KALTECKOREA

BlogApplication notes

Why does insulation resistance not recover after a water-displacing spray?

Type
Application notes
Published
23 November 2026
Prepared by
Jonghwan Moon
Product group
Maintenance Aids

Spraying again and re-testing is the usual response when insulation resistance stays low, but pushing surface water away is not the same as returning the insulation to a dry, clean state. What actually holds the reading down can be water left in gaps and windings, a conductive film of dissolved salt and dirt, a residual film that holds dust, spraying too little and testing too soon, or insulation that had already aged, and sometimes two or more at once.

Background

The day after heavy rain, someone opens the terminal box of a motor that took a soaking and sprays it with a water-displacing spray. The visible water is gone, but the insulation resistance tester still reads low, and a second spray barely moves it. The plant needs the equipment back, yet nobody can say whether it is safe to switch on at this reading.

There are two kinds of loss. The line stands while the reading is awaited, and switching on in a hurry can lose the equipment to an earth fault or insulation breakdown and injure someone. Electrical equipment that has been in water can be extremely hazardous if re-energised without proper evaluation, and the residue left by seawater and salt spray is especially damaging because it is corrosive and conductive (NEMA, 2019).

Insulation resistance is found by applying a DC voltage across the insulation and measuring the current that flows. That current has a part that passes through the body of the insulation and a part that runs along leakage paths over its surface, and moisture changes the value surprisingly much. Insulation resistance falls as temperature rises, so readings can only be compared if they are taken at the same temperature or corrected to a 40°C base (USBR, 1991). The test procedure and interpretation for rotating machines are set out in a recommended practice (IEEE, 2013).

In such cases the technical team sets up the five hypotheses below and rules them out one by one. The start is always the same: correct the present reading to 40°C, compare it with the equipment's past test records, and check the spray's technical data sheet, the TDS, for what it is meant for and the conditions for use on electrical equipment.

Hypothesis 1: water left in gaps

After a flood, a wash-down or a roof leak, when a lot of water has got in, suspect the inside before the surface. Where the winding sits in the slots, between coil and core, inside the bundled end windings, and at the bottom of the terminal box and the cable entry, water collects easily and spray hardly reaches. Picture the day a motor is lifted out of a drainage pump pit that flooded and then drained. The outside is wiped, the end windings and terminal box are sprayed evenly, and the resistance is measured straight away; it stays low, and when the motor is tilted a little water runs out of a gap underneath.

Water-displacing sprays descend from surface-chemical methods for pushing water off surfaces, developed to salvage flooded equipment (Baker et al., 1961). Such compounds are specified to leave an ultra-thin film on metal, displace water and prevent corrosion (DoD, 2005). Displacement happens only on surfaces the liquid actually reaches and wets, so water pooled deep in a narrow gap, or water the insulation has absorbed, stays where it is. The organic insulation of generator and transformer windings readily takes up moisture from the surrounding air and oil, and moisture in a winding lowers insulation resistance surprisingly far. One record shows a large generator whose winding was more thoroughly dried after a 168-hour dry-out run than early in service (USBR, 1991).

Water that remains shows up in the curve of resistance against time. Apply the DC voltage for ten minutes, note the one-minute and ten-minute values, and divide the ten-minute value by the one-minute value to get the polarisation index. The drier the insulation, the larger this ratio, and the difference between moist and dry insulation is clearer at high temperature, so a test taken hot, soon after running, is more sensitive (USBR, 1991). At the same time, look for water marks at the bottom of the terminal box, at the drain holes low on the frame and at the slot ends.

If water remains inside, the answer is drying, not more spray. Open the drain holes to let pooled water out, then dry with methods that spread heat evenly, such as hot air, heat lamps or a makeshift drying enclosure under covers. One manufacturer's instructions say no point should exceed 125°C, local hot spots must be avoided, and lower temperatures need longer drying (General Electric, n.d.). Measure several times under the same conditions while drying and watch for the 40°C-corrected value and the polarisation index to rise and then level off, and have flooded motors evaluated with the manufacturer by qualified people (NEMA, 2019).

Hypothesis 2: salt and dirt left

If the water was not clean, the problem stays after the water has gone. Sea breeze and spray at a coastal plant, floodwater mixed with sewage and oil, drift from a cooling tower, and a wash-down with process water are such cases. A coastal pump station after a typhoon is one such place. The wet motor was sprayed and left to dry for a day, and on a clear afternoon the resistance came up a fair way, but measured again the next humid morning it has dropped back.

Water can be dried or pushed away, but the salt dissolved in it stays on the surface, because displacing water and dissolving salt away are different jobs. Chemicals, sewage and oil carried in floodwater harm the equipment's performance, and seawater residue is both corrosive and conductive (NEMA, 2019). Once the humidity of the air rises above the level in equilibrium with the salt's saturated solution, the salt draws in moisture and becomes a thin water film; for sodium chloride that is about 75% relative humidity at room temperature (Greenspan, 1977). In tests on circuit boards contaminated with sodium chloride, leakage current rose considerably once contamination passed a certain level and surface humidity approached the salt's critical humidity (Verdingovas et al., 2014). A reading that rises and falls with the weather can come from such a conductive film that forms and vanishes with humidity.

The clues are the shape of the resistance curve and how it moves with the weather. If the ten-minute curve levels off at a lower than normal value within about three minutes, leakage current is large compared with absorption current, and the winding should be thoroughly cleaned and retested or investigated further (USBR, 1991). Measure the same equipment on a humid day and a dry one, or in the morning and the afternoon of the same day, and see whether the 40°C-corrected value swings widely with humidity. Also look for white powder or stains on terminal blocks and end windings.

If salt and dirt are the cause, a washing step is needed. Dissolve the salt out with water or a cleaner, dry thoroughly and test again. Agree the cleaning method and cleaner with the manufacturer first. An unsuitable cleaner can damage the equipment further, and even switchgear and large equipment can return to service only after careful cleaning, drying and testing (NEMA, 2019). If it keeps happening near the coast or a cooling tower, review the terminal box sealing and the enclosure rating as well.

Hypothesis 3: residue holding dust

Where the spray has been applied to terminal blocks and windings at every routine inspection to keep moisture away, look at the film left behind. Dusty plants such as cement, foundry, timber, coal and textile works, and open motors cooled by drawing in outside air, are the usual places. Consider the day an open motor in a foundry is opened up. For months the terminal block and end windings have been sprayed at every inspection, and now a thin black, sticky grime covers them and comes off greasy on a fingertip.

The soft film that water-displacing compounds leave is meant for indoor protection and short outdoor protection, and is not made to stand in for other corrosion preventives over periods longer than a month (DoD, 2005). An oily surface acts like flypaper, attracting airborne dust and holding it firmly, and neither suction nor compressed air shifts that grime well (General Electric, n.d.). Settled dust does little harm on its own until humidity passes a threshold, above which resistance drops by orders of magnitude, and the more dust has settled, the lower that threshold humidity becomes (Song et al., 2013).

The same happens on machine windings. Dirt and oil on exposed insulation weaken it and can lead to failure (USBR, 1991), and conductive contamination on winding surfaces causes tracking, where current burns a path along the surface (Stone et al., 2014). Over time, a film sprayed on to keep moisture away ends up making a surface that is more vulnerable to it.

Start with the eyes. Look for oily grime on terminal blocks, leads, end windings and around vents, and for scorched lines or branching burn marks on the surface. Next, clean just one terminal block with a dry cloth or a method the manufacturer allows and compare that circuit's resistance before and after; that gives a sense of how far the surface film was pulling the reading down. Find in the inspection records when and how often the spray was applied, and match that with when the resistance began to fall.

If film and dust together look responsible, first stop the habit of routine spraying. Remove the built-up grime by the manufacturer's method, but never pour liquid solvent straight onto the windings, because liquid solvent carries conductive contaminants such as metal dust and carbon deep into hidden areas (General Electric, n.d.). Use the spray only where the TDS allows, and note that even the electrical grade is specified for connector plugs and contact points (DoD, 2005). For motors in dusty places, review the enclosure type and air intake filters as well.

Hypothesis 4: rushed spray and test

This hypothesis arises when a restart is urgent. It applies when the spray went briefly into the terminal box without the covers fully off, when the reading was taken straight after spraying, or when a reading from a cold morning is compared with a record taken hot in service. On a night shift, a conveyor motor stops after rain blew in. Only the terminal box cover comes off, the spray goes in for a few seconds, the tester goes on at once, and at the low reading the motor is sprayed again and measured again.

Displacement happens only where the liquid meets the water, so if too little was sprayed or it went the wrong way, the water stays. Water that is pushed away does not vanish either; it runs down and collects in low gaps, and the remaining moisture leaves only by evaporating. Evaporation takes time and heat, and the lower the temperature, the longer drying takes (General Electric, n.d.). The temperature at the time of testing changes the value too. Insulation resistance falls as temperature rises, so a hot reading taken just after running and a reading on a cold morning cannot be compared as they stand; measure the temperature and correct to a 40°C base, using the average of the winding's embedded temperature detectors or of several thermometers placed around it (USBR, 1991).

Check the records first: where and how much was sprayed, how many minutes after spraying the reading was taken, and the winding temperature at the time. If none of that was noted, measure from now on at set intervals with the same voltage, duration and connections, and see whether the corrected value is still rising or has already stopped. Still rising means time was short; stuck at a low value means moving on to the other hypotheses.

When time turns out to have been short, put the order right. Open the covers and drain holes and spray so the liquid reaches where water has pooled, keep to the waiting time the TDS gives, and then dry with heat. Judge not on a single reading but when readings taken one after another under the same conditions have settled, because insulation resistance can vary widely even on identical equipment under identical conditions, which makes change more telling than absolute value (USBR, 1991). The threshold for restarting follows the recommended practice and the manufacturer's criteria (IEEE, 2013).

Hypothesis 5: already aged insulation

With long-serving equipment, the water may only have been the trigger, with the cause already there. Motors that ran hot for years, that went through overloads and frequent starts, or that were rewound in the past, and equipment that always sits somewhere hot such as a boiler house or beside a drying oven, are the cases. Take an old fan motor in a boiler house. After a pipe leaked on it, it was sprayed and dried, but the reading will not come up. Leafing through past inspection records shows that insulation resistance had been creeping down year by year before the leak.

The thermal ageing of organic insulation comes from chemical reactions within the material, and those reactions speed up as temperature rises (Dakin, 1948). Over time the binder in some insulation changes and the measured resistance can drop, but the more noticeable effect of age on leakage current is the development of cracks and contamination (USBR, 1991). Cracked insulation gives water a way in, and moisture and dirt that enter there stay where no sprayed film can reach. So aged insulation tends to lose more resistance than new insulation from the same wetting and to recover less of it. Whether flooded equipment can be reconditioned also depends on its age, how deeply it was flooded and how long it was under water (NEMA, 2019).

The judgement rests on the records. Lay out the same equipment's insulation resistance and polarisation index, corrected to 40°C, year by year, and see whether they were falling before the wetting. If the winding is visible, look for cracked or crumbling varnish and darkened colour. Because the insulation resistance test alone cannot catch every weakened insulation, more than one method, such as a high-voltage DC test or a power factor test, is recommended (USBR, 1991). The minimum polarisation index recommended for rotating machines is also a reference (IEEE, 2013).

If the insulation is judged to have aged, the remedy goes beyond spraying and drying on site. One manufacturer's instructions state that if the 40°C-corrected resistance does not reach a satisfactory value after proper drying and cleaning, thorough cleaning or complete reconditioning is needed (General Electric, n.d.). Send the motor to a repair shop to decide between re-varnishing, rewinding and replacement, and choose the enclosure and insulation class of the next motor in that position with both heat and moisture in mind.

Finding the cause

The five hypotheses need not be investigated all at once. Begin with what records and a repeat measurement can clear. Where and how much was sprayed, and when and at what temperature the reading was taken, are confirmed from the records and a few retests, and past inspection records only need opening. Checks that need dismantling and cleaning come after.

The first clue is how the value moves over time. If the corrected value keeps rising across measurements taken hours apart under the same conditions, waiting and heat were short, and draining pooled water and drying will do. If it rises and falls with the weather or the time of day, look at conductive films that come and go with humidity: leftover salt and an oily film loaded with dust. If the value had been creeping down year by year, suspect aged insulation first.

Next is the shape of the curve. A ten-minute curve that flattens early at a low value means large surface leakage, so look at what sits on the surface: salt, dust and oily film. A curve that climbs slowly with a low polarisation index points to moisture inside the insulation. To the eye, white powder leans towards salt, black sticky grime towards residual film and dust, and cracked varnish towards ageing.

If that still does not settle it, run control trials that change one thing at a time. Clean just one terminal block and read that circuit, dry thoroughly with heat and measure again, then wash and dry by a method the manufacturer allows and measure once more. Change only one thing each time, and log the temperature and correct to 40°C every time, or there is no telling which step moved the reading. The final check is that readings and polarisation index taken one after another under the same conditions pass the criteria and hold steady.

The hypotheses easily overlap. A winding carrying salt draws moisture back and soon loses its reading again after drying, and dust stuck in an oily film holds moisture too. Aged, cracked insulation leaves a way open for water and dirt. In such cases, finish washing the surface and drying the inside first, and treat whatever low reading remains as ageing, because until the winding is washed and dried the share due to ageing cannot be told apart.

Limits and cautions

The pass criteria for insulation resistance and polarisation index, the test voltage and the drying temperature differ by equipment type, rated voltage and insulation class, so numbers follow the recommended practice and the equipment manufacturer's criteria, and the spray's intended use and waiting time follow the product's TDS. For equipment containing electronics, such as drives, control panels and signalling and protection devices, replacing components or returning them to the manufacturer for cleaning, recalibration and testing is recommended over drying them on site (NEMA, 2019).

Safety matters too. Insulation resistance testing uses high DC voltage, so qualified people should do it, and the winding should be earthed afterwards to drain the remaining charge. Inspect and clean only after isolating the supply and applying locks and tags (OSHA, n.d.). Sprays are usually flammable, so ventilate according to the product's safety data sheet, the SDS, never spray onto live equipment, hot surfaces or near sparks, and apply heat only after the solvent has fully evaporated.

Sources

  1. Baker, H. R., Leach, P. B., Singleterry, C. R., & Zisman, W. A. (1961). Surface chemical methods of displacing water and/or oils and salvaging flooded equipment. Part 1: Practical applications (NRL Report 5606). Naval Research Laboratory.
  2. Dakin, T. W. (1948). Electrical insulation deterioration treated as a chemical rate phenomenon. Transactions of the American Institute of Electrical Engineers, 67(1), 113–122. https://doi.org/10.1109/T-AIEE.1948.5059649
  3. General Electric. (n.d.). Direct current motors and generators: Instructions (GEH-5304A). Retrieved November 2026. https://www.manualslib.com/manual/58390/Ge-Geh-5304a.html
  4. Greenspan, L. (1977). Humidity fixed points of binary saturated aqueous solutions. Journal of Research of the National Bureau of Standards, Section A: Physics and Chemistry, 81A(1), 89–96. https://doi.org/10.6028/jres.081A.011
  5. Institute of Electrical and Electronics Engineers [IEEE]. (2013). IEEE Std 43-2013, IEEE recommended practice for testing insulation resistance of electrical machinery. https://doi.org/10.1109/IEEESTD.2014.6754111
  6. National Electrical Manufacturers Association [NEMA]. (2019). Evaluating water-damaged electrical equipment (NEMA GD 1-2019). https://www.nema.org/docs/default-source/standards-document-library/nema-gd-1-2019-evaluating-water-damaged-electrical-equipment-guide.pdf
  7. Occupational Safety and Health Administration [OSHA]. (n.d.). Control of hazardous energy (lockout/tagout). U.S. Department of Labor. Retrieved November 2026. https://www.osha.gov/control-hazardous-energy
  8. Song, B., Azarian, M. H., & Pecht, M. G. (2013). Effect of temperature and relative humidity on the impedance degradation of dust-contaminated electronics. Journal of The Electrochemical Society, 160(3), C97–C105. https://doi.org/10.1149/2.024303jes
  9. Stone, G. C., Culbert, I., Boulter, E. A., & Dhirani, H. (2014). Electrical insulation for rotating machines: Design, evaluation, aging, testing, and repair (2nd ed.). Wiley-IEEE Press.
  10. U.S. Bureau of Reclamation [USBR]. (1991). Testing solid insulation of electrical equipment (Facilities Instructions, Standards, and Techniques, Vol. 3-1). https://www.usbr.gov/power/data/fist/fist3_1/vol3-1.pdf
  11. U.S. Department of Defense [DoD]. (2005). MIL-PRF-81309F, Corrosion preventive compounds, water displacing, ultra-thin film. https://everyspec.com/MIL-PRF/MIL-PRF-080000-99999/MIL-PRF-81309F_18419/
  12. Verdingovas, V., Jellesen, M. S., & Ambat, R. (2014). Impact of NaCl contamination and climatic conditions on the reliability of printed circuit board assemblies. IEEE Transactions on Device and Materials Reliability, 14(1), 42–51. https://doi.org/10.1109/TDMR.2013.2293792

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Site setup

    We confirm process conditions and needs first.

  2. 02
    Spec design

    We set the product spec and selection criteria.

  3. 03
    Comparison

    We compare matching candidates and propose.

  4. 04
    Tailored supply

    We supply on time and manage the stock.

  5. 05
    Site check

    We visit, check conditions of use and record.

  6. 06
    Use management

    We track use and change cycles to catch issues.

  7. 07
    Regular analysis

    We analyze the records and send a yearly report.