KALTEC

Customer storiesPrecision machinist of aerospace aluminum parts

AerospaceCorrosion Prevention

Packaging alone ended oiling and pre-assembly cleaning at an aerospace aluminum machinist

Customer
Precision machinist of aerospace aluminum parts
Industry
Aerospace
Product group
Corrosion Prevention
Process · Material
Storage between machining and delivery to assembly · Aerospace aluminum alloys (2xxx and 7xxx series)

A precision machinist that supplies aluminum aircraft parts to an aircraft manufacturer's assembly line switched rust protection during the wait before assembly to VCI packaging. Nothing is applied to the part; the package itself holds a protective atmosphere, so surface quality holds through humid summers with frequent condensation, and degreasing and cleaning before assembly are no longer needed.

The customer precision-machines aluminum parts for aircraft and supplies them to an aircraft manufacturer's assembly line. Finished parts wait in storage for a period before they are called into assembly, and their surface quality during that wait becomes assembly quality. Aircraft assembly is sensitive to the precision of mating faces and fastener locations, so the surface condition of delivered parts is a basic condition the company has to meet.

The parts are made from high-strength aerospace aluminum alloys. These alloys machine well and are strong, but in humid conditions their surfaces oxidize locally with ease, which makes storage management part of quality. The customer's standard was to hold surface quality through storage with no rust-preventive oil on the part, and to send parts straight into assembly without cleaning or degreasing.

Even when condensation formed, machined and mating faces could not be contaminated or oxidized, and complex shapes had to be protected evenly all over. The protection itself could have no effect on assembly quality. Because the wait could stretch, the approach needed to be packaging-based, with performance that holds over time.

The challenge: keeping aluminum sound through summer condensation with no oil and no washing

In summer, rising temperature and humidity in the shop brought frequent condensation on aluminum surfaces and repeated concern about local oxidation and corrosion. The existing answer was rust-preventive oil, which added two steps before assembly, degreasing and cleaning. Those steps lengthened lead time, and there was concern that the cleaning step could affect assembly accuracy. On complex shapes the oil went on unevenly, and the parts sat in standard packaging with an oil film on their surfaces.

"If we put oil on, the people doing assembly have to wipe it all off. What our customer wanted wasn't parts without corrosion. It was parts they could use right away."Shipping quality lead, customer

The customer asked for a way to keep surfaces sound in storage without oil and without adding steps before assembly. What it needed was not a faster way to remove an oil film but a method that left nothing on the surface in the first place. So before comparing protection performance, the customer and our team set out to define the condition in which the assembly line should receive the parts.

The solution: protecting through the air in the package instead of a coating on the part

In the first one to two weeks, the customer and our team reviewed storage temperature and humidity, when condensation occurred, part shapes and sizes, and the packaging in use. Condensation was worst in the rainy season and on midsummer mornings. Staining appeared first on the touching faces of stacked plate-type parts and in machined pockets.

Aluminum grows a natural oxide film a few nanometers thick that serves it well in air. When water and chloride are present together, though, that film breaks down locally, pitting starts there, and white aluminum hydroxide spots or stains are left behind. In high-strength alloys containing copper, copper-rich particles in the microstructure act as local cathodes and make this easier. Machined faces, with freshly exposed metal, are especially sensitive.

The problem in a summer warehouse is not rain but dew point. Air at 30°C and 80% relative humidity has a dew point of about 26°C, so a part coming out of an air-conditioned machining area, or one that cooled overnight, gathers water immediately if its surface is colder than that. Water trapped between stacked parts dries slowly and leaves stains. That is why the touching faces and the pockets were the first places to show it.

The criterion, then, was not "how strongly does it protect" but "what condition does the assembly line receive". In week three we compared the options by working principle, not by brand. A rust-preventive oil film protects reliably but brings cleaning with it, a water-based dry film is oil-free but still leaves something on the surface, and VCI packaging applies nothing to the part and protects through the air inside the package. Weighing suitability for aluminum, package size and sealing method, protection period, and the film's composition and recyclability as well, the customer chose VCI packaging film.

The inhibitor in the film slowly vaporizes, fills the closed package and adsorbs on the metal as a protective layer of molecular thickness. If condensation forms, inhibitor dissolves into that water too and lowers its corrosivity. Because nothing was applied to the surface, the inhibitor disperses into the air once the package is opened and leaves nothing to clean off, but the protective concentration holds only while the package stays closed. The film protects aluminum, carbon steel, stainless, copper, brass and cast iron, offers protection for up to 5 years, and is non-toxic and recyclable.

Adoption: from a split summer lot to the packaging standard

Machining, inspection and the flow into assembly stayed as they were, and only the storage packaging was to change. From week four to week eleven, one lot was split in summer between the old method and VCI packaging, and machined and mating faces were inspected and compared at intervals. Because both halves came from the same lot, material and machining conditions were the same on each side.

The changeover came from month three, with the sealing and opening procedure written into the packaging standard. Parts go into the VCI packaging film as soon as machining and inspection are done, with dry surfaces, and air is pressed out lightly before the package is closed by heat seal or tape. An opened package is closed again for storage and is opened for good just before the parts go into assembly. The working principle, that protection depends on a closed package, is built directly into that procedure.

The results: parts that go into assembly unwashed, even in summer

Follow-up confirmed first that corrosion was suppressed through summer storage. When condensation formed briefly in hot, humid storage, the protective atmosphere inside the package stopped oxidation, and part quality held steady throughout storage. However complex the part, every surface inside the package is protected under the same conditions, so the uneven coverage that came with oil is gone. Protection moved from applied rust-preventive oil to vapor-phase protection inside the package, and nothing is left on the surface.

With degreasing and cleaning dropped, the extra steps before assembly went from 2 to 0. Parts are unpacked and used, the flow continues uninterrupted, and lead time is shorter. The saving is roughly the half day per shipment once spent washing and drying. The non-toxic, recyclable film also lightens the load on shop safety and the environment.

For the customer's own customer, the aircraft manufacturer, the biggest change is the condition of what arrives. Parts can go into assembly as soon as they are unpacked. The variable that cleaning used to introduce into assembly accuracy is gone as well.

"In the rainy season I used to dread walking into the warehouse. Now I just check the packages are properly closed. The best part is that nobody on the assembly side talks about cleaning anymore."Production control lead, customer

What's next: package sizes by part and a rule for resealing

The customer and our team are working out package sizes by part dimension to cut film use. They are also setting a rule for resealing packages from which the assembly line has taken only some parts. A further question is whether the same packaging can serve shipments to overseas assembly plants.

Product and site consultation

Leave your company, site and the product groups in use. Our engineer will get in touch to go through your site conditions and concerns. Materials, equipment, operating conditions and downstream steps show what should change and what can stay. If nothing needs to change, we will say so.

Contact us
After you contact us
  1. 01
    Register

    You fill in your company, site and the product groups in use.

  2. 02
    Call back

    Our engineer calls to go through site conditions and concerns.

  3. 03
    Site database

    Materials, equipment, operating conditions, products in use and past problems are recorded per site.

  4. 04
    Proposal and quotation

    You get a proposal and trial plan that compare brands by composition and working principle.

  5. 05
    Purchase, delivery, application

    The confirmed product reaches your site when needed, and we check the initial condition together.

  6. 06
    Usage management

    Consumption and change intervals are checked and adjusted, and the results go into the site database.