continuously exposed to water ingress, and any equipment can become susceptible when shut down for long periods (ASTM International, 2023b). Think of the day before a restart after a long outage. At the oil-water boundary in the sight glass of the filter unit sits a translucent, jelly-like layer, and the filters plug sooner than usual.

Bacteria feed on water in the oil, on hydrocarbons, and on nitrogen, phosphorus and sulfur from the additives, and they thrive in slow-flow spots, on particle surfaces and at the oil-water boundary. Water at 0.5 mL per litre of turbine oil, or 500 ppm, is enough for growth, and the optimum temperature is 24 to 49 °C, with 49 °C being the normal operating temperature of a turbine lubrication system (Winslow et al., 2005). The same article explains that bacteria-laden oil holds water instead of readily releasing it, that the bacteria form emulsions as part of their life cycle, and that corrosive by-products and foam follow. The standard guide on microbial contamination also lists water emulsification as one form of biodeterioration (ASTM International, 2023b).

Several signs can be seen on the floor. Look for filters plugging often with jelly-like material, sluggish control response, emulsion that will not break, and failures in the water separability and foam tests. Bacterial contamination, however, can only be confirmed by laboratory analysis (Winslow et al., 2005). Take separate samples of the water at the tank bottom, the oil-water boundary layer and the material caught in the filters, and send them to a laboratory that does microbiological testing.

The condition operators can most easily influence is the water in the oil, so prevention starts with keeping water low. The sequence used on a system with confirmed contamination was: drain the contaminated oil, clean the tank, coolers and filter housings, flush at high flow and temperature with new flush oil, fill with dry new oil, and only then add the biocide the supplier recommends. Adding biocide first without the other steps can release a mass of dead bacteria at once and plug filters and control lines (Winslow et al., 2005).

Hypothesis 5: weak purification

The purification equipment deserves suspicion when maintenance of centrifuges, coalescers or vacuum dehydrators has slipped, when water ingress has grown but the purification equipment has not, or when the purifier runs only a few hours a day. A coalescer is a filter whose element gathers small droplets into large drops that fall out. Consider a case where no leak can be found, yet the water figure rises a little each month. The purifier is running, and samples of oil going into it and coming out of it look equally cloudy.

How water is removed depends on its form. Letting the oil stand without agitation so water settles removes free water only. A centrifuge or water-absorbing filter media works faster but removes only emulsified and free water, while a vacuum dehydrator removes dissolved water as well (Holdmeyer, 2022). Each device handles certain forms, so if the device does not match the form of the water that remains, the water figure stays put however long it runs. A coalescer loses water removal efficiency as contaminants deposit on its surface. If the oil's water separability has already failed, protection against water-related oxidation is tied to the performance of the purification equipment (Kamal, 2013).

The first check is to sample before and after the purification equipment and measure water by Karl Fischer titration, a method that uses a reagent reacting with water to measure very small amounts (ASTM International, 2025a). If the difference is small, look at the equipment. Check the vacuum level and temperature of a vacuum dehydrator, the bowl cleaning interval of a centrifuge, the differential pressure and change history of coalescer elements, and the daily running hours and flow against the records. Water limits vary by equipment and manufacturer, but an earlier edition of the in-service monitoring practice for turbine oils set 1,000 ppm as a warning level, and a target below 200 ppm is the usual recommendation for in-service oil (Kamal, 2013).

For an equipment cause, restore the maintenance intervals first. Clean the bowl, replace plugged elements, bring vacuum and flow back to their design values, and measure water before and after again. If the remaining water is dissolved or in very fine emulsion, a centrifuge alone will struggle to bring it down, so consider adding vacuum dehydration. If oil leaving the serviced equipment is still cloudy, the oil's own water separability has failed, so return to oxidation products and the materials that may have got in.

Hypothesis 6: short residence time

This covers running the reservoir close to its low level, the period after a modification that raised circulation flow, systems with small tanks, return oil falling from above the surface and stirring the tank, and damaged baffles inside the tank. Look at a system running near its low level after leaks drew the tank down without a top-up. Almost no water comes from the tank bottom drain, yet samples of oil going to the bearings are cloudy, and the surface below the return line is always churning.

Water needs time to leave the oil. Free water settles to the bottom when the oil is not agitated, and as oil temperature rises the oil can hold more dissolved water, while cooling lowers that amount so free water separates more readily (Holdmeyer, 2022). So how much water separability matters depends on the system's residence time and the amount of water coming in, and small sumps with short residence times need better water separability (Kamal, 2013). The time oil spends in the tank is the oil volume in the tank divided by the circulation flow, so a lower level or higher flow also shortens the time droplets have to reach the bottom. Water that does not get down in that time is drawn back into the pump and goes round the system again.

Residence time comes straight from a calculation. Divide the oil actually in the tank now by the circulation flow, and compare the result with the design value or the manufacturer's data. Check the level, the height of the return line outlet, the state of the baffles and the tank oil temperature as well. If a reservoir sample separates cleanly in the laboratory water separability test but water will not leave the oil in the plant tank, time and flow in the tank are more likely than the oil.

The first step is to bring the level back to normal. Route return oil below the surface, repair damaged baffles, and drain water collected at the bottom at set intervals. If tank size or flow cannot easily change, consider a separate purification loop that draws oil from the tank bottom, cleans it and returns it. Agree any change to tank or piping design with the equipment manufacturer.

Finding the cause

Six hypotheses do not mean six separate investigations. Rule them out starting with what is easy to check. Tank level, the return line, and the operating state and maintenance records of the purification equipment can be seen on the spot, and water before and after the purifier needs only two sample bottles. Clear the equipment causes such as tank time and purification first, then move on to the oil.

The fork in the road is the laboratory water separability test. If the reservoir sample separates cleanly in the test, the oil still knows how to release water, so look at what fails to give the water time and a path, such as residence time or purification. If the sample leaves an emulsion layer in the test too, the oil itself has changed, so look among oxidation products, grease and preservative, detergents and microbes.

The shape of the symptom separates those four. Gradual worsening over years with darker oil and a rising MPC points to oxidation products. A sudden collapse right after maintenance, cleaning or a top-up points to material that got in, such as grease, preservative or detergent, and a metal like calcium that the new oil lacks, found by elemental analysis, firms up that suspicion. A jelly-like layer with plugged filters after a long shutdown calls for microbiological testing.

If that still does not settle it, run control tests. Put a new oil drum sample and a reservoir sample into the water separability test on the same day at the same laboratory, and send samples from before and after the purifier with them. When changing things on the floor, such as restoring the level, servicing the purifier or a partial oil change, change one at a time, or there is no telling which one worked. The job is done only when the water figure and the water separability result have moved back towards the new oil values.

The hypotheses can overlap. Water that lingers in oil speeds up oxidation (Hong & Jang, 2023) and gives bacteria a place to grow (Winslow et al., 2005), and oxidised oil in turn holds water so it lingers longer. Group II and III oils have been reported to retain water separability less well (TMI Staff, 2014), so a small contamination arriving with short residence time makes the symptom larger. In such cases, put the water entry paths and the purification equipment right first and then look at the oil's properties, because while water keeps coming in, the effect of an oil change cannot be compared fairly.

Limits and cautions

Water separability pass criteria, water control values, purification operating conditions and tank residence time differ by oil, turbine and manufacturer, so numeric decisions follow the oil's TDS and the turbine manufacturer's criteria. The laboratory water separability test does not reproduce conditions inside the tank, so read its results as a trend against the new oil value and earlier results. Confirming microbes, choosing a biocide, and large flushes and oil changes are decided with the laboratory, the supplier and the equipment manufacturer.

Safety matters too. For biocides and cleaners, follow the product's safety data sheet, the SDS, for protective equipment and ventilation, and wear gloves and eye protection when handling oil and water with bacterial growth. Watch for hot oil and steam when opening a tank drain or sampling in service, and clean inside a tank only after following confined space procedures and locking out the equipment.

Sources

  1. ASTM International. (2020). ASTM D7155-20, Standard practice for evaluating compatibility of mixtures of turbine lubricating oils. https://store.astm.org/d7155-20.html
  2. ASTM International. (2021). ASTM D1401-21, Standard test method for water separability of petroleum oils and synthetic fluids. https://store.astm.org/d1401-21.html
  3. ASTM International. (2023a). ASTM D6439-23, Standard guide for cleaning, flushing, and purification of steam, gas, and hydroelectric turbine lubrication systems. https://doi.org/10.1520/D6439-23
  4. ASTM International. (2023b). ASTM D8506-23, Standard guide for microbial contamination and biodeterioration in turbine oils and turbine oil systems. https://store.astm.org/d8506-23.html
  5. ASTM International. (2025a). ASTM D6304-25, Standard test method for determination of water in petroleum products, lubricating oils, and additives by coulometric Karl Fischer titration. https://store.astm.org/d6304-25.html
  6. ASTM International. (2025b). ASTM D7843-25e1, Standard test method for measurement of lubricant generated insoluble color bodies in in-service turbine oils using membrane patch colorimetry. https://store.astm.org/d7843-25e01.html
  7. Holdmeyer, D. (2022, January). The basics of lubricant water contamination. Tribology & Lubrication Technology. https://www.stle.org/files/TLTArchives/2022/01_January/Lubrication_Fundamentals.aspx
  8. Hong, S.-H., & Jang, E. K. (2023). Varnish formation and removal in lubrication systems: A review. Materials, 16(10), 3737. https://doi.org/10.3390/ma16103737
  9. Kamal, G. (2013). In-service condition monitoring of turbine oils. In Proceedings of the Second Middle East Turbomachinery Symposium. Turbomachinery Laboratory, Texas A&M University. https://turbolab.tamu.edu/wp-content/uploads/2018/08/METS2Tutorial8.pdf
  10. Malcolm, M. (2015, June). Turbine oil analysis report interpretation. Tribology & Lubrication Technology. Summary of an STLE webinar by M. McMahon. https://www.stle.org/files/TLTArchives/2015/06_June/Webinars.aspx
  11. McGuire, N. (2016, September). Fundamentals of rust preventives used for temporary corrosion protection. Tribology & Lubrication Technology. Summary of an STLE webinar by G. Moran and B. Faber. https://stle.org/images/pdf/STLE_ORG/BOK/LS/Metalworking/Fundamentals%20of%20RUST%20PREVENTIVES%20used%20for%20temporary%20corrosion%20protection.pdf
  12. Nimr, N. K., Mohe, S. N., Nimr, H. K., & Mahmood, A. M. (2026). Nano-clay enhanced demulsification of oxidized turbine oils for improved water separation efficiency. Journal of Nanostructures, 16(2), 1602–1609. https://doi.org/10.22052/JNS.2026.02.012
  13. TMI Staff & Contributors. (2014, September 2). Understanding turbine oil demulsibility. Turbomachinery International. https://www.turbomachinerymag.com/view/understanding-turbine-oil-demulsibility
  14. Van Rensselar, J. (2017, December). Grease chemistry: Thickener structure. Tribology & Lubrication Technology. Summary of an STLE webinar by P. Shiller. https://www.stle.org/files/TLTArchives/2017/12_December/Webinars.aspx
  15. Winslow, R., Naman, T., & Jenneman, G. (2005, March). Effects of bacterial contamination on steam turbine oil systems. Tribology & Lubrication Technology, 26–35. https://www.stle.org/images/pdf/STLE_ORG/BOK/LS/Turbine%20Oils/Effects%20of%20Bacterial%20Contamination%20on%20Steam%20Turbine%20Oil%20Systems_tlt%20article_March05.pdf

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.